Mon Apr 19 08:39:03 2021

Number of Points = 3646
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.454494	-0.098348	0.000000	-0.000087	0.310175

1.391754	-0.087844	0.005005	-0.000075	0.310170
1.592182	-0.125780	0.010010	-0.000112	0.310163
1.358780	-0.079885	0.015014	-0.000069	0.310179
1.421611	-0.092759	0.020019	-0.000081	0.310173
1.231049	-0.055974	0.025024	-0.000045	0.310183
0.671437	0.048318	0.030029	0.000059	0.310195
1.277139	-0.065939	0.035034	-0.000054	0.310175
1.141333	-0.039018	0.040038	-0.000028	0.310185
0.669645	0.047748	0.045043	0.000059	0.310190
1.051065	-0.020445	0.050048	-0.000012	0.310195
0.987307	-0.053930	0.055053	0.000000	0.309985
0.706420	-0.026780	0.060058	0.000053	0.309874
0.899499	-0.060780	0.065062	0.000017	0.309879
0.891966	-0.061630	0.070067	0.000018	0.309868
1.243736	-0.127977	0.075072	-0.000047	0.309857
1.008130	-0.084952	0.080077	-0.000003	0.309858
1.475306	-0.172304	0.085082	-0.000090	0.309846
1.463617	-0.166732	0.090086	-0.000088	0.309862
1.026952	-0.151817	0.095091	-0.000007	0.309561
1.334710	-0.214561	0.100096	-0.000064	0.309529
0.750825	-0.104606	0.105101	0.000045	0.309547
0.907012	-0.135462	0.110106	0.000016	0.309535
1.309634	-0.209409	0.115110	-0.000059	0.309532
0.859057	-0.149332	0.120115	0.000024	0.309430
0.789675	-0.170623	0.125120	0.000037	0.309271
1.089331	-0.229600	0.130125	-0.000018	0.309250
1.435606	-0.293985	0.135130	-0.000083	0.309243
1.102987	-0.230119	0.140134	-0.000021	0.309259
0.674362	-0.218266	0.145139	0.000059	0.308950
0.908474	-0.267188	0.150144	0.000015	0.308920
0.952337	-0.275952	0.155149	0.000007	0.308916
1.023017	-0.289447	0.160154	-0.000006	0.308913
0.815261	-0.306586	0.165158	0.000033	0.308656
0.730198	-0.301249	0.170163	0.000049	0.308608
0.869001	-0.324049	0.175168	0.000023	0.308620
0.554157	-0.275200	0.180173	0.000082	0.308580
0.434596	-0.312428	0.185178	0.000104	0.308304
0.444701	-0.311494	0.190182	0.000102	0.308317
0.795711	-0.381215	0.195187	0.000037	0.308289
0.957600	-0.450867	0.200192	0.000007	0.308100
0.784115	-0.439100	0.205197	0.000039	0.308007
1.043271	-0.489563	0.210202	-0.000009	0.307991
0.664483	-0.464487	0.215206	0.000061	0.307785
0.924425	-0.539269	0.220211	0.000013	0.307656
1.297482	-0.607873	0.225216	-0.000057	0.307652
0.953266	-0.608241	0.230221	0.000008	0.307356
0.866092	-0.594598	0.235226	0.000024	0.307345
0.873715	-0.616206	0.240230	0.000022	0.307250
0.473730	-0.590915	0.245235	0.000097	0.307027
0.750261	-0.640945	0.250240	0.000045	0.307028
0.371291	-0.612883	0.255245	0.000116	0.306835
0.652913	-0.684136	0.260250	0.000064	0.306741
0.674618	-0.703908	0.265254	0.000060	0.306666
0.435916	-0.715704	0.270259	0.000104	0.306405
0.937546	-0.807817	0.275264	0.000011	0.306401
0.851229	-0.850115	0.280269	0.000027	0.306127
1.041474	-0.894140	0.285274	-0.000009	0.306082
1.353775	-1.001398	0.290278	-0.000067	0.305843
0.592192	-0.877864	0.295283	0.000075	0.305773
0.806580	-0.950328	0.300288	0.000035	0.305614
0.765043	-0.962770	0.305293	0.000043	0.305519
0.697783	-0.993443	0.310298	0.000056	0.305316
0.391920	-0.963429	0.315302	0.000113	0.305195
0.687940	-1.057867	0.320307	0.000058	0.305002
0.700918	-1.089974	0.325312	0.000055	0.304861
0.353773	-1.065639	0.330317	0.000120	0.304677
0.160371	-1.059572	0.335322	0.000156	0.304539
0.815510	-1.215366	0.340326	0.000034	0.304364
0.554553	-1.193595	0.345331	0.000083	0.304242
0.660325	-1.266502	0.350336	0.000063	0.303987
0.410653	-1.237459	0.355341	0.000109	0.303909
1.074220	-1.422703	0.360346	-0.000014	0.303601
0.768023	-1.383555	0.365350	0.000043	0.303522
0.873046	-1.457606	0.370355	0.000023	0.303260
1.073196	-1.528539	0.375360	-0.000014	0.303095
0.606955	-1.467329	0.380365	0.000073	0.302982
0.610075	-1.536558	0.385370	0.000072	0.302654
0.512098	-1.537297	0.390374	0.000091	0.302566
0.425477	-1.571419	0.395379	0.000107	0.302327
0.397550	-1.610179	0.400384	0.000112	0.302117
0.297585	-1.617431	0.405389	0.000131	0.301995
0.685959	-1.746678	0.410394	0.000059	0.301714
0.353977	-1.719021	0.415398	0.000120	0.301557
-0.426200	-1.608555	0.420403	0.000266	0.301407
-0.588007	-1.632334	0.425408	0.000296	0.301151
-0.614326	-1.649774	0.430413	0.000301	0.301045
