Thu Mar 11 20:36:06 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.725764	-0.168770	0.000000	-0.000078	0.722129

0.680434	-0.189846	0.005005	-0.000070	0.722071
0.759249	-0.202630	0.010010	-0.000085	0.722074
0.678941	-0.188907	0.015014	-0.000070	0.722073
0.651751	-0.187782	0.020019	-0.000065	0.722066
0.660928	-0.184908	0.025024	-0.000067	0.722075
0.616343	-0.181083	0.030029	-0.000058	0.722067
0.585152	-0.170544	0.035034	-0.000053	0.722077
0.463094	-0.148791	0.040038	-0.000030	0.722077
0.316592	-0.125468	0.045043	-0.000003	0.722072
0.554334	-0.165080	0.050048	-0.000047	0.722077
0.537777	-0.166405	0.055053	-0.000044	0.722069
0.444341	-0.146530	0.060058	-0.000027	0.722075
0.417743	-0.184408	0.065062	-0.000022	0.721992
0.540571	-0.334722	0.070067	-0.000045	0.721739
0.629742	-0.347048	0.075072	-0.000061	0.721747
0.531561	-0.334590	0.080077	-0.000043	0.721737
0.537634	-0.330689	0.085082	-0.000044	0.721747
0.525180	-0.329326	0.090086	-0.000042	0.721745
0.438691	-0.318077	0.095091	-0.000026	0.721737
0.568331	-0.445342	0.100096	-0.000050	0.721532
0.578267	-0.498188	0.105101	-0.000052	0.721432
0.399657	-0.463387	0.110106	-0.000019	0.721438
0.489443	-0.480072	0.115110	-0.000036	0.721437
0.350433	-0.457483	0.120115	-0.000010	0.721433
0.544391	-0.587862	0.125120	-0.000046	0.721244
0.322341	-0.611798	0.130125	-0.000005	0.721120
0.496193	-0.642262	0.135130	-0.000037	0.721121
0.553935	-0.650542	0.140134	-0.000048	0.721125
0.393165	-0.673080	0.145139	-0.000018	0.721024
0.532565	-0.768859	0.150144	-0.000044	0.720885
0.730178	-0.808156	0.155149	-0.000081	0.720877
0.624104	-0.788019	0.160154	-0.000061	0.720879
0.663200	-0.917359	0.165158	-0.000068	0.720639
0.436354	-0.928769	0.170163	-0.000026	0.720537
0.478671	-0.931211	0.175168	-0.000034	0.720547
0.341987	-0.968660	0.180173	-0.000009	0.720426
0.344959	-1.070802	0.185178	-0.000009	0.720226
0.511960	-1.100405	0.190182	-0.000040	0.720226
0.201554	-1.076891	0.195187	0.000017	0.720164
0.355900	-1.236180	0.200192	-0.000011	0.719904
0.175413	-1.208535	0.205197	0.000022	0.719895
0.307869	-1.259676	0.210202	-0.000003	0.719841
0.123191	-1.346413	0.215206	0.000032	0.719605
0.190973	-1.361040	0.220211	0.000019	0.719601
0.348444	-1.446636	0.225216	-0.000010	0.719487
0.089892	-1.514101	0.230221	0.000038	0.719264
0.115496	-1.513260	0.235226	0.000033	0.719274
0.166957	-1.629018	0.240230	0.000023	0.719064
0.063304	-1.665376	0.245235	0.000043	0.718956
0.334569	-1.732700	0.250240	-0.000008	0.718919
0.130022	-1.837018	0.255245	0.000030	0.718641
0.060520	-1.821299	0.260250	0.000043	0.718648
-0.004419	-1.915166	0.265254	0.000055	0.718440
0.065595	-1.971616	0.270259	0.000042	0.718353
0.074928	-2.034801	0.275264	0.000040	0.718232
-0.123533	-2.109408	0.280269	0.000077	0.718015
0.004677	-2.148148	0.285274	0.000053	0.717983
0.076218	-2.301020	0.290278	0.000040	0.717707
-0.136419	-2.267512	0.295283	0.000080	0.717698
-0.062486	-2.427387	0.300288	0.000066	0.717408
-0.117492	-2.433599	0.305293	0.000076	0.717377
-0.306825	-2.519997	0.310298	0.000111	0.717139
-0.510577	-2.509928	0.315302	0.000149	0.717088
-2.407949	-2.283865	0.320307	0.000502	0.716866
-3.602621	-2.123737	0.325312	0.000725	0.716762
-3.458819	-2.154185	0.330317	0.000698	0.716753
-3.225261	-2.253699	0.335322	0.000654	0.716638
-4.686185	-2.089368	0.340326	0.000926	0.716448
-4.545317	-2.117006	0.345331	0.000900	0.716444
-4.162453	-2.180694	0.350336	0.000829	0.716453
-4.678732	-2.177946	0.355341	0.000925	0.716276
-5.631237	-2.083242	0.360346	0.001102	0.716128
-5.096425	-2.176129	0.365350	0.001002	0.716133
-5.459735	-2.114467	0.370355	0.001070	0.716127
-5.465509	-2.144664	0.375360	0.001071	0.716065
-6.197762	-2.108745	0.380365	0.001207	0.715878
-6.010882	-2.139615	0.385370	0.001172	0.715883
-6.090570	-2.123275	0.390374	0.001187	0.715887
-6.174544	-2.111331	0.395379	0.001203	0.715881
-6.138448	-2.238522	0.400384	0.001196	0.715642
-7.616978	-2.025431	0.405389	0.001471	0.715542
-7.421355	-2.059475	0.410394	0.001435	0.715544
-6.786212	-2.171501	0.415398	0.001316	0.715546
-7.299989	-2.081847	0.420403	0.001412	0.715543
-7.342340	-2.165959	0.425408	0.001420	0.715361
-8.272989	-2.066577	0.430413	0.001593	0.715230
-7.966653	-2.118457	0.435418	0.001536	0.715235
-8.062619	-2.102524	0.440422	0.001554	0.715233
-8.338870	-2.055536	0.445427	0.001605	0.715229
-7.866915	-2.135070	0.450432	0.001517	0.715238
-8.609981	-2.157247	0.455437	0.001655	0.714931
-9.367987	-2.034225	0.460442	0.001796	0.714907
-8.961041	-2.105289	0.465446	0.001721	0.714910
-8.849464	-2.129515	0.470451	0.001700	0.714902
-9.089410	-2.082581	0.475456	0.001744	0.714910
-9.103829	-2.082355	0.480461	0.001747	0.714906
-9.120245	-2.196008	0.485466	0.001750	0.714675
-9.917458	-2.087814	0.490470	0.001898	0.714608
-9.860634	-2.100554	0.495475	0.001888	0.714602
-9.589610	-2.145400	0.500480	0.001837	0.714609
-10.074053	-2.061750	0.505485	0.001927	0.714604
-10.373756	-2.006924	0.510490	0.001983	0.714607
-9.617381	-2.206597	0.515494	0.001842	0.714478
-10.936587	-2.073891	0.520499	0.002088	0.714275
-10.579492	-2.132778	0.525504	0.002021	0.714285
-10.978170	-2.065622	0.530509	0.002095	0.714277
-10.926952	-2.074612	0.535514	0.002086	0.714278
-10.629425	-2.125322	0.540518	0.002030	0.714282
-11.000544	-2.063980	0.545523	0.002099	0.714273
-10.856862	-2.219168	0.550528	0.002073	0.714016
-11.740709	-2.086663	0.555533	0.002237	0.713966
-12.111937	-2.018503	0.560538	0.002306	0.713970
-11.377151	-2.148611	0.565542	0.002169	0.713972
-11.665804	-2.101487	0.570547	0.002223	0.713964
-11.882000	-2.058710	0.575552	0.002263	0.713972
-11.723251	-2.105160	0.580557	0.002233	0.713936
-12.254178	-2.154657	0.585562	0.002332	0.713650
-12.281759	-2.148391	0.590566	0.002337	0.713653
-12.945249	-2.033655	0.595571	0.002461	0.713646
-12.394553	-2.127789	0.600576	0.002358	0.713654
-12.395840	-2.132017	0.605581	0.002358	0.713645
-12.962390	-2.031098	0.610586	0.002464	0.713645
-12.348194	-2.181218	0.615590	0.002349	0.713565
-13.379491	-2.104208	0.620595	0.002541	0.713352
-13.325241	-2.109108	0.625600	0.002531	0.713362
-13.647909	-2.055446	0.630605	0.002591	0.713354
-13.466431	-2.088391	0.635610	0.002557	0.713353
-13.290487	-2.116896	0.640614	0.002524	0.713359
-13.623066	-2.062685	0.645619	0.002586	0.713349
-13.299771	-2.185363	0.650624	0.002526	0.713220
-14.341945	-2.100159	0.655629	0.002720	0.713020
-14.316475	-2.105935	0.660634	0.002715	0.713018
-14.144455	-2.134175	0.665638	0.002683	0.713023
-14.310289	-2.108806	0.670643	0.002714	0.713015
-14.387950	-2.090010	0.675648	0.002728	0.713024
-14.589793	-2.058265	0.680653	0.002766	0.713016
-14.535686	-2.136597	0.685658	0.002756	0.712880
-15.173752	-2.108327	0.690662	0.002875	0.712710
-15.381544	-2.075284	0.695667	0.002913	0.712702
-15.398874	-2.067474	0.700672	0.002916	0.712711
-15.250787	-2.097136	0.705677	0.002889	0.712705
-15.372313	-2.074720	0.710682	0.002911	0.712707
-15.183969	-2.105517	0.715686	0.002876	0.712712
-15.253349	-2.131085	0.720691	0.002889	0.712637
-16.095193	-2.105621	0.725696	0.003046	0.712389
-15.979138	-2.129378	0.730701	0.003024	0.712383
-16.254301	-2.078607	0.735706	0.003075	0.712387
-15.896178	-2.139619	0.740710	0.003008	0.712392
-16.438234	-2.047562	0.745715	0.003109	0.712383
-16.368676	-2.056804	0.750720	0.003096	0.712390
-16.265817	-2.081228	0.755725	0.003077	0.712378
-16.997106	-2.096093	0.760730	0.003213	0.712089
-17.177300	-2.062518	0.765734	0.003247	0.712092
-17.171202	-2.068679	0.770739	0.003245	0.712082
-16.989565	-2.096327	0.775744	0.003212	0.712091
-17.221186	-2.059033	0.780749	0.003255	0.712083
-17.260508	-2.050677	0.785754	0.003262	0.712086
-16.997518	-2.096620	0.790758	0.003213	0.712088
-17.464950	-2.120028	0.795763	0.003300	0.711876
-18.274791	-2.030363	0.800768	0.003450	0.711767
-17.713144	-2.133048	0.805773	0.003346	0.711762
-18.096756	-2.067181	0.810778	0.003417	0.711757
-18.307462	-2.026642	0.815782	0.003456	0.711763
-18.062986	-2.075747	0.820787	0.003411	0.711752
-17.825834	-2.112077	0.825792	0.003367	0.711764
-18.068088	-2.123618	0.830797	0.003412	0.711655
-19.056137	-2.049489	0.835802	0.003596	0.711452
-18.537996	-2.139063	0.840806	0.003499	0.711458
-19.103058	-2.043285	0.845811	0.003604	0.711448
-19.118436	-2.036223	0.850816	0.003607	0.711457
-18.842306	-2.088150	0.855821	0.003555	0.711451
-19.258919	-2.013581	0.860826	0.003633	0.711452
-18.895324	-2.083872	0.865830	0.003565	0.711441
-19.332031	-2.158885	0.870835	0.003647	0.711136
-19.717956	-2.087358	0.875840	0.003718	0.711142
-20.028385	-2.033940	0.880845	0.003776	0.711138
-19.761313	-2.083079	0.885850	0.003726	0.711135
-19.266098	-2.168961	0.890854	0.003634	0.711140
-19.777556	-2.080306	0.895859	0.003729	0.711135
-19.713291	-2.135193	0.900864	0.003717	0.711049
-20.451461	-2.093844	0.905869	0.003854	0.710869
-20.532552	-2.079063	0.910874	0.003869	0.710870
-20.345360	-2.110918	0.915878	0.003835	0.710873
-20.314451	-2.120436	0.920883	0.003829	0.710865
-19.984672	-2.175394	0.925888	0.003767	0.710873
-20.533379	-2.081584	0.930893	0.003869	0.710865
-21.038359	-2.141874	0.935898	0.003963	0.710565
-21.330593	-2.106349	0.940902	0.004018	0.710532
-21.903644	-2.009056	0.945907	0.004124	0.710523
-21.482388	-2.079615	0.950912	0.004046	0.710532
-21.382123	-2.099029	0.955917	0.004027	0.710529
-21.545058	-2.070211	0.960922	0.004057	0.710528
-21.624893	-2.053387	0.965926	0.004072	0.710534
-21.820801	-2.102583	0.970931	0.004109	0.710366
-22.670067	-2.025050	0.975936	0.004267	0.710218
-22.215155	-2.109150	0.980941	0.004182	0.710213
-22.663799	-2.028867	0.985946	0.004265	0.710213
-22.256041	-2.099759	0.990950	0.004189	0.710217
-22.373622	-2.084256	0.995955	0.004211	0.710206
-22.638219	-2.031461	1.000960	0.004260	0.710218
-22.595860	-2.069145	1.005965	0.004252	0.710157
-23.337863	-2.071534	1.010970	0.004391	0.709889
-23.453538	-2.047662	1.015974	0.004412	0.709895
-23.714458	-2.005986	1.020979	0.004461	0.709886
-23.058485	-2.119554	1.025984	0.004338	0.709892
-23.486327	-2.044968	1.030989	0.004418	0.709889
-23.613768	-2.021537	1.035994	0.004442	0.709891
-23.098741	-2.111899	1.040998	0.004346	0.709894
-23.523703	-2.151066	1.046003	0.004425	0.709664
-24.534695	-2.005177	1.051008	0.004613	0.709596
-24.071494	-2.089271	1.056013	0.004527	0.709593
-24.097077	-2.086998	1.061018	0.004531	0.709588
-24.455330	-2.018802	1.066022	0.004598	0.709597
-24.330239	-2.047790	1.071027	0.004575	0.709584
-23.859579	-2.125839	1.076032	0.004487	0.709596
-24.326962	-2.171944	1.081037	0.004574	0.709337
-25.433361	-2.012191	1.086042	0.004780	0.709262
-25.065921	-2.075709	1.091046	0.004711	0.709266
-25.100954	-2.073817	1.096051	0.004718	0.709258
-25.640552	-1.974746	1.101056	0.004818	0.709263
-25.331800	-2.032017	1.106061	0.004761	0.709259
-25.330890	-2.033294	1.111066	0.004760	0.709257
-25.396185	-2.054675	1.116070	0.004772	0.709191
-26.142842	-2.042661	1.121075	0.004911	0.708949
-25.915556	-2.080345	1.126080	0.004869	0.708955
-26.375043	-1.999917	1.131085	0.004955	0.708952
-26.436441	-1.988685	1.136090	0.004966	0.708953
-25.855700	-2.089051	1.141094	0.004858	0.708959
-26.176128	-2.036254	1.146099	0.004917	0.708950
-26.028014	-2.059827	1.151104	0.004890	0.708956
-26.118403	-2.178687	1.156109	0.004907	0.708686
-27.017096	-2.044958	1.161114	0.005074	0.708633
-27.077980	-2.031596	1.166118	0.005085	0.708638
-27.101089	-2.032487	1.171123	0.005089	0.708628
-27.035892	-2.039453	1.176128	0.005077	0.708638
-26.916842	-2.061667	1.181133	0.005055	0.708636
-26.983167	-2.050882	1.186138	0.005067	0.708634
-27.164714	-2.132238	1.191142	0.005101	0.708406
-27.791511	-2.052408	1.196147	0.005217	0.708343
-28.081034	-1.996388	1.201152	0.005271	0.708352
-27.765155	-2.055475	1.206157	0.005212	0.708346
-27.797933	-2.050317	1.211162	0.005218	0.708345
-27.668876	-2.068901	1.216166	0.005194	0.708354
-27.937787	-2.024968	1.221171	0.005244	0.708346
-28.199844	-2.123970	1.226176	0.005293	0.708054
-28.565105	-2.080342	1.231181	0.005361	0.708011
-28.821662	-2.035103	1.236186	0.005409	0.708010
-28.310478	-2.122422	1.241190	0.005314	0.708018
-28.600559	-2.076853	1.246195	0.005367	0.708006
-28.751310	-2.045957	1.251200	0.005395	0.708014
-28.606737	-2.088683	1.256205	0.005369	0.707980
-29.111660	-2.140776	1.261210	0.005463	0.707695
-29.529984	-2.063123	1.266214	0.005540	0.707702
-30.156590	-1.956673	1.271219	0.005657	0.707691
-29.657965	-2.040083	1.276224	0.005564	0.707702
-29.539634	-2.062870	1.281229	0.005542	0.707699
-29.667575	-2.041567	1.286234	0.005566	0.707696
-29.516373	-2.065971	1.291238	0.005537	0.707701
-29.825897	-2.157812	1.296243	0.005595	0.707407
-30.402067	-2.070538	1.301248	0.005702	0.707376
-30.523530	-2.050232	1.306253	0.005725	0.707373
-30.121535	-2.124086	1.311258	0.005650	0.707369
-30.296307	-2.089144	1.316262	0.005682	0.707377
-30.588176	-2.040993	1.321267	0.005737	0.707369
-30.375507	-2.093002	1.326272	0.005697	0.707341
-31.151919	-2.085601	1.331277	0.005841	0.707078
-31.497804	-2.026730	1.336282	0.005906	0.707073
-31.623473	-1.999454	1.341286	0.005929	0.707083
-31.422035	-2.040125	1.346291	0.005892	0.707073
-31.172081	-2.081552	1.351296	0.005845	0.707080
-31.569754	-2.012167	1.356301	0.005919	0.707077
-31.421617	-2.039255	1.361306	0.005891	0.707075
-31.214610	-2.200100	1.366310	0.005853	0.706827
-32.606989	-1.993937	1.371315	0.006112	0.706742
-32.329051	-2.040239	1.376320	0.006060	0.706749
-32.071692	-2.087496	1.381325	0.006012	0.706746
-32.646051	-1.986031	1.386330	0.006119	0.706745
-32.255979	-2.050494	1.391334	0.006046	0.706755
-31.755956	-2.146019	1.396339	0.005953	0.706742
-32.369542	-2.160181	1.401344	0.006067	0.706494
-33.293601	-2.023684	1.406349	0.006239	0.706438
-33.162749	-2.048818	1.411354	0.006215	0.706434
-32.528371	-2.157533	1.416358	0.006097	0.706443
-33.239250	-2.034410	1.421363	0.006229	0.706436
-33.139491	-2.048680	1.426368	0.006210	0.706443
-32.910310	-2.091498	1.431373	0.006168	0.706439
-33.793321	-2.093292	1.436378	0.006332	0.706119
-33.884568	-2.072778	1.441382	0.006349	0.706128
-34.126032	-2.033795	1.446387	0.006394	0.706120
-33.812299	-2.087142	1.451392	0.006335	0.706125
-34.009393	-2.053699	1.456397	0.006372	0.706122
-34.295074	-2.004194	1.461402	0.006425	0.706119
-33.767637	-2.095170	1.466406	0.006327	0.706125
-34.525156	-2.077578	1.471411	0.006468	0.705889
-35.274382	-1.960573	1.476416	0.006607	0.705856
-34.879095	-2.028383	1.481421	0.006534	0.705862
-34.824641	-2.040402	1.486426	0.006523	0.705857
-35.025022	-2.001521	1.491430	0.006561	0.705864
-35.009894	-2.009091	1.496435	0.006558	0.705854
-34.685982	-2.063634	1.501440	0.006497	0.705861
-34.907500	-2.118150	1.506445	0.006539	0.705672
-36.113557	-1.980991	1.511450	0.006763	0.705515
-35.342246	-2.112307	1.516454	0.006619	0.705528
-35.841152	-2.028123	1.521459	0.006712	0.705518
-36.185111	-1.964578	1.526464	0.006776	0.705523
-35.573651	-2.074807	1.531469	0.006662	0.705521
-35.852006	-2.029086	1.536474	0.006714	0.705513
-36.114904	-2.041661	1.541478	0.006763	0.705393
-36.841036	-2.005880	1.546483	0.006898	0.705205
-36.367924	-2.086561	1.551488	0.006810	0.705212
-36.839242	-2.003685	1.556493	0.006898	0.705210
-36.674680	-2.035293	1.561498	0.006867	0.705206
-36.050281	-2.142867	1.566502	0.006751	0.705213
-36.821682	-2.010217	1.571507	0.006894	0.705204
-37.065667	-2.040748	1.576512	0.006939	0.705055
-37.754722	-2.001955	1.581517	0.007068	0.704886
-37.347644	-2.078813	1.586522	0.006992	0.704877
-37.453643	-2.054900	1.591526	0.007012	0.704887
-37.988253	-1.963373	1.596531	0.007111	0.704880
-37.583603	-2.033326	1.601536	0.007036	0.704884
-37.600150	-2.030398	1.606541	0.007039	0.704884
-37.664055	-2.031583	1.611546	0.007050	0.704859
-37.893123	-2.123658	1.616550	0.007093	0.704592
-38.266311	-2.062882	1.621555	0.007162	0.704580
-38.688707	-1.984656	1.626560	0.007241	0.704586
-38.169767	-2.076884	1.631565	0.007144	0.704587
-38.397732	-2.039868	1.636570	0.007187	0.704580
-38.779622	-1.965532	1.641574	0.007258	0.704592
-38.809562	-1.971023	1.646579	0.007263	0.704571
-38.953799	-2.100116	1.651584	0.007290	0.704259
-39.266727	-2.044813	1.656589	0.007348	0.704258
-39.808354	-1.950131	1.661594	0.007449	0.704254
-39.182656	-2.057252	1.666598	0.007333	0.704263
-39.332867	-2.034289	1.671603	0.007360	0.704256
-39.528330	-1.997372	1.676608	0.007397	0.704260
-39.261961	-2.045891	1.681613	0.007347	0.704258
-39.788133	-2.093428	1.686618	0.007445	0.703973
-40.194866	-2.031152	1.691622	0.007521	0.703953
-40.454406	-1.988849	1.696627	0.007569	0.703945
-39.898359	-2.085724	1.701632	0.007465	0.703950
-39.876252	-2.090694	1.706637	0.007461	0.703948
-40.420867	-1.994431	1.711642	0.007562	0.703946
-39.938782	-2.093096	1.716646	0.007473	0.703921
-40.606703	-2.119467	1.721651	0.007597	0.703627
-41.029851	-2.040913	1.726656	0.007676	0.703634
-41.125033	-2.024468	1.731661	0.007693	0.703633
-41.059647	-2.039397	1.736666	0.007681	0.703626
-40.987734	-2.047019	1.741670	0.007668	0.703637
-41.319347	-1.992830	1.746675	0.007729	0.703627
-41.128467	-2.048274	1.751680	0.007694	0.703584
-41.601658	-2.084505	1.756685	0.007782	0.703341
-42.120247	-1.995120	1.761690	0.007878	0.703335
-41.980945	-2.016074	1.766694	0.007852	0.703342
-41.885643	-2.037805	1.771699	0.007834	0.703333
-41.963906	-2.020665	1.776704	0.007849	0.703340
-41.974572	-2.017587	1.781709	0.007851	0.703342
-41.745408	-2.097748	1.786714	0.007808	0.703263
-42.687043	-2.057701	1.791718	0.007983	0.703005
-42.892629	-2.025048	1.796723	0.008022	0.702997
-42.997195	-2.005383	1.801728	0.008041	0.702999
-42.650332	-2.066749	1.806733	0.007976	0.703000
-42.861243	-2.031330	1.811738	0.008016	0.702996
-42.620723	-2.069329	1.816742	0.007971	0.703006
-42.516662	-2.140342	1.821747	0.007951	0.702900
-43.510168	-2.067683	1.826752	0.008136	0.702689
-43.555831	-2.059177	1.831757	0.008145	0.702690
-43.838396	-2.011212	1.836762	0.008197	0.702685
-43.558131	-2.057190	1.841766	0.008145	0.702693
-43.814849	-2.014374	1.846771	0.008193	0.702687
-43.831440	-2.010009	1.851776	0.008196	0.702690
-43.358742	-2.160515	1.856781	0.008108	0.702557
-44.909223	-1.979954	1.861786	0.008396	0.702363
-44.474007	-2.054374	1.866790	0.008315	0.702370
-44.634095	-2.030446	1.871795	0.008345	0.702360
-44.567541	-2.038667	1.876800	0.008332	0.702368
-44.543481	-2.043945	1.881805	0.008328	0.702366
-44.705724	-2.016390	1.886810	0.008358	0.702363
-44.444783	-2.107413	1.891814	0.008309	0.702273
-45.631561	-1.998295	1.896819	0.008530	0.702066
-45.357477	-2.044835	1.901824	0.008479	0.702071
-45.282010	-2.058160	1.906829	0.008465	0.702072
-45.764466	-1.973236	1.911834	0.008555	0.702069
-45.233854	-2.065904	1.916838	0.008456	0.702074
-45.294143	-2.057762	1.921843	0.008467	0.702068
-45.309024	-2.115250	1.926848	0.008470	0.701947
-46.592920	-1.986561	1.931853	0.008709	0.701744
-46.358916	-2.031010	1.936858	0.008665	0.701739
-46.251751	-2.044780	1.941862	0.008645	0.701750
-46.477142	-2.010745	1.946867	0.008687	0.701737
-46.345902	-2.030582	1.951872	0.008663	0.701745
-46.365329	-2.025405	1.956877	0.008666	0.701748
-46.257812	-2.075147	1.961882	0.008646	0.701687
-47.056249	-2.054148	1.966886	0.008795	0.701441
-47.065614	-2.056587	1.971891	0.008796	0.701433
-47.314723	-2.009953	1.976896	0.008843	0.701437
-47.119428	-2.045648	1.981901	0.008806	0.701436
-47.485649	-1.984222	1.986906	0.008874	0.701428
-47.078196	-2.051195	1.991910	0.008799	0.701440
-47.152972	-2.068802	1.996915	0.008812	0.701377
-47.797948	-2.081088	2.001920	0.008932	0.701120

-48.198670	-2.009097	2.011917	0.009007	0.701121
-48.020873	-2.042506	2.021914	0.008974	0.701118
-48.069417	-2.035013	2.031910	0.008983	0.701116
-48.008483	-2.044110	2.041907	0.008971	0.701119
-48.102528	-2.026844	2.051904	0.008988	0.701121
-48.052241	-2.036898	2.061901	0.008979	0.701119
-48.035140	-2.042230	2.071898	0.008976	0.701114
-48.008672	-2.046571	2.081894	0.008971	0.701115
-47.834733	-2.075896	2.091891	0.008938	0.701119
-48.115431	-2.026426	2.101888	0.008990	0.701118
-48.208869	-2.010234	2.111885	0.009007	0.701117
-47.967421	-2.054607	2.121882	0.008962	0.701115
-47.727949	-2.014387	2.131878	0.008918	0.701283
-47.141874	-2.045332	2.141875	0.008808	0.701432
-47.398995	-2.000223	2.151872	0.008856	0.701431
-47.141690	-2.044721	2.161869	0.008808	0.701434
-47.143445	-2.045881	2.171866	0.008808	0.701431
-46.938554	-1.999686	2.181862	0.008770	0.701599
-45.996261	-2.097899	2.191859	0.008595	0.701741
-46.340055	-2.036099	2.201856	0.008658	0.701742
-46.195099	-2.064116	2.211853	0.008631	0.701738
-46.326737	-2.006661	2.221850	0.008656	0.701807
-45.481066	-2.029975	2.231846	0.008498	0.702065
-45.274382	-2.065173	2.241843	0.008459	0.702068
-45.634842	-2.001601	2.251840	0.008526	0.702067
-45.423888	-1.983383	2.261837	0.008487	0.702180
-44.631678	-2.034009	2.271834	0.008339	0.702364
-44.701064	-2.021334	2.281830	0.008352	0.702365
-44.576583	-2.043884	2.291827	0.008329	0.702364
-44.232848	-1.979212	2.301824	0.008265	0.702619
-43.859353	-2.013289	2.311821	0.008195	0.702685
-43.851532	-2.014805	2.321818	0.008193	0.702685
-43.835619	-1.963847	2.331814	0.008190	0.702794
-42.801280	-2.046760	2.341811	0.007998	0.702999
-42.935318	-2.022171	2.351808	0.008022	0.703001
-42.807113	-2.045964	2.361805	0.007999	0.702999
-42.219301	-2.025346	2.371802	0.007889	0.703253
-42.069803	-2.012445	2.381798	0.007861	0.703333
-41.877876	-2.046245	2.391795	0.007825	0.703334
-41.864712	-2.039074	2.401792	0.007823	0.703354
-41.265974	-2.008291	2.411789	0.007711	0.703631
-41.239860	-2.014385	2.421786	0.007706	0.703629
-41.002837	-2.057425	2.431782	0.007662	0.703627
-40.706432	-2.027424	2.441779	0.007606	0.703795
-40.359500	-2.013695	2.451776	0.007542	0.703947
-40.206986	-2.040969	2.461773	0.007513	0.703948
-40.372686	-2.003993	2.471770	0.007544	0.703963
-39.602301	-1.997170	2.481766	0.007400	0.704254
-39.254489	-2.058604	2.491763	0.007335	0.704255
-39.218356	-2.064237	2.501760	0.007329	0.704257
-38.906803	-2.044418	2.511757	0.007270	0.704409
-38.362355	-2.054737	2.521754	0.007169	0.704584
-38.209741	-2.082571	2.531750	0.007140	0.704583
-38.488494	-2.032609	2.541747	0.007192	0.704584
-37.905763	-2.031962	2.551744	0.007083	0.704795
-37.667180	-2.029765	2.561741	0.007039	0.704885
-37.718963	-2.022634	2.571738	0.007048	0.704881
-37.588796	-1.986900	2.581734	0.007024	0.705000
-36.749143	-2.033385	2.591731	0.006868	0.705208
-36.888110	-2.009277	2.601728	0.006893	0.705207
-36.814570	-2.013347	2.611725	0.006879	0.705226
-36.247165	-1.969590	2.621722	0.006774	0.705517
-35.724288	-2.062031	2.631718	0.006676	0.705519
-36.124660	-1.990935	2.641715	0.006751	0.705519
-35.505630	-1.981377	2.651712	0.006635	0.705760
-35.023075	-2.020040	2.661709	0.006545	0.705856
-35.308617	-1.970621	2.671706	0.006598	0.705853
-34.996124	-1.981332	2.681702	0.006540	0.705944
-34.297531	-2.016939	2.691699	0.006410	0.706123
-34.148537	-2.044670	2.701696	0.006382	0.706121
-34.299888	-2.016296	2.711693	0.006410	0.706124
-33.478741	-2.015899	2.721690	0.006257	0.706419
-33.426829	-2.014540	2.731686	0.006247	0.706441
-33.540353	-1.994465	2.741683	0.006268	0.706441
-33.064871	-1.999568	2.751680	0.006180	0.706601
-32.414221	-2.044552	2.761677	0.006058	0.706744
-32.613535	-2.009301	2.771674	0.006095	0.706743
-32.614369	-1.992582	2.781670	0.006095	0.706777
-31.847478	-1.980457	2.791667	0.005952	0.707076
-31.433607	-2.055130	2.801664	0.005875	0.707074
