KGT3462_Position 5_00025 LC.txt
Dataset description:
This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in...
Source: SA508-F_300C_1DPA_(ID-110)
Additional Information