-0.010975	-1.818444	0.435418	0.000188	0.300761
0.431370	-1.929739	0.440422	0.000106	0.300612
0.597515	-1.998961	0.445427	0.000075	0.300424
0.216539	-1.979721	0.450432	0.000146	0.300183
0.723606	-2.126202	0.455437	0.000052	0.299921
0.760117	-2.177172	0.460442	0.000045	0.299707
0.325481	-2.135716	0.465446	0.000126	0.299526
-0.329033	-2.070922	0.470451	0.000248	0.299264
0.048264	-2.183188	0.475456	0.000178	0.299052
0.129894	-2.241278	0.480461	0.000163	0.298843
-0.175936	-2.233725	0.485466	0.000220	0.298610
0.017991	-2.325093	0.490470	0.000184	0.298338
-0.118068	-2.341840	0.495475	0.000209	0.298137
-0.166808	-2.371523	0.500480	0.000218	0.297950
-0.170359	-2.430478	0.505485	0.000219	0.297660
-0.077703	-2.502500	0.510490	0.000202	0.297392
-0.203203	-2.523382	0.515494	0.000225	0.297179
-0.570728	-2.503560	0.520499	0.000293	0.296950
-4.744045	-1.783830	0.525504	0.001070	0.296761
-3.242342	-2.090608	0.530509	0.000791	0.296596
-3.754363	-2.039079	0.535514	0.000886	0.296393
-3.987105	-2.039647	0.540518	0.000929	0.296184
-4.206763	-2.019030	0.545523	0.000970	0.296089
-3.938297	-2.126309	0.550528	0.000920	0.295803
-4.417278	-2.053476	0.555533	0.001009	0.295734
-4.876559	-2.012394	0.560538	0.001095	0.295526
-4.203146	-2.160708	0.565542	0.000970	0.295399
-4.527697	-2.152746	0.570547	0.001030	0.295149
-4.811471	-2.137178	0.575552	0.001083	0.294972
-5.139519	-2.104846	0.580557	0.001144	0.294838
-5.093553	-2.168143	0.585562	0.001135	0.294569
-5.100987	-2.180652	0.590566	0.001137	0.294500
-6.093964	-2.055976	0.595571	0.001322	0.294226
-5.690854	-2.138330	0.600576	0.001247	0.294181
-6.196923	-2.105428	0.605581	0.001341	0.293890
-6.843996	-1.999619	0.610586	0.001461	0.293832
-6.484927	-2.113447	0.615590	0.001395	0.293593
-6.476499	-2.136929	0.620595	0.001393	0.293485
-7.556448	-1.982461	0.625600	0.001594	0.293278
-7.259455	-2.053367	0.630605	0.001539	0.293195
-7.376209	-2.076843	0.635610	0.001561	0.292974
-7.447558	-2.078510	0.640614	0.001574	0.292902
-8.661229	-1.909352	0.645619	0.001800	0.292647
-7.516962	-2.128437	0.650624	0.001587	0.292592
-7.702388	-2.149855	0.655629	0.001621	0.292319
-8.160045	-2.074913	0.660634	0.001707	0.292279
-8.879786	-1.997157	0.665638	0.001841	0.292016
-8.272109	-2.112707	0.670643	0.001728	0.291990
-8.499842	-2.127834	0.675648	0.001770	0.291710
-8.768782	-2.080086	0.680653	0.001820	0.291704
-8.648384	-2.166367	0.685658	0.001798	0.291385
-9.510212	-2.008341	0.690662	0.001958	0.291391
-9.959712	-1.978943	0.695667	0.002042	0.291131
-9.296718	-2.112706	0.700672	0.001918	0.291065
-9.436528	-2.124486	0.705677	0.001944	0.290880
-10.087958	-2.035326	0.710682	0.002066	0.290735
-9.913023	-2.085949	0.715686	0.002033	0.290641
-10.160094	-2.071733	0.720691	0.002079	0.290488
-10.153808	-2.087496	0.725696	0.002078	0.290415
-11.006102	-1.984894	0.730701	0.002237	0.290154
-10.845150	-2.012981	0.735706	0.002207	0.290160
-11.264898	-1.988301	0.740710	0.002285	0.289902
-11.676253	-1.923686	0.745715	0.002361	0.289851
-11.474982	-1.987356	0.750720	0.002324	0.289716
-12.258003	-1.878450	0.755725	0.002470	0.289549
-12.199648	-1.893928	0.760730	0.002459	0.289524
-12.432923	-1.895580	0.765734	0.002502	0.289304
-12.438057	-1.906513	0.770739	0.002503	0.289245
-12.333156	-1.945895	0.775744	0.002484	0.289143
-12.734709	-1.921400	0.780749	0.002559	0.288900
-12.657873	-1.936605	0.785754	0.002544	0.288894
-12.681304	-1.974530	0.790758	0.002549	0.288682
-12.884809	-1.959693	0.795763	0.002587	0.288571
-13.107901	-1.927402	0.800768	0.002628	0.288529
-12.937553	-2.010917	0.805773	0.002597	0.288266
-13.765211	-1.856574	0.810778	0.002751	0.288285
-13.552075	-1.932595	0.815782	0.002711	0.288098
-14.247526	-1.826183	0.820787	0.002840	0.287997
-13.872526	-1.893787	0.825792	0.002771	0.288000
-14.585028	-1.828103	0.830797	0.002903	0.287679
-14.599951	-1.830201	0.835802	0.002906	0.287655
-14.514513	-1.847849	0.840806	0.002890	0.287644
-14.873735	-1.842427	0.845811	0.002957	0.287342
-15.152718	-1.788302	0.850816	0.003009	0.287359
-14.958184	-1.839733	0.855821	0.002973	0.287278
-14.935273	-1.897271	0.860826	0.002969	0.287009
-15.253223	-1.836444	0.865830	0.003028	0.287025