-31.768307	-1.993801	2.811661	0.005937	0.707078
-31.077088	-2.026805	2.821658	0.005809	0.707259
-30.615763	-2.054832	2.831654	0.005723	0.707368
-30.946036	-1.995110	2.841651	0.005784	0.707370
-30.712110	-2.019169	2.851648	0.005740	0.707406
-30.078251	-1.987473	2.861645	0.005622	0.707696
-29.870695	-2.024240	2.871642	0.005583	0.707697
-29.859505	-2.027369	2.881638	0.005581	0.707695
-29.515297	-1.992003	2.891635	0.005517	0.707889
-29.022553	-2.020040	2.901632	0.005425	0.708009
-29.231100	-1.983927	2.911629	0.005464	0.708008
-29.072334	-1.970750	2.921626	0.005434	0.708091
-28.243365	-1.991542	2.931622	0.005279	0.708346
-28.170360	-2.004714	2.941619	0.005266	0.708346
-28.105505	-2.015420	2.951616	0.005254	0.708348
-27.697521	-1.970102	2.961613	0.005177	0.708584
-27.259399	-2.022988	2.971610	0.005096	0.708635
-27.347735	-2.008536	2.981606	0.005112	0.708633
-27.103492	-1.999042	2.991603	0.005066	0.708739
-26.319786	-2.031352	3.001600	0.004920	0.708954
-26.437925	-2.011980	3.011597	0.004942	0.708951
-26.226377	-2.050234	3.021594	0.004903	0.708950
-25.991353	-1.974840	3.031590	0.004859	0.709185
-25.399830	-2.044847	3.041587	0.004749	0.709256
-25.512999	-2.022339	3.051584	0.004770	0.709261
-25.587540	-1.966604	3.061581	0.004783	0.709347
-24.429248	-2.051738	3.071578	0.004568	0.709589
-24.500242	-2.038856	3.081574	0.004581	0.709590
-24.410368	-2.053666	3.091571	0.004564	0.709593
-24.117256	-2.025212	3.101568	0.004509	0.709754
-23.571642	-2.054793	3.111565	0.004407	0.709890
-23.527233	-2.062516	3.121562	0.004399	0.709891
-23.733555	-2.025986	3.131558	0.004437	0.709890
-22.805101	-2.056132	3.141555	0.004264	0.710161
-23.051367	-1.983231	3.151552	0.004310	0.710219
-22.842392	-2.020946	3.161549	0.004271	0.710219
-22.684704	-1.981660	3.171546	0.004241	0.710353
-22.093637	-1.999088	3.181542	0.004131	0.710529
-22.008058	-2.013052	3.191539	0.004115	0.710532
-21.882926	-2.034887	3.201536	0.004092	0.710533
-21.225582	-1.984759	3.211533	0.003969	0.710867
-21.124511	-2.002031	3.221530	0.003950	0.710869
-21.080320	-2.009088	3.231526	0.003942	0.710871
-20.630388	-2.029056	3.241523	0.003858	0.710991
-20.254783	-2.023158	3.251520	0.003788	0.711137
-20.289124	-2.017200	3.261517	0.003794	0.711137
-20.125252	-2.046132	3.271514	0.003764	0.711138
-19.628009	-1.980368	3.281510	0.003671	0.711446
-19.280200	-2.038314	3.291507	0.003606	0.711454
-19.426201	-2.012184	3.301504	0.003633	0.711455
-19.008730	-1.995745	3.311501	0.003555	0.711636
-18.599241	-2.008082	3.321498	0.003479	0.711757
-18.585088	-2.009785	3.331494	0.003476	0.711759
-18.549930	-1.979284	3.341491	0.003469	0.711833
-17.696921	-2.001891	3.351488	0.003310	0.712091
-17.361322	-2.061812	3.361485	0.003248	0.712091
-17.616406	-2.017736	3.371482	0.003295	0.712088
-17.287762	-1.983695	3.381478	0.003234	0.712273
-16.626570	-2.045176	3.391475	0.003111	0.712386
-16.831412	-2.007700	3.401472	0.003149	0.712388
-16.679143	-2.006703	3.411469	0.003120	0.712444
-16.071674	-1.983042	3.421466	0.003007	0.712707
-15.652050	-2.058324	3.431462	0.002929	0.712706
-15.762745	-2.037388	3.441459	0.002949	0.712709
-15.344459	-2.013184	3.451456	0.002871	0.712906
-14.911228	-2.031634	3.461453	0.002790	0.713023
-14.967762	-2.022311	3.471450	0.002801	0.713021
-14.995215	-2.003836	3.481446	0.002806	0.713049
-14.182607	-1.992321	3.491443	0.002654	0.713360
-14.054775	-2.015769	3.501440	0.002630	0.713359
-14.014269	-2.022558	3.511437	0.002623	0.713360
-13.614895	-2.013005	3.521434	0.002548	0.713521
-13.100018	-2.039538	3.531430	0.002452	0.713651
-13.357528	-1.994015	3.541427	0.002500	0.713650
-13.389039	-1.967925	3.551424	0.002506	0.713691
-12.463600	-1.993703	3.561421	0.002333	0.713968
-12.281612	-2.026759	3.571418	0.002299	0.713967
-12.302017	-2.022066	3.581414	0.002303	0.713969
-12.047089	-1.967074	3.591411	0.002255	0.714169
-11.198601	-2.061711	3.601408	0.002097	0.714281
-11.344162	-2.036844	3.611405	0.002124	0.714280
-11.163655	-2.070777	3.621402	0.002090	0.714276
-10.357893	-2.062982	3.631398	0.001940	0.714577
-9.910386	-2.127045	3.641395	0.001857	0.714608
-9.950978	-2.120840	3.651392	0.001864	0.714607
-10.065894	-2.100568	3.661389	0.001886	0.714606
-9.859823	-2.045831	3.671386	0.001847	0.714788
-9.205777	-2.102973	3.681382	0.001725	0.714906
-9.387777	-2.070278	3.691379	0.001759	0.714907
-9.078520	-2.124628	3.701376	0.001701	0.714909
-8.559788	-2.086116	3.711373	0.001605	0.715169
-8.522670	-2.063617	3.721370	0.001597	0.715227
-8.258203	-2.109356	3.731366	0.001548	0.715230
-8.314399	-2.081027	3.741363	0.001558	0.715266
-7.663701	-2.056375	3.751360	0.001437	0.715545
-7.270733	-2.126344	3.761357	0.001364	0.715546
-7.276440	-2.126198	3.771354	0.001365	0.715544
-7.230468	-2.081173	3.781350	0.001356	0.715650
-6.373926	-2.115627	3.791347	0.001196	0.715884
-6.297153	-2.129544	3.801344	0.001182	0.715884
-6.290916	-2.130934	3.811341	0.001181	0.715884
-6.234371	-2.092500	3.821338	0.001170	0.715980
-5.503873	-2.145630	3.831334	0.001034	0.716133
-5.629718	-2.124281	3.841331	0.001057	0.716131
-5.575156	-2.132189	3.851328	0.001047	0.716135
-4.973784	-2.107681	3.861325	0.000935	0.716396
-4.837326	-2.107285	3.871322	0.000909	0.716445
-4.816331	-2.110475	3.881318	0.000905	0.716446
-4.603775	-2.092408	3.891315	0.000866	0.716557
-3.853219	-2.125310	3.901312	0.000726	0.716757
-3.986937	-2.103390	3.911309	0.000751	0.716753
-3.848273	-2.128527	3.921306	0.000725	0.716753
-3.221860	-2.085799	3.931302	0.000608	0.717058
-3.010056	-2.111006	3.941299	0.000568	0.717083
-2.666466	-2.171381	3.951296	0.000504	0.717085
-2.956998	-2.074080	3.961293	0.000558	0.717176
-2.123438	-2.120483	3.971290	0.000403	0.717378
-2.110574	-2.121948	3.981286	0.000400	0.717380
-2.033650	-2.135257	3.991283	0.000386	0.717381
-1.715602	-2.061893	4.001280	0.000326	0.717638
-1.458792	-2.074424	4.011277	0.000278	0.717704
-1.418972	-2.081836	4.021274	0.000271	0.717703
-1.610860	-1.957296	4.031270	0.000306	0.717882
-1.301726	-1.944957	4.041267	0.000249	0.718016
-1.178656	-1.965140	4.051264	0.000226	0.718019
-0.925780	-1.846446	4.061261	0.000178	0.718343
-0.809526	-1.862208	4.071258	0.000157	0.718353
-0.752630	-1.799829	4.081254	0.000146	0.718496
-0.754398	-1.725878	4.091251	0.000146	0.718642
-0.707437	-1.679442	4.101248	0.000137	0.718750
-0.681698	-1.578042	4.111245	0.000132	0.718960
-0.817053	-1.482511	4.121242	0.000157	0.719101
-0.635241	-1.430771	4.131238	0.000123	0.719267
-0.529007	-1.325277	4.141235	0.000103	0.719512
-0.412293	-1.287468	4.151232	0.000081	0.719628
-0.308864	-1.167052	4.161229	0.000062	0.719902
-0.484089	-1.047863	4.171226	0.000094	0.720076
-0.381575	-0.972797	4.181222	0.000075	0.720260
-0.427157	-0.820918	4.191219	0.000083	0.720543
-0.338332	-0.703165	4.201216	0.000067	0.720806
-0.288992	-0.614084	4.211213	0.000057	0.720999
-0.203846	-0.526665	4.221210	0.000041	0.721201
-0.124916	-0.411279	4.231206	0.000026	0.721456
0.064850	-0.298842	4.241203	-0.000009	0.721743
-0.107177	-0.118581	4.251200	0.000022	0.722038
-0.086595	0.014071	4.261197	0.000018	0.722306
0.000000	0.167095	4.271194	0.000002	0.722636

-0.074934	0.842254	4.276198	0.000016	0.723934
0.305557	2.027387	4.281203	-0.000056	0.726385
0.628594	3.826470	4.286208	-0.000118	0.730001
0.727567	6.219564	4.291213	-0.000138	0.734671
0.940136	9.090091	4.296218	-0.000179	0.740264
1.154043	12.455742	4.301222	-0.000221	0.746757
1.453946	16.249229	4.306227	-0.000280	0.754028
1.966789	20.412038	4.311232	-0.000378	0.761988
2.354338	25.001868	4.316237	-0.000453	0.770611
2.645745	29.970678	4.321242	-0.000511	0.779796
3.246832	35.241003	4.326246	-0.000626	0.789515
3.756420	40.838995	4.331251	-0.000725	0.799668
4.231407	46.752605	4.336256	-0.000817	0.810236
4.731126	52.946304	4.341261	-0.000914	0.821158
5.077169	59.433027	4.346266	-0.000983	0.832390
5.894263	66.068776	4.351270	-0.001139	0.843863
6.796983	72.911659	4.356275	-0.001312	0.855549
7.256263	80.038903	4.361280	-0.001402	0.867415
8.035710	87.310042	4.366285	-0.001552	0.879444
8.613817	94.782129	4.371290	-0.001665	0.891573
9.510131	102.365937	4.376294	-0.001837	0.903802
10.112664	110.147104	4.381299	-0.001954	0.916092
10.997907	117.990578	4.386304	-0.002124	0.928391
11.587361	126.023225	4.391309	-0.002239	0.940735
12.309621	134.127149	4.396314	-0.002379	0.953060
13.435462	142.263685	4.401318	-0.002594	0.965378
14.051640	150.571066	4.406323	-0.002714	0.977659
14.417896	159.002677	4.411328	-0.002788	0.989903
15.232491	167.403222	4.416333	-0.002945	1.002064
16.057747	175.837168	4.421338	-0.003104	1.014128
16.860800	184.316789	4.426342	-0.003259	1.026107
17.427789	192.875402	4.431347	-0.003371	1.037999
18.027387	201.440816	4.436352	-0.003488	1.049773
18.482539	210.073971	4.441357	-0.003578	1.061474
19.087827	218.698560	4.446362	-0.003697	1.073069
19.632100	227.328704	4.451366	-0.003804	1.084534
20.244170	235.963978	4.456371	-0.003923	1.095900
20.622406	244.630125	4.461376	-0.004000	1.107137
21.555234	253.224502	4.466381	-0.004179	1.118291
22.029560	261.883836	4.471386	-0.004273	1.129317
22.670993	270.525089	4.476390	-0.004398	1.140249
23.253149	279.185344	4.481395	-0.004512	1.151088
24.061630	287.779547	4.486400	-0.004668	1.161792
24.752923	296.382119	4.491405	-0.004803	1.172384
25.076492	305.028002	4.496410	-0.004869	1.182857
26.052414	313.568837	4.501414	-0.005056	1.193246
26.732047	322.143674	4.506419	-0.005188	1.203525
26.978099	330.787451	4.511424	-0.005240	1.213711
27.631677	339.342224	4.516429	-0.005367	1.223789
28.327001	347.899154	4.521434	-0.005502	1.233795
28.817592	356.447322	4.526438	-0.005599	1.243671
29.694920	364.929870	4.531443	-0.005768	1.253469
30.206335	373.453019	4.536448	-0.005869	1.263166
30.764838	381.975288	4.541453	-0.005979	1.272797
31.203321	390.475001	4.546458	-0.006066	1.282308
31.768065	398.966406	4.551462	-0.006177	1.291763
32.302502	407.435370	4.556467	-0.006282	1.301119
32.675278	415.983880	4.561472	-0.006357	1.310465
33.294298	424.477448	4.566477	-0.006478	1.319730
33.868006	432.868764	4.571482	-0.006590	1.328813
34.477911	441.276453	4.576486	-0.006709	1.337857
35.104115	449.649575	4.581491	-0.006831	1.346807
35.532650	458.075815	4.586496	-0.006917	1.355719
36.024598	466.459331	4.591501	-0.007014	1.364539
36.252066	474.878294	4.596506	-0.007062	1.373293
36.578823	483.267492	4.601510	-0.007128	1.381979
36.973483	491.647931	4.606515	-0.007207	1.390612
37.249591	500.028052	4.611520	-0.007264	1.399171
37.482410	508.399404	4.616525	-0.007313	1.407663
38.203277	516.679377	4.621530	-0.007452	1.416093
38.533141	525.021846	4.626534	-0.007519	1.424470
38.645100	533.405757	4.631539	-0.007546	1.432804
39.213695	541.673765	4.636544	-0.007657	1.441049
40.054347	549.933389	4.641549	-0.007819	1.449283
40.324425	558.268726	4.646554	-0.007875	1.457453
40.771808	566.566299	4.651558	-0.007964	1.465568
41.223371	574.912137	4.656563	-0.008053	1.473686
41.584273	583.188442	4.661568	-0.008126	1.481678
42.576099	591.375892	4.666573	-0.008316	1.489641
43.543872	599.573664	4.671578	-0.008502	1.497567
43.869789	607.871358	4.676582	-0.008568	1.505447
44.096302	616.199379	4.681587	-0.008615	1.513299
44.381842	624.476433	4.686592	-0.008674	1.521071
44.753203	632.745240	4.691597	-0.008749	1.528809
45.207260	640.992420	4.696602	-0.008839	1.536501
45.523311	649.262936	4.701606	-0.008903	1.544155
45.928675	657.526103	4.706611	-0.008984	1.551777
46.441222	665.744383	4.711616	-0.009085	1.559338
46.908739	673.969757	4.716621	-0.009177	1.566861
47.189771	682.225833	4.721626	-0.009235	1.574348
47.586446	690.445968	4.726630	-0.009314	1.581785
48.151325	698.650207	4.731635	-0.009425	1.589197
48.413941	706.906711	4.736640	-0.009479	1.596577
48.980074	715.083745	4.741645	-0.009590	1.603896
49.262503	723.317714	4.746650	-0.009648	1.611192
49.463538	731.573709	4.751654	-0.009691	1.618462
50.026591	739.733398	4.756659	-0.009801	1.625667
50.401934	747.997757	4.761664	-0.009876	1.632904
50.910993	756.182478	4.766669	-0.009977	1.640059
51.071349	764.393617	4.771674	-0.010012	1.647157
51.514926	772.591297	4.776678	-0.010100	1.654252
52.045301	780.742426	4.781683	-0.010204	1.661289
52.303769	788.948940	4.786688	-0.010258	1.668306
52.928057	797.126578	4.791693	-0.010379	1.675319
53.085284	805.318450	4.796698	-0.010414	1.682251
53.560030	813.489058	4.801702	-0.010508	1.689179
53.930135	821.684686	4.806707	-0.010582	1.696086
54.377739	829.840547	4.811712	-0.010671	1.702942
54.889194	838.021793	4.816717	-0.010771	1.709800
54.961746	846.246906	4.821722	-0.010790	1.716609
55.498614	854.377842	4.826726	-0.010896	1.723374
55.899759	862.540891	4.831731	-0.010976	1.730121
56.039880	870.742736	4.836736	-0.011007	1.736840
56.513429	878.886819	4.841741	-0.011101	1.743529
57.043117	887.016097	4.846746	-0.011205	1.750187
57.379685	895.200295	4.851750	-0.011273	1.756839
57.788744	903.334988	4.856755	-0.011354	1.763436
58.340252	911.478186	4.861760	-0.011462	1.770032
58.686882	919.664647	4.866765	-0.011532	1.776613
58.929759	927.823474	4.871770	-0.011583	1.783135
59.468483	935.982488	4.876774	-0.011689	1.789669
59.932592	944.172955	4.881779	-0.011780	1.796195
60.230249	952.300244	4.886784	-0.011841	1.802628
60.626815	960.435600	4.891789	-0.011920	1.809056
61.175834	968.550934	4.896794	-0.012028	1.815463
61.521713	976.695499	4.901798	-0.012098	1.821846
62.019757	984.820149	4.906803	-0.012196	1.828210
62.297642	992.989887	4.911808	-0.012253	1.834560
62.526354	1001.151944	4.916813	-0.012301	1.840876
62.750404	1009.291067	4.921818	-0.012348	1.847153
63.287459	1017.426479	4.926822	-0.012453	1.853442
63.533651	1025.575528	4.931827	-0.012505	1.859686
63.666547	1033.721407	4.936832	-0.012535	1.865893
64.217801	1041.875471	4.941837	-0.012643	1.872135
64.721820	1049.977092	4.946842	-0.012742	1.878310
64.821641	1058.122746	4.951846	-0.012766	1.884452
65.152774	1066.255118	4.956851	-0.012833	1.890590
65.434706	1074.391396	4.961856	-0.012891	1.896706
66.023823	1082.480130	4.966861	-0.013006	1.902801
66.524590	1090.579059	4.971866	-0.013104	1.908874
66.918109	1098.725964	4.976870	-0.013183	1.914952
67.302339	1106.824914	4.981875	-0.013260	1.920973
67.556386	1114.945276	4.986880	-0.013313	1.926977
67.844606	1123.106092	4.991885	-0.013372	1.932996
68.358348	1131.187912	4.996890	-0.013473	1.938963
68.572448	1139.312472	5.001894	-0.013518	1.944910
68.898738	1147.464408	5.006899	-0.013584	1.950870
69.102585	1155.621533	5.011904	-0.013627	1.956803
69.407257	1163.720347	5.016909	-0.013689	1.962687
69.607092	1171.822523	5.021914	-0.013732	1.968544
69.934634	1179.946059	5.026918	-0.013798	1.974413
70.288816	1188.025896	5.031923	-0.013870	1.980236
70.578529	1196.119289	5.036928	-0.013929	1.986044
70.925756	1204.249168	5.041933	-0.013999	1.991868
71.207914	1212.354664	5.046938	-0.014057	1.997650
71.503192	1220.446608	5.051942	-0.014117	2.003407
71.787984	1228.566970	5.056947	-0.014175	2.009167
71.849018	1236.708891	5.061952	-0.014192	2.014902
72.511472	1244.754020	5.066957	-0.014321	2.020615
72.701727	1252.870483	5.071962	-0.014362	2.026313
73.010719	1261.002105	5.076966	-0.014424	2.032017
73.511071	1269.081050	5.081971	-0.014523	2.037689
73.776250	1277.160933	5.086976	-0.014578	2.043321
74.320732	1285.234775	5.091981	-0.014684	2.048962
74.710359	1293.337254	5.096986	-0.014762	2.054592
75.129103	1301.421899	5.101990	-0.014846	2.060197
75.256650	1309.557584	5.106995	-0.014875	2.065792
75.692975	1317.643642	5.112000	-0.014961	2.071368
76.062962	1325.749386	5.117005	-0.015036	2.076937
76.161468	1333.862752	5.122010	-0.015059	2.082469
76.586458	1341.934888	5.127014	-0.015144	2.087990
77.097425	1350.032879	5.132019	-0.015244	2.093523
77.268254	1358.143696	5.137024	-0.015281	2.099016
77.806718	1366.213389	5.142029	-0.015387	2.104503
78.149614	1374.325180	5.147034	-0.015456	2.109985
78.545318	1382.467288	5.152038	-0.015535	2.115478
78.714722	1390.566209	5.157043	-0.015572	2.120906
78.896232	1398.632455	5.162048	-0.015611	2.126300
79.188719	1406.743579	5.167053	-0.015671	2.131720
79.573290	1414.795419	5.172058	-0.015748	2.137096
79.777956	1422.894591	5.177062	-0.015791	2.142473
79.984629	1430.987223	5.182067	-0.015835	2.147832
80.287888	1439.072648	5.187072	-0.015897	2.153181
80.623590	1447.149745	5.192077	-0.015965	2.158516
81.013907	1455.191805	5.197082	-0.016043	2.163819
81.224176	1463.297491	5.202086	-0.016087	2.169133
81.542965	1471.401077	5.207091	-0.016152	2.174444
81.919166	1479.460550	5.212096	-0.016227	2.179718
82.376777	1487.535276	5.217101	-0.016318	2.184996
82.477621	1495.661821	5.222106	-0.016342	2.190263
82.623015	1503.792269	5.227110	-0.016374	2.195523
83.135144	1511.818430	5.232115	-0.016475	2.200737
83.451322	1519.860027	5.237120	-0.016539	2.205931
83.585811	1527.992270	5.242125	-0.016570	2.211154
83.729338	1536.083420	5.247130	-0.016602	2.216339
84.588879	1544.073438	5.252134	-0.016767	2.221512
84.930957	1552.170049	5.257139	-0.016836	2.226694
85.193220	1560.257820	5.262144	-0.016890	2.231852
85.599014	1568.356019	5.267149	-0.016971	2.237017
85.636642	1576.437613	5.272154	-0.016983	2.242126
85.719340	1584.533379	5.277158	-0.017004	2.247237
86.206781	1592.603435	5.282163	-0.017100	2.252356
86.471506	1600.680113	5.287168	-0.017155	2.257448
86.797087	1608.759783	5.292173	-0.017221	2.262535
87.201976	1616.811359	5.297178	-0.017302	2.267600
87.580661	1624.947042	5.302182	-0.017377	2.272704
87.904992	1633.027902	5.307187	-0.017443	2.277758
88.247704	1641.052134	5.312192	-0.017512	2.282766
88.525541	1649.134486	5.317197	-0.017569	2.287795
88.792388	1657.201939	5.322202	-0.017624	2.292802
88.942570	1665.293133	5.327206	-0.017658	2.297802
89.306626	1673.341953	5.332211	-0.017731	2.302784
89.673904	1681.394276	5.337216	-0.017804	2.307757
89.926360	1689.497822	5.342221	-0.017857	2.312742
89.966206	1697.589304	5.347226	-0.017870	2.317690
90.234727	1705.640750	5.352230	-0.017925	2.322622
90.457475	1713.704708	5.357235	-0.017972	2.327548
90.933824	1721.743913	5.362240	-0.018066	2.332469
91.191544	1729.847958	5.367245	-0.018119	2.337401
91.265914	1737.925980	5.372250	-0.018138	2.342292
91.471975	1745.997136	5.377254	-0.018182	2.347179
91.801459	1754.089832	5.382259	-0.018249	2.352079
92.096631	1762.137187	5.387264	-0.018309	2.356939
92.395062	1770.181637	5.392269	-0.018370	2.361787
92.735806	1778.231118	5.397274	-0.018438	2.366632
92.944342	1786.305971	5.402278	-0.018483	2.371471
93.480502	1794.350808	5.407283	-0.018588	2.376308
93.726105	1802.408057	5.412288	-0.018639	2.381120
94.121443	1810.482771	5.417293	-0.018718	2.385944
94.311284	1818.564146	5.422298	-0.018758	2.390747
94.512747	1826.651895	5.427302	-0.018801	2.395544
94.974209	1834.670453	5.432307	-0.018892	2.400311
95.386695	1842.696136	5.437312	-0.018975	2.405069
95.608434	1850.801396	5.442317	-0.019021	2.409849
95.634736	1858.907575	5.447322	-0.019031	2.414605
96.028603	1866.929213	5.452326	-0.019110	2.419331
96.256996	1875.021356	5.457331	-0.019158	2.424076
96.505979	1883.080425	5.462336	-0.019210	2.428793
96.941242	1891.226600	5.467341	-0.019296	2.433567
97.191698	1899.250118	5.472346	-0.019348	2.438246
97.336707	1907.299601	5.477350	-0.019380	2.442923
97.722942	1915.325332	5.482355	-0.019457	2.447595
97.774230	1923.400080	5.487360	-0.019472	2.452261
98.082880	1931.470340	5.492365	-0.019535	2.456935
98.342009	1939.506702	5.497370	-0.019589	2.461578
98.907319	1947.522201	5.502374	-0.019699	2.466222
99.205262	1955.612614	5.507379	-0.019760	2.470880
99.345453	1963.680045	5.512384	-0.019791	2.475505
99.656505	1971.739609	5.517389	-0.019855	2.480129
99.838234	1979.771172	5.522394	-0.019894	2.484719
99.957145	1987.853882	5.527398	-0.019921	2.489325
100.271937	1995.935632	5.532403	-0.019985	2.493936
100.589695	2003.972882	5.537408	-0.020050	2.498514
100.879262	2012.036734	5.542413	-0.020109	2.503096
101.025209	2020.087856	5.547418	-0.020141	2.507652
101.449854	2028.168578	5.552422	-0.020226	2.512237
101.804991	2036.222720	5.557427	-0.020297	2.516793
102.038627	2044.252189	5.562432	-0.020346	2.521318
102.472786	2052.283083	5.567437	-0.020432	2.525851
102.661040	2060.372437	5.572442	-0.020473	2.530390
102.866116	2068.438764	5.577446	-0.020516	2.534909
103.080800	2076.493734	5.582451	-0.020561	2.539415
103.330068	2084.518036	5.587456	-0.020613	2.543898
103.695665	2092.588832	5.592461	-0.020687	2.548407
103.751662	2100.689805	5.597466	-0.020702	2.552903
104.136204	2108.697680	5.602470	-0.020779	2.557363
104.618291	2116.721850	5.607475	-0.020874	2.561830
104.516658	2124.804373	5.612480	-0.020861	2.566281
104.911119	2132.863803	5.617485	-0.020939	2.570747
105.168924	2140.928567	5.622490	-0.020993	2.575198
105.331759	2148.970996	5.627494	-0.021028	2.579622
105.642202	2157.030474	5.632499	-0.021091	2.584058
106.020174	2165.062959	5.637504	-0.021167	2.588477
106.281614	2173.283129	5.642509	-0.021221	2.592982
106.518211	2181.334803	5.647514	-0.021271	2.597386
106.981285	2189.291326	5.652518	-0.021362	2.601746
107.553676	2197.284101	5.657523	-0.021474	2.606125
107.768343	2205.325394	5.662528	-0.021519	2.610500
108.059795	2213.406563	5.667533	-0.021579	2.614894
108.268655	2221.420681	5.672538	-0.021623	2.619238
108.309338	2229.475150	5.677542	-0.021636	2.623586
108.631966	2237.529904	5.682547	-0.021701	2.627946
108.968290	2245.571555	5.687552	-0.021769	2.632292
109.318241	2253.632593	5.692557	-0.021840	2.636642
109.388901	2261.690810	5.697562	-0.021858	2.640965
109.605843	2269.716565	5.702566	-0.021904	2.645273
109.894870	2277.764245	5.707571	-0.021963	2.649591
110.072001	2285.835424	5.712576	-0.022001	2.653906
110.385584	2293.884679	5.717581	-0.022065	2.658212
110.796970	2301.895265	5.722586	-0.022147	2.662497
110.981253	2309.951401	5.727590	-0.022186	2.666784
111.120551	2318.053220	5.732595	-0.022218	2.671086
111.317681	2326.129266	5.737600	-0.022260	2.675370
111.696878	2334.122341	5.742605	-0.022336	2.679616
111.829941	2342.160505	5.747610	-0.022366	2.683863
112.124101	2350.190225	5.752614	-0.022426	2.688109
112.580540	2358.244139	5.757619	-0.022516	2.692371
112.502350	2366.339214	5.762624	-0.022507	2.696614
112.771936	2374.365196	5.767629	-0.022562	2.700836
113.225606	2382.379394	5.772634	-0.022652	2.705057
113.347345	2390.442011	5.777638	-0.022680	2.709276
113.583404	2398.540729	5.782643	-0.022729	2.713514
113.612759	2406.571955	5.787648	-0.022740	2.717697
114.113606	2414.591753	5.792653	-0.022839	2.721898
114.323215	2422.642692	5.797658	-0.022883	2.726090
114.531847	2430.680948	5.802662	-0.022927	2.730268
114.958237	2438.749857	5.807667	-0.023012	2.734470
115.126071	2446.771384	5.812672	-0.023048	2.738625
115.279621	2454.820816	5.817677	-0.023082	2.742787
115.563609	2462.856235	5.822682	-0.023141	2.746943
115.764670	2470.939294	5.827686	-0.023183	2.751112
116.041309	2479.064774	5.832691	-0.023240	2.755302
116.219600	2487.040084	5.837696	-0.023279	2.759402
116.511055	2495.060456	5.842701	-0.023338	2.763526
116.740480	2503.086195	5.847706	-0.023386	2.767643
116.858599	2511.149900	5.852710	-0.023414	2.771766
117.395249	2519.165144	5.857715	-0.023519	2.775883
117.416900	2527.204168	5.862720	-0.023528	2.779976
117.597211	2535.242732	5.867725	-0.023567	2.784071
118.004045	2543.273684	5.872730	-0.023648	2.788171
118.353305	2551.324606	5.877734	-0.023718	2.792270
118.715616	2559.385436	5.882739	-0.023791	2.796370
118.826857	2567.419316	5.887744	-0.023817	2.800435
119.128977	2575.435468	5.892749	-0.023879	2.804497
119.224238	2583.502767	5.897754	-0.023902	2.808566
119.420618	2591.557148	5.902758	-0.023944	2.812628
119.835563	2599.595072	5.907763	-0.024026	2.816690
120.205800	2607.614456	5.912768	-0.024100	2.820733
120.347291	2615.654905	5.917773	-0.024132	2.824768
120.607008	2623.734657	5.922778	-0.024186	2.828823
120.910326	2631.804914	5.927782	-0.024248	2.832871
121.130955	2639.854957	5.932787	-0.024294	2.836897
121.325128	2647.873774	5.937792	-0.024335	2.840901
121.648332	2655.879947	5.942797	-0.024401	2.844901
121.778587	2663.930761	5.947802	-0.024430	2.848905
121.903413	2671.972175	5.952806	-0.024459	2.852900
122.306377	2680.012455	5.957811	-0.024539	2.856903
122.480550	2688.052755	5.962816	-0.024577	2.860889
122.654895	2696.089165	5.967821	-0.024615	2.864866
123.065445	2704.110310	5.972826	-0.024697	2.868844
123.359483	2712.159695	5.977830	-0.024757	2.872824
123.711034	2720.222230	5.982835	-0.024827	2.876807
123.826238	2728.250657	5.987840	-0.024854	2.880756
124.081529	2736.266256	5.992845	-0.024907	2.884700
124.240514	2744.323477	5.997850	-0.024942	2.888654
124.359763	2752.375165	6.002854	-0.024969	2.892598
124.633687	2760.460415	6.007859	-0.025026	2.896561
124.949229	2768.444015	6.012864	-0.025090	2.900471
125.073891	2776.524467	6.017869	-0.025118	2.904413
125.352469	2784.545021	6.022874	-0.025175	2.908329
125.643959	2792.637515	6.027878	-0.025235	2.912275
125.632730	2800.755770	6.032883	-0.025238	2.916211
125.731038	2808.712364	6.037888	-0.025262	2.920071
126.299648	2816.675786	6.042893	-0.025373	2.923953
126.549367	2824.715391	6.047898	-0.025425	2.927850
126.425933	2832.772931	6.052902	-0.025407	2.931730
126.822712	2840.840137	6.057907	-0.025486	2.935638
127.043955	2848.819241	6.062912	-0.025533	2.939488
127.206730	2856.893955	6.067917	-0.025568	2.943377
127.559475	2864.914572	6.072922	-0.025639	2.947244
127.652555	2872.957729	6.077926	-0.025662	2.951104
127.944163	2881.031796	6.082931	-0.025722	2.954983
128.155441	2889.021379	6.087936	-0.025766	2.958813
128.411954	2897.058447	6.092941	-0.025819	2.962663
128.483934	2905.108250	6.097946	-0.025838	2.966504
128.682739	2913.150992	6.102950	-0.025880	2.970343
129.018304	2921.196178	6.107955	-0.025948	2.974186
129.293790	2929.212983	6.112960	-0.026005	2.978007
129.654090	2937.245680	6.117965	-0.026077	2.981835
129.979967	2945.255628	6.122970	-0.026143	2.985645
130.404869	2953.278008	6.127974	-0.026228	2.989461
130.986692	2961.351091	6.132979	-0.026341	2.993305
130.945839	2969.411423	6.137984	-0.026339	2.997106
131.153796	2977.429154	6.142989	-0.026383	3.000894
131.487567	2985.436556	6.147994	-0.026450	3.004679
131.779338	2993.463978	6.152998	-0.026510	3.008467
131.683440	3001.577035	6.158003	-0.026497	3.012271
131.942745	3009.602398	6.163008	-0.026551	3.016046
132.272649	3017.614554	6.168013	-0.026618	3.019814
132.362420	3025.641293	6.173018	-0.026640	3.023572
132.459113	3033.688720	6.178022	-0.026663	3.027336
132.763498	3041.768785	6.183027	-0.026725	3.031120
132.882714	3049.814666	6.188032	-0.026753	3.034875
133.216845	3057.805315	6.193037	-0.026820	3.038609
133.492571	3065.817401	6.198042	-0.026877	3.042346
133.629022	3073.868018	6.203046	-0.026907	3.046090
133.976145	3081.889361	6.208051	-0.026977	3.049825
134.232602	3089.931411	6.213056	-0.027030	3.053561
134.562602	3097.975892	6.218061	-0.027097	3.057298
134.689350	3106.018103	6.223066	-0.027126	3.061018
134.757717	3114.018595	6.228070	-0.027144	3.064713
135.275805	3122.052648	6.233075	-0.027246	3.068439
135.310384	3130.152172	6.238080	-0.027258	3.072168
135.670989	3138.232448	6.243085	-0.027330	3.075899
135.882204	3146.209988	6.248090	-0.027375	3.079572
136.117821	3154.199459	6.253094	-0.027424	3.083246
136.195191	3162.239843	6.258099	-0.027444	3.086933
136.469731	3170.272695	6.263104	-0.027500	3.090620
136.749283	3178.321620	6.268109	-0.027557	3.094310
136.919252	3186.350947	6.273114	-0.027594	3.097983
137.112158	3194.349897	6.278118	-0.027635	3.101638
137.638228	3202.382623	6.283123	-0.027739	3.105319
137.829035	3210.416110	6.288128	-0.027780	3.108980
138.025465	3218.508819	6.293133	-0.027821	3.112665
138.261339	3226.548074	6.298138	-0.027871	3.116323
138.422873	3234.547075	6.303142	-0.027906	3.119955
138.646473	3242.590046	6.308147	-0.027953	3.123605
138.847287	3250.597814	6.313152	-0.027996	3.127234
139.046571	3258.660804	6.318157	-0.028038	3.130884
139.210405	3266.709797	6.323162	-0.028074	3.134521
139.533714	3274.719929	6.328166	-0.028139	3.138144
139.873031	3282.729583	6.333171	-0.028208	3.141763
139.858246	3290.770880	6.338176	-0.028210	3.145376
139.915826	3298.821992	6.343181	-0.028226	3.148993
140.287966	3306.873952	6.348186	-0.028301	3.152620
140.724411	3314.887957	6.353190	-0.028388	3.156228
140.935543	3322.896979	6.358195	-0.028432	3.159820
141.073804	3330.924403	6.363200	-0.028463	3.163414
141.672498	3338.919196	6.368205	-0.028580	3.167008
141.844291	3346.988501	6.373210	-0.028617	3.170613
141.956755	3355.025111	6.378214	-0.028643	3.174197
142.275510	3363.074867	6.383219	-0.028708	3.177791
142.394744	3371.070832	6.388224	-0.028736	3.181349
142.475952	3379.118878	6.393229	-0.028756	3.184924
142.836255	3387.147173	6.398234	-0.028828	3.188499
143.169222	3395.174578	6.403238	-0.028896	3.192067
143.341916	3403.267388	6.408243	-0.028933	3.195654
143.573171	3411.237959	6.413248	-0.028982	3.199185
143.864462	3419.278997	6.418253	-0.029041	3.202746
143.771305	3427.338652	6.423258	-0.029029	3.206295
143.797059	3435.332105	6.428262	-0.029039	3.209816
144.429806	3443.410564	6.433267	-0.029162	3.213396
144.642548	3451.408525	6.438272	-0.029207	3.216919
144.746053	3459.444852	6.443277	-0.029232	3.220450
144.992911	3467.467345	6.448282	-0.029283	3.223978
145.025489	3475.528088	6.453286	-0.029294	3.227509
145.294278	3483.568473	6.458291	-0.029350	3.231037
145.590137	3491.603109	6.463296	-0.029410	3.234560
145.877746	3499.614504	6.468301	-0.029469	3.238068
146.082913	3507.650988	6.473306	-0.029512	3.241581
146.031515	3515.666275	6.478310	-0.029508	3.245070
146.388268	3523.671820	6.483315	-0.029580	3.248567
146.455946	3531.697030	6.488320	-0.029598	3.252057
146.808177	3539.748598	6.493325	-0.029669	3.255567
147.056605	3547.753020	6.498330	-0.029720	3.259048
147.285870	3555.764279	6.503334	-0.029768	3.262527
147.603706	3563.822307	6.508339	-0.029833	3.266027
147.599479	3571.841217	6.513344	-0.029837	3.269493
147.976206	3579.892536	6.518349	-0.029913	3.272984
148.176234	3587.937563	6.523354	-0.029955	3.276462
148.252139	3595.924930	6.528358	-0.029975	3.279906
148.734986	3603.952851	6.533363	-0.030070	3.283381
148.914179	3611.984974	6.538368	-0.030108	3.286841
149.000209	3620.025323	6.543373	-0.030130	3.290298
149.196397	3628.097033	6.548378	-0.030172	3.293768
149.437385	3636.131068	6.553382	-0.030222	3.297221
149.803016	3644.130387	6.558387	-0.030295	3.300660
149.855927	3652.123079	6.563392	-0.030310	3.304080
149.883075	3660.200955	6.568397	-0.030321	3.307533
150.304168	3668.241273	6.573402	-0.030404	3.310980
150.385852	3676.284406	6.578406	-0.030425	3.314413
150.714268	3684.298672	6.583411	-0.030491	3.317838
150.921588	3692.292442	6.588416	-0.030535	3.321247
151.321859	3700.278989	6.593421	-0.030615	3.324657
151.440668	3708.328857	6.598426	-0.030642	3.328079
151.823691	3716.332952	6.603430	-0.030719	3.331488
151.870650	3724.427950	6.608435	-0.030733	3.334920
151.882718	3732.473114	6.613440	-0.030741	3.338326
152.210149	3740.473154	6.618445	-0.030807	3.341721
152.720785	3748.465554	6.623450	-0.030907	3.345116
152.546189	3756.514702	6.628454	-0.030880	3.348506
152.877384	3764.565915	6.633459	-0.030947	3.351912
152.979823	3772.614840	6.638464	-0.030971	3.355305
153.429026	3780.584157	6.643469	-0.031060	3.358674
153.631145	3788.634235	6.648474	-0.031103	3.362065
153.819705	3796.658739	6.653478	-0.031144	3.365441
153.923656	3804.702366	6.658483	-0.031168	3.368818
153.975071	3812.748174	6.663488	-0.031183	3.372191
154.212202	3820.783999	6.668493	-0.031233	3.375563
154.459703	3828.783771	6.673498	-0.031284	3.378917
154.395548	3836.821054	6.678502	-0.031277	3.382272
154.818272	3844.837049	6.683507	-0.031361	3.385632
154.909318	3852.866005	6.688512	-0.031384	3.388983
155.421384	3860.936475	6.693517	-0.031484	3.392362
155.621140	3869.003214	6.698522	-0.031527	3.395726
155.856334	3876.945075	6.703526	-0.031576	3.399035
156.161799	3884.974664	6.708531	-0.031638	3.402380
156.213911	3892.978493	6.713536	-0.031653	3.405702
156.308533	3901.003963	6.718541	-0.031676	3.409031
156.610578	3909.060077	6.723546	-0.031737	3.412377
156.659562	3917.093121	6.728550	-0.031752	3.415701
156.976315	3925.101291	6.733555	-0.031816	3.419021
157.079973	3933.131201	6.738560	-0.031841	3.422340
157.254695	3941.160838	6.743565	-0.031879	3.425657
157.506508	3949.193533	6.748570	-0.031931	3.428975
157.751426	3957.205103	6.753574	-0.031982	3.432281
157.937039	3965.289375	6.758579	-0.032022	3.435612
157.987923	3973.254952	6.763584	-0.032036	3.438886
158.261089	3981.268670	6.768589	-0.032092	3.442184
158.590645	3989.297820	6.773594	-0.032159	3.445487
158.610776	3997.303461	6.778598	-0.032168	3.448767
158.897591	4005.380685	6.783603	-0.032227	3.452082
158.936797	4013.415477	6.788608	-0.032239	3.455368
159.098388	4021.450401	6.793613	-0.032275	3.458655
159.374816	4029.467769	6.798618	-0.032332	3.461936
159.571858	4037.463983	6.803622	-0.032374	3.465202
159.872527	4045.523992	6.808627	-0.032435	3.468494
159.814859	4053.594229	6.813632	-0.032429	3.471776
160.206665	4061.614880	6.818637	-0.032508	3.475049
160.549711	4069.633301	6.823642	-0.032577	3.478317
160.421215	4077.625091	6.828646	-0.032558	3.481555
160.840041	4085.613493	6.833651	-0.032641	3.484807
160.924207	4093.639726	6.838656	-0.032662	3.488060
161.250683	4101.669161	6.843661	-0.032729	3.491319
161.466074	4109.745085	6.848666	-0.032774	3.494590
161.671784	4117.723476	6.853670	-0.032818	3.497819
162.010775	4125.796510	6.858675	-0.032886	3.501087
162.233849	4133.765368	6.863680	-0.032933	3.504306
162.217776	4141.796640	6.868685	-0.032935	3.507539
162.607035	4149.867667	6.873690	-0.033013	3.510799
162.709915	4157.876758	6.878694	-0.033037	3.514021
162.939042	4165.923995	6.883699	-0.033085	3.517260
163.065841	4173.910315	6.888704	-0.033114	3.520468
163.284990	4181.907832	6.893709	-0.033160	3.523681
163.593681	4189.958959	6.898714	-0.033223	3.526915
163.526786	4197.974384	6.903718	-0.033216	3.530120
164.006778	4206.043075	6.908723	-0.033311	3.533360
164.459304	4214.040144	6.913728	-0.033400	3.536567
164.526345	4222.067531	6.918733	-0.033418	3.539772
164.700709	4230.105901	6.923738	-0.033456	3.542982
164.911021	4238.105816	6.928742	-0.033500	3.546175
165.141669	4246.175099	6.933747	-0.033548	3.549392
165.445059	4254.247167	6.938752	-0.033610	3.552611
165.675611	4262.314045	6.943757	-0.033658	3.555822
165.712296	4270.268147	6.948762	-0.033670	3.558979
165.881592	4278.257318	6.953766	-0.033707	3.562152
166.232674	4286.274158	6.958771	-0.033778	3.565338
166.452849	4294.292996	6.963776	-0.033824	3.568518
166.531605	4302.330287	6.968781	-0.033844	3.571698
166.666910	4310.364310	6.973786	-0.033875	3.574876
166.964374	4318.366782	6.978790	-0.033935	3.578043
166.986087	4326.425914	6.983795	-0.033945	3.581222
167.126339	4334.401154	6.988800	-0.033976	3.584368
167.284985	4342.435295	6.993805	-0.034011	3.587536
167.360597	4350.484215	6.998810	-0.034030	3.590704
167.610348	4358.495919	7.003814	-0.034082	3.593859
168.108320	4366.506459	7.008819	-0.034180	3.597018
168.228608	4374.500435	7.013824	-0.034208	3.600157
168.478046	4382.508139	7.018829	-0.034260	3.603303
168.639352	4390.572326	7.023834	-0.034295	3.606465
168.791249	4398.570097	7.028838	-0.034328	3.609598
169.097125	4406.631873	7.033843	-0.034391	3.612758
169.289213	4414.684921	7.038848	-0.034432	3.615909
169.290729	4422.660894	7.043853	-0.034437	3.619021
169.519271	4430.703054	7.048858	-0.034485	3.622163
169.571721	4438.707746	7.053862	-0.034500	3.625282
169.713560	4446.768477	7.058867	-0.034532	3.628423
169.998634	4454.789309	7.063872	-0.034590	3.631550
170.305730	4462.835753	7.068877	-0.034653	3.634684
170.602312	4470.854615	7.073882	-0.034713	3.637805
170.621441	4478.906972	7.078886	-0.034722	3.640929
170.783814	4486.887048	7.083891	-0.034758	3.644025
170.961114	4494.887484	7.088896	-0.034796	3.647128
171.351654	4502.899548	7.093901	-0.034874	3.650237
171.489731	4510.960970	7.098906	-0.034905	3.653357
171.420585	4518.998213	7.103910	-0.034897	3.656459
171.927050	4526.969868	7.108915	-0.034997	3.659548
172.060680	4535.014319	7.113920	-0.035027	3.662653
172.157045	4543.047104	7.118925	-0.035050	3.665750
172.244962	4551.075941	7.123930	-0.035072	3.668842
172.316510	4559.125696	7.128934	-0.035091	3.671939
172.538709	4567.157542	7.133939	-0.035137	3.675031
172.766828	4575.151927	7.138944	-0.035185	3.678106
172.903153	4583.171451	7.143949	-0.035216	3.681186
173.087215	4591.170947	7.148954	-0.035255	3.684256
173.156149	4599.219102	7.153958	-0.035274	3.687340
173.270763	4607.251419	7.158963	-0.035300	3.690416
173.430803	4615.284230	7.163968	-0.035335	3.693491
173.716271	4623.293487	7.168973	-0.035394	3.696557
173.875425	4631.276073	7.173978	-0.035429	3.699608
173.902267	4639.299368	7.178982	-0.035439	3.702668
174.199075	4647.339591	7.183987	-0.035499	3.705739
174.169962	4655.384013	7.188992	-0.035499	3.708800
174.507164	4663.451575	7.193997	-0.035567	3.711877
174.672768	4671.526391	7.199002	-0.035604	3.714950
174.877524	4679.470567	7.204006	-0.035647	3.717972
175.272800	4687.473274	7.209011	-0.035726	3.721018
175.293546	4695.434201	7.214016	-0.035735	3.724037
175.361872	4703.487611	7.219021	-0.035753	3.727089
175.522384	4711.508789	7.224026	-0.035788	3.730129
175.754510	4719.526264	7.229030	-0.035837	3.733167
175.914107	4727.592159	7.234035	-0.035872	3.736219
175.855262	4735.571790	7.239040	-0.035866	3.739230
176.119446	4743.573130	7.244045	-0.035921	3.742255
176.480022	4751.598227	7.249050	-0.035993	3.745289
176.637966	4759.645970	7.254054	-0.036028	3.748324
176.968967	4767.718584	7.259059	-0.036095	3.751369
177.016360	4775.720000	7.264064	-0.036109	3.754379
177.011187	4783.761873	7.269069	-0.036113	3.757401
177.353108	4791.791310	7.274074	-0.036182	3.760423
177.570609	4799.731774	7.279078	-0.036228	3.763407
177.846075	4807.799243	7.284083	-0.036284	3.766437
177.694840	4815.839366	7.289088	-0.036262	3.769445
177.963974	4823.848565	7.294093	-0.036317	3.772448
178.453864	4831.907668	7.299098	-0.036413	3.775473
178.214659	4839.938997	7.304102	-0.036374	3.778468
178.657069	4847.948037	7.309107	-0.036462	3.781468
178.618627	4855.933102	7.314112	-0.036460	3.784446
178.675050	4863.989147	7.319117	-0.036476	3.787450
178.834152	4872.027876	7.324122	-0.036511	3.790447
179.274641	4880.039506	7.329126	-0.036598	3.793438
179.483565	4888.076441	7.334131	-0.036642	3.796431
179.506595	4895.991272	7.339136	-0.036652	3.799373
179.628143	4904.067126	7.344141	-0.036680	3.802374
180.104423	4912.043539	7.349146	-0.036774	3.805343
180.025617	4920.090083	7.354150	-0.036764	3.808324
180.238432	4928.149493	7.359155	-0.036809	3.811313
180.583426	4936.157850	7.364160	-0.036879	3.814285
180.797118	4944.138838	7.369165	-0.036924	3.817241
180.936248	4952.198884	7.374170	-0.036955	3.820222
180.859119	4960.166937	7.379174	-0.036946	3.823162
181.196037	4968.233309	7.384179	-0.037014	3.826145
181.261389	4976.215763	7.389184	-0.037031	3.829089
181.259225	4984.333730	7.394189	-0.037036	3.832079
181.612739	4992.302919	7.399194	-0.037107	3.835020
181.709315	5000.309066	7.404198	-0.037131	3.837967
181.886038	5008.358536	7.409203	-0.037169	3.840928
182.232490	5016.309501	7.414208	-0.037239	3.843855
182.380866	5024.355239	7.419213	-0.037272	3.846811
182.433287	5032.379373	7.424218	-0.037287	3.849754
182.494168	5040.433928	7.429222	-0.037303	3.852706
182.804658	5048.468910	7.434227	-0.037366	3.855654
182.921529	5056.485021	7.439232	-0.037393	3.858588
183.012658	5064.483077	7.444237	-0.037416	3.861514
183.342077	5072.491272	7.449242	-0.037482	3.864445
183.581719	5080.550825	7.454246	-0.037532	3.867391
183.840897	5088.559905	7.459251	-0.037586	3.870317
183.908775	5096.793817	7.464256	-0.037604	3.873319
184.170155	5104.817832	7.469261	-0.037658	3.876246
184.163091	5112.733741	7.474266	-0.037662	3.879126
184.238884	5120.689743	7.479270	-0.037681	3.882020
184.790570	5128.690733	7.484275	-0.037789	3.884938
184.928721	5136.701101	7.489280	-0.037820	3.887848
184.846279	5144.730978	7.494285	-0.037810	3.890760
185.064387	5152.786261	7.499290	-0.037856	3.893684
185.298756	5160.780449	7.504294	-0.037905	3.896584
185.490843	5168.777743	7.509299	-0.037946	3.899482
185.594512	5176.785704	7.514304	-0.037971	3.902380
185.882174	5184.808224	7.519309	-0.038029	3.905285
186.174620	5192.837464	7.524314	-0.038089	3.908190
186.384357	5200.855453	7.529318	-0.038133	3.911087
186.640081	5208.904831	7.534323	-0.038186	3.913994
186.821375	5216.901724	7.539328	-0.038225	3.916879
186.882819	5224.863021	7.544333	-0.038242	3.919747
187.269222	5232.922993	7.549338	-0.038319	3.922653
187.403605	5240.913305	7.554342	-0.038350	3.925528
187.389158	5248.992702	7.559347	-0.038352	3.928431
187.564289	5256.995442	7.564352	-0.038390	3.931307
187.665275	5265.010457	7.569357	-0.038414	3.934184
187.960778	5273.053030	7.574362	-0.038475	3.937072
187.928004	5281.016848	7.579366	-0.038474	3.939924
188.366042	5289.039857	7.584371	-0.038561	3.942803
188.379322	5297.082930	7.589376	-0.038568	3.945680
188.537544	5305.092419	7.594381	-0.038603	3.948545
188.877794	5313.153969	7.599386	-0.038672	3.951430
189.060242	5321.191639	7.604390	-0.038711	3.954302
189.111295	5329.198714	7.609395	-0.038726	3.957158
189.492205	5337.155308	7.614400	-0.038802	3.960000
189.718697	5345.176984	7.619405	-0.038850	3.962861
189.867126	5353.192511	7.624410	-0.038882	3.965716
189.926120	5361.187423	7.629414	-0.038899	3.968559
190.264984	5369.244199	7.634419	-0.038967	3.971428
190.261551	5377.305609	7.639424	-0.038972	3.974290
190.470333	5385.289745	7.644429	-0.039016	3.977126
190.548032	5393.326367	7.649434	-0.039036	3.979977
190.834518	5401.340490	7.654438	-0.039094	3.982821
190.998055	5409.358272	7.659443	-0.039130	3.985663
191.170106	5417.387635	7.664448	-0.039167	3.988506
191.328991	5425.402216	7.669453	-0.039202	3.991342
191.407128	5433.481989	7.674458	-0.039222	3.994198
191.535781	5441.462645	7.679462	-0.039251	3.997017
191.877984	5449.467563	7.684467	-0.039320	3.999847
191.952590	5457.526806	7.689472	-0.039340	4.002689
192.194083	5465.517760	7.694477	-0.039390	4.005508
192.617541	5473.533742	7.699482	-0.039474	4.008336
192.690928	5481.563313	7.704486	-0.039493	4.011162
192.851955	5489.613320	7.709491	-0.039528	4.013994
192.738401	5497.666207	7.714496	-0.039512	4.016821
193.038380	5505.616523	7.719501	-0.039573	4.019617
193.307154	5513.664700	7.724506	-0.039629	4.022444
193.240763	5521.652317	7.729510	-0.039622	4.025243
193.551004	5529.720821	7.734515	-0.039685	4.028074
193.682262	5537.743159	7.739520	-0.039715	4.030884
193.733467	5545.841596	7.744525	-0.039729	4.033718
194.046424	5553.845104	7.749530	-0.039793	4.036520
194.237434	5561.727228	7.754534	-0.039834	4.039276
194.606029	5569.785270	7.759539	-0.039908	4.042094
194.652193	5577.785834	7.764544	-0.039922	4.044886
194.755936	5585.810118	7.769549	-0.039946	4.047684
194.978422	5593.819751	7.774554	-0.039993	4.050478
195.217621	5601.826235	7.779558	-0.040043	4.053268
195.390459	5609.907561	7.784563	-0.040080	4.056082
195.641091	5617.899696	7.789568	-0.040132	4.058863
195.717205	5625.913647	7.794573	-0.040152	4.061648
195.983851	5633.900089	7.799578	-0.040207	4.064424
195.936751	5641.940999	7.804582	-0.040203	4.067213
196.252434	5649.932955	7.809587	-0.040267	4.069988
196.422628	5657.991414	7.814592	-0.040304	4.072781
196.444556	5666.000135	7.819597	-0.040314	4.075554
196.867310	5674.026174	7.824602	-0.040398	4.078336
196.893736	5682.018650	7.829606	-0.040408	4.081100
197.087362	5690.028878	7.834611	-0.040449	4.083870
197.193723	5698.068903	7.839616	-0.040474	4.086647
197.254254	5706.043836	7.844621	-0.040491	4.089399
197.653039	5714.144049	7.849626	-0.040570	4.092197
197.726256	5722.124917	7.854630	-0.040589	4.094947
198.005487	5730.142181	7.859635	-0.040646	4.097711
198.057466	5738.172871	7.864640	-0.040661	4.100475
198.265730	5746.170287	7.869645	-0.040706	4.103227
198.319035	5754.192739	7.874650	-0.040721	4.105984
198.407682	5762.207440	7.879654	-0.040743	4.108737
198.592417	5770.273068	7.884659	-0.040782	4.111507
198.908456	5778.305564	7.889664	-0.040846	4.114265
199.079056	5786.356341	7.894669	-0.040883	4.117026
199.158822	5794.307457	7.899674	-0.040904	4.119750
199.430060	5802.314259	7.904678	-0.040959	4.122493
199.610731	5810.313423	7.909683	-0.040998	4.125230
199.679903	5818.376001	7.914688	-0.041016	4.127987
199.820811	5826.347186	7.919693	-0.041048	4.130711
200.276994	5834.391846	7.924698	-0.041138	4.133462
200.416981	5842.427861	7.929702	-0.041170	4.136204
200.351742	5850.490404	7.934707	-0.041163	4.138951
200.604363	5858.509314	7.939712	-0.041215	4.141685
200.800921	5866.453049	7.944717	-0.041257	4.144391
200.927435	5874.524824	7.949722	-0.041286	4.147139
201.093983	5882.524343	7.954726	-0.041322	4.149860
201.512654	5890.575526	7.959731	-0.041405	4.152600
201.675511	5898.604312	7.964736	-0.041441	4.155327
201.785893	5906.558330	7.969741	-0.041467	4.158027
202.124995	5914.625770	7.974746	-0.041535	4.160765
202.129048	5922.554353	7.979750	-0.041541	4.163452
202.340528	5930.643351	7.984755	-0.041586	4.166193
202.615862	5938.662692	7.989760	-0.041642	4.168909
202.919668	5946.705822	7.994765	-0.041704	4.171632
202.784270	5954.760713	7.999770	-0.041684	4.174352
202.925240	5962.725609	8.004774	-0.041716	4.177044
203.294690	5970.692779	8.009779	-0.041790	4.179736
203.579966	5978.749506	8.014784	-0.041848	4.182456
203.638224	5986.722646	8.019789	-0.041865	4.185144
203.772691	5994.801395	8.024794	-0.041895	4.187867
203.702518	6002.810417	8.029798	-0.041887	4.190562
204.077479	6010.924492	8.034803	-0.041962	4.193295
204.148667	6018.916207	8.039808	-0.041981	4.195982
204.520466	6026.848703	8.044813	-0.042055	4.198651
204.529024	6034.897386	8.049818	-0.042062	4.201353
204.619774	6042.823952	8.054822	-0.042084	4.204013
204.898889	6050.896894	8.059827	-0.042142	4.206723
205.044089	6058.891689	8.064832	-0.042174	4.209403
205.183819	6066.944976	8.069837	-0.042205	4.212101
205.447059	6074.965190	8.074842	-0.042260	4.214787
205.540418	6082.954698	8.079846	-0.042282	4.217460
205.666747	6090.974492	8.084851	-0.042311	4.220142
205.894250	6098.991741	8.089856	-0.042359	4.222821
206.033473	6106.976576	8.094861	-0.042390	4.225488
206.199209	6115.028465	8.099866	-0.042426	4.228175
206.305115	6123.026412	8.104870	-0.042451	4.230843
206.747219	6131.092774	8.109875	-0.042539	4.233534
206.827034	6139.142121	8.114880	-0.042559	4.236215
206.771642	6147.100999	8.119885	-0.042554	4.238862
206.889220	6155.154758	8.124890	-0.042581	4.241541
206.921785	6163.110816	8.129894	-0.042592	4.244185
207.266377	6171.185314	8.134899	-0.042662	4.246870
207.366797	6179.171216	8.139904	-0.042686	4.249521
207.681065	6187.196697	8.144909	-0.042750	4.252185