-15.837334	-1.753475	0.870835	0.003136	0.286907
-15.653431	-1.819425	0.875840	0.003102	0.286743
-16.134842	-1.731860	0.880845	0.003192	0.286743
-15.952294	-1.798049	0.885850	0.003158	0.286577
-15.782607	-1.862934	0.890854	0.003126	0.286405
-15.578116	-1.905348	0.895859	0.003088	0.286378
-15.725444	-1.924709	0.900864	0.003116	0.286145
-15.598780	-1.963853	0.905869	0.003092	0.286063
-16.038403	-1.897172	0.910874	0.003174	0.285996
-16.295684	-1.896295	0.915878	0.003222	0.285764
-16.575021	-1.843956	0.920883	0.003274	0.285771
-16.531867	-1.876673	0.925888	0.003266	0.285645
-17.518327	-1.718545	0.930893	0.003450	0.285538
-17.705775	-1.684514	0.935898	0.003485	0.285537
-17.014825	-1.841493	0.940902	0.003356	0.285378
-17.226130	-1.845680	0.945907	0.003395	0.285162
-16.881467	-1.908164	0.950912	0.003331	0.285163
-17.230418	-1.893716	0.955917	0.003396	0.284914
-17.669376	-1.826097	0.960922	0.003478	0.284852
-17.901600	-1.785491	0.965926	0.003521	0.284844
-18.501022	-1.735092	0.970931	0.003633	0.284546
-18.037569	-1.819907	0.975936	0.003547	0.284543
-18.302966	-1.777682	0.980941	0.003596	0.284512
-18.479624	-1.798648	0.985946	0.003629	0.284242
-17.991148	-1.886506	0.990950	0.003538	0.284247
-18.786510	-1.762118	0.995955	0.003686	0.284144
-19.195090	-1.730461	1.000960	0.003762	0.283926
-18.659895	-1.829804	1.005965	0.003662	0.283916
-19.124844	-1.770713	1.010970	0.003749	0.283786
-19.272293	-1.779900	1.015974	0.003776	0.283602
-19.059403	-1.819473	1.020979	0.003737	0.283598
-18.301374	-1.998420	1.025984	0.003596	0.283388
-19.250793	-1.850493	1.030989	0.003773	0.283262
-19.144772	-1.873100	1.035994	0.003753	0.283245
-19.111300	-1.931461	1.040998	0.003747	0.282977
-19.550866	-1.852983	1.046003	0.003828	0.282970
-19.544547	-1.881926	1.051008	0.003827	0.282827
-19.841654	-1.864862	1.056013	0.003883	0.282638
-19.997239	-1.838106	1.061018	0.003912	0.282630
-20.334674	-1.814749	1.066022	0.003974	0.282436
-20.460944	-1.814074	1.071027	0.003998	0.282321
-19.898565	-1.917847	1.076032	0.003893	0.282313
-19.812227	-1.998077	1.081037	0.003877	0.281982
-20.619422	-1.850134	1.086042	0.004028	0.281988
-20.758923	-1.841490	1.091046	0.004054	0.281902
-20.650591	-1.901153	1.096051	0.004033	0.281697
-20.792191	-1.874976	1.101056	0.004060	0.281699
-20.899836	-1.901642	1.106061	0.004080	0.281461
-21.075392	-1.889395	1.111066	0.004113	0.281360
-21.176631	-1.873246	1.116070	0.004131	0.281348
-21.110452	-1.942470	1.121075	0.004119	0.281054
-21.468660	-1.872979	1.126080	0.004186	0.281076
-21.701319	-1.863523	1.131085	0.004229	0.280907
-22.495678	-1.747047	1.136090	0.004377	0.280763
-21.775955	-1.877903	1.141094	0.004243	0.280763
-21.840305	-1.901660	1.146099	0.004255	0.280580
-22.283038	-1.833215	1.151104	0.004338	0.280517
-21.863399	-1.916983	1.156109	0.004259	0.280479
-22.417709	-1.875472	1.161114	0.004363	0.280173
-22.588308	-1.842388	1.166118	0.004394	0.280183
-22.839023	-1.823937	1.171123	0.004441	0.280043
-22.663353	-1.891709	1.176128	0.004408	0.279858
-22.521310	-1.917731	1.181133	0.004382	0.279857
-23.630619	-1.765559	1.186138	0.004588	0.279600
-23.345592	-1.827295	1.191142	0.004535	0.279549
-23.356950	-1.828204	1.196147	0.004538	0.279533
-23.929351	-1.777041	1.201152	0.004644	0.279259
-23.884420	-1.784208	1.206157	0.004636	0.279264
-23.517230	-1.867996	1.211162	0.004568	0.279176
-23.524971	-1.917786	1.216166	0.004569	0.278910
-24.045977	-1.823888	1.221171	0.004666	0.278906
-24.111729	-1.841728	1.226176	0.004678	0.278751
-24.406840	-1.814815	1.231181	0.004733	0.278612
-24.631924	-1.774571	1.236186	0.004775	0.278608
-24.170202	-1.905492	1.241190	0.004689	0.278364
-24.412125	-1.878469	1.246195	0.004734	0.278276
-25.084857	-1.758459	1.251200	0.004859	0.278264
-25.206426	-1.783480	1.256205	0.004882	0.278018
-25.440156	-1.741171	1.261210	0.004926	0.278017
-24.923511	-1.852901	1.266214	0.004829	0.277924
-25.612652	-1.779304	1.271219	0.004958	0.277655
-25.280317	-1.839293	1.276224	0.004896	0.277657
-25.411026	-1.842655	1.281229	0.004920	0.277516
-26.223850	-1.725544	1.286234	0.005072	0.277355
-26.232095	-1.721557	1.291238	0.005073	0.277368