208.103823	6195.259215	8.149914	-0.042834	4.254862
207.780702	6203.250326	8.154918	-0.042779	4.257506
207.993854	6211.288288	8.159923	-0.042824	4.260168
208.371334	6219.285396	8.164928	-0.042899	4.262817
208.583256	6227.285469	8.169933	-0.042944	4.265464
208.983594	6235.353640	8.174938	-0.043024	4.268134
209.260246	6243.355586	8.179942	-0.043081	4.270778
209.263522	6251.438872	8.184947	-0.043087	4.273446
209.356395	6259.469959	8.189952	-0.043109	4.276095
209.624994	6267.392559	8.194957	-0.043164	4.278708
209.843859	6275.459824	8.199962	-0.043211	4.281367
209.742132	6283.408491	8.204966	-0.043197	4.283983
210.073371	6291.443123	8.209971	-0.043264	4.286629
210.358978	6299.468808	8.214976	-0.043322	4.289270
210.262201	6307.477709	8.219981	-0.043310	4.291900
210.401864	6315.538917	8.224986	-0.043341	4.294549
210.456860	6323.575833	8.229990	-0.043356	4.297186
210.570807	6331.559149	8.234995	-0.043383	4.299805
210.700121	6339.575601	8.240000	-0.043412	4.302434
210.915880	6347.534881	8.245005	-0.043458	4.305043
211.409624	6355.615560	8.250010	-0.043555	4.307692
211.374492	6363.586896	8.255014	-0.043554	4.310299
211.628619	6371.647048	8.260019	-0.043606	4.312936
211.855524	6379.692803	8.265024	-0.043654	4.315567
211.783110	6387.627059	8.270029	-0.043646	4.318157
211.905994	6395.699417	8.275034	-0.043674	4.320792
212.031319	6403.650311	8.280038	-0.043702	4.323387
212.388894	6411.720610	8.285043	-0.043774	4.326020
212.412792	6419.735305	8.290048	-0.043784	4.328631
212.416208	6427.711178	8.295053	-0.043790	4.331227
212.732582	6435.808856	8.300058	-0.043854	4.333864
212.680346	6443.809101	8.305062	-0.043850	4.336465
212.923850	6451.753035	8.310067	-0.043900	4.339048
213.063407	6459.822287	8.315072	-0.043932	4.341670
213.332897	6467.811967	8.320077	-0.043987	4.344265
213.299190	6475.855207	8.325082	-0.043986	4.346873
213.496632	6483.853233	8.330086	-0.044028	4.349467
214.001923	6491.935630	8.335091	-0.044128	4.352089
214.000265	6500.036251	8.340096	-0.044133	4.354712
214.035564	6507.937386	8.345101	-0.044144	4.357269
214.465566	6515.973452	8.350106	-0.044230	4.359871
214.452005	6523.942037	8.355110	-0.044232	4.362446
214.594979	6531.918092	8.360115	-0.044264	4.365023
214.841999	6539.957871	8.365120	-0.044316	4.367620
214.816998	6547.961258	8.370125	-0.044316	4.370202
214.916641	6556.019329	8.375130	-0.044340	4.372801
215.249114	6564.038163	8.380134	-0.044407	4.375387
215.264207	6572.038649	8.385139	-0.044415	4.377963
215.597981	6580.030278	8.390144	-0.044483	4.380537
215.826351	6588.039334	8.395149	-0.044531	4.383115
216.110647	6596.080375	8.400154	-0.044589	4.385701
215.999087	6604.083710	8.405158	-0.044573	4.388272
216.159829	6612.162803	8.410163	-0.044609	4.390867
216.391854	6620.175446	8.415168	-0.044657	4.393440
216.471935	6628.148743	8.420173	-0.044677	4.395997
216.705881	6636.181608	8.425178	-0.044726	4.398573
216.846505	6644.214992	8.430182	-0.044758	4.401147
216.970222	6652.176359	8.435187	-0.044786	4.403697
217.264640	6660.192318	8.440192	-0.044846	4.406263
217.369238	6668.159492	8.445197	-0.044871	4.408811
217.653801	6676.251584	8.450202	-0.044929	4.411399
217.726298	6684.310818	8.455206	-0.044948	4.413973
217.795628	6692.376801	8.460211	-0.044966	4.416548
218.180036	6700.333053	8.465216	-0.045043	4.419088
218.226388	6708.369688	8.470221	-0.045057	4.421651
218.442478	6716.406512	8.475226	-0.045102	4.424213
218.684488	6724.373178	8.480230	-0.045153	4.426751
218.916197	6732.416298	8.485235	-0.045201	4.429312
219.066066	6740.473203	8.490240	-0.045234	4.431875
219.310712	6748.457857	8.495245	-0.045285	4.434415
219.482437	6756.527828	8.500250	-0.045323	4.436979
219.500091	6764.477797	8.505254	-0.045331	4.439504
219.616352	6772.495914	8.510259	-0.045358	4.442049
220.061409	6780.474894	8.515264	-0.045446	4.444581
220.230627	6788.512494	8.520269	-0.045483	4.447130
220.237277	6796.559852	8.525274	-0.045490	4.449679
220.259824	6804.593878	8.530278	-0.045499	4.452223
220.481003	6812.606324	8.535283	-0.045545	4.454759
220.557127	6820.602522	8.540288	-0.045565	4.457289
220.576582	6828.569411	8.545293	-0.045574	4.459807
220.864166	6836.636451	8.550298	-0.045633	4.462356
220.988172	6844.620149	8.555302	-0.045661	4.464877
221.206971	6852.638984	8.560307	-0.045707	4.467408
221.583474	6860.660655	8.565312	-0.045782	4.469939
221.666238	6868.668536	8.570317	-0.045803	4.472463
221.683814	6876.767957	8.575322	-0.045812	4.475015
221.795122	6884.734101	8.580327	-0.045838	4.477523
222.076715	6892.679126	8.585331	-0.045895	4.480024
222.347487	6900.714229	8.590336	-0.045951	4.482551
222.414485	6908.705400	8.595341	-0.045969	4.485063
222.809821	6916.788249	8.600346	-0.046048	4.487603
222.747909	6924.790831	8.605351	-0.046042	4.490115
222.676607	6932.856695	8.610355	-0.046034	4.492645
222.956593	6940.863993	8.615360	-0.046091	4.495157
222.978545	6948.828465	8.620365	-0.046100	4.497653
223.211471	6956.868240	8.625370	-0.046149	4.500172
223.200659	6964.836978	8.630375	-0.046152	4.502666
223.439526	6972.855873	8.635379	-0.046202	4.505176
223.652517	6980.947475	8.640384	-0.046247	4.507706
223.692005	6988.909259	8.645389	-0.046260	4.510195
223.970503	6997.027494	8.650394	-0.046317	4.512731
224.097511	7005.051576	8.655399	-0.046346	4.515236
224.228355	7012.990055	8.660403	-0.046375	4.517713
224.562343	7020.995512	8.665408	-0.046443	4.520210
224.513476	7028.961254	8.670413	-0.046439	4.522692
224.634223	7036.970252	8.675418	-0.046467	4.525187
224.853971	7044.995072	8.680423	-0.046513	4.527686
225.085957	7052.996232	8.685427	-0.046561	4.530176
225.171654	7061.094248	8.690432	-0.046583	4.532694
225.266844	7069.092241	8.695437	-0.046606	4.535179
225.403844	7077.083349	8.700442	-0.046637	4.537662
225.645235	7085.077261	8.705447	-0.046687	4.540144
225.630654	7093.090221	8.710451	-0.046689	4.542630
225.828066	7101.074157	8.715456	-0.046731	4.545106
226.157775	7109.149481	8.720461	-0.046798	4.547609
226.320851	7117.182875	8.725466	-0.046834	4.550098
226.404275	7125.234254	8.730471	-0.046855	4.552590
226.679271	7133.222545	8.735475	-0.046911	4.555062
226.837597	7141.288543	8.740480	-0.046946	4.557557
226.748300	7149.218669	8.745485	-0.046934	4.560007
226.841668	7157.280652	8.750490	-0.046957	4.562498
226.927855	7165.245961	8.755495	-0.046978	4.564957
227.208848	7173.272544	8.760499	-0.047036	4.567434
227.414648	7181.292738	8.765504	-0.047080	4.569908
227.465725	7189.334113	8.770509	-0.047095	4.572386
227.756449	7197.364903	8.775514	-0.047154	4.574860
227.707968	7205.340348	8.780519	-0.047150	4.577316
227.981567	7213.353640	8.785523	-0.047206	4.579782
228.038228	7221.416627	8.790528	-0.047222	4.582262
228.062183	7229.355068	8.795533	-0.047232	4.584702
228.195418	7237.448962	8.800538	-0.047262	4.587189
228.655615	7245.451017	8.805543	-0.047353	4.589646
228.527649	7253.493269	8.810547	-0.047335	4.592114
228.788645	7261.537103	8.815552	-0.047388	4.594581
229.020754	7269.473357	8.820557	-0.047437	4.597014
229.237806	7277.497511	8.825562	-0.047483	4.599473
229.074201	7285.549937	8.830567	-0.047458	4.601938
229.529373	7293.513196	8.835571	-0.047548	4.604376
229.708698	7301.574985	8.840576	-0.047586	4.606842
229.785156	7309.520698	8.845581	-0.047606	4.609271
229.802349	7317.609651	8.850586	-0.047614	4.611743
230.085573	7325.620091	8.855591	-0.047672	4.614189
230.085207	7333.703437	8.860595	-0.047678	4.616657
230.194906	7341.635547	8.865600	-0.047703	4.619076
230.329625	7349.679417	8.870605	-0.047734	4.621529
230.620870	7357.643690	8.875610	-0.047793	4.623956
230.411325	7365.685678	8.880615	-0.047759	4.626406
230.719367	7373.663649	8.885619	-0.047822	4.628834
230.859371	7381.777109	8.890624	-0.047853	4.631303
230.963415	7389.782976	8.895629	-0.047878	4.633737
231.087779	7397.783888	8.900634	-0.047906	4.636169
231.170174	7405.762253	8.905639	-0.047927	4.638593
231.410826	7413.750287	8.910643	-0.047977	4.641018
231.573553	7421.771245	8.915648	-0.048013	4.643452
231.854894	7429.795735	8.920653	-0.048070	4.645885
232.021852	7437.835587	8.925658	-0.048107	4.648322
232.103919	7445.840330	8.930663	-0.048127	4.650748
232.238717	7453.891728	8.935667	-0.048158	4.653186
232.411458	7461.918638	8.940672	-0.048195	4.655615
232.351745	7469.869547	8.945677	-0.048189	4.658020
232.490611	7477.903752	8.950682	-0.048221	4.660449
232.703332	7485.930085	8.955687	-0.048265	4.662874
232.809305	7493.901331	8.960691	-0.048290	4.665281
232.924536	7501.936783	8.965696	-0.048317	4.667707
233.146711	7509.941738	8.970701	-0.048364	4.670122
233.534168	7518.074912	8.975706	-0.048441	4.672574
233.626342	7526.088861	8.980711	-0.048464	4.674989
233.602034	7534.058738	8.985715	-0.048465	4.677390
233.991515	7541.995406	8.990720	-0.048542	4.679779
233.888046	7550.037451	8.995725	-0.048528	4.682199
234.140901	7558.004595	9.000730	-0.048581	4.684595
234.357438	7566.048434	9.005735	-0.048626	4.687012
234.611385	7574.017746	9.010739	-0.048679	4.689406
234.622255	7582.146786	9.015744	-0.048686	4.691847
234.645715	7590.084547	9.020749	-0.048696	4.694230
234.958413	7598.177086	9.025754	-0.048759	4.696657
235.031371	7606.097368	9.030759	-0.048778	4.699032
234.977928	7614.135452	9.035763	-0.048774	4.701440
235.302756	7622.153203	9.040768	-0.048839	4.703841
235.371297	7630.190019	9.045773	-0.048857	4.706247
235.574866	7638.158928	9.050778	-0.048901	4.708631
235.857557	7646.224457	9.055783	-0.048958	4.711042
235.831877	7654.212420	9.060787	-0.048959	4.713430
236.012561	7662.267759	9.065792	-0.048998	4.715836
236.184000	7670.224724	9.070797	-0.049035	4.718212
236.459865	7678.301750	9.075802	-0.049092	4.720622
236.582235	7686.281195	9.080807	-0.049120	4.723002
236.518807	7694.275653	9.085811	-0.049113	4.725385
236.670743	7702.355713	9.090816	-0.049147	4.727793
236.746401	7710.342797	9.095821	-0.049166	4.730171
236.903251	7718.411278	9.100826	-0.049201	4.732573
237.119580	7726.417324	9.105831	-0.049246	4.734954
237.370597	7734.407879	9.110835	-0.049298	4.737330
237.414239	7742.440405	9.115840	-0.049312	4.739717
237.357164	7750.430783	9.120845	-0.049306	4.742091
237.825423	7758.427437	9.125850	-0.049399	4.744464
237.818848	7766.503241	9.130855	-0.049403	4.746861
237.796174	7774.448206	9.135859	-0.049404	4.749218
238.011779	7782.586155	9.140864	-0.049450	4.751630
238.185714	7790.556093	9.145869	-0.049487	4.753991
238.342481	7798.625820	9.150874	-0.049522	4.756381
238.318575	7806.503493	9.155879	-0.049522	4.758713
238.709677	7814.568255	9.160883	-0.049601	4.761098
238.850897	7822.581444	9.165888	-0.049632	4.763467
238.893029	7830.528815	9.170893	-0.049645	4.765816
238.916877	7838.580320	9.175898	-0.049655	4.768195
238.936572	7846.560727	9.180903	-0.049664	4.770551
239.100128	7854.629449	9.185907	-0.049700	4.772932
239.412494	7862.674548	9.190912	-0.049763	4.775304
239.388213	7870.614520	9.195917	-0.049764	4.777645
239.500353	7878.687351	9.200922	-0.049790	4.780024
239.520405	7886.678201	9.205927	-0.049799	4.782377
239.975023	7894.680002	9.210931	-0.049889	4.784731
240.092445	7902.740681	9.215936	-0.049916	4.787103
240.164817	7910.663564	9.220941	-0.049935	4.789433
240.356650	7918.789625	9.225946	-0.049976	4.791821
240.381935	7926.797319	9.230951	-0.049986	4.794174
240.543531	7934.797136	9.235955	-0.050021	4.796522
240.675839	7942.736678	9.240960	-0.050051	4.798852
240.653441	7950.774670	9.245965	-0.050052	4.801211
240.937309	7958.765901	9.250970	-0.050111	4.803553
241.149115	7966.844207	9.255975	-0.050155	4.805920
241.351130	7974.808110	9.260979	-0.050198	4.808252
241.364421	7982.904158	9.265984	-0.050206	4.810622
241.338521	7990.296171	9.270989	-0.050206	4.812786
241.598443	7994.836666	9.275994	-0.050257	4.814113

241.908688	7997.252822	9.280999	-0.050317	4.814818
241.859598	7998.590650	9.286003	-0.050309	4.815210
241.829424	7999.119664	9.291008	-0.050303	4.815365
241.927889	7999.789569	9.296013	-0.050322	4.815560
241.973309	7999.843692	9.301018	-0.050331	4.815576
241.923948	7999.791651	9.306023	-0.050322	4.815561
242.099622	7999.787033	9.311027	-0.050354	4.815558
242.156191	7999.837067	9.316032	-0.050365	4.815573
242.175118	7999.810689	9.321037	-0.050369	4.815565
242.162318	7999.859597	9.326042	-0.050366	4.815579
242.256194	7999.804542	9.331047	-0.050384	4.815563
242.203289	7999.791946	9.336051	-0.050374	4.815559
242.362407	7999.824426	9.341056	-0.050404	4.815568
242.428287	7999.826568	9.346061	-0.050416	4.815568
242.695568	7999.854398	9.351066	-0.050466	4.815575
242.500414	7999.809600	9.356071	-0.050430	4.815563
242.621536	7999.829720	9.361075	-0.050452	4.815568
242.531828	7999.830405	9.366080	-0.050436	4.815569
242.515517	7999.804523	9.371085	-0.050433	4.815562
242.417315	7999.837099	9.376090	-0.050414	4.815572
242.494245	7999.810595	9.381095	-0.050429	4.815563
242.476213	7999.819917	9.386099	-0.050426	4.815566
242.607637	7999.815649	9.391104	-0.050450	4.815564
242.727736	7999.798386	9.396109	-0.050472	4.815559
242.849142	7999.849472	9.401114	-0.050495	4.815573
242.671309	7999.826307	9.406119	-0.050462	4.815567
242.824308	7999.825593	9.411123	-0.050491	4.815566
242.952775	7999.827683	9.416128	-0.050515	4.815566
242.774100	7999.813045	9.421133	-0.050481	4.815563
242.849309	7999.836691	9.426138	-0.050496	4.815569
242.990407	7999.815499	9.431143	-0.050522	4.815562
242.992752	7999.900953	9.436147	-0.050522	4.815587
242.906911	7999.919850	9.441152	-0.050506	4.815593
242.815635	7999.874602	9.446157	-0.050490	4.815581
243.098316	7999.836490	9.451162	-0.050542	4.815568
243.074786	7999.919389	9.456167	-0.050538	4.815592
242.948138	7999.905595	9.461171	-0.050514	4.815589
243.203678	7999.844622	9.466176	-0.050562	4.815570
243.173584	7999.827057	9.471181	-0.050556	4.815565
243.290566	7999.929319	9.476186	-0.050578	4.815594
243.298573	7999.834435	9.481191	-0.050580	4.815567
243.222540	7999.842815	9.486195	-0.050566	4.815569
243.264162	7999.896878	9.491200	-0.050574	4.815585
243.091979	7999.860992	9.496205	-0.050542	4.815575
243.348501	7999.923882	9.501210	-0.050589	4.815592
243.365523	7999.835550	9.506215	-0.050593	4.815567
243.316473	7999.851841	9.511219	-0.050584	4.815572
243.322512	7999.847674	9.516224	-0.050585	4.815570
243.278368	7999.839490	9.521229	-0.050577	4.815568
243.411566	7999.859807	9.526234	-0.050601	4.815573
243.425098	7999.937970	9.531239	-0.050604	4.815596
243.410979	7999.839524	9.536243	-0.050601	4.815567
243.549805	7999.861000	9.541248	-0.050627	4.815573
243.437105	7999.844229	9.546253	-0.050606	4.815569
243.452331	7999.849820	9.551258	-0.050609	4.815570
243.573696	7999.935072	9.556263	-0.050632	4.815595
243.454038	7999.862671	9.561267	-0.050610	4.815574
243.596666	7999.853248	9.566272	-0.050636	4.815571
243.728027	7999.829762	9.571277	-0.050661	4.815563
243.729597	7999.859687	9.576282	-0.050661	4.815572
243.747495	7999.857848	9.581287	-0.050665	4.815571
243.706241	7999.869996	9.586291	-0.050657	4.815575
243.682954	7999.876029	9.591296	-0.050653	4.815577
243.689086	7999.845173	9.596301	-0.050654	4.815568
243.828694	7999.867730	9.601306	-0.050680	4.815574
243.683547	7999.884597	9.606311	-0.050653	4.815579
243.543954	7999.864186	9.611315	-0.050627	4.815574
243.563480	7999.898673	9.616320	-0.050631	4.815584
243.616085	7999.935833	9.621325	-0.050641	4.815595
243.490690	7999.900706	9.626330	-0.050618	4.815585
243.412094	7999.870609	9.631335	-0.050603	4.815577
243.641711	7999.880748	9.636339	-0.050646	4.815578
243.718583	7999.908693	9.641344	-0.050660	4.815586
243.778635	7999.861629	9.646349	-0.050671	4.815572
243.790669	7999.873574	9.651354	-0.050674	4.815576
243.637019	7999.849732	9.656359	-0.050645	4.815569
243.666125	7999.856616	9.661363	-0.050651	4.815571
243.842425	7999.905393	9.666368	-0.050684	4.815585
243.708213	7999.866919	9.671373	-0.050659	4.815574
243.822803	7999.881597	9.676378	-0.050680	4.815578
243.728949	7999.861929	9.681383	-0.050663	4.815572
243.594670	7999.842672	9.686387	-0.050638	4.815567
243.731435	7999.861980	9.691392	-0.050663	4.815572
243.742982	7999.855767	9.696397	-0.050665	4.815571
244.013915	7999.880457	9.701402	-0.050716	4.815577
243.861975	7999.832087	9.706407	-0.050688	4.815563
243.815269	7999.860161	9.711411	-0.050679	4.815572
243.928145	7999.885487	9.716416	-0.050700	4.815578
243.881034	7999.931705	9.721421	-0.050691	4.815592
243.914886	7999.892757	9.726426	-0.050698	4.815581
243.929978	7999.876992	9.731431	-0.050701	4.815576
243.769569	7999.853041	9.736435	-0.050671	4.815570
243.950217	7999.879468	9.741440	-0.050705	4.815577
243.723878	7999.844836	9.746445	-0.050662	4.815567
243.835426	7999.882953	9.751450	-0.050683	4.815578
243.980690	7999.891723	9.756455	-0.050710	4.815580
243.802014	7999.869610	9.761459	-0.050677	4.815574
244.043689	7999.892757	9.766464	-0.050722	4.815580
243.979505	7999.846879	9.771469	-0.050710	4.815567
244.045437	7999.863970	9.776474	-0.050723	4.815572
243.869198	7999.879264	9.781479	-0.050690	4.815577
244.001734	7999.886760	9.786483	-0.050715	4.815578
243.941943	7999.887930	9.791488	-0.050704	4.815579
243.696005	7999.861522	9.796493	-0.050658	4.815572
243.889164	7999.883881	9.801498	-0.050694	4.815578
243.922410	7999.845991	9.806503	-0.050700	4.815567
243.913415	7999.847986	9.811507	-0.050699	4.815567
244.209295	7999.885893	9.816512	-0.050754	4.815577
244.177109	7999.874699	9.821517	-0.050748	4.815574
244.241645	7999.908850	9.826522	-0.050760	4.815584
244.025871	7999.872255	9.831527	-0.050720	4.815574
243.977252	7999.847982	9.836531	-0.050711	4.815567
244.070084	7999.874051	9.841536	-0.050728	4.815574
243.971122	7999.861774	9.846541	-0.050710	4.815571
243.949306	7999.874237	9.851546	-0.050706	4.815575
244.119494	7999.962419	9.856551	-0.050738	4.815600
244.198531	7999.872956	9.861555	-0.050752	4.815573
244.189342	7999.900572	9.866560	-0.050751	4.815582
244.123417	7999.857868	9.871565	-0.050738	4.815569
244.153400	7999.891458	9.876570	-0.050744	4.815579
244.122063	7999.854654	9.881575	-0.050738	4.815568
243.997402	7999.871854	9.886579	-0.050715	4.815574
244.076941	7999.878489	9.891584	-0.050730	4.815576
244.054305	7999.855706	9.896589	-0.050726	4.815569
244.137954	7999.900844	9.901594	-0.050742	4.815582
244.250546	7999.865310	9.906599	-0.050763	4.815571
244.007557	7999.857099	9.911603	-0.050717	4.815570
244.303468	7999.893939	9.916608	-0.050773	4.815579
244.138785	7999.848564	9.921613	-0.050742	4.815567
244.207692	7999.883854	9.926618	-0.050755	4.815577
244.000739	7999.901852	9.931623	-0.050716	4.815583
244.085518	7999.901099	9.936627	-0.050732	4.815582
244.023545	7999.911843	9.941632	-0.050721	4.815586
244.001676	7999.849569	9.946637	-0.050717	4.815567
243.899178	7999.882075	9.951642	-0.050698	4.815577
244.073153	7999.891312	9.956647	-0.050730	4.815579
244.085565	7999.892586	9.961651	-0.050733	4.815580
243.983055	7999.898401	9.966656	-0.050714	4.815582
244.026772	7999.862816	9.971661	-0.050722	4.815571
244.212116	7999.872237	9.976666	-0.050756	4.815573
244.223432	7999.909795	9.981671	-0.050758	4.815584
244.042443	7999.867358	9.986675	-0.050725	4.815572
244.120755	7999.895326	9.991680	-0.050739	4.815580
244.033248	7999.866152	9.996685	-0.050723	4.815572
244.070562	7999.878508	10.001690	-0.050730	4.815576
244.185074	7999.885711	10.006695	-0.050752	4.815577
244.022334	7999.869194	10.011699	-0.050721	4.815573
244.016120	7999.885114	10.016704	-0.050720	4.815578
244.062928	7999.849579	10.021709	-0.050729	4.815567
244.048148	7999.880307	10.026714	-0.050726	4.815576
244.016204	7999.844561	10.031719	-0.050721	4.815566
244.115301	7999.832296	10.036723	-0.050739	4.815562
244.340387	7999.864783	10.041728	-0.050781	4.815570
244.134309	7999.857172	10.046733	-0.050743	4.815569
244.113212	7999.888865	10.051738	-0.050739	4.815578
244.245092	7999.858982	10.056743	-0.050763	4.815569
244.249466	7999.941269	10.061747	-0.050764	4.815593
244.217986	7999.885244	10.066752	-0.050759	4.815577
244.167791	7999.854540	10.071757	-0.050749	4.815568
244.088765	7999.887428	10.076762	-0.050735	4.815578
244.046956	7999.855792	10.081767	-0.050727	4.815569
244.064510	7999.840068	10.086771	-0.050730	4.815564
244.104680	7999.867417	10.091776	-0.050738	4.815572
243.876208	7999.843428	10.096781	-0.050695	4.815566
244.188367	7999.863449	10.101786	-0.050753	4.815571
244.238956	7999.937945	10.106791	-0.050763	4.815592
244.188401	7999.875205	10.111795	-0.050754	4.815574
244.175077	7999.886739	10.116800	-0.050751	4.815577
244.065748	7999.857210	10.121805	-0.050731	4.815569
244.199178	7999.863653	10.126810	-0.050756	4.815571
244.131105	7999.858282	10.131815	-0.050743	4.815569
244.121733	7999.856000	10.136819	-0.050742	4.815569
244.222506	7999.866183	10.141824	-0.050760	4.815571
244.184474	7999.841015	10.146829	-0.050753	4.815564
244.147550	7999.873519	10.151834	-0.050747	4.815574
244.191417	7999.855019	10.156839	-0.050755	4.815568
244.267539	7999.849854	10.161843	-0.050769	4.815566
244.424086	7999.868417	10.166848	-0.050798	4.815571
244.336310	7999.826426	10.171853	-0.050782	4.815559
244.376658	7999.847372	10.176858	-0.050789	4.815565
244.368824	7999.854724	10.181863	-0.050788	4.815567
244.261733	7999.859397	10.186867	-0.050768	4.815569
244.351010	7999.883273	10.191872	-0.050785	4.815576
244.186197	7999.867790	10.196877	-0.050754	4.815572
244.247556	7999.889078	10.201882	-0.050766	4.815578
244.321395	7999.855049	10.206887	-0.050780	4.815567
244.211094	7999.961098	10.211891	-0.050759	4.815599
244.372827	7999.882587	10.216896	-0.050789	4.815575
244.219592	7999.829924	10.221901	-0.050761	4.815561
244.472420	7999.847915	10.226906	-0.050808	4.815565
244.421293	7999.866309	10.231911	-0.050798	4.815570
244.350025	7999.853412	10.236915	-0.050785	4.815567
244.335083	7999.862784	10.241920	-0.050783	4.815570
244.369276	7999.846262	10.246925	-0.050789	4.815565
244.298779	7999.852597	10.251930	-0.050776	4.815567
244.425023	7999.898427	10.256935	-0.050800	4.815580
244.548985	7999.870551	10.261939	-0.050823	4.815571
244.480860	7999.865179	10.266944	-0.050810	4.815570
244.363294	7999.861140	10.271949	-0.050788	4.815569
244.480797	7999.874799	10.276954	-0.050810	4.815572
244.481730	7999.854534	10.281959	-0.050810	4.815567
244.294840	7999.851504	10.286963	-0.050776	4.815567
244.307436	7999.890150	10.291968	-0.050778	4.815578
244.489494	7999.842932	10.296973	-0.050812	4.815563
244.444995	7999.891328	10.301978	-0.050804	4.815577
244.532618	7999.878877	10.306983	-0.050820	4.815573
244.693244	7999.862273	10.311987	-0.050850	4.815568
244.564549	7999.886880	10.316992	-0.050826	4.815576
244.597514	7999.869271	10.321997	-0.050832	4.815570
244.667278	7999.884289	10.327002	-0.050846	4.815574
244.541666	7999.881187	10.332007	-0.050822	4.815574
244.400740	7999.859686	10.337011	-0.050796	4.815568
244.408934	7999.875839	10.342016	-0.050798	4.815573
244.315496	7999.849771	10.347021	-0.050780	4.815566
244.256222	7999.868032	10.352026	-0.050769	4.815572
244.417114	7999.865312	10.357031	-0.050799	4.815570
244.378434	7999.942629	10.362035	-0.050792	4.815593
244.405314	7999.882214	10.367040	-0.050797	4.815575
244.343858	7999.872680	10.372045	-0.050786	4.815572
244.323093	7999.876619	10.377050	-0.050782	4.815574
244.303583	7999.881646	10.382055	-0.050779	4.815575
244.272777	7999.842716	10.387059	-0.050773	4.815564
244.564354	7999.867742	10.392064	-0.050827	4.815570
244.504226	7999.860365	10.397069	-0.050816	4.815568
244.432980	7999.878432	10.402074	-0.050803	4.815574