-25.917431	-1.817015	1.296243	0.005015	0.277168
-26.301234	-1.775729	1.301248	0.005086	0.277019
-25.852177	-1.856774	1.306253	0.005003	0.277023
-26.288728	-1.827711	1.311258	0.005084	0.276759
-26.067014	-1.875076	1.316262	0.005043	0.276722
-26.618282	-1.785500	1.321267	0.005145	0.276667
-26.831034	-1.797418	1.326272	0.005185	0.276402
-26.892789	-1.783898	1.331277	0.005196	0.276413
-27.109198	-1.772881	1.336282	0.005237	0.276265
-27.613673	-1.710449	1.341286	0.005331	0.276111
-27.262839	-1.776791	1.346291	0.005265	0.276098
-27.262324	-1.811065	1.351296	0.005265	0.275918
-27.861934	-1.727426	1.356301	0.005377	0.275785
-27.683878	-1.760138	1.361306	0.005344	0.275783
-27.230770	-1.875811	1.366310	0.005259	0.275608
-27.634329	-1.820967	1.371315	0.005335	0.275511
-27.597692	-1.833071	1.376320	0.005328	0.275482
-27.882279	-1.835616	1.381325	0.005381	0.275197
-28.513554	-1.720824	1.386330	0.005498	0.275197
-28.466890	-1.747715	1.391334	0.005490	0.275100
-28.450558	-1.793109	1.396339	0.005487	0.274876
-28.571954	-1.770338	1.401344	0.005509	0.274880
-28.582613	-1.802538	1.406349	0.005511	0.274700
-29.264013	-1.706025	1.411354	0.005638	0.274555
-28.556736	-1.834668	1.416358	0.005506	0.274555
-28.988677	-1.803296	1.421363	0.005587	0.274306
-29.404012	-1.735420	1.426368	0.005664	0.274266
-29.507285	-1.714360	1.431373	0.005683	0.274278
-29.992946	-1.690485	1.436378	0.005774	0.273937
-29.148728	-1.847774	1.441382	0.005617	0.273917
-29.607810	-1.777227	1.446387	0.005702	0.273849
-30.178165	-1.715521	1.451392	0.005808	0.273626
-30.400707	-1.673649	1.456397	0.005850	0.273634
-30.305117	-1.715581	1.461402	0.005832	0.273504
-29.880337	-1.832898	1.466406	0.005753	0.273292
-30.168787	-1.778217	1.471411	0.005807	0.273303
-30.541222	-1.749523	1.476416	0.005876	0.273096
-30.652839	-1.743654	1.481421	0.005897	0.273020
-30.591440	-1.756757	1.486426	0.005885	0.273009
-30.565454	-1.819049	1.491430	0.005881	0.272704
-30.934994	-1.758715	1.496435	0.005949	0.272667
-30.781117	-1.805005	1.501440	0.005921	0.272570
-30.966756	-1.810745	1.506445	0.005955	0.272360
-31.240372	-1.761278	1.511450	0.006006	0.272358
-30.982882	-1.844601	1.516454	0.005958	0.272164
-31.424060	-1.790444	1.521459	0.006041	0.272025
-31.677129	-1.743030	1.526464	0.006088	0.272033
-31.052564	-1.911716	1.531469	0.005971	0.271739
-31.733669	-1.789247	1.536474	0.006098	0.271732
-32.148277	-1.734411	1.541478	0.006175	0.271622
-32.222217	-1.761340	1.546483	0.006189	0.271406
-31.613012	-1.873539	1.551488	0.006076	0.271399
-31.785215	-1.887267	1.556493	0.006108	0.271158
-32.002937	-1.864071	1.561498	0.006149	0.271071
-31.852227	-1.907553	1.566502	0.006120	0.270985
-32.597822	-1.810351	1.571507	0.006259	0.270779
-32.773432	-1.778968	1.576512	0.006292	0.270776
-32.157836	-1.926334	1.581517	0.006177	0.270587
-32.339734	-1.909943	1.586522	0.006211	0.270498
-32.110373	-1.978765	1.591526	0.006169	0.270352
-32.909389	-1.869778	1.596531	0.006317	0.270158
-32.848465	-1.880230	1.601536	0.006306	0.270161
-33.107917	-1.889945	1.606541	0.006354	0.269856
-33.553927	-1.809750	1.611546	0.006437	0.269851
-33.052907	-1.929628	1.616550	0.006344	0.269696
-34.066685	-1.775381	1.621555	0.006533	0.269534
-33.514840	-1.880484	1.626560	0.006430	0.269509
-33.696952	-1.894538	1.631565	0.006464	0.269255
-34.280710	-1.789155	1.636570	0.006573	0.269251
-34.300492	-1.810133	1.641574	0.006576	0.269118
-34.297732	-1.851587	1.646579	0.006576	0.268898
-33.855068	-1.934188	1.651584	0.006494	0.268887
-34.134412	-1.934320	1.656589	0.006546	0.268612
-34.796897	-1.819102	1.661594	0.006669	0.268584
-34.437805	-1.907596	1.666598	0.006602	0.268459
-34.977881	-1.844171	1.671603	0.006703	0.268271
-34.933163	-1.853856	1.676608	0.006694	0.268262
-34.690307	-1.946116	1.681613	0.006649	0.268002
-34.969836	-1.900766	1.686618	0.006701	0.267973
-35.400351	-1.850056	1.691622	0.006781	0.267823
-35.512362	-1.864507	1.696627	0.006802	0.267635
-35.089107	-1.944660	1.701632	0.006724	0.267618
-35.503747	-1.923815	1.706637	0.006801	0.267322
-35.674551	-1.895800	1.711642	0.006833	0.267306
-35.479734	-1.966028	1.716646	0.006796	0.267117
-36.357317	-1.827622	1.721651	0.006960	0.267002