244.615784	7999.872865	10.407079	-0.050837	4.815571
244.653794	7999.866014	10.412083	-0.050844	4.815569
244.686553	7999.869755	10.417088	-0.050850	4.815570
244.495831	7999.853851	10.422093	-0.050815	4.815566
244.457376	7999.889532	10.427098	-0.050808	4.815577
244.365524	7999.881640	10.432103	-0.050791	4.815575
244.162036	7999.867665	10.437107	-0.050753	4.815572
244.309186	7999.883939	10.442112	-0.050780	4.815576
244.429603	7999.850668	10.447117	-0.050803	4.815566
244.336094	7999.867305	10.452122	-0.050785	4.815571
244.368363	7999.839007	10.457127	-0.050791	4.815562
244.588808	7999.909856	10.462131	-0.050833	4.815582
244.517913	7999.857462	10.467136	-0.050819	4.815567
244.493021	7999.858131	10.472141	-0.050815	4.815567
244.524781	7999.870397	10.477146	-0.050821	4.815571
244.641789	7999.868032	10.482151	-0.050843	4.815570
244.524025	7999.845839	10.487155	-0.050821	4.815564
244.538260	7999.865294	10.492160	-0.050824	4.815569
244.796562	7999.831059	10.497165	-0.050872	4.815558
244.759267	7999.849677	10.502170	-0.050865	4.815564
244.666679	7999.962420	10.507175	-0.050848	4.815597
244.533398	7999.837478	10.512179	-0.050823	4.815561
244.611946	7999.880398	10.517184	-0.050838	4.815573
244.560718	7999.845407	10.522189	-0.050828	4.815563
244.608720	7999.865410	10.527194	-0.050837	4.815569
244.669765	7999.864271	10.532199	-0.050849	4.815568
244.477100	7999.849404	10.537203	-0.050813	4.815565
244.514215	7999.866027	10.542208	-0.050820	4.815570
244.825773	7999.848672	10.547213	-0.050878	4.815563
244.811157	7999.884741	10.552218	-0.050875	4.815574
244.803367	7999.879281	10.557223	-0.050874	4.815572
244.762588	7999.867948	10.562227	-0.050866	4.815569
244.774506	7999.868147	10.567232	-0.050869	4.815569
244.762031	7999.854070	10.572237	-0.050866	4.815565
244.679161	7999.854865	10.577242	-0.050851	4.815566
244.730321	7999.870649	10.582247	-0.050861	4.815570
244.582015	7999.831945	10.587251	-0.050833	4.815559
244.764639	7999.855202	10.592256	-0.050867	4.815565
244.688910	7999.851843	10.597261	-0.050853	4.815565
244.555466	7999.953245	10.602266	-0.050828	4.815595
244.605765	7999.878263	10.607271	-0.050838	4.815573
244.560862	7999.870065	10.612275	-0.050829	4.815571
244.707128	7999.824401	10.617280	-0.050857	4.815557
244.633813	7999.834960	10.622285	-0.050843	4.815560
244.652111	7999.845940	10.627290	-0.050846	4.815563
244.841704	7999.861837	10.632295	-0.050882	4.815567
244.849617	7999.853430	10.637299	-0.050883	4.815564
244.837232	7999.880994	10.642304	-0.050881	4.815572
244.914227	7999.948446	10.647309	-0.050896	4.815592
244.921272	7999.873828	10.652314	-0.050897	4.815570
244.946961	7999.876387	10.657319	-0.050902	4.815571
244.761699	7999.872315	10.662323	-0.050867	4.815570
244.963686	7999.894820	10.667328	-0.050905	4.815576
244.808700	7999.863481	10.672333	-0.050876	4.815567
244.719292	7999.868440	10.677338	-0.050860	4.815569
244.829329	7999.881977	10.682343	-0.050880	4.815573
244.613603	7999.868870	10.687347	-0.050840	4.815570
244.694737	7999.876599	10.692352	-0.050855	4.815572
244.717624	7999.849217	10.697357	-0.050860	4.815564
244.856050	7999.865351	10.702362	-0.050885	4.815568
244.855651	7999.873891	10.707367	-0.050885	4.815570
244.874309	7999.872065	10.712371	-0.050889	4.815570
245.009229	7999.894548	10.717376	-0.050914	4.815576
244.785958	7999.843949	10.722381	-0.050873	4.815562
244.671308	7999.852769	10.727386	-0.050851	4.815565
244.793601	7999.875047	10.732391	-0.050874	4.815571
245.027907	7999.855369	10.737395	-0.050918	4.815564
244.981855	7999.883454	10.742400	-0.050909	4.815572
244.907780	7999.849158	10.747405	-0.050896	4.815563
244.676962	7999.881716	10.752410	-0.050853	4.815573
244.961820	7999.864995	10.757415	-0.050906	4.815567
244.679226	7999.847598	10.762419	-0.050853	4.815563
244.808633	7999.895616	10.767424	-0.050877	4.815577
244.858169	7999.881478	10.772429	-0.050887	4.815572
244.743519	7999.905246	10.777434	-0.050865	4.815580
244.801947	7999.865629	10.782439	-0.050876	4.815568
244.928252	7999.849535	10.787443	-0.050900	4.815563
245.062213	7999.876274	10.792448	-0.050925	4.815570
244.790090	7999.943393	10.797453	-0.050874	4.815591
244.951943	7999.883035	10.802458	-0.050905	4.815572
244.810288	7999.875401	10.807463	-0.050878	4.815571
244.848193	7999.861075	10.812467	-0.050885	4.815567
244.933136	7999.903032	10.817472	-0.050901	4.815578
244.740105	7999.858263	10.822477	-0.050865	4.815566
244.846784	7999.887761	10.827482	-0.050885	4.815574
244.854862	7999.854799	10.832487	-0.050887	4.815565
244.957810	7999.857545	10.837491	-0.050906	4.815565
244.837232	7999.883351	10.842496	-0.050884	4.815573
244.752476	7999.869168	10.847501	-0.050868	4.815569
244.833729	7999.850208	10.852506	-0.050883	4.815563
244.749040	7999.891545	10.857511	-0.050868	4.815576
244.590293	7999.849468	10.862515	-0.050838	4.815564
244.786442	7999.878284	10.867520	-0.050875	4.815572
244.949093	7999.844630	10.872525	-0.050905	4.815561
244.916454	7999.872933	10.877530	-0.050899	4.815570
244.927907	7999.856041	10.882535	-0.050901	4.815565
244.992462	7999.825065	10.887539	-0.050913	4.815555
245.162691	7999.871611	10.892544	-0.050945	4.815568
245.022712	7999.923795	10.897549	-0.050919	4.815584
245.093165	7999.854477	10.902554	-0.050932	4.815563
245.159868	7999.860905	10.907559	-0.050945	4.815565
244.863729	7999.865709	10.912563	-0.050890	4.815568
244.815267	7999.878807	10.917568	-0.050881	4.815572
245.046800	7999.865491	10.922573	-0.050924	4.815567
244.782334	7999.870810	10.927578	-0.050875	4.815570
244.834767	7999.859923	10.932583	-0.050884	4.815566
244.901148	7999.846059	10.937587	-0.050897	4.815562
244.915435	7999.887936	10.942592	-0.050900	4.815574
244.759543	7999.853379	10.947597	-0.050871	4.815565
244.938615	7999.865902	10.952602	-0.050904	4.815567
245.107336	7999.864378	10.957607	-0.050935	4.815566
244.957481	7999.841663	10.962611	-0.050908	4.815560
245.056855	7999.907344	10.967616	-0.050926	4.815579
244.911558	7999.907125	10.972621	-0.050899	4.815580
245.033450	7999.849320	10.977626	-0.050922	4.815562
245.066127	7999.876549	10.982631	-0.050928	4.815570
244.839515	7999.852587	10.987635	-0.050886	4.815564
244.926850	7999.862553	10.992640	-0.050902	4.815567
244.749514	7999.846866	10.997645	-0.050869	4.815563
244.795582	7999.858296	11.002650	-0.050878	4.815566
244.941455	7999.879890	11.007655	-0.050905	4.815572
244.918321	7999.842150	11.012659	-0.050901	4.815561
244.910876	7999.865524	11.017664	-0.050900	4.815567
244.895429	7999.854602	11.022669	-0.050897	4.815564
244.964744	7999.840786	11.027674	-0.050910	4.815560
244.750393	7999.876814	11.032679	-0.050870	4.815572
244.879197	7999.857558	11.037683	-0.050894	4.815565
245.050620	7999.952169	11.042688	-0.050926	4.815592
244.912969	7999.863456	11.047693	-0.050900	4.815567
244.891253	7999.869515	11.052698	-0.050896	4.815569
245.054518	7999.877511	11.057703	-0.050927	4.815570
245.066301	7999.826459	11.062707	-0.050929	4.815555
245.073447	7999.872491	11.067712	-0.050931	4.815569
245.001247	7999.878798	11.072717	-0.050917	4.815571
245.074922	7999.869323	11.077722	-0.050931	4.815568
244.836495	7999.890012	11.082727	-0.050887	4.815575
244.960606	7999.864274	11.087731	-0.050910	4.815567
244.984930	7999.860404	11.092736	-0.050914	4.815566
244.869400	7999.843586	11.097741	-0.050893	4.815561
245.032362	7999.885743	11.102746	-0.050923	4.815573
245.175799	7999.869928	11.107751	-0.050950	4.815567
245.022770	7999.848229	11.112755	-0.050922	4.815562
245.054339	7999.885049	11.117760	-0.050928	4.815572
245.246274	7999.875360	11.122765	-0.050963	4.815569
244.952965	7999.880210	11.127770	-0.050909	4.815572
245.158819	7999.958298	11.132775	-0.050947	4.815593
245.217370	7999.853553	11.137779	-0.050958	4.815562
245.113412	7999.883901	11.142784	-0.050939	4.815572
245.038105	7999.864532	11.147789	-0.050925	4.815567
244.726503	7999.886168	11.152794	-0.050867	4.815574
244.967546	7999.880480	11.157799	-0.050912	4.815572
244.887068	7999.871705	11.162803	-0.050897	4.815569
244.994937	7999.898019	11.167808	-0.050917	4.815577
244.920787	7999.870128	11.172813	-0.050903	4.815569
245.112280	7999.874312	11.177818	-0.050939	4.815569
245.021406	7999.886721	11.182823	-0.050922	4.815573
244.983908	7999.850884	11.187827	-0.050915	4.815563
245.095090	7999.888997	11.192832	-0.050936	4.815573
245.035153	7999.872014	11.197837	-0.050925	4.815569
245.018767	7999.867482	11.202842	-0.050922	4.815567
245.238089	7999.884931	11.207847	-0.050963	4.815572
245.001687	7999.858675	11.212851	-0.050919	4.815565
244.941987	7999.886538	11.217856	-0.050908	4.815573
244.900811	7999.853844	11.222861	-0.050900	4.815564
244.899667	7999.835681	11.227866	-0.050900	4.815559
244.970371	7999.859256	11.232871	-0.050913	4.815565
244.890866	7999.939114	11.237875	-0.050899	4.815589
244.938284	7999.849137	11.242880	-0.050908	4.815562
244.976305	7999.861504	11.247885	-0.050915	4.815566
244.920800	7999.873420	11.252890	-0.050905	4.815570
244.891981	7999.887905	11.257895	-0.050899	4.815574
244.780007	7999.858332	11.262899	-0.050878	4.815566
244.836231	7999.879537	11.267904	-0.050889	4.815572
244.959500	7999.869801	11.272909	-0.050912	4.815568
245.043426	7999.873305	11.277914	-0.050928	4.815569
245.103407	7999.868946	11.282919	-0.050939	4.815567
245.098181	7999.827227	11.287923	-0.050938	4.815555
245.030195	7999.849618	11.292928	-0.050925	4.815562
245.098462	7999.850732	11.297933	-0.050938	4.815562
245.068274	7999.874804	11.302938	-0.050933	4.815569
245.107620	7999.957661	11.307943	-0.050940	4.815593
245.208951	7999.846137	11.312947	-0.050959	4.815560
245.229024	7999.889177	11.317952	-0.050963	4.815573
244.805868	7999.873767	11.322957	-0.050884	4.815570
244.953175	7999.852676	11.327962	-0.050911	4.815563
245.036191	7999.883925	11.332967	-0.050927	4.815572
245.016189	7999.864388	11.337971	-0.050923	4.815567
245.102012	7999.902089	11.342976	-0.050939	4.815577
245.232190	7999.857231	11.347981	-0.050964	4.815563
245.153276	7999.880511	11.352986	-0.050949	4.815571
245.245102	7999.872399	11.357991	-0.050966	4.815568
245.059199	7999.864046	11.362995	-0.050932	4.815566
244.995742	7999.902525	11.368000	-0.050920	4.815578
245.247499	7999.874590	11.373005	-0.050967	4.815568
245.140243	7999.858974	11.378010	-0.050947	4.815564
245.181176	7999.900216	11.383015	-0.050955	4.815576
244.978037	7999.869162	11.388019	-0.050917	4.815568
245.158172	7999.899854	11.393024	-0.050951	4.815576
245.141591	7999.868627	11.398029	-0.050947	4.815567
245.132016	7999.879154	11.403034	-0.050946	4.815570
245.130274	7999.889808	11.408039	-0.050946	4.815573
245.124599	7999.886518	11.413043	-0.050945	4.815572
245.116888	7999.888534	11.418048	-0.050943	4.815573
245.222212	7999.878506	11.423053	-0.050963	4.815570
245.213929	7999.864497	11.428058	-0.050961	4.815566
245.187719	7999.882227	11.433063	-0.050957	4.815571
245.151966	7999.864569	11.438067	-0.050950	4.815566
245.329167	7999.872792	11.443072	-0.050983	4.815567
245.293687	7999.851935	11.448077	-0.050976	4.815562
245.168333	7999.849904	11.453082	-0.050953	4.815562
245.353289	7999.873201	11.458087	-0.050988	4.815567
245.350761	7999.936159	11.463091	-0.050987	4.815586
245.465950	7999.854756	11.468096	-0.051009	4.815562
245.396606	7999.853635	11.473101	-0.050996	4.815562
245.181760	7999.866165	11.478106	-0.050956	4.815566
245.260244	7999.867446	11.483111	-0.050971	4.815566
245.086437	7999.853951	11.488115	-0.050938	4.815563
245.244376	7999.871470	11.493120	-0.050968	4.815567
245.278179	7999.846400	11.498125	-0.050974	4.815560
245.186818	7999.870546	11.503130	-0.050957	4.815567
245.266163	7999.872908	11.508135	-0.050972	4.815568
245.307080	7999.866105	11.513139	-0.050980	4.815566
245.196476	7999.879261	11.518144	-0.050959	4.815570
245.396135	7999.863292	11.523149	-0.050996	4.815564
245.222762	7999.860481	11.528154	-0.050964	4.815564
245.396517	7999.880393	11.533159	-0.050997	4.815569
245.547914	7999.933040	11.538163	-0.051025	4.815584
245.444596	7999.870508	11.543168	-0.051006	4.815566
245.418143	7999.853000	11.548173	-0.051001	4.815561
245.361855	7999.871310	11.553178	-0.050990	4.815567
245.369716	7999.892797	11.558183	-0.050992	4.815573
245.365227	7999.857496	11.563187	-0.050991	4.815563
245.434954	7999.875717	11.568192	-0.051004	4.815568
245.379901	7999.855610	11.573197	-0.050994	4.815562
245.289576	7999.853080	11.578202	-0.050977	4.815562
245.228622	7999.857434	11.583207	-0.050966	4.815563
245.109739	7999.855509	11.588211	-0.050944	4.815563
245.159736	7999.881951	11.593216	-0.050953	4.815571
245.316904	7999.887713	11.598221	-0.050983	4.815572
245.229045	7999.854260	11.603226	-0.050966	4.815562
245.403874	7999.881663	11.608231	-0.050999	4.815570
245.328414	7999.838803	11.613235	-0.050985	4.815557
245.319322	7999.861082	11.618240	-0.050983	4.815564
245.318194	7999.846122	11.623245	-0.050983	4.815560
245.429050	7999.947224	11.628250	-0.051004	4.815589
245.451880	7999.898486	11.633255	-0.051008	4.815574
245.238236	7999.867261	11.638259	-0.050969	4.815566
245.363290	7999.871433	11.643264	-0.050992	4.815567
245.265787	7999.868787	11.648269	-0.050974	4.815567
245.056121	7999.846168	11.653274	-0.050935	4.815561
245.127973	7999.863356	11.658279	-0.050948	4.815566
245.264259	7999.847425	11.663283	-0.050974	4.815560
245.108348	7999.863049	11.668288	-0.050945	4.815566
245.022522	7999.840306	11.673293	-0.050929	4.815559
244.982211	7999.844996	11.678298	-0.050921	4.815561
245.187753	7999.877168	11.683303	-0.050960	4.815569
245.176079	7999.858833	11.688307	-0.050958	4.815564
245.259956	7999.883690	11.693312	-0.050973	4.815571
245.405201	7999.965065	11.698317	-0.051000	4.815594
245.387344	7999.871891	11.703322	-0.050997	4.815567
245.244270	7999.895197	11.708327	-0.050971	4.815574
245.281340	7999.872315	11.713331	-0.050978	4.815567
245.509068	7999.898443	11.718336	-0.051020	4.815574
245.323678	7999.870879	11.723341	-0.050986	4.815567
245.175848	7999.861009	11.728346	-0.050958	4.815565
245.320636	7999.870841	11.733351	-0.050985	4.815567
245.289516	7999.846851	11.738355	-0.050979	4.815560
245.160367	7999.851165	11.743360	-0.050955	4.815562
245.150194	7999.853141	11.748365	-0.050954	4.815562
245.367091	7999.852399	11.753370	-0.050994	4.815561
245.369510	7999.864189	11.758375	-0.050994	4.815565
245.180229	7999.863254	11.763379	-0.050959	4.815565
245.372414	7999.879195	11.768384	-0.050995	4.815569
245.352241	7999.871399	11.773389	-0.050991	4.815567
245.094429	7999.869351	11.778394	-0.050944	4.815567
245.161989	7999.885402	11.783399	-0.050956	4.815572
245.174644	7999.854650	11.788403	-0.050959	4.815563
245.063058	7999.878467	11.793408	-0.050938	4.815570
245.237823	7999.864229	11.798413	-0.050970	4.815565
245.379509	7999.854792	11.803418	-0.050997	4.815562
245.252276	7999.865543	11.808423	-0.050973	4.815566
245.176080	7999.943319	11.813427	-0.050959	4.815589
245.389855	7999.898752	11.818432	-0.050999	4.815575
245.286634	7999.890674	11.823437	-0.050980	4.815573
245.041669	7999.870685	11.828442	-0.050934	4.815568
245.133817	7999.890338	11.833447	-0.050952	4.815573
245.101069	7999.859916	11.838451	-0.050946	4.815565
245.078575	7999.863827	11.843456	-0.050941	4.815566
245.165214	7999.855631	11.848461	-0.050958	4.815563
245.221434	7999.848009	11.853466	-0.050968	4.815561
245.207836	7999.870215	11.858471	-0.050966	4.815567
245.180556	7999.864439	11.863475	-0.050961	4.815566
245.178878	7999.864417	11.868480	-0.050960	4.815566
245.232651	7999.889853	11.873485	-0.050970	4.815573
245.234591	7999.866401	11.878490	-0.050971	4.815566
245.352988	7999.879007	11.883495	-0.050993	4.815569
245.391027	7999.848667	11.888499	-0.051000	4.815560
245.087109	7999.875766	11.893504	-0.050944	4.815569
245.106100	7999.868606	11.898509	-0.050947	4.815567
245.112576	7999.836687	11.903514	-0.050948	4.815558
245.276589	7999.885267	11.908519	-0.050979	4.815571
245.184516	7999.858152	11.913523	-0.050962	4.815564
245.115074	7999.884790	11.918528	-0.050949	4.815572
245.324692	7999.867915	11.923533	-0.050988	4.815566
245.316577	7999.880601	11.928538	-0.050987	4.815570
245.283474	7999.891813	11.933543	-0.050981	4.815573
245.139711	7999.872400	11.938547	-0.050954	4.815568
245.305947	7999.884716	11.943552	-0.050985	4.815571
245.271736	7999.890571	11.948557	-0.050979	4.815573
245.202983	7999.937506	11.953562	-0.050966	4.815587
245.371112	7999.865505	11.958567	-0.050997	4.815565
245.201680	7999.867028	11.963571	-0.050966	4.815566
245.171806	7999.883632	11.968576	-0.050960	4.815571
245.390638	7999.869042	11.973581	-0.051001	4.815566
245.275602	7999.868246	11.978586	-0.050980	4.815566
245.348398	7999.885450	11.983591	-0.050993	4.815571
245.149835	7999.864079	11.988595	-0.050957	4.815566
245.106062	7999.877253	11.993600	-0.050948	4.815570
245.280554	7999.881161	11.998605	-0.050981	4.815570
245.233854	7999.854783	12.003610	-0.050972	4.815562
245.342397	7999.875771	12.008615	-0.050993	4.815568
245.174204	7999.867705	12.013619	-0.050961	4.815567
245.389630	7999.897903	12.018624	-0.051002	4.815574
245.384588	7999.878608	12.023629	-0.051001	4.815569
245.397613	7999.854269	12.028634	-0.051003	4.815562
245.358305	7999.871786	12.033639	-0.050996	4.815567
245.366716	7999.840965	12.038643	-0.050998	4.815558
245.285283	7999.872746	12.043648	-0.050982	4.815567
245.159207	7999.874974	12.048653	-0.050959	4.815569
245.198778	7999.863878	12.053658	-0.050966	4.815565
245.241477	7999.879525	12.058663	-0.050974	4.815570
245.274513	7999.864052	12.063667	-0.050981	4.815565
245.287755	7999.874950	12.068672	-0.050983	4.815568
245.379540	7999.878582	12.073677	-0.051000	4.815569
245.231039	7999.858024	12.078682	-0.050973	4.815563
245.243234	7999.883852	12.083687	-0.050975	4.815571
245.444746	7999.914892	12.088691	-0.051013	4.815579
245.353527	7999.838677	12.093696	-0.050996	4.815557
245.424889	7999.868670	12.098701	-0.051009	4.815566
245.281216	7999.853529	12.103706	-0.050982	4.815562
245.287655	7999.884602	12.108711	-0.050984	4.815571
245.265539	7999.870368	12.113715	-0.050980	4.815567
245.383760	7999.850941	12.118720	-0.051002	4.815561
245.604796	7999.865214	12.123725	-0.051043	4.815564
245.587411	7999.884156	12.128730	-0.051040	4.815569
245.639328	7999.886073	12.133735	-0.051050	4.815570
245.669490	7999.950631	12.138739	-0.051055	4.815588
245.638796	7999.872195	12.143744	-0.051050	4.815566
245.428857	7999.867722	12.148749	-0.051011	4.815565
245.191107	7999.829699	12.153754	-0.050966	4.815555
245.352519	7999.872899	12.158759	-0.050996	4.815567
245.319109	7999.844602	12.163763	-0.050990	4.815559
245.369836	7999.872124	12.168768	-0.051000	4.815567
245.424589	7999.857004	12.173773	-0.051010	4.815562
245.410198	7999.836489	12.178778	-0.051007	4.815556
245.360332	7999.876257	12.183783	-0.050998	4.815568
245.414034	7999.944400	12.188787	-0.051008	4.815588
245.360329	7999.861320	12.193792	-0.050998	4.815564
245.397511	7999.873675	12.198797	-0.051005	4.815567
245.236414	7999.851844	12.203802	-0.050975	4.815562
245.588561	7999.876790	12.208807	-0.051041	4.815567
245.447082	7999.841398	12.213811	-0.051015	4.815557
245.319599	7999.871363	12.218816	-0.050991	4.815567
245.513760	7999.854237	12.223821	-0.051027	4.815561
245.398197	7999.854501	12.228826	-0.051006	4.815562
245.352575	7999.886863	12.233831	-0.050997	4.815571
245.469767	7999.877028	12.238835	-0.051019	4.815568
245.280601	7999.902788	12.243840	-0.050984	4.815576
245.232581	7999.879592	12.248845	-0.050975	4.815570
245.455185	7999.865064	12.253850	-0.051017	4.815564
245.785095	7999.873633	12.258855	-0.051078	4.815565
245.591809	7999.931357	12.263859	-0.051042	4.815583
245.366877	7999.868984	12.268864	-0.051001	4.815566
245.430878	7999.861488	12.273869	-0.051012	4.815563
245.451939	7999.854362	12.278874	-0.051016	4.815561
245.375970	7999.881961	12.283879	-0.051002	4.815570
245.421105	7999.867752	12.288883	-0.051011	4.815565
245.468325	7999.879202	12.293888	-0.051020	4.815568
245.643198	7999.878846	12.298893	-0.051052	4.815567
245.500184	7999.862647	12.303898	-0.051026	4.815563
245.546240	7999.884755	12.308903	-0.051034	4.815570
245.506779	7999.856359	12.313907	-0.051027	4.815562
245.670163	7999.837666	12.318912	-0.051058	4.815555
245.718127	7999.853398	12.323917	-0.051067	4.815560
245.429964	7999.862602	12.328922	-0.051013	4.815564
245.325486	7999.884399	12.333927	-0.050994	4.815571
245.428037	7999.858311	12.338931	-0.051013	4.815562
245.551905	7999.894495	12.343936	-0.051036	4.815572
245.648420	7999.893934	12.348941	-0.051054	4.815572
245.297519	7999.878629	12.353946	-0.050989	4.815569
245.488852	7999.891352	12.358951	-0.051024	4.815572
245.424768	7999.861489	12.363955	-0.051012	4.815563
245.373660	7999.867070	12.368960	-0.051003	4.815565
245.440730	7999.970664	12.373965	-0.051016	4.815595
245.623851	7999.844454	12.378970	-0.051050	4.815557
245.709659	7999.871478	12.383975	-0.051066	4.815565
245.604324	7999.853757	12.388979	-0.051046	4.815560
245.638262	7999.879939	12.393984	-0.051053	4.815568
245.513672	7999.861904	12.398989	-0.051029	4.815563
245.367664	7999.870215	12.403994	-0.051002	4.815566
245.686579	7999.913839	12.408999	-0.051062	4.815577
245.386372	7999.868394	12.414003	-0.051006	4.815566
245.409012	7999.866632	12.419008	-0.051010	4.815565
245.654647	7999.866358	12.424013	-0.051056	4.815564
245.613082	7999.862485	12.429018	-0.051048	4.815563
245.586513	7999.885549	12.434023	-0.051044	4.815570
245.527665	7999.849364	12.439027	-0.051033	4.815559
245.520811	7999.883424	12.444032	-0.051031	4.815569
245.709363	7999.897171	12.449037	-0.051067	4.815572
245.681061	7999.861482	12.454042	-0.051061	4.815562
245.752079	7999.885064	12.459047	-0.051075	4.815569
245.712093	7999.871607	12.464051	-0.051067	4.815565
245.604906	7999.963829	12.469056	-0.051047	4.815592
245.447708	7999.883338	12.474061	-0.051018	4.815570
245.495684	7999.873446	12.479066	-0.051027	4.815567
245.500704	7999.883142	12.484071	-0.051028	4.815569
245.441524	7999.859765	12.489075	-0.051017	4.815563
245.644233	7999.878012	12.494080	-0.051055	4.815567
245.767012	7999.888554	12.499085	-0.051078	4.815570
245.565676	7999.866069	12.504090	-0.051041	4.815564
245.602829	7999.901913	12.509095	-0.051048	4.815574
245.474523	7999.860328	12.514099	-0.051024	4.815563
245.365026	7999.886315	12.519104	-0.051003	4.815571
245.455343	7999.882450	12.524109	-0.051020	4.815569
245.501171	7999.835153	12.529114	-0.051029	4.815555
245.523073	7999.856869	12.534119	-0.051033	4.815562
245.513671	7999.870602	12.539123	-0.051031	4.815566
245.586593	7999.881401	12.544128	-0.051045	4.815568
245.631010	7999.915228	12.549133	-0.051053	4.815578
245.411034	7999.896711	12.554138	-0.051012	4.815574
245.484233	7999.903244	12.559143	-0.051026	4.815575
245.439581	7999.845936	12.564147	-0.051018	4.815559
245.400205	7999.867724	12.569152	-0.051011	4.815565
245.562485	7999.879975	12.574157	-0.051041	4.815568
245.289670	7999.860601	12.579162	-0.050990	4.815564
245.592193	7999.909297	12.584167	-0.051047	4.815577
245.563531	7999.856520	12.589171	-0.051041	4.815561
245.653958	7999.874010	12.594176	-0.051058	4.815566
245.890488	7999.975021	12.599181	-0.051102	4.815594
245.734367	7999.856109	12.604186	-0.051073	4.815560
245.802750	7999.861497	12.609191	-0.051086	4.815562
245.633753	7999.843808	12.614195	-0.051055	4.815557
245.621423	7999.847884	12.619200	-0.051052	4.815558