-36.475803	-1.810715	1.726656	0.006982	0.266977
-36.679246	-1.819333	1.731661	0.007020	0.266729
-36.660495	-1.824377	1.736666	0.007016	0.266720
-36.371346	-1.907370	1.741670	0.006962	0.266555
-36.781289	-1.865923	1.746675	0.007039	0.266375
-36.516137	-1.915489	1.751680	0.006989	0.266367
-36.376623	-1.997675	1.756685	0.006964	0.266058
-36.842243	-1.915362	1.761690	0.007050	0.266045
-36.659039	-1.985507	1.766694	0.007016	0.265845
-37.012927	-1.941650	1.771699	0.007082	0.265733
-37.219295	-1.917531	1.776704	0.007120	0.265660
-36.978588	-1.994337	1.781709	0.007076	0.265480
-37.000415	-1.992607	1.786714	0.007080	0.265467
-37.421618	-1.975218	1.791718	0.007158	0.265144
-37.898370	-1.890087	1.796723	0.007247	0.265135
-37.563406	-1.984437	1.801728	0.007185	0.264952
-37.869946	-1.952163	1.806733	0.007242	0.264824
-38.204814	-1.904373	1.811738	0.007304	0.264752
-38.767393	-1.846877	1.816742	0.007409	0.264507
-38.706610	-1.858119	1.821747	0.007397	0.264506
-39.037417	-1.829258	1.826752	0.007459	0.264334
-39.265472	-1.806636	1.831757	0.007502	0.264231
-39.117275	-1.835816	1.836762	0.007474	0.264218
-38.747979	-1.961708	1.841766	0.007405	0.263896
-39.599867	-1.810240	1.846771	0.007564	0.263877
-39.527767	-1.845803	1.851776	0.007550	0.263754
-39.539658	-1.876061	1.856781	0.007553	0.263576
-39.910590	-1.809123	1.861786	0.007622	0.263573
-39.795492	-1.874604	1.866790	0.007600	0.263328
-40.026886	-1.844612	1.871795	0.007643	0.263261
-39.838787	-1.894916	1.876800	0.007608	0.263172
-40.434497	-1.823368	1.881805	0.007719	0.262970
-40.598879	-1.792768	1.886810	0.007750	0.262973
-40.690650	-1.811304	1.891814	0.007767	0.262779
-41.625684	-1.664014	1.896819	0.007941	0.262653
-41.383035	-1.710041	1.901824	0.007896	0.262643
-41.082852	-1.801786	1.906829	0.007840	0.262438
-41.922266	-1.668356	1.911834	0.007996	0.262332
-41.287326	-1.786575	1.916838	0.007878	0.262316
-40.959139	-1.902158	1.921843	0.007817	0.262008
-41.675393	-1.774827	1.926848	0.007950	0.261991
-41.496545	-1.824080	1.931853	0.007917	0.261899
-41.725857	-1.818533	1.936858	0.007960	0.261699
-41.719157	-1.817859	1.941862	0.007959	0.261709
-42.314025	-1.752905	1.946867	0.008069	0.261469
-41.936658	-1.842038	1.951872	0.007999	0.261356
-41.720401	-1.888868	1.956877	0.007959	0.261314
-42.312933	-1.828862	1.961882	0.008069	0.261049
-41.972271	-1.891591	1.966886	0.008006	0.261045
-41.799601	-1.960884	1.971891	0.007974	0.260835
-43.132825	-1.732829	1.976896	0.008222	0.260754
-42.832815	-1.792061	1.981901	0.008166	0.260728
-42.442805	-1.907959	1.986906	0.008094	0.260478
-42.298074	-1.933016	1.991910	0.008067	0.260485
-42.899262	-1.866341	1.996915	0.008179	0.260248
-42.874921	-1.893883	2.001920	0.008174	0.260119

-43.216880	-1.885007	2.011917	0.008238	0.259822
-43.302232	-1.908175	2.021914	0.008254	0.259606
-43.271295	-1.939726	2.031910	0.008248	0.259461
-43.583379	-1.928292	2.041907	0.008306	0.259208
-43.823817	-1.898042	2.051904	0.008351	0.259132
-44.329885	-1.852798	2.061901	0.008445	0.258870
-44.228600	-1.871393	2.071898	0.008426	0.258869
-44.534309	-1.854343	2.081894	0.008483	0.258653
-44.526467	-1.871566	2.091891	0.008482	0.258564
-44.549061	-1.868022	2.101888	0.008486	0.258561
-44.371246	-1.901265	2.111885	0.008453	0.258556
-44.508776	-1.919720	2.121882	0.008479	0.258312
-44.673828	-1.903102	2.131878	0.008509	0.258237
-45.044868	-1.829782	2.141875	0.008578	0.258269
-45.294302	-1.785006	2.151872	0.008625	0.258266
-45.390694	-1.768059	2.161869	0.008643	0.258262
-45.197763	-1.803080	2.171866	0.008607	0.258262
-45.476907	-1.749962	2.181862	0.008659	0.258275
-45.076311	-1.766433	2.191859	0.008584	0.258591
-44.340346	-1.904868	2.201856	0.008448	0.258566
-44.026197	-1.964209	2.211853	0.008389	0.258553
-44.323838	-1.908574	2.221850	0.008445	0.258561
-44.470388	-1.881380	2.231846	0.008472	0.258564
-44.241434	-1.922026	2.241843	0.008429	0.258570
-44.453395	-1.884756	2.251840	0.008469	0.258562
-44.296482	-1.866812	2.261837	0.008440	0.258823
-43.880968	-1.935315	2.271834	0.008362	0.258862
-43.756333	-1.958804	2.281830	0.008339	0.258857
-43.643157	-1.977677	2.291827	0.008318	0.258867
-43.550936	-1.945294	2.301824	0.008301	0.259142
-43.409564	-1.961620	2.311821	0.008275	0.259194
-43.829382	-1.882578	2.321818	0.008353	0.259209
-43.832423	-1.840692	2.331814	0.008353	0.259439
-43.038081	-1.976593	2.341811	0.008205	0.259487
-43.640759	-1.844212	2.351808	0.008318	0.259614
-43.270552	-1.871973	2.361805	0.008249	0.259835
-44.056612	-1.708838	2.371802	0.008395	0.259947
-43.080785	-1.848639	2.381798	0.008213	0.260157
-42.826322	-1.879527	2.391795	0.008166	0.260242
-43.209089	-1.762486	2.401792	0.008237	0.260506
-42.848344	-1.809344	2.411789	0.008170	0.260610
-42.653479	-1.821805	2.421786	0.008134	0.260738
-42.690405	-1.774320	2.431782	0.008141	0.260964
-42.293125	-1.829608	2.441779	0.008067	0.261058
-42.239663	-1.784877	2.451776	0.008057	0.261360
-41.991740	-1.808732	2.461773	0.008011	0.261477
-41.683779	-1.825809	2.471770	0.007954	0.261693
-41.579693	-1.808964	2.481766	0.007934	0.261890
-41.148451	-1.870562	2.491763	0.007854	0.261983
-41.225028	-1.796291	2.501760	0.007868	0.262317
-41.062412	-1.799096	2.511757	0.007838	0.262464
-41.278858	-1.727666	2.521754	0.007878	0.262641
-40.424955	-1.825501	2.531750	0.007719	0.262958
-39.860702	-1.909216	2.541747	0.007614	0.263062
-39.867829	-1.873715	2.551744	0.007616	0.263250
-39.810273	-1.839741	2.561741	0.007605	0.263494
-39.991824	-1.777610	2.571738	0.007639	0.263654
-39.833721	-1.760491	2.581734	0.007609	0.263906
-39.300217	-1.808140	2.591731	0.007510	0.264176
-39.474208	-1.742883	2.601728	0.007542	0.264360
-38.918519	-1.814473	2.611725	0.007439	0.264522
-38.801933	-1.778125	2.621722	0.007417	0.264837
-38.071384	-1.881264	2.631718	0.007281	0.264999
-38.058041	-1.853151	2.641715	0.007279	0.265166
-38.016823	-1.799557	2.651712	0.007271	0.265499
-37.664438	-1.834727	2.661709	0.007206	0.265657
-37.712407	-1.795824	2.671706	0.007215	0.265821
-37.020289	-1.876120	2.681702	0.007086	0.266069
-36.543219	-1.922878	2.691699	0.006997	0.266287
-36.831078	-1.838132	2.701696	0.007051	0.266463
-36.480652	-1.856020	2.711693	0.006985	0.266712
-36.291084	-1.845373	2.721690	0.006950	0.266956
-36.101949	-1.844175	2.731686	0.006915	0.267149
-35.394990	-1.943155	2.741683	0.006783	0.267309
-35.726360	-1.822293	2.751680	0.006845	0.267637
-35.841550	-1.756667	2.761677	0.006867	0.267879
-35.441043	-1.790579	2.771674	0.006792	0.268089
-34.734304	-1.886910	2.781670	0.006660	0.268263
-34.784748	-1.818179	2.791667	0.006670	0.268584
-34.029309	-1.922715	2.801664	0.006529	0.268761
-34.215382	-1.853204	2.811661	0.006564	0.268953
-33.892548	-1.859885	2.821658	0.006504	0.269233
-33.590166	-1.870027	2.831654	0.006448	0.269474
-33.683475	-1.816463	2.841651	0.006465	0.269670
-32.918169	-1.921441	2.851648	0.006323	0.269854
-32.710594	-1.902261	2.861645	0.006284	0.270159
-32.411236	-1.918540	2.871642	0.006228	0.270363
-32.435482	-1.878614	2.881638	0.006233	0.270553
-32.253409	-1.872150	2.891635	0.006199	0.270765
-32.006438	-1.866459	2.901632	0.006153	0.271035
-32.310233	-1.768788	2.911629	0.006209	0.271262
-31.836988	-1.812084	2.921626	0.006121	0.271490
-31.302398	-1.865506	2.931622	0.006022	0.271723
-30.598546	-1.943439	2.941619	0.005891	0.271990
-30.260681	-1.970844	2.951616	0.005828	0.272171
-30.099783	-1.970862	2.961613	0.005798	0.272326
-29.932984	-1.943589	2.971610	0.005767	0.272632
-29.697037	-1.946490	2.981606	0.005723	0.272844
-30.031282	-1.844571	2.991603	0.005785	0.273062
-30.087719	-1.789190	3.001600	0.005796	0.273301
-29.882534	-1.768975	3.011597	0.005758	0.273606
-28.663072	-1.949926	3.021594	0.005531	0.273822
-28.876805	-1.870346	3.031590	0.005570	0.274037
-28.848006	-1.829608	3.041587	0.005565	0.274279
-28.372055	-1.867632	3.051584	0.005477	0.274535
-28.257081	-1.841076	3.061581	0.005455	0.274785
-27.978286	-1.847988	3.071578	0.005403	0.275016
-27.719045	-1.851788	3.081574	0.005355	0.275244
-27.113406	-1.911802	3.091571	0.005242	0.275507
-26.755022	-1.940683	3.101568	0.005176	0.275698
-27.402260	-1.781526	3.111565	0.005296	0.275915
-26.777105	-1.852235	3.121562	0.005180	0.276140
-26.495519	-1.858513	3.131558	0.005127	0.276376
-26.123264	-1.865359	3.141555	0.005058	0.276694
-25.695287	-1.907427	3.151552	0.004978	0.276881