245.703848	7999.868448	12.624205	-0.051068	4.815564
245.671074	7999.852973	12.629210	-0.051062	4.815560
245.824807	7999.919539	12.634215	-0.051090	4.815578
245.760735	7999.871524	12.639219	-0.051079	4.815565
245.760056	7999.870451	12.644224	-0.051079	4.815564
245.829045	7999.904677	12.649229	-0.051091	4.815574
245.485899	7999.896971	12.654234	-0.051028	4.815573
245.625088	7999.904577	12.659239	-0.051054	4.815575
245.458684	7999.864509	12.664243	-0.051023	4.815564
245.695876	7999.888655	12.669248	-0.051067	4.815570
245.622018	7999.889596	12.674253	-0.051053	4.815571
245.538459	7999.855145	12.679258	-0.051038	4.815561
245.701207	7999.875946	12.684263	-0.051068	4.815566
245.982518	7999.854898	12.689267	-0.051120	4.815559
245.673442	7999.880844	12.694272	-0.051063	4.815568
245.899467	7999.884523	12.699277	-0.051105	4.815568
245.650299	7999.867667	12.704282	-0.051059	4.815564
245.630852	7999.891914	12.709287	-0.051055	4.815571
245.643627	7999.864366	12.714291	-0.051058	4.815563
245.721831	7999.968143	12.719296	-0.051072	4.815593
245.607637	7999.906501	12.724301	-0.051051	4.815576
245.409358	7999.856306	12.729306	-0.051014	4.815562
245.597951	7999.880730	12.734311	-0.051049	4.815568
245.567827	7999.856756	12.739315	-0.051044	4.815561
245.677492	7999.863882	12.744320	-0.051064	4.815563
245.728444	7999.902086	12.749325	-0.051074	4.815574
245.535120	7999.843429	12.754330	-0.051038	4.815557
245.680466	7999.888505	12.759335	-0.051065	4.815570
245.566594	7999.869577	12.764339	-0.051044	4.815565
245.621448	7999.848052	12.769344	-0.051054	4.815558
245.652913	7999.869923	12.774349	-0.051060	4.815565
245.561117	7999.860963	12.779354	-0.051043	4.815562
245.699087	7999.872819	12.784359	-0.051069	4.815565
245.554276	7999.868336	12.789363	-0.051042	4.815565
245.350396	7999.869300	12.794368	-0.051004	4.815566
245.626689	7999.889811	12.799373	-0.051056	4.815571
245.478768	7999.883142	12.804378	-0.051028	4.815569
245.681500	7999.887509	12.809383	-0.051066	4.815570
245.561902	7999.880233	12.814387	-0.051044	4.815568
245.715290	7999.873122	12.819392	-0.051072	4.815565
245.684620	7999.870493	12.824397	-0.051067	4.815565
245.483377	7999.866161	12.829402	-0.051029	4.815564
245.562797	7999.981702	12.834407	-0.051044	4.815598
245.668346	7999.877720	12.839411	-0.051064	4.815567
245.523790	7999.875376	12.844416	-0.051037	4.815567
245.661075	7999.880816	12.849421	-0.051063	4.815568
245.669860	7999.847865	12.854426	-0.051064	4.815558
245.637595	7999.911409	12.859431	-0.051058	4.815577
245.660579	7999.856267	12.864435	-0.051063	4.815561
245.674521	7999.876786	12.869440	-0.051065	4.815567
245.777462	7999.904089	12.874445	-0.051085	4.815574
245.691711	7999.889889	12.879450	-0.051069	4.815570
245.717909	7999.889252	12.884455	-0.051074	4.815570
245.727806	7999.853117	12.889459	-0.051076	4.815559
245.714901	7999.864657	12.894464	-0.051073	4.815563
245.698859	7999.866537	12.899469	-0.051070	4.815563
245.730742	7999.858519	12.904474	-0.051076	4.815561
245.736062	7999.894913	12.909479	-0.051077	4.815572
245.734227	7999.864993	12.914483	-0.051077	4.815563
245.864453	7999.888469	12.919488	-0.051101	4.815569
245.911400	7999.910592	12.924493	-0.051110	4.815575
245.734049	7999.876752	12.929498	-0.051077	4.815566
245.782718	7999.915986	12.934503	-0.051086	4.815577
245.761915	7999.893232	12.939507	-0.051083	4.815571
245.810228	7999.899361	12.944512	-0.051092	4.815572
245.912877	7999.905305	12.949517	-0.051111	4.815574
245.775401	7999.878520	12.954522	-0.051085	4.815567
245.653671	7999.904307	12.959527	-0.051063	4.815575
245.691347	7999.880368	12.964531	-0.051070	4.815567
245.731554	7999.867147	12.969536	-0.051077	4.815563
245.801831	7999.885378	12.974541	-0.051090	4.815568
245.602999	7999.873610	12.979546	-0.051054	4.815566
245.687003	7999.877116	12.984551	-0.051069	4.815567
245.847314	7999.860508	12.989555	-0.051099	4.815561
245.845254	7999.857277	12.994560	-0.051099	4.815560
245.916964	7999.900089	12.999565	-0.051112	4.815572
245.918523	7999.873427	13.004570	-0.051113	4.815564
245.903481	7999.904152	13.009575	-0.051110	4.815573
245.843911	7999.894648	13.014579	-0.051099	4.815571
245.938038	7999.880167	13.019584	-0.051116	4.815566
246.059594	7999.903503	13.024589	-0.051139	4.815572
245.825549	7999.869809	13.029594	-0.051096	4.815564
245.929403	7999.890721	13.034599	-0.051115	4.815569
245.937612	7999.910078	13.039603	-0.051117	4.815575
245.807449	7999.792656	13.044608	-0.051092	4.815541
245.902063	7999.841178	13.049613	-0.051110	4.815555
245.932697	7999.928166	13.054618	-0.051116	4.815580
245.921569	7999.866064	13.059623	-0.051114	4.815562
245.997448	7999.833136	13.064627	-0.051128	4.815552
246.050105	7999.810507	13.069632	-0.051138	4.815545
246.124113	7999.870440	13.074637	-0.051152	4.815562
245.884317	7999.870819	13.079642	-0.051107	4.815564
246.192211	7999.912131	13.084647	-0.051165	4.815574
246.244932	7999.893775	13.089651	-0.051174	4.815569
246.156235	7999.875255	13.094656	-0.051158	4.815564
246.339323	7999.885711	13.099661	-0.051192	4.815566
246.266127	7999.877052	13.104666	-0.051179	4.815564
246.225644	7999.893483	13.109671	-0.051171	4.815569
246.280038	7999.883696	13.114675	-0.051181	4.815566
245.953526	7999.906155	13.119680	-0.051121	4.815574
246.303896	7999.900111	13.124685	-0.051186	4.815570
246.154976	7999.901967	13.129690	-0.051158	4.815572
246.261244	7999.899429	13.134695	-0.051178	4.815570
246.226370	7999.877513	13.139699	-0.051172	4.815564
245.972603	7999.872326	13.144704	-0.051124	4.815564
246.106980	7999.885193	13.149709	-0.051150	4.815567
245.926916	7999.863053	13.154714	-0.051116	4.815561
246.038588	7999.895837	13.159719	-0.051137	4.815570
246.044114	7999.873511	13.164723	-0.051138	4.815564
246.148791	7999.876285	13.169728	-0.051158	4.815564
246.370920	7999.900188	13.174733	-0.051199	4.815570
246.239668	7999.958920	13.179738	-0.051175	4.815588
246.429563	7999.888340	13.184743	-0.051210	4.815566
246.317611	7999.889729	13.189747	-0.051189	4.815567
246.127982	7999.890923	13.194752	-0.051154	4.815568
246.105133	7999.899099	13.199757	-0.051150	4.815571
246.022300	7999.874268	13.204762	-0.051134	4.815564
246.066339	7999.881396	13.209767	-0.051143	4.815566
245.995123	7999.875973	13.214771	-0.051130	4.815565
245.950422	7999.862440	13.219776	-0.051121	4.815561
246.097197	7999.903269	13.224781	-0.051149	4.815572
246.066743	7999.853664	13.229786	-0.051143	4.815558
245.950716	7999.889154	13.234791	-0.051122	4.815569
246.085501	7999.897757	13.239795	-0.051147	4.815571
245.929901	7999.899504	13.244800	-0.051118	4.815572
245.939689	7999.901804	13.249805	-0.051120	4.815572
246.098025	7999.888367	13.254810	-0.051149	4.815568
246.192751	7999.867491	13.259815	-0.051167	4.815561
246.038285	7999.874595	13.264819	-0.051138	4.815564
246.158800	7999.858408	13.269824	-0.051161	4.815559
246.353302	7999.908555	13.274829	-0.051197	4.815572
246.007637	7999.879452	13.279834	-0.051133	4.815566
245.966618	7999.899078	13.284839	-0.051125	4.815572
246.244374	7999.898259	13.289843	-0.051177	4.815570
246.099736	7999.882033	13.294848	-0.051150	4.815566
246.182093	7999.914341	13.299853	-0.051165	4.815575
245.869870	7999.888986	13.304858	-0.051107	4.815569
245.987196	7999.893034	13.309863	-0.051129	4.815570
246.014578	7999.906297	13.314867	-0.051134	4.815573
246.116927	7999.885544	13.319872	-0.051154	4.815567
246.189270	7999.897402	13.324877	-0.051167	4.815570
246.146915	7999.887110	13.329882	-0.051159	4.815567
246.197503	7999.916766	13.334887	-0.051169	4.815576
246.197804	7999.882610	13.339891	-0.051169	4.815566
246.351477	7999.906468	13.344896	-0.051198	4.815572
246.211109	7999.912733	13.349901	-0.051172	4.815574
246.164765	7999.874615	13.354906	-0.051163	4.815563
246.444849	7999.889851	13.359911	-0.051215	4.815567
246.422336	7999.884152	13.364915	-0.051211	4.815565
246.296522	7999.886383	13.369920	-0.051188	4.815566
246.111249	7999.922883	13.374925	-0.051153	4.815578
246.156392	7999.861695	13.379930	-0.051162	4.815560
245.979775	7999.887658	13.384935	-0.051129	4.815568
246.123096	7999.882519	13.389939	-0.051156	4.815566
246.011342	7999.864692	13.394944	-0.051135	4.815561
246.168592	7999.899285	13.399949	-0.051164	4.815571
246.069304	7999.860307	13.404954	-0.051146	4.815560
246.151355	7999.897948	13.409959	-0.051161	4.815570
246.236845	7999.881192	13.414963	-0.051177	4.815565
246.152414	7999.856336	13.419968	-0.051161	4.815558
246.389213	7999.902899	13.424973	-0.051206	4.815571
246.441444	7999.874925	13.429978	-0.051215	4.815562
246.300047	7999.898258	13.434983	-0.051189	4.815570
246.302100	7999.895094	13.439987	-0.051190	4.815569
246.275774	7999.893603	13.444992	-0.051185	4.815568
246.279515	7999.924634	13.449997	-0.051186	4.815577
246.034804	7999.876885	13.455002	-0.051140	4.815565
246.195782	7999.901929	13.460007	-0.051170	4.815571
246.032439	7999.915296	13.465011	-0.051140	4.815576
246.032838	7999.890750	13.470016	-0.051140	4.815569
245.991666	7999.924254	13.475021	-0.051132	4.815579
246.041910	7999.880232	13.480026	-0.051142	4.815566
245.971195	7999.888697	13.485031	-0.051129	4.815568
245.932321	7999.887004	13.490035	-0.051121	4.815568
246.009865	7999.872254	13.495040	-0.051136	4.815563
246.127787	7999.878447	13.500045	-0.051158	4.815565
246.166149	7999.950613	13.505050	-0.051165	4.815586
246.340824	7999.887259	13.510055	-0.051198	4.815566
246.297107	7999.876945	13.515059	-0.051190	4.815563
246.057119	7999.871982	13.520064	-0.051145	4.815563
246.232494	7999.878041	13.525069	-0.051178	4.815564
246.209316	7999.860586	13.530074	-0.051173	4.815559
245.986364	7999.883661	13.535079	-0.051132	4.815567
246.143322	7999.881947	13.540083	-0.051161	4.815566
246.107839	7999.862157	13.545088	-0.051155	4.815560
246.304205	7999.903792	13.550093	-0.051191	4.815571
245.982442	7999.864401	13.555098	-0.051132	4.815561
245.943793	7999.895810	13.560103	-0.051124	4.815571
246.065920	7999.867904	13.565107	-0.051147	4.815562
245.945735	7999.856347	13.570112	-0.051125	4.815559
246.119639	7999.893346	13.575117	-0.051157	4.815569
246.237018	7999.852550	13.580122	-0.051179	4.815557
246.287643	7999.886478	13.585127	-0.051189	4.815566
246.072012	7999.884047	13.590131	-0.051149	4.815567
246.254018	7999.889146	13.595136	-0.051183	4.815567
246.153727	7999.889657	13.600141	-0.051164	4.815568
245.991676	7999.871013	13.605146	-0.051134	4.815563
246.228729	7999.897293	13.610151	-0.051178	4.815570
246.223050	7999.895071	13.615155	-0.051177	4.815569
245.973052	7999.868591	13.620160	-0.051131	4.815562
246.122926	7999.892387	13.625165	-0.051159	4.815569
245.980432	7999.869790	13.630170	-0.051132	4.815563
245.914728	7999.853780	13.635175	-0.051120	4.815558
245.856357	7999.966014	13.640179	-0.051109	4.815592
246.039598	7999.865430	13.645184	-0.051143	4.815561
246.036913	7999.905965	13.650189	-0.051143	4.815573
245.999899	7999.859457	13.655194	-0.051136	4.815560
245.952084	7999.859753	13.660199	-0.051127	4.815560
246.081693	7999.865069	13.665203	-0.051151	4.815561
245.990728	7999.828361	13.670208	-0.051134	4.815551
246.051810	7999.876339	13.675213	-0.051146	4.815564
246.127513	7999.863694	13.680218	-0.051160	4.815560
246.015584	7999.873626	13.685223	-0.051139	4.815564
246.002225	7999.879820	13.690227	-0.051137	4.815566
246.110809	7999.881591	13.695232	-0.051157	4.815566
246.035769	7999.898528	13.700237	-0.051143	4.815571
245.876101	7999.879923	13.705242	-0.051114	4.815566
245.994726	7999.909617	13.710247	-0.051136	4.815574
246.029289	7999.884559	13.715251	-0.051142	4.815567
246.067449	7999.962060	13.720256	-0.051150	4.815589
246.114739	7999.900907	13.725261	-0.051158	4.815571
245.939402	7999.860693	13.730266	-0.051126	4.815560
245.914581	7999.900868	13.735271	-0.051121	4.815572
246.008588	7999.868235	13.740275	-0.051139	4.815562
246.225406	7999.837597	13.745280	-0.051179	4.815552
246.349668	7999.896212	13.750285	-0.051202	4.815569
246.166172	7999.859068	13.755290	-0.051168	4.815559
246.245565	7999.892395	13.760295	-0.051183	4.815568
246.281891	7999.880179	13.765299	-0.051190	4.815564
246.315170	7999.884996	13.770304	-0.051196	4.815566
246.132618	7999.900186	13.775309	-0.051162	4.815571
245.996332	7999.855267	13.780314	-0.051137	4.815558
246.030020	7999.870769	13.785319	-0.051143	4.815563
245.947378	7999.888650	13.790323	-0.051128	4.815568
246.022412	7999.857843	13.795328	-0.051142	4.815559
246.084904	7999.891964	13.800333	-0.051154	4.815569
246.115440	7999.849757	13.805338	-0.051159	4.815556
246.059729	7999.875550	13.810343	-0.051149	4.815564
246.223892	7999.896375	13.815347	-0.051180	4.815569
246.401014	7999.867228	13.820352	-0.051213	4.815560
246.364322	7999.900804	13.825357	-0.051206	4.815570
246.127336	7999.876671	13.830362	-0.051162	4.815564
246.291173	7999.885746	13.835367	-0.051193	4.815566
246.207615	7999.903612	13.840371	-0.051177	4.815572
246.124049	7999.878770	13.845376	-0.051162	4.815565
246.255750	7999.900135	13.850381	-0.051186	4.815570
246.091498	7999.866507	13.855386	-0.051156	4.815561
246.245357	7999.881826	13.860391	-0.051184	4.815565
246.137717	7999.968703	13.865395	-0.051164	4.815591
246.084640	7999.855735	13.870400	-0.051155	4.815558
246.077195	7999.886583	13.875405	-0.051153	4.815567
246.171307	7999.868900	13.880410	-0.051171	4.815562
246.292716	7999.881556	13.885415	-0.051193	4.815565
246.356586	7999.866584	13.890419	-0.051205	4.815560
246.234383	7999.869942	13.895424	-0.051183	4.815562
246.340296	7999.909039	13.900429	-0.051203	4.815572
246.416268	7999.894264	13.905434	-0.051217	4.815568
246.175046	7999.912770	13.910439	-0.051172	4.815574
246.251273	7999.900135	13.915443	-0.051186	4.815570
246.258895	7999.862894	13.920448	-0.051188	4.815559
246.340859	7999.887722	13.925453	-0.051203	4.815566
246.252398	7999.861732	13.930458	-0.051187	4.815559
246.320224	7999.891668	13.935463	-0.051199	4.815567
246.410721	7999.903822	13.940467	-0.051216	4.815571
246.412182	7999.882497	13.945472	-0.051217	4.815564
246.260374	7999.893915	13.950477	-0.051188	4.815568
246.383632	7999.872434	13.955482	-0.051211	4.815562
246.213246	7999.914515	13.960487	-0.051180	4.815575
246.307208	7999.887219	13.965491	-0.051197	4.815566
246.181544	7999.869166	13.970496	-0.051174	4.815562
246.280431	7999.879321	13.975501	-0.051192	4.815564
246.409180	7999.861133	13.980506	-0.051216	4.815558
246.356818	7999.947840	13.985511	-0.051207	4.815584
246.480525	7999.895403	13.990515	-0.051230	4.815568
246.224617	7999.850675	13.995520	-0.051182	4.815556
246.611143	7999.911418	14.000525	-0.051254	4.815572
246.569271	7999.890456	14.005530	-0.051247	4.815566
246.387325	7999.904587	14.010535	-0.051213	4.815571
246.407786	7999.896384	14.015539	-0.051217	4.815568
246.288690	7999.865625	14.020544	-0.051194	4.815560
246.493488	7999.908465	14.025549	-0.051233	4.815572
246.310389	7999.877734	14.030554	-0.051199	4.815563
246.195439	7999.904699	14.035559	-0.051177	4.815572
246.372969	7999.878762	14.040563	-0.051210	4.815563
246.245538	7999.848935	14.045568	-0.051187	4.815555
246.392052	7999.897235	14.050573	-0.051214	4.815569
246.596213	7999.882408	14.055578	-0.051252	4.815563
246.245833	7999.868176	14.060583	-0.051187	4.815561
246.443759	7999.890618	14.065587	-0.051224	4.815567
246.350620	7999.891245	14.070592	-0.051207	4.815567
246.276646	7999.910335	14.075597	-0.051193	4.815573
246.230661	7999.881832	14.080602	-0.051184	4.815565
246.374701	7999.880976	14.085607	-0.051211	4.815564
246.458563	7999.895157	14.090611	-0.051227	4.815568
246.290471	7999.873211	14.095616	-0.051196	4.815562
246.419324	7999.899869	14.100621	-0.051220	4.815569
246.287365	7999.868901	14.105626	-0.051195	4.815561
246.360389	7999.903193	14.110631	-0.051209	4.815571
246.283791	7999.893412	14.115635	-0.051195	4.815568
246.255481	7999.852384	14.120640	-0.051190	4.815556
246.330515	7999.911266	14.125645	-0.051204	4.815573
246.107878	7999.896975	14.130650	-0.051162	4.815570
246.216379	7999.907286	14.135655	-0.051182	4.815572
246.319316	7999.905762	14.140659	-0.051202	4.815572
246.307574	7999.869274	14.145664	-0.051200	4.815561
246.309463	7999.905613	14.150669	-0.051200	4.815572
246.466769	7999.879347	14.155674	-0.051229	4.815563
246.440309	7999.878922	14.160679	-0.051224	4.815563
246.534402	7999.896474	14.165683	-0.051242	4.815568
246.304834	7999.886341	14.170688	-0.051199	4.815566
246.447466	7999.898275	14.175693	-0.051226	4.815569
246.501815	7999.878877	14.180698	-0.051236	4.815563
246.289746	7999.898925	14.185703	-0.051197	4.815570
246.388926	7999.900543	14.190707	-0.051215	4.815570
246.215044	7999.863555	14.195712	-0.051183	4.815560
246.234256	7999.898040	14.200717	-0.051187	4.815570
246.303706	7999.898106	14.205722	-0.051200	4.815569
246.419367	7999.906399	14.210727	-0.051221	4.815571
246.318769	7999.889821	14.215731	-0.051203	4.815567
246.272219	7999.873054	14.220736	-0.051194	4.815562
246.204229	7999.889038	14.225741	-0.051181	4.815567
246.272414	7999.853849	14.230746	-0.051194	4.815557
246.407783	7999.950015	14.235751	-0.051219	4.815584
246.695594	7999.883162	14.240755	-0.051273	4.815563
246.308744	7999.884352	14.245760	-0.051201	4.815565
246.576609	7999.902593	14.250765	-0.051251	4.815569
246.648757	7999.910178	14.255770	-0.051265	4.815571
246.487644	7999.907564	14.260775	-0.051235	4.815571
246.588036	7999.914540	14.265779	-0.051253	4.815573
246.280166	7999.895661	14.270784	-0.051196	4.815569
246.610065	7999.959755	14.275789	-0.051258	4.815586
246.313831	7999.714707	14.280794	-0.051202	4.815516

246.144336	7996.373578	14.285799	-0.051169	4.814539
246.317822	7990.796475	14.290803	-0.051197	4.812907
246.324746	7983.989703	14.295808	-0.051194	4.810915
246.331587	7976.667566	14.300813	-0.051191	4.808772
246.292506	7969.067700	14.305818	-0.051179	4.806546
245.994283	7961.172342	14.310823	-0.051118	4.804234
246.037477	7953.411703	14.315827	-0.051121	4.801959
246.050141	7945.361631	14.320832	-0.051118	4.799597
246.186264	7937.472636	14.325837	-0.051139	4.797282
246.161574	7929.443671	14.330842	-0.051129	4.794925
246.143876	7921.423022	14.335847	-0.051120	4.792569
246.182405	7913.385887	14.340851	-0.051122	4.790207
245.988426	7905.370694	14.345856	-0.051081	4.787851
245.703802	7897.369952	14.350861	-0.051023	4.785499
245.755447	7889.462667	14.355866	-0.051027	4.783171
245.644907	7881.418190	14.360871	-0.051002	4.780803
245.755108	7873.472836	14.365875	-0.051017	4.778462
245.615093	7865.398899	14.370880	-0.050986	4.776082
245.560817	7857.402117	14.375885	-0.050971	4.773724
245.459442	7849.366407	14.380890	-0.050947	4.771354
245.361209	7841.368611	14.385895	-0.050923	4.768993
245.449331	7833.443679	14.390899	-0.050934	4.766652
245.452891	7825.345196	14.395904	-0.050930	4.764259
245.343553	7817.443714	14.400909	-0.050904	4.761924
245.369674	7809.358846	14.405914	-0.050904	4.759532
245.108910	7801.442455	14.410919	-0.050850	4.757190
245.173506	7793.390363	14.415923	-0.050857	4.754806
245.173021	7785.324714	14.420928	-0.050852	4.752417
245.383634	7777.328613	14.425933	-0.050886	4.750046
245.222372	7769.321936	14.430938	-0.050851	4.747673
244.915638	7761.320965	14.435943	-0.050789	4.745300
244.960353	7753.387674	14.440947	-0.050792	4.742945
244.838961	7745.307394	14.445952	-0.050764	4.740546
244.710223	7737.349892	14.450957	-0.050735	4.738182
244.872090	7729.328891	14.455962	-0.050760	4.735797
244.549286	7721.315664	14.460967	-0.050695	4.733414
244.642559	7713.304186	14.465971	-0.050707	4.731030
244.507201	7705.321892	14.470976	-0.050677	4.728654
244.566570	7697.355886	14.475981	-0.050682	4.726281
244.448839	7689.307490	14.480986	-0.050655	4.723883
244.559175	7681.331128	14.485991	-0.050671	4.721504
244.670028	7673.356664	14.490995	-0.050686	4.719125
244.508449	7665.335863	14.496000	-0.050651	4.716731
244.296769	7657.310445	14.501005	-0.050606	4.714335
244.228754	7649.346722	14.506010	-0.050589	4.711956
244.162568	7641.264911	14.511015	-0.050571	4.709540
244.103494	7633.336562	14.516019	-0.050555	4.707169
244.011734	7625.285797	14.521024	-0.050533	4.704760
244.197518	7617.302647	14.526029	-0.050562	4.702369
244.094468	7609.341328	14.531034	-0.050538	4.699985
243.756601	7601.350261	14.536039	-0.050470	4.697590
244.165536	7593.294290	14.541043	-0.050541	4.695174
243.918990	7585.290261	14.546048	-0.050490	4.692773
243.866041	7577.281200	14.551053	-0.050475	4.690369
243.821628	7569.265929	14.556058	-0.050461	4.687962
243.957079	7561.299443	14.561063	-0.050481	4.685568
243.720456	7553.349494	14.566067	-0.050432	4.683179
243.541828	7545.297125	14.571072	-0.050394	4.680757
243.713141	7537.331667	14.576077	-0.050421	4.678359
243.702353	7529.327884	14.581082	-0.050413	4.675950
243.511359	7521.208250	14.586087	-0.050373	4.673504
243.550497	7513.176821	14.591091	-0.050375	4.671083
243.370579	7505.178627	14.596096	-0.050336	4.668671
243.390320	7497.284766	14.601101	-0.050335	4.666290
243.391557	7489.198419	14.606106	-0.050330	4.663848
243.001326	7481.243005	14.611111	-0.050252	4.661446
243.150619	7473.274117	14.616115	-0.050275	4.659038
243.139630	7465.260251	14.621120	-0.050267	4.656615
243.172933	7457.234199	14.626125	-0.050268	4.654187
243.183483	7449.226701	14.631130	-0.050265	4.651763
243.089475	7441.204543	14.636135	-0.050243	4.649334
243.018970	7433.271154	14.641139	-0.050224	4.646930
243.005557	7425.216427	14.646144	-0.050217	4.644489
242.804588	7417.251987	14.651149	-0.050174	4.642073
242.786426	7409.206769	14.656154	-0.050166	4.639632
242.815803	7401.276906	14.661159	-0.050166	4.637224
242.933942	7393.234169	14.666163	-0.050183	4.634781
242.808415	7385.137794	14.671168	-0.050154	4.632320
242.589503	7377.157542	14.676173	-0.050108	4.629893
242.630666	7369.213623	14.681178	-0.050111	4.627476
242.358751	7361.182350	14.686183	-0.050055	4.625031
242.489299	7353.194616	14.691187	-0.050074	4.622598
242.280123	7345.164821	14.696192	-0.050030	4.620151
242.411826	7337.243852	14.701197	-0.050049	4.617736
242.463212	7329.208303	14.706202	-0.050054	4.615285
242.303448	7321.155575	14.711207	-0.050019	4.612827
242.553739	7313.140784	14.716211	-0.050060	4.610379
242.160367	7305.162190	14.721216	-0.049982	4.607941
242.083592	7297.148944	14.726221	-0.049962	4.605491
242.237038	7289.190799	14.731226	-0.049986	4.603057
242.017439	7281.152594	14.736231	-0.049940	4.600597
242.084280	7273.215230	14.741235	-0.049947	4.598166
242.001038	7265.178364	14.746240	-0.049927	4.595704
241.977304	7257.123342	14.751245	-0.049917	4.593235
241.744458	7249.127007	14.756250	-0.049868	4.590782
241.752524	7241.095884	14.761255	-0.049865	4.588318
242.039966	7233.147728	14.766259	-0.049913	4.585878
241.574099	7225.102967	14.771264	-0.049821	4.583406
241.510710	7217.149994	14.776269	-0.049804	4.580961
241.601152	7209.123721	14.781274	-0.049816	4.578493
241.544596	7201.149878	14.786279	-0.049800	4.576040
241.495952	7193.108336	14.791283	-0.049786	4.573564
241.489569	7185.103452	14.796288	-0.049780	4.571098
241.484071	7177.077578	14.801293	-0.049774	4.568625
241.332097	7169.112294	14.806298	-0.049740	4.566168
241.293312	7161.098302	14.811303	-0.049728	4.563696
241.364008	7153.219650	14.816307	-0.049736	4.561263
241.159003	7145.121058	14.821312	-0.049692	4.558762
241.104575	7137.205066	14.826317	-0.049677	4.556315
241.221801	7129.161301	14.831322	-0.049694	4.553828
241.059287	7121.108165	14.836327	-0.049658	4.551337