-25.468111	-1.914054	3.161549	0.004936	0.277062
-24.946131	-1.962064	3.171546	0.004839	0.277307
-25.007671	-1.898941	3.181542	0.004850	0.277578
-24.594564	-1.933761	3.191539	0.004774	0.277788
-24.791401	-1.851175	3.201536	0.004810	0.278031
-24.928771	-1.778641	3.211533	0.004836	0.278279
-25.144086	-1.677043	3.221530	0.004876	0.278603
-24.371163	-1.767766	3.231526	0.004732	0.278862
-23.882048	-1.810176	3.241523	0.004641	0.279103
-23.723480	-1.793853	3.251520	0.004612	0.279337
-23.039438	-1.881606	3.261517	0.004484	0.279527
-23.120786	-1.801952	3.271514	0.004499	0.279862
-23.215268	-1.735485	3.281510	0.004517	0.280117
-22.561962	-1.806863	3.291507	0.004395	0.280362
-21.865249	-1.895849	3.301504	0.004266	0.280556
-21.778761	-1.876205	3.311501	0.004250	0.280739
-21.424396	-1.888689	3.321498	0.004184	0.281006
-21.174642	-1.898890	3.331494	0.004137	0.281187
-20.995284	-1.888562	3.341491	0.004104	0.281408
-20.532757	-1.918986	3.351488	0.004018	0.281684
-20.249427	-1.927155	3.361485	0.003965	0.281907
-20.367403	-1.866576	3.371482	0.003987	0.282107
-19.906414	-1.910166	3.381478	0.003901	0.282313
-19.542077	-1.917130	3.391475	0.003833	0.282617
-19.384998	-1.902462	3.401472	0.003804	0.282838
-18.783993	-1.979158	3.411469	0.003692	0.283005
-18.794466	-1.932008	3.421466	0.003694	0.283236
-18.752745	-1.885560	3.431462	0.003687	0.283512
-18.131747	-1.961485	3.441459	0.003571	0.283701
-18.464892	-1.857918	3.451456	0.003633	0.283920
-18.276435	-1.832651	3.461453	0.003598	0.284223
-17.798688	-1.874204	3.471450	0.003509	0.284453
-17.530031	-1.885267	3.481446	0.003459	0.284645
-17.497681	-1.842536	3.491443	0.003453	0.284892
-17.034972	-1.877463	3.501440	0.003367	0.285142
-16.898251	-1.842708	3.511437	0.003341	0.285444
-16.830286	-1.816541	3.521434	0.003329	0.285640
-16.599196	-1.821078	3.531430	0.003286	0.285829
-16.682017	-1.751270	3.541427	0.003301	0.286106
-16.026114	-1.817052	3.551424	0.003179	0.286376
-15.043554	-1.948355	3.561421	0.002996	0.286615
-15.136955	-1.896974	3.571418	0.003014	0.286789
-14.572275	-1.961170	3.581414	0.002909	0.286983
-14.547025	-1.905989	3.591411	0.002904	0.287284
-14.247229	-1.924167	3.601408	0.002848	0.287467
-13.886697	-1.954255	3.611405	0.002781	0.287645
-13.808830	-1.907331	3.621402	0.002766	0.287952
-13.399109	-1.940306	3.631398	0.002690	0.288161
-13.340940	-1.914670	3.641395	0.002679	0.288342
-12.735215	-1.981295	3.651392	0.002567	0.288560
-12.504843	-1.971011	3.661389	0.002524	0.288822
-13.019559	-1.834510	3.671386	0.002620	0.289037
-12.156832	-1.951513	3.681382	0.002459	0.289236
-12.289814	-1.873462	3.691379	0.002484	0.289505
-12.130099	-1.852364	3.701376	0.002454	0.289756
-11.846604	-1.860649	3.711373	0.002401	0.289971
-11.476593	-1.885811	3.721370	0.002332	0.290181
-10.757190	-1.955913	3.731366	0.002199	0.290484
-10.709402	-1.932058	3.741363	0.002190	0.290646
-10.642264	-1.908802	3.751360	0.002177	0.290822
-10.472657	-1.891035	3.761357	0.002146	0.291064
-10.085626	-1.905471	3.771354	0.002074	0.291341
-9.718137	-1.930641	3.781350	0.002005	0.291548
-9.385337	-1.953654	3.791347	0.001943	0.291734
-8.892674	-1.991401	3.801344	0.001852	0.291991
-8.896911	-1.949782	3.811341	0.001852	0.292193
-8.628873	-1.961708	3.821338	0.001803	0.292375
-7.592027	-2.101409	3.831334	0.001610	0.292616
-7.754304	-2.030887	3.841331	0.001640	0.292819
-7.484686	-2.048534	3.851328	0.001590	0.292973
-7.267164	-2.031511	3.861325	0.001549	0.293253
-6.902870	-2.067389	3.871322	0.001481	0.293402
-6.034175	-2.193642	3.881318	0.001320	0.293558
-5.897501	-2.170746	3.891315	0.001294	0.293793
-6.153189	-2.098721	3.901312	0.001342	0.293919
-5.872967	-2.088087	3.911309	0.001290	0.294222
-5.737318	-2.080288	3.921306	0.001265	0.294381
-5.569088	-2.081439	3.931302	0.001233	0.294526
-5.381278	-2.051272	3.941299	0.001198	0.294841
-5.192546	-2.049053	3.951296	0.001163	0.295020
-4.748497	-2.099998	3.961293	0.001081	0.295166
-4.442818	-2.087346	3.971290	0.001024	0.295500
-4.339443	-2.082719	3.981286	0.001004	0.295615
-4.282866	-2.064989	3.991283	0.000994	0.295752
-3.826097	-2.084564	4.001280	0.000909	0.296062
-3.463714	-2.121412	4.011277	0.000841	0.296203