241.070453	7113.112045	14.841331	-0.049655	4.548862
240.876709	7105.119374	14.846336	-0.049614	4.546386
241.073665	7097.117872	14.851341	-0.049646	4.543907
240.724105	7089.152023	14.856346	-0.049575	4.541436
240.594092	7081.094764	14.861351	-0.049546	4.538936
240.751465	7073.159885	14.866355	-0.049570	4.536474
240.478019	7065.109400	14.871360	-0.049514	4.533973
240.421850	7057.077111	14.876365	-0.049499	4.531477
240.744335	7049.101929	14.881370	-0.049553	4.528998
240.490406	7041.103904	14.886375	-0.049501	4.526510
240.266295	7033.112176	14.891379	-0.049454	4.524022
240.400932	7025.161392	14.896384	-0.049474	4.521546
240.564417	7017.119542	14.901389	-0.049499	4.519041
240.605393	7009.169139	14.906394	-0.049502	4.516562
240.427864	7001.049726	14.911399	-0.049464	4.514029
240.147587	6993.034784	14.916403	-0.049406	4.511527
240.154147	6985.037012	14.921408	-0.049402	4.509029
240.185693	6977.056450	14.926413	-0.049403	4.506535
240.066958	6969.032691	14.931418	-0.049376	4.504027
239.921796	6961.104490	14.936423	-0.049344	4.501546
239.793734	6953.073865	14.941427	-0.049315	4.499032
239.750816	6945.087860	14.946432	-0.049302	4.496531
239.834672	6937.057309	14.951437	-0.049312	4.494015
239.765814	6929.057596	14.956442	-0.049294	4.491507
239.799965	6921.013611	14.961447	-0.049295	4.488984
239.826419	6913.080624	14.966451	-0.049295	4.486494
239.894323	6905.011479	14.971456	-0.049302	4.483960
239.626250	6897.072562	14.976461	-0.049247	4.481465
239.711008	6889.031180	14.981466	-0.049258	4.478937
239.548892	6881.066441	14.986471	-0.049223	4.476431
239.726659	6873.031088	14.991475	-0.049251	4.473902
239.580981	6865.010784	14.996480	-0.049218	4.471376
239.436636	6856.999024	15.001485	-0.049186	4.468851
239.507048	6849.051730	15.006490	-0.049194	4.466346
239.225567	6840.991337	15.011495	-0.049137	4.463802
239.386380	6833.076694	15.016499	-0.049162	4.461304
239.015505	6825.017755	15.021504	-0.049087	4.458758
239.279555	6817.046577	15.026509	-0.049131	4.456240
239.254173	6809.005467	15.031514	-0.049121	4.453697
239.189568	6801.010903	15.036519	-0.049104	4.451168
239.277185	6793.035705	15.041523	-0.049115	4.448643
238.787313	6785.000670	15.046528	-0.049019	4.446097
239.023763	6776.965666	15.051533	-0.049058	4.443551
238.944517	6769.022138	15.056538	-0.049038	4.441032
238.804583	6760.992504	15.061543	-0.049007	4.438484
238.882513	6753.052993	15.066547	-0.049016	4.435964
238.844552	6744.968287	15.071552	-0.049004	4.433396
238.903333	6736.945826	15.076557	-0.049010	4.430846
238.890476	6729.001635	15.081562	-0.049002	4.428320
238.812923	6721.001145	15.086567	-0.048983	4.425774
238.721047	6712.998649	15.091571	-0.048960	4.423226
238.577230	6704.955543	15.096576	-0.048928	4.420663
238.398092	6697.003876	15.101581	-0.048890	4.418127
238.355134	6688.992111	15.106586	-0.048877	4.415572
238.289454	6680.967761	15.111591	-0.048859	4.413011
238.402972	6672.950146	15.116595	-0.048875	4.410452
238.361703	6664.942565	15.121600	-0.048863	4.407893
238.176672	6656.960546	15.126605	-0.048823	4.405341
238.297207	6648.996748	15.131610	-0.048840	4.402794
238.129714	6640.974045	15.136615	-0.048804	4.400226
238.324589	6632.990936	15.141619	-0.048835	4.397670
238.225285	6624.992081	15.146624	-0.048811	4.395107
238.168649	6616.943663	15.151629	-0.048796	4.392526
238.150213	6608.961607	15.156634	-0.048787	4.389965
237.898149	6600.969864	15.161639	-0.048735	4.387399
237.810588	6592.999412	15.166643	-0.048714	4.384838
237.650997	6585.001933	15.171648	-0.048679	4.382267
237.714268	6576.969250	15.176653	-0.048685	4.379685
237.756123	6569.022197	15.181658	-0.048688	4.377128
237.573819	6560.986994	15.186663	-0.048649	4.374541
237.608946	6552.978704	15.191667	-0.048650	4.371961
237.597607	6544.952776	15.196672	-0.048643	4.369374
237.488668	6536.989615	15.201677	-0.048618	4.366805
237.708432	6528.976468	15.206682	-0.048653	4.364221
237.449569	6521.003444	15.211687	-0.048600	4.361645
237.551189	6512.979821	15.216691	-0.048614	4.359054
237.347868	6505.088667	15.221696	-0.048571	4.356501
237.235608	6496.959166	15.226701	-0.048545	4.353871
237.359636	6488.865508	15.231706	-0.048563	4.351252
237.171345	6480.879463	15.236711	-0.048522	4.348665
237.251607	6472.939888	15.241715	-0.048532	4.346093
237.068493	6464.919048	15.246720	-0.048493	4.343491
237.003831	6456.925608	15.251725	-0.048476	4.340897
237.016404	6448.968985	15.256730	-0.048473	4.338314
236.740243	6440.945478	15.261735	-0.048416	4.335706
236.904677	6432.939451	15.266739	-0.048442	4.333105
236.920648	6424.925105	15.271744	-0.048440	4.330499
236.500728	6416.949183	15.276749	-0.048356	4.327900
236.719608	6408.926623	15.281754	-0.048392	4.325290
236.688260	6400.950849	15.286759	-0.048381	4.322691
236.674183	6392.928758	15.291763	-0.048373	4.320076
236.637153	6384.959904	15.296768	-0.048361	4.317476
236.620428	6376.945680	15.301773	-0.048353	4.314860
236.445705	6368.922800	15.306778	-0.048315	4.312238
236.425330	6360.865924	15.311783	-0.048306	4.309605
236.401031	6352.957251	15.316787	-0.048297	4.307019
236.402606	6344.946848	15.321792	-0.048292	4.304398
236.281177	6336.951910	15.326797	-0.048264	4.301780
236.191266	6328.926835	15.331802	-0.048242	4.299150
236.114370	6320.933057	15.336807	-0.048223	4.296529
235.999481	6312.881376	15.341811	-0.048196	4.293887
235.893327	6304.893447	15.346816	-0.048171	4.291265
235.861999	6296.904781	15.351821	-0.048160	4.288641
235.805050	6288.908373	15.356826	-0.048144	4.286013
235.591047	6280.910441	15.361831	-0.048099	4.283381
235.667931	6272.932851	15.366835	-0.048109	4.280757
235.510904	6264.921595	15.371840	-0.048074	4.278119
235.577546	6256.936079	15.376845	-0.048081	4.275489
235.471460	6248.884223	15.381850	-0.048057	4.272834
235.408308	6240.825882	15.386855	-0.048040	4.270175
235.434307	6232.873307	15.391859	-0.048039	4.267551
235.190052	6224.865740	15.396864	-0.047989	4.264905
235.198319	6216.881956	15.401869	-0.047985	4.262266
235.254388	6208.893328	15.406874	-0.047990	4.259626
235.030035	6200.918238	15.411879	-0.047943	4.256985
235.076184	6192.889849	15.416883	-0.047947	4.254328
235.038494	6184.899878	15.421888	-0.047935	4.251680
235.106187	6176.876189	15.426893	-0.047942	4.249021
234.981032	6168.912788	15.431898	-0.047914	4.246379
234.822099	6160.877305	15.436903	-0.047879	4.243711
234.805640	6152.906798	15.441907	-0.047871	4.241063
234.659791	6144.883003	15.446912	-0.047838	4.238396
234.764866	6136.919975	15.451917	-0.047853	4.235749
234.873684	6128.913004	15.456922	-0.047868	4.233086
234.782739	6120.869065	15.461927	-0.047846	4.230407
234.903240	6112.929907	15.466931	-0.047863	4.227763
234.638995	6104.900338	15.471936	-0.047809	4.225084
234.570224	6096.950615	15.476941	-0.047791	4.222431
234.413913	6088.936550	15.481946	-0.047757	4.219755
234.495940	6080.971838	15.486951	-0.047767	4.217095
234.564609	6072.908871	15.491955	-0.047774	4.214401
234.502330	6064.900775	15.496960	-0.047758	4.211723
234.258560	6056.881942	15.501965	-0.047707	4.209037
234.352143	6048.946431	15.506970	-0.047719	4.206381
234.091561	6040.925409	15.511975	-0.047666	4.203690
234.140435	6032.941821	15.516979	-0.047670	4.201014
234.003981	6024.943107	15.521984	-0.047639	4.198329
233.998742	6016.925884	15.526989	-0.047633	4.195638
233.915675	6008.846620	15.531994	-0.047612	4.192923
233.636846	6000.784494	15.536999	-0.047555	4.190210
233.737967	5992.850895	15.542003	-0.047569	4.187543
233.683344	5984.841145	15.547008	-0.047554	4.184846
233.584252	5976.849164	15.552013	-0.047530	4.182153
233.691616	5968.883365	15.557018	-0.047545	4.179470
233.571571	5960.942205	15.562023	-0.047517	4.176791
233.607648	5952.887237	15.567027	-0.047519	4.174073
233.549566	5944.892421	15.572032	-0.047503	4.171373
233.388184	5936.845330	15.577037	-0.047468	4.168652
233.456077	5928.884414	15.582042	-0.047475	4.165961
233.162597	5920.868982	15.587047	-0.047415	4.163246
233.344330	5912.883184	15.592051	-0.047444	4.160544
233.277947	5904.872362	15.597056	-0.047427	4.157830
233.110144	5896.885973	15.602061	-0.047390	4.155121
233.264809	5888.871550	15.607066	-0.047414	4.152404
233.168495	5880.834333	15.612071	-0.047391	4.149675
233.127508	5872.910763	15.617075	-0.047378	4.146983
232.968782	5864.853286	15.622080	-0.047343	4.144242
233.301247	5856.856207	15.627085	-0.047400	4.141526
233.182947	5848.873053	15.632090	-0.047373	4.138808
232.869168	5840.901323	15.637095	-0.047309	4.136089
232.911215	5832.891865	15.642099	-0.047312	4.133361
232.843885	5824.852314	15.647104	-0.047294	4.130618
232.750472	5816.899577	15.652109	-0.047272	4.127903
232.616157	5808.888728	15.657114	-0.047242	4.125166
232.522667	5800.898190	15.662119	-0.047219	4.122435
232.485742	5792.884420	15.667123	-0.047207	4.119694
232.372041	5784.927220	15.672128	-0.047181	4.116970
232.428532	5776.870497	15.677133	-0.047186	4.114213
232.298712	5768.862633	15.682138	-0.047157	4.111467
232.099807	5760.840041	15.687143	-0.047115	4.108714
232.281532	5752.826593	15.692147	-0.047143	4.105968
232.162824	5744.832683	15.697152	-0.047116	4.103222
231.984307	5736.891002	15.702157	-0.047078	4.100491
232.281779	5728.899037	15.707162	-0.047128	4.097748
232.206810	5720.878715	15.712167	-0.047109	4.094988
232.024374	5712.918815	15.717171	-0.047070	4.092246
232.077470	5704.881685	15.722176	-0.047074	4.089478
232.001331	5696.888587	15.727181	-0.047055	4.086722
231.989526	5688.920988	15.732186	-0.047048	4.083974
231.805190	5680.934901	15.737191	-0.047008	4.081215
231.795506	5672.930130	15.742195	-0.047001	4.078450
231.879721	5664.908957	15.747200	-0.047012	4.075679
231.717951	5656.890531	15.752205	-0.046977	4.072904
231.783681	5648.873807	15.757210	-0.046984	4.070130
231.469119	5640.915910	15.762215	-0.046920	4.067369
231.644351	5632.893922	15.767219	-0.046947	4.064592
231.437185	5624.933616	15.772224	-0.046904	4.061828
231.310096	5616.901761	15.777229	-0.046875	4.059039
231.394468	5608.962844	15.782234	-0.046885	4.056283
231.366760	5600.883106	15.787239	-0.046875	4.053475
231.427521	5592.901296	15.792243	-0.046881	4.050700
231.410994	5584.912952	15.797248	-0.046873	4.047920
231.234099	5576.874175	15.802253	-0.046835	4.045118
231.212448	5568.965193	15.807258	-0.046826	4.042362
231.146591	5560.901523	15.812263	-0.046808	4.039549
231.417989	5552.926493	15.817267	-0.046854	4.036770
231.144018	5544.891020	15.822272	-0.046798	4.033960
230.855973	5536.804720	15.827277	-0.046739	4.031130
230.757363	5528.862341	15.832282	-0.046715	4.028351
230.554691	5520.875640	15.837287	-0.046672	4.025553
230.724205	5512.907637	15.842291	-0.046699	4.022765
230.684955	5504.876825	15.847296	-0.046686	4.019950
230.468702	5496.915579	15.852301	-0.046641	4.017155
230.431705	5488.892401	15.857306	-0.046629	4.014339
230.396386	5480.868580	15.862311	-0.046617	4.011521
230.564137	5472.858173	15.867315	-0.046643	4.008709
230.392966	5464.890799	15.872320	-0.046606	4.005904
230.196988	5456.847730	15.877325	-0.046565	4.003071
230.374094	5448.911339	15.882330	-0.046592	4.000279
230.220972	5440.922003	15.887335	-0.046559	3.997461
230.219673	5432.909283	15.892339	-0.046553	3.994635
230.288414	5424.870713	15.897344	-0.046561	3.991799
230.186585	5416.829819	15.902349	-0.046537	3.988958
230.185757	5408.839464	15.907354	-0.046532	3.986134
230.070554	5400.884824	15.912359	-0.046505	3.983319
230.094183	5392.920539	15.917363	-0.046504	3.980501
229.931335	5384.925723	15.922368	-0.046469	3.977667
229.814496	5376.929224	15.927373	-0.046442	3.974831
229.923921	5368.898718	15.932378	-0.046457	3.971984
229.831337	5360.903774	15.937383	-0.046435	3.969145
229.640603	5352.934227	15.942387	-0.046394	3.966311
229.664663	5344.944345	15.947392	-0.046393	3.963472
229.660470	5336.927329	15.952397	-0.046387	3.960620
229.477519	5328.979984	15.957402	-0.046348	3.957788
229.636785	5320.900874	15.962407	-0.046373	3.954913
229.551577	5312.886783	15.967411	-0.046352	3.952055
229.250187	5304.893495	15.972416	-0.046290	3.949198
229.289895	5296.908586	15.977421	-0.046293	3.946348
229.474401	5288.938885	15.982426	-0.046322	3.943505
229.224994	5280.958827	15.987431	-0.046270	3.940647
229.197143	5272.979754	15.992435	-0.046260	3.937792
229.163049	5264.972801	15.997440	-0.046249	3.934925
229.148446	5256.906270	16.002445	-0.046241	3.932035
229.153436	5248.960463	16.007450	-0.046236	3.929186
229.027486	5240.954847	16.012455	-0.046208	3.926311
229.184053	5232.980806	16.017459	-0.046232	3.923451
228.927132	5225.014465	16.022464	-0.046179	3.920584
228.715120	5217.001435	16.027469	-0.046134	3.917698
228.700860	5208.979058	16.032474	-0.046126	3.914811
228.588332	5200.948607	16.037479	-0.046100	3.911917
228.716554	5192.936822	16.042483	-0.046119	3.909032
228.590735	5184.961390	16.047488	-0.046090	3.906153
228.561230	5176.930679	16.052493	-0.046080	3.903254
228.645858	5168.963927	16.057498	-0.046090	3.900378
228.570821	5160.963047	16.062503	-0.046071	3.897484
228.685357	5152.939186	16.067507	-0.046087	3.894584
228.376130	5144.939345	16.072512	-0.046025	3.891682
228.371687	5136.941503	16.077517	-0.046019	3.888785
228.441283	5128.987868	16.082522	-0.046027	3.885902
228.399486	5120.973810	16.087527	-0.046014	3.882994
228.214903	5113.006098	16.092531	-0.045974	3.880097
228.300367	5105.024736	16.097536	-0.045985	3.877199
228.097128	5096.975649	16.102541	-0.045942	3.874268
228.084361	5088.728615	16.107546	-0.045934	3.871266
227.819204	5080.824770	16.112551	-0.045880	3.868383
227.875551	5072.869142	16.117555	-0.045885	3.865484
227.863381	5064.930918	16.122560	-0.045878	3.862589
227.803148	5056.899558	16.127565	-0.045861	3.859656
227.944142	5048.981131	16.132570	-0.045883	3.856766
227.859433	5040.936808	16.137575	-0.045862	3.853824
227.817396	5032.931275	16.142579	-0.045849	3.850894
227.813690	5024.977455	16.147584	-0.045843	3.847982
227.829575	5016.920399	16.152589	-0.045841	3.845030
227.649170	5009.038849	16.157594	-0.045802	3.842136
227.595543	5001.006503	16.162599	-0.045787	3.839187
227.428459	4993.053903	16.167603	-0.045750	3.836263
227.401854	4985.025603	16.172608	-0.045740	3.833312
227.085534	4976.963995	16.177613	-0.045676	3.830340
227.350438	4969.025655	16.182618	-0.045720	3.827424
227.334968	4960.974627	16.187623	-0.045712	3.824457
227.177111	4953.050628	16.192627	-0.045678	3.821533
227.179517	4945.034710	16.197632	-0.045673	3.818575
227.169644	4937.024029	16.202637	-0.045666	3.815617
227.328858	4929.064646	16.207642	-0.045691	3.812679
227.059247	4921.003832	16.212647	-0.045635	3.809692
227.111454	4913.070623	16.217651	-0.045640	3.806757
226.944044	4905.031698	16.222656	-0.045604	3.803776
226.789425	4897.088485	16.227661	-0.045570	3.800828
226.756919	4889.076998	16.232666	-0.045559	3.797856
226.602704	4881.078174	16.237671	-0.045525	3.794883
226.589034	4873.006786	16.242675	-0.045517	3.791883
226.499690	4865.036948	16.247680	-0.045495	3.788918
226.354513	4857.015517	16.252685	-0.045463	3.785929
226.487885	4849.066728	16.257690	-0.045483	3.782972
226.350931	4841.046604	16.262695	-0.045452	3.779979
226.268296	4833.090687	16.267699	-0.045431	3.777010
226.273412	4825.063863	16.272704	-0.045427	3.774013
226.057581	4817.064365	16.277709	-0.045382	3.771020
226.186667	4809.060303	16.282714	-0.045401	3.768030
226.197184	4801.032270	16.287719	-0.045398	3.765026
226.088407	4793.097960	16.292723	-0.045372	3.762052
225.994255	4785.071662	16.297728	-0.045350	3.759041
226.038118	4777.104882	16.302733	-0.045353	3.756054
226.186452	4769.110526	16.307738	-0.045375	3.753056
226.030057	4761.023485	16.312743	-0.045341	3.750014
225.894963	4753.062924	16.317747	-0.045310	3.747017
225.997133	4745.054157	16.322752	-0.045324	3.744006
225.888333	4737.103970	16.327757	-0.045299	3.741009
225.712107	4729.143751	16.332762	-0.045261	3.738004
225.484665	4721.108039	16.337767	-0.045213	3.734968
225.481197	4713.093722	16.342771	-0.045208	3.731942
225.435987	4705.104256	16.347776	-0.045194	3.728922
225.552570	4697.109334	16.352781	-0.045211	3.725901
225.368549	4689.160665	16.357786	-0.045171	3.722889
225.369455	4681.139110	16.362791	-0.045166	3.719850
225.361177	4673.166689	16.367795	-0.045160	3.716828
225.287449	4665.113677	16.372800	-0.045141	3.713771
225.300814	4657.042801	16.377805	-0.045138	3.710707
225.325194	4649.103521	16.382810	-0.045137	3.707690
225.188760	4641.069565	16.387815	-0.045107	3.704631
225.076360	4633.159620	16.392819	-0.045081	3.701617
224.941643	4625.181449	16.397824	-0.045051	3.698575
224.780672	4617.159248	16.402829	-0.045015	3.695512
225.027307	4609.133305	16.407834	-0.045056	3.692456
224.884508	4601.143695	16.412839	-0.045025	3.689401
224.678517	4593.184549	16.417843	-0.044981	3.686353
224.755412	4585.181486	16.422848	-0.044990	3.683294
224.825487	4577.165936	16.427853	-0.044998	3.680227
224.800445	4569.237507	16.432858	-0.044988	3.677188
224.596968	4561.203909	16.437863	-0.044945	3.674102
224.618169	4553.184832	16.442867	-0.044944	3.671025
224.412991	4545.210471	16.447872	-0.044901	3.667956
224.434498	4537.178866	16.452877	-0.044900	3.664869
224.460857	4529.212899	16.457882	-0.044899	3.661804
224.329486	4521.206778	16.462887	-0.044870	3.658717
224.301737	4513.206086	16.467891	-0.044859	3.655633
224.390001	4505.210710	16.472896	-0.044871	3.652551
224.340605	4497.152271	16.477901	-0.044856	3.649438
224.161553	4489.228357	16.482906	-0.044818	3.646371
224.041099	4481.239377	16.487911	-0.044790	3.643278
223.939498	4473.260776	16.492915	-0.044766	3.640187
223.986371	4465.272271	16.497920	-0.044770	3.637094
223.873577	4457.258181	16.502925	-0.044744	3.633983
223.841059	4449.234962	16.507930	-0.044732	3.630869
223.898659	4441.235651	16.512935	-0.044738	3.627763
223.697560	4433.218749	16.517939	-0.044695	3.624641
223.928117	4425.228250	16.522944	-0.044733	3.621539
223.833008	4417.243403	16.527949	-0.044710	3.618427
223.840400	4409.299869	16.532954	-0.044707	3.615331
223.791714	4401.263114	16.537959	-0.044692	3.612195
223.678223	4393.268343	16.542963	-0.044666	3.609070
223.566805	4385.309953	16.547968	-0.044640	3.605957
223.496633	4377.296499	16.552973	-0.044622	3.602821
223.475666	4369.326397	16.557978	-0.044613	3.599701
223.254074	4361.378423	16.562983	-0.044567	3.596581
223.244674	4353.329859	16.567987	-0.044560	3.593424
223.242140	4345.318094	16.572992	-0.044554	3.590280
223.078046	4337.327434	16.577997	-0.044518	3.587136
223.000898	4329.353421	16.583002	-0.044499	3.583999
222.913057	4321.372934	16.588007	-0.044477	3.580856
222.887283	4313.376747	16.593011	-0.044467	3.577706
222.867944	4305.345985	16.598016	-0.044459	3.574539
222.809123	4297.352930	16.603021	-0.044443	3.571384
222.904116	4289.358821	16.608026	-0.044455	3.568230
222.682969	4281.365841	16.613031	-0.044409	3.565064
222.656445	4273.404330	16.618035	-0.044399	3.561914
222.770985	4265.409476	16.623040	-0.044415	3.558752
222.869124	4257.377231	16.628045	-0.044428	3.555571
222.724591	4249.329306	16.633050	-0.044396	3.552375
222.485527	4241.298117	16.638055	-0.044346	3.549179
222.488797	4233.334653	16.643059	-0.044342	3.546014
222.476187	4225.357525	16.648064	-0.044334	3.542841
222.229644	4217.352648	16.653069	-0.044283	3.539647
222.460335	4209.420904	16.658074	-0.044321	3.536493
222.167705	4201.409759	16.663079	-0.044261	3.533290
221.904550	4193.390494	16.668083	-0.044207	3.530081
222.065153	4185.386247	16.673088	-0.044232	3.526887
221.943133	4177.388104	16.678093	-0.044204	3.523685
222.094639	4169.437972	16.683098	-0.044227	3.520508
221.998103	4161.426725	16.688103	-0.044204	3.517295
222.115334	4153.418874	16.693107	-0.044221	3.514088
222.007678	4145.448825	16.698112	-0.044196	3.510885
221.773938	4137.423598	16.703117	-0.044147	3.507654
221.746471	4129.462084	16.708122	-0.044137	3.504452
221.738706	4121.477647	16.713127	-0.044130	3.501238
221.677356	4113.510916	16.718131	-0.044113	3.498027
221.775154	4105.508939	16.723136	-0.044127	3.494803
221.782415	4097.468034	16.728141	-0.044123	3.491558
221.652958	4089.506346	16.733146	-0.044093	3.488338
221.482190	4081.521364	16.738151	-0.044057	3.485104
221.406357	4073.553362	16.743155	-0.044037	3.481877
221.440498	4065.587186	16.748160	-0.044038	3.478651
221.358919	4057.554430	16.753165	-0.044018	3.475391
221.395427	4049.540644	16.758170	-0.044020	3.472140
221.452510	4041.531948	16.763175	-0.044025	3.468888
221.143123	4033.525423	16.768179	-0.043962	3.465622
221.107938	4025.598217	16.773184	-0.043951	3.462395
221.055578	4017.540388	16.778189	-0.043936	3.459111
220.821549	4009.620386	16.783194	-0.043887	3.455873
220.819550	4001.582968	16.788199	-0.043882	3.452593
220.950613	3993.545512	16.793203	-0.043901	3.449313
220.939750	3985.562989	16.798208	-0.043894	3.446049
220.821515	3977.591410	16.803213	-0.043867	3.442782
220.705629	3969.637167	16.808218	-0.043840	3.439519
220.715870	3961.650580	16.813223	-0.043837	3.436244
220.386754	3953.629383	16.818227	-0.043770	3.432940
220.769428	3945.583622	16.823232	-0.043836	3.429647
220.553489	3937.622604	16.828237	-0.043791	3.426366
220.480556	3929.649219	16.833242	-0.043772	3.423081
220.375341	3921.662712	16.838247	-0.043748	3.419786
220.437053	3913.701180	16.843251	-0.043754	3.416504
220.264421	3905.664651	16.848256	-0.043717	3.413180
219.984691	3897.672864	16.853261	-0.043659	3.409868
220.192232	3889.701234	16.858266	-0.043693	3.406577
220.303535	3881.703041	16.863271	-0.043708	3.403269
220.235475	3873.707243	16.868275	-0.043691	3.399953
220.160372	3865.762745	16.873280	-0.043672	3.396654
220.115737	3857.698716	16.878285	-0.043658	3.393303
220.024333	3849.658624	16.883290	-0.043636	3.389958
219.729957	3841.696884	16.888295	-0.043576	3.386635
219.929081	3833.712607	16.893299	-0.043608	3.383316
219.826397	3825.736209	16.898304	-0.043584	3.379987
219.669259	3817.779077	16.903309	-0.043549	3.376660
219.677176	3809.782947	16.908314	-0.043545	3.373320
219.774446	3801.744579	16.913319	-0.043558	3.369962
219.607523	3793.791196	16.918323	-0.043522	3.366627
219.490735	3785.825095	16.923328	-0.043495	3.363284
219.540241	3777.802840	16.928333	-0.043499	3.359921
219.608676	3769.851628	16.933338	-0.043507	3.356586
219.267107	3761.825622	16.938343	-0.043438	3.353200
219.247563	3753.793386	16.943347	-0.043429	3.349820
219.357667	3745.815827	16.948352	-0.043445	3.346465
219.128005	3737.808380	16.953357	-0.043397	3.343081
219.219520	3729.857354	16.958362	-0.043409	3.339729
219.207083	3721.875324	16.963367	-0.043401	3.336357
219.106876	3713.872890	16.968371	-0.043378	3.332970
218.983132	3705.873333	16.973376	-0.043349	3.329579
218.815078	3697.898401	16.978381	-0.043313	3.326194
218.874895	3689.909402	16.983386	-0.043319	3.322808
218.636767	3681.955546	16.988391	-0.043269	3.319422
218.655069	3673.963753	16.993395	-0.043268	3.316026
218.709263	3665.927085	16.998400	-0.043273	3.312609
218.548552	3657.905318	17.003405	-0.043238	3.309187
218.412789	3649.948998	17.008410	-0.043207	3.305790
218.575094	3641.915111	17.013415	-0.043232	3.302367
218.407678	3633.982500	17.018419	-0.043196	3.298972
218.297467	3626.023828	17.023424	-0.043170	3.295564
218.250601	3617.983203	17.028429	-0.043156	3.292121
218.371690	3610.010907	17.033434	-0.043174	3.288709
218.160340	3602.018612	17.038439	-0.043129	3.285272
217.883410	3594.050157	17.043443	-0.043073	3.281840
218.043670	3586.038974	17.048448	-0.043097	3.278402
218.020876	3578.067235	17.053453	-0.043088	3.274970
217.910667	3570.055315	17.058458	-0.043062	3.271515
217.913466	3562.039449	17.063463	-0.043058	3.268058
217.918123	3554.046353	17.068467	-0.043053	3.264608
217.783894	3546.108355	17.073472	-0.043023	3.261172
217.777799	3538.088420	17.078477	-0.043017	3.257702
217.697929	3530.106153	17.083482	-0.042997	3.254242
217.577503	3522.094408	17.088487	-0.042969	3.250764
217.383087	3514.129044	17.093491	-0.042928	3.247299
217.357106	3506.139464	17.098496	-0.042918	3.243827
217.298265	3498.152175	17.103501	-0.042902	3.240350
217.509372	3490.187119	17.108506	-0.042936	3.236891
217.325851	3482.140493	17.113511	-0.042897	3.233376
217.192509	3474.098746	17.118515	-0.042867	3.229862
217.217653	3466.143156	17.123520	-0.042866	3.226387
217.067190	3458.157628	17.128525	-0.042833	3.222889
217.288240	3450.188752	17.133530	-0.042869	3.219410
217.036954	3442.221536	17.138535	-0.042817	3.215908
216.923942	3434.209556	17.143539	-0.042791	3.212388
216.930889	3426.228481	17.148544	-0.042787	3.208883
216.706698	3418.244640	17.153549	-0.042740	3.205363
216.693577	3410.293622	17.158554	-0.042733	3.201863
216.661267	3402.308521	17.163559	-0.042722	3.198343
216.892234	3394.283120	17.168563	-0.042759	3.194812
216.739179	3386.327132	17.173568	-0.042726	3.191292
216.404463	3378.319024	17.178573	-0.042658	3.187737
216.749291	3370.285251	17.183578	-0.042717	3.184196
216.584716	3362.342228	17.188583	-0.042682	3.180669
216.496308	3354.359275	17.193587	-0.042660	3.177124
216.550882	3346.341291	17.198592	-0.042665	3.173566
216.387225	3338.330184	17.203597	-0.042629	3.169997
216.357616	3330.381813	17.208602	-0.042619	3.166458
216.008717	3322.406771	17.213607	-0.042549	3.162889
216.254197	3314.396469	17.218611	-0.042589	3.159327
216.163013	3306.465574	17.223616	-0.042567	3.155781
215.933459	3298.441985	17.228621	-0.042519	3.152183
216.170447	3290.403005	17.233626	-0.042558	3.148595
216.097804	3282.406865	17.238631	-0.042540	3.145008
215.863965	3274.477424	17.243635	-0.042491	3.141441
215.741965	3266.496103	17.248640	-0.042463	3.137850
215.723077	3258.486072	17.253645	-0.042454	3.134247
215.575913	3250.515939	17.258650	-0.042422	3.130653
215.422767	3242.533475	17.263655	-0.042388	3.127048
215.652311	3234.503027	17.268659	-0.042426	3.123435
215.561422	3226.562599	17.273664	-0.042404	3.119843
215.453414	3218.580633	17.278669	-0.042378	3.116229
215.516952	3210.584005	17.283674	-0.042385	3.112610
215.390118	3202.599130	17.288679	-0.042356	3.108985
215.273464	3194.598557	17.293683	-0.042330	3.105348
215.406593	3186.625645	17.298688	-0.042349	3.101731
215.124741	3178.641220	17.303693	-0.042292	3.098086
215.210821	3170.637546	17.308698	-0.042302	3.094445
215.114493	3162.671900	17.313703	-0.042279	3.090808
215.087637	3154.670394	17.318707	-0.042269	3.087154
214.894461	3146.706126	17.323712	-0.042228	3.083504
214.640118	3138.748042	17.328717	-0.042176	3.079851
214.899731	3130.756869	17.333722	-0.042219	3.076201
214.817204	3122.713959	17.338727	-0.042198	3.072508
214.685495	3114.681022	17.343731	-0.042169	3.068812
214.670314	3106.700889	17.348736	-0.042161	3.065142
214.537502	3098.739652	17.353741	-0.042131	3.061471
214.610350	3090.770333	17.358746	-0.042139	3.057801
214.416042	3082.792690	17.363751	-0.042098	3.054110
214.405922	3074.781527	17.368755	-0.042091	3.050408
214.465997	3066.816024	17.373760	-0.042097	3.046726
214.435846	3058.839128	17.378765	-0.042086	3.043030
214.358647	3050.872101	17.383770	-0.042067	3.039331
214.505608	3042.895602	17.388775	-0.042089	3.035635
214.254500	3034.915060	17.393779	-0.042037	3.031913
214.062418	3026.930261	17.398784	-0.041996	3.028187
214.108204	3018.904479	17.403789	-0.041999	3.024449
214.071323	3010.964100	17.408794	-0.041987	3.020742
213.944585	3002.992802	17.413799	-0.041959	3.017012
214.001601	2994.958134	17.418803	-0.041964	3.013257
214.133906	2986.947532	17.423808	-0.041984	3.009512
213.806693	2979.007831	17.428813	-0.041918	3.005772
213.833104	2971.038243	17.433818	-0.041917	3.002032
213.662325	2963.067543	17.438823	-0.041880	2.998276
213.706136	2955.074272	17.443827	-0.041883	2.994516
213.614777	2947.077542	17.448832	-0.041861	2.990743
213.661463	2939.052490	17.453837	-0.041865	2.986959
213.475168	2931.109917	17.458842	-0.041825	2.983197
213.548036	2923.112248	17.463847	-0.041833	2.979417
213.472684	2915.156325	17.468851	-0.041814	2.975644
213.241510	2907.191675	17.473856	-0.041766	2.971855
213.236454	2899.148032	17.478861	-0.041760	2.968035
213.034368	2891.192329	17.483866	-0.041717	2.964242
213.037074	2883.247828	17.488871	-0.041713	2.960460
213.023992	2875.255623	17.493875	-0.041705	2.956649
213.034246	2867.265329	17.498880	-0.041702	2.952835
213.057880	2859.232337	17.503885	-0.041701	2.948997
213.039805	2851.248209	17.508890	-0.041693	2.945175
212.882137	2843.307833	17.513895	-0.041658	2.941362
212.820837	2835.293236	17.518899	-0.041642	2.937513
213.076335	2827.332604	17.523904	-0.041684	2.933702
212.980115	2819.328460	17.528909	-0.041661	2.929846
212.623544	2811.393147	17.533914	-0.041589	2.926005
212.678666	2803.416907	17.538919	-0.041595	2.922160
212.667165	2795.422268	17.543923	-0.041587	2.918299
212.481002	2787.490306	17.548928	-0.041548	2.914453
212.255646	2779.394127	17.553933	-0.041500	2.910520
212.361174	2771.414075	17.558938	-0.041515	2.906656
212.320703	2763.458775	17.563943	-0.041502	2.902791
212.239200	2755.467942	17.568947	-0.041482	2.898901
212.299565	2747.535593	17.573952	-0.041488	2.895042
212.187511	2739.508142	17.578957	-0.041462	2.891122
212.334918	2731.524134	17.583962	-0.041484	2.887233
212.179581	2723.576235	17.588967	-0.041450	2.883339
212.086642	2715.574195	17.593971	-0.041428	2.879417
212.119943	2707.649828	17.598976	-0.041429	2.875534
211.893084	2699.653410	17.603981	-0.041381	2.871597
212.067361	2691.634511	17.608986	-0.041409	2.867665
211.942944	2683.674024	17.613991	-0.041380	2.863740
211.587445	2675.697990	17.618995	-0.041309	2.859789
211.900460	2667.726695	17.624000	-0.041362	2.855872
211.713123	2659.722310	17.629005	-0.041322	2.851906
211.509920	2651.759954	17.634010	-0.041279	2.847954
211.522339	2643.779918	17.639015	-0.041276	2.843999
211.383576	2635.819965	17.644019	-0.041246	2.840041
211.521972	2627.861637	17.649024	-0.041266	2.836093
211.221935	2619.852049	17.654029	-0.041205	2.832090
211.242018	2611.856858	17.659034	-0.041204	2.828106
211.169926	2603.871581	17.664039	-0.041185	2.824117
211.046502	2595.907872	17.669043	-0.041157	2.820129
211.186894	2587.944561	17.674048	-0.041178	2.816152
211.051511	2579.946923	17.679053	-0.041148	2.812135
211.014554	2571.949458	17.684058	-0.041136	2.808119
211.061676	2563.961213	17.689063	-0.041139	2.804106
210.997197	2556.016471	17.694067	-0.041122	2.800103
211.070330	2548.062880	17.699072	-0.041131	2.796098
210.923929	2540.069444	17.704077	-0.041098	2.792054
210.724908	2532.117224	17.709082	-0.041056	2.788022
210.625837	2524.123100	17.714087	-0.041033	2.783968
210.642600	2516.133340	17.719091	-0.041031	2.779918
210.662198	2508.190517	17.724096	-0.041029	2.775886
210.519485	2500.172661	17.729101	-0.040997	2.771800
210.466912	2492.202103	17.734106	-0.040982	2.767738
210.289622	2484.231589	17.739111	-0.040944	2.763662
210.275374	2476.254402	17.744115	-0.040936	2.759587
210.312797	2468.301228	17.749120	-0.040938	2.755521
210.078670	2460.270567	17.754125	-0.040890	2.751393
210.077129	2452.255663	17.759130	-0.040884	2.747280
209.999262	2444.303669	17.764135	-0.040864	2.743189
209.762814	2436.352641	17.769139	-0.040815	2.739083
209.976977	2428.386280	17.774144	-0.040850	2.734991
209.859156	2420.375039	17.779149	-0.040823	2.730848
209.678512	2412.426939	17.784154	-0.040784	2.726729
209.610996	2404.466629	17.789159	-0.040767	2.722603
209.547378	2396.496899	17.794163	-0.040750	2.718467
209.551350	2388.534859	17.799168	-0.040745	2.714332
209.338152	2380.550359	17.804173	-0.040700	2.710166
209.486645	2372.566635	17.809178	-0.040723	2.706017
209.463821	2364.599496	17.814183	-0.040713	2.701859
209.380197	2356.623286	17.819187	-0.040693	2.697686
209.246596	2348.678002	17.824192	-0.040663	2.693520
209.201913	2340.646268	17.829197	-0.040649	2.689307
209.116456	2332.692089	17.834202	-0.040628	2.685126
209.152221	2324.741012	17.839207	-0.040630	2.680948
209.107665	2316.762875	17.844211	-0.040616	2.676744
209.197535	2308.780380	17.849216	-0.040628	2.672540
209.102525	2300.767329	17.854221	-0.040605	2.668301
208.911211	2292.828909	17.859226	-0.040564	2.664088
208.843840	2284.860953	17.864231	-0.040547	2.659861
208.673410	2276.917704	17.869235	-0.040510	2.655634
208.642707	2268.922569	17.874240	-0.040499	2.651382
208.603925	2260.915195	17.879245	-0.040487	2.647115
208.544297	2252.973025	17.884250	-0.040470	2.642875
208.363165	2245.029958	17.889255	-0.040432	2.638620
208.487722	2237.032133	17.894259	-0.040450	2.634349
208.667173	2229.036066	17.899264	-0.040478	2.630076
208.439332	2221.073279	17.904269	-0.040430	2.625786
208.305739	2213.133147	17.909274	-0.040400	2.621508
208.368756	2205.157938	17.914279	-0.040407	2.617217
208.179235	2197.178831	17.919283	-0.040367	2.612900
208.054173	2189.215107	17.924288	-0.040338	2.608588
208.197851	2181.215021	17.929293	-0.040360	2.604267
208.073436	2173.287158	17.934298	-0.040331	2.599961
207.945614	2165.345066	17.939303	-0.040303	2.595639
208.130612	2157.159805	17.944307	-0.040332	2.591199
207.962983	2149.213534	17.949312	-0.040295	2.586858
207.820776	2141.275507	17.954317	-0.040264	2.582516
207.716848	2133.344389	17.959322	-0.040239	2.578172
207.688736	2125.413449	17.964327	-0.040229	2.573827
207.492301	2117.422458	17.969331	-0.040187	2.569430
207.581567	2109.470212	17.974336	-0.040199	2.565066
207.649475	2101.508641	17.979341	-0.040206	2.560688
207.452010	2093.572463	17.984346	-0.040164	2.556298
207.307760	2085.611941	17.989351	-0.040132	2.551891
207.313893	2077.605280	17.994355	-0.040128	2.547461
207.260686	2069.654977	17.999360	-0.040113	2.543051
207.095802	2061.691429	18.004365	-0.040078	2.538617
207.121664	2053.736617	18.009370	-0.040077	2.534195
207.219148	2045.738094	18.014375	-0.040090	2.529745
207.033425	2037.792896	18.019379	-0.040051	2.525297
207.039178	2029.846189	18.024384	-0.040047	2.520854
206.968965	2021.885647	18.029389	-0.040028	2.516390
206.904462	2013.917688	18.034394	-0.040011	2.511914
206.834416	2005.924451	18.039399	-0.039993	2.507415
206.876183	1997.938932	18.044403	-0.039996	2.502921
206.777520	1990.015436	18.049408	-0.039972	2.498444
206.413580	1982.074555	18.054413	-0.039899	2.493929
206.316989	1974.094365	18.059418	-0.039876	2.489403
206.464735	1966.095673	18.064423	-0.039899	2.484877
206.397394	1958.145161	18.069427	-0.039881	2.480354
206.315726	1950.220089	18.074432	-0.039861	2.475836
206.142406	1942.249283	18.079437	-0.039823	2.471276
206.181632	1934.260097	18.084442	-0.039825	2.466714
206.191778	1926.293000	18.089447	-0.039822	2.462154
206.075468	1918.340341	18.094451	-0.039795	2.457584
206.124688	1910.392245	18.099456	-0.039799	2.453020
205.939481	1902.423299	18.104461	-0.039760	2.448419
205.855493	1894.468577	18.109466	-0.039739	2.443824
206.016285	1886.496369	18.114471	-0.039764	2.439230
205.783906	1878.565043	18.119475	-0.039715	2.434620
205.854379	1870.495709	18.124480	-0.039723	2.429945
205.666110	1862.559244	18.129485	-0.039683	2.425318
205.641484	1854.616904	18.134490	-0.039673	2.420691
205.610853	1846.683603	18.139495	-0.039663	2.416060
205.524715	1838.699257	18.144499	-0.039642	2.411386
205.433645	1830.758254	18.149504	-0.039619	2.406729
205.206403	1822.822903	18.154509	-0.039572	2.402054
205.130226	1814.874500	18.159514	-0.039553	2.397375
205.158178	1806.891483	18.164519	-0.039553	2.392674
205.347733	1798.875300	18.169523	-0.039583	2.387958
205.167922	1790.966220	18.174528	-0.039544	2.383266
204.995013	1783.035055	18.179533	-0.039507	2.378552
204.772031	1775.098601	18.184538	-0.039460	2.373822
204.738655	1767.115117	18.189543	-0.039449	2.369069
204.764512	1759.131839	18.194547	-0.039449	2.364312
204.897308	1751.190376	18.199552	-0.039468	2.359578
204.828886	1743.238267	18.204557	-0.039450	2.354813
204.580933	1735.261840	18.209562	-0.039399	2.350009
204.458201	1727.317604	18.214567	-0.039371	2.345224
204.280973	1719.381509	18.219571	-0.039333	2.340430
204.277184	1711.432790	18.224576	-0.039327	2.335633
204.247906	1703.441974	18.229581	-0.039317	2.330798
204.230780	1695.486419	18.234586	-0.039308	2.325976
204.165559	1687.551614	18.239591	-0.039291	2.321152
204.087742	1679.607638	18.244595	-0.039272	2.316311
204.128602	1671.641822	18.249600	-0.039274	2.311457
203.931830	1663.698465	18.254605	-0.039232	2.306587
203.915428	1655.737837	18.259610	-0.039224	2.301711
204.054409	1647.780858	18.264615	-0.039245	2.296839
204.027553	1639.802111	18.269619	-0.039235	2.291930
203.931781	1631.875767	18.274624	-0.039212	2.287037
203.818583	1623.935768	18.279629	-0.039186	2.282124
203.703919	1616.017924	18.284634	-0.039159	2.277213
203.622650	1608.023614	18.289639	-0.039139	2.272247
203.634233	1600.005365	18.294643	-0.039136	2.267264
203.802580	1592.052799	18.299648	-0.039162	2.262323
203.502710	1584.141573	18.304653	-0.039101	2.257358
203.414564	1576.203539	18.309658	-0.039080	2.252383
203.366813	1568.258568	18.314663	-0.039066	2.247396
203.263123	1560.311767	18.319667	-0.039041	2.242392
203.010617	1552.416177	18.324672	-0.038989	2.237395
202.983208	1544.449105	18.329677	-0.038979	2.232363
203.179289	1536.458345	18.334682	-0.039010	2.227324
203.070824	1528.535861	18.339687	-0.038985	2.222289
202.873078	1520.601252	18.344691	-0.038943	2.217228
202.871965	1512.655024	18.349696	-0.038938	2.212165
202.782743	1504.691285	18.354701	-0.038916	2.207071
202.573659	1496.788705	18.359706	-0.038872	2.201994
202.759851	1488.819976	18.364711	-0.038901	2.196898
202.519640	1480.881160	18.369715	-0.038852	2.191771
202.400666	1472.929632	18.374720	-0.038824	2.186635
202.448230	1464.968169	18.379725	-0.038828	2.181496
202.401141	1457.032600	18.384730	-0.038814	2.176352
202.502089	1449.062571	18.389735	-0.038828	2.171188
202.079628	1441.164860	18.394739	-0.038744	2.166010
202.076682	1433.229613	18.399744	-0.038738	2.160834
202.161180	1425.277510	18.404749	-0.038749	2.155642
201.971563	1417.344424	18.409754	-0.038709	2.150425
201.919750	1409.396506	18.414759	-0.038694	2.145198
201.891712	1401.440660	18.419763	-0.038684	2.139956
201.908282	1393.528371	18.424768	-0.038682	2.134733
201.832963	1385.567115	18.429773	-0.038662	2.129457
201.868499	1377.636460	18.434778	-0.038664	2.124199
201.599228	1369.759012	18.439783	-0.038609	2.118933
201.297445	1361.814365	18.444787	-0.038547	2.113607
201.529429	1353.790196	18.449792	-0.038585	2.108265
201.436809	1345.850353	18.454797	-0.038563	2.102935
201.237991	1337.952805	18.459802	-0.038521	2.097609
201.209819	1330.012959	18.464807	-0.038511	2.092258
201.295829	1322.040365	18.469811	-0.038522	2.086882
201.274077	1314.141203	18.474816	-0.038512	2.081532
201.018478	1306.250016	18.479821	-0.038460	2.076149
200.919519	1298.305996	18.484826	-0.038436	2.070733
201.157964	1290.329658	18.489831	-0.038475	2.065314
200.883945	1282.428023	18.494835	-0.038419	2.059880
200.787604	1274.529590	18.499840	-0.038396	2.054452
200.720397	1266.574603	18.504845	-0.038379	2.048974
200.750966	1258.633572	18.509850	-0.038379	2.043501
200.737678	1250.730135	18.514855	-0.038372	2.038034
200.539863	1242.807826	18.519859	-0.038330	2.032521
200.564922	1234.842906	18.524864	-0.038329	2.026985
200.472831	1226.920339	18.529869	-0.038307	2.021453
200.345950	1219.008596	18.534874	-0.038278	2.015909
200.371736	1211.064304	18.539879	-0.038278	2.010342
200.089225	1203.163471	18.544883	-0.038220	2.004759
200.051254	1195.268916	18.549888	-0.038208	1.999190
199.888081	1187.348143	18.554893	-0.038173	1.993573
199.811156	1179.411460	18.559898	-0.038153	1.987939
199.878813	1171.480387	18.564903	-0.038161	1.982308
199.760532	1163.566695	18.569907	-0.038134	1.976653
199.719475	1155.644130	18.574912	-0.038121	1.970984
199.537899	1147.715588	18.579917	-0.038082	1.965280
199.456694	1139.819004	18.584922	-0.038062	1.959592
199.648825	1131.878916	18.589927	-0.038092	1.953886
199.447828	1123.915027	18.594931	-0.038050	1.948104
199.407184	1116.001956	18.599936	-0.038037	1.942358
199.392907	1108.089271	18.604941	-0.038029	1.936599
199.337312	1100.166178	18.609946	-0.038014	1.930810
199.236112	1092.263731	18.614951	-0.037990	1.925014
199.177671	1084.352994	18.619955	-0.037974	1.919199
199.296151	1076.437380	18.624960	-0.037991	1.913383
198.921090	1068.556706	18.629965	-0.037916	1.907519
199.041856	1060.616551	18.634970	-0.037934	1.901649
198.950877	1052.731866	18.639975	-0.037912	1.895778
198.754191	1044.808909	18.644979	-0.037870	1.889848
198.573624	1036.936213	18.649984	-0.037831	1.883939
198.642081	1029.016122	18.654989	-0.037839	1.878005
198.631481	1021.089550	18.659994	-0.037832	1.872037
198.464199	1013.189866	18.664999	-0.037795	1.866053
198.235864	1005.289788	18.670003	-0.037748	1.860042
198.516239	997.366021	18.675008	-0.037795	1.854052
198.504075	989.440884	18.680013	-0.037788	1.848008
198.126247	981.590847	18.685018	-0.037712	1.841959
198.422882	973.658566	18.690023	-0.037762	1.835906
198.040522	965.789839	18.695027	-0.037686	1.829801
197.901773	957.908120	18.700032	-0.037655	1.823695
197.792496	950.011748	18.705037	-0.037630	1.817561
197.882860	942.086213	18.710042	-0.037641	1.811407
197.656793	934.211862	18.715047	-0.037594	1.805234
197.654067	926.318486	18.720051	-0.037589	1.799052
197.717680	918.397698	18.725056	-0.037595	1.792835
197.551833	910.469948	18.730061	-0.037559	1.786562
197.458394	902.584293	18.735066	-0.037537	1.780310
197.587687	894.689564	18.740071	-0.037556	1.774057
197.350731	886.812307	18.745075	-0.037507	1.767749
197.194439	878.954069	18.750080	-0.037473	1.761444
197.120867	871.077371	18.755085	-0.037454	1.755112
197.180661	863.173452	18.760090	-0.037460	1.748752
196.923333	855.319499	18.765095	-0.037407	1.742369
196.805534	847.440205	18.770099	-0.037380	1.735959
196.840155	839.546641	18.775104	-0.037381	1.729534
196.887626	831.652865	18.780109	-0.037385	1.723086
196.804814	823.788907	18.785114	-0.037365	1.716622
196.701922	815.909721	18.790119	-0.037340	1.710118
196.607802	808.016592	18.795123	-0.037318	1.703578
196.366720	800.188082	18.800128	-0.037268	1.697048
196.155675	792.321759	18.805133	-0.037223	1.690465
196.220598	784.419462	18.810138	-0.037230	1.683863
196.237295	776.568290	18.815143	-0.037229	1.677271
196.094627	768.687459	18.820147	-0.037197	1.670607
196.060168	760.825938	18.825152	-0.037185	1.663947
196.014584	752.969226	18.830157	-0.037172	1.657262
195.805539	745.115459	18.835162	-0.037128	1.650531
195.740044	737.255364	18.840167	-0.037111	1.643787
195.820052	729.384395	18.845171	-0.037120	1.637025
195.500137	721.519012	18.850176	-0.037056	1.630185
195.320539	713.653870	18.855181	-0.037017	1.623336
195.434712	705.771237	18.860186	-0.037034	1.616483
195.308469	697.935648	18.865191	-0.037005	1.609609
195.082859	690.102579	18.870195	-0.036958	1.602693
194.995570	682.275256	18.875200	-0.036937	1.595772
195.057719	674.390919	18.880205	-0.036943	1.588792
194.954111	666.551527	18.885210	-0.036919	1.581797
194.765396	658.742639	18.890215	-0.036879	1.574785
194.779765	650.864256	18.895219	-0.036876	1.567710
194.722219	643.041947	18.900224	-0.036860	1.560643
194.537897	635.231595	18.905229	-0.036821	1.553535
194.484314	627.366151	18.910234	-0.036806	1.546364
194.693809	619.502483	18.915239	-0.036840	1.539200
194.503117	611.689451	18.920243	-0.036800	1.531990
194.511001	603.856084	18.925248	-0.036796	1.524756
194.492594	596.041753	18.930253	-0.036787	1.517502
194.178531	588.248616	18.935258	-0.036724	1.510188
194.104161	580.431456	18.940263	-0.036705	1.502852
194.109696	572.595579	18.945267	-0.036701	1.495474
194.114350	564.775701	18.950272	-0.036697	1.488076
194.034136	556.970194	18.955277	-0.036677	1.480640
193.612249	549.208268	18.960282	-0.036593	1.473155
193.614574	541.342663	18.965287	-0.036589	1.465599
193.476712	533.551836	18.970291	-0.036558	1.458054
193.544215	525.732005	18.975296	-0.036566	1.450475
193.469432	517.935767	18.980301	-0.036547	1.442855
193.417211	510.149040	18.985306	-0.036532	1.435208
193.262891	502.370896	18.990311	-0.036498	1.427512
193.203879	494.570826	18.995315	-0.036482	1.419768
193.078719	486.807352	19.000320	-0.036454	1.412007
192.870554	479.035446	19.005325	-0.036410	1.404181
193.039087	471.231575	19.010330	-0.036437	1.396342
192.915943	463.453741	19.015335	-0.036409	1.388436
192.483894	455.724415	19.020339	-0.036323	1.380482
192.476793	447.954499	19.025344	-0.036317	1.372512
192.294705	440.190842	19.030349	-0.036278	1.364472
192.167672	432.446172	19.035354	-0.036249	1.356414
192.141134	424.679492	19.040359	-0.036239	1.348302
191.993450	416.921680	19.045363	-0.036207	1.340128
191.925347	409.181588	19.050368	-0.036189	1.331938
191.882874	401.416769	19.055373	-0.036176	1.323675
191.818211	393.685444	19.060378	-0.036159	1.315392
191.763954	385.818185	19.065383	-0.036144	1.306911
191.477575	378.131657	19.070387	-0.036086	1.298530
191.575715	370.379952	19.075392	-0.036099	1.290093
191.384163	362.685423	19.080397	-0.036059	1.281610
191.158527	355.005961	19.085402	-0.036012	1.273080
191.230931	347.268035	19.090407	-0.036020	1.264484
191.128466	339.569775	19.095411	-0.035996	1.255840
191.100075	331.868513	19.100416	-0.035986	1.247147
190.897292	324.209119	19.105421	-0.035943	1.238408
190.796227	316.507811	19.110426	-0.035919	1.229577
190.847291	308.800052	19.115431	-0.035924	1.220705
190.548415	301.158669	19.120435	-0.035863	1.211777
190.500109	293.488555	19.125440	-0.035849	1.202798
190.476756	285.822354	19.130445	-0.035840	1.193761
190.369062	278.162441	19.135450	-0.035815	1.184645
190.274904	270.527409	19.140455	-0.035793	1.175492
190.024220	262.897208	19.145459	-0.035741	1.166240
189.932198	255.280451	19.150464	-0.035719	1.156964
189.782897	247.617889	19.155469	-0.035686	1.147544
189.843408	239.962142	19.160474	-0.035693	1.138099
189.908406	232.330425	19.165479	-0.035700	1.128606
189.482161	224.784183	19.170483	-0.035616	1.119034
189.266683	217.211435	19.175488	-0.035571	1.109391
189.178365	209.617994	19.180493	-0.035549	1.099666
188.948050	202.055268	19.185498	-0.035502	1.089861
188.895848	194.483958	19.190503	-0.035487	1.079997
188.670740	186.930536	19.195507	-0.035440	1.070026
188.356626	179.410159	19.200512	-0.035377	1.059984
187.901400	171.917958	19.205517	-0.035287	1.049851
187.590457	164.412045	19.210522	-0.035225	1.039635
187.288086	156.919514	19.215527	-0.035163	1.029337
186.900534	149.441403	19.220531	-0.035086	1.018934
186.451987	141.990922	19.225536	-0.034998	1.008448
186.131300	134.533192	19.230541	-0.034934	0.997873
185.785304	127.042204	19.235546	-0.034864	0.987130
185.337900	119.624318	19.240551	-0.034776	0.976349
184.956004	112.191719	19.245555	-0.034700	0.965443
184.610375	104.794329	19.250560	-0.034631	0.954473
184.063798	97.424768	19.255565	-0.034525	0.943365
183.543811	90.067040	19.260570	-0.034423	0.932149
183.532135	82.646351	19.265575	-0.034416	0.920836
183.035942	75.316653	19.270579	-0.034319	0.909392
182.483061	68.015753	19.275584	-0.034212	0.897831
181.871270	60.962430	19.280589	-0.034093	0.886496