-3.100589	-2.154140	4.021274	0.000774	0.296366
-3.081037	-2.094664	4.031270	0.000770	0.296673
-2.825020	-2.111333	4.041267	0.000723	0.296819
-2.711848	-2.096464	4.051264	0.000702	0.296991
-2.379311	-2.097528	4.061261	0.000640	0.297280
-1.823575	-2.170636	4.071258	0.000536	0.297416
-1.618045	-2.166613	4.081254	0.000498	0.297617
-1.390571	-2.151480	4.091251	0.000456	0.297891
-0.971884	-2.202885	4.101248	0.000378	0.298011
-0.894525	-2.170212	4.111245	0.000363	0.298238
-0.776561	-2.149054	4.121242	0.000341	0.298444
-1.142527	-2.043364	4.131238	0.000410	0.298634
-1.046091	-2.009476	4.141235	0.000392	0.298883
-0.845564	-1.985046	4.151232	0.000354	0.299177
-0.602826	-1.987938	4.161229	0.000309	0.299376
-0.318529	-1.996992	4.171226	0.000256	0.299582
0.138485	-2.029963	4.181222	0.000171	0.299824
-0.232001	-1.902288	4.191219	0.000240	0.300115
-0.460027	-1.802947	4.201216	0.000282	0.300394
-0.470212	-1.752054	4.211213	0.000284	0.300630
-0.724998	-1.649836	4.221210	0.000332	0.300898
-0.523583	-1.622381	4.231206	0.000294	0.301206
-0.815169	-1.501531	4.241203	0.000349	0.301532
-0.187513	-1.550841	4.251200	0.000232	0.301842
0.164013	-1.554086	4.261197	0.000166	0.302133
0.245257	-1.503356	4.271194	0.000151	0.302446
-0.040042	-1.377339	4.281190	0.000204	0.302800
0.240197	-1.359396	4.291187	0.000152	0.303129
0.203471	-1.281677	4.301184	0.000159	0.303468
-0.190829	-1.136539	4.311181	0.000232	0.303818
-0.497601	-0.984571	4.321178	0.000289	0.304276
-0.315333	-0.938974	4.331174	0.000255	0.304650
-0.293809	-0.860406	4.341171	0.000251	0.305041
-0.093780	-0.802280	4.351168	0.000214	0.305489
0.026725	-0.744604	4.361165	0.000192	0.305865
0.048751	-0.664858	4.371162	0.000187	0.306261
0.038315	-0.563667	4.381158	0.000189	0.306730
0.109192	-0.488077	4.391155	0.000176	0.307146
0.332573	-0.437336	4.401152	0.000135	0.307576
0.497416	-0.361762	4.411149	0.000104	0.308072
0.324171	-0.242441	4.421146	0.000136	0.308484
0.614222	-0.183546	4.431142	0.000082	0.309007
0.426975	-0.057635	4.441139	0.000117	0.309437
0.506887	0.041092	4.451136	0.000102	0.309966
0.000000	0.225988	4.461133	0.000196	0.310399

-0.243741	0.538696	4.466138	0.000241	0.311647
-0.167960	1.084959	4.471142	0.000227	0.314236
0.288045	1.839027	4.476147	0.000142	0.318066
0.693721	2.896555	4.481152	0.000065	0.323171
0.752988	4.311914	4.486157	0.000053	0.329494
1.030597	5.982191	4.491162	0.000001	0.336965
1.630640	7.888913	4.496166	-0.000112	0.345510
1.918437	10.170184	4.501171	-0.000167	0.355147
2.518058	12.693378	4.506176	-0.000281	0.365712
2.642027	15.626742	4.511181	-0.000306	0.377224
3.184438	18.814021	4.516186	-0.000409	0.389621
3.463808	22.382082	4.521190	-0.000463	0.402834
3.476242	26.336043	4.526195	-0.000468	0.416800
3.779528	30.584223	4.531200	-0.000527	0.431477
4.046838	35.171013	4.536205	-0.000580	0.446748
4.373869	40.101502	4.541210	-0.000644	0.462624
4.998980	45.321492	4.546214	-0.000764	0.479010
5.525939	50.904569	4.551219	-0.000865	0.495862
5.962030	56.859763	4.556224	-0.000951	0.513163
6.143787	63.166709	4.561229	-0.000988	0.530734
6.754880	69.723408	4.566234	-0.001107	0.548605
7.658868	76.539004	4.571238	-0.001279	0.566706
8.929011	83.601330	4.576243	-0.001520	0.585020
9.429213	91.084448	4.581248	-0.001618	0.603454
10.162079	98.789201	4.586253	-0.001760	0.621954
10.415158	106.839230	4.591258	-0.001812	0.640504
10.427036	115.162384	4.596262	-0.001820	0.659037
10.844643	123.606869	4.601267	-0.001903	0.677477
12.782472	131.984060	4.606272	-0.002269	0.695852
13.545678	140.745422	4.611277	-0.002417	0.714106
14.811615	149.593561	4.616282	-0.002659	0.732253
15.922341	158.615116	4.621286	-0.002871	0.750240
16.847796	167.772638	4.626291	-0.003050	0.768000
17.362779	177.129171	4.631296	-0.003152	0.785590
18.664604	186.419630	4.636301	-0.003400	0.802926
19.019740	195.962662	4.641306	-0.003472	0.820044
19.628267	205.511238	4.646310	-0.003592	0.836900
20.539668	215.017926	4.651315	-0.003768	0.853441
22.912264	224.314608	4.656320	-0.004216	0.869746
23.875319	233.887631	4.661325	-0.004401	0.885795
24.838002	243.484689	4.666330	-0.004587	0.901596
26.436053	252.965842	4.671334	-0.004890	0.917118
27.441238	262.536111	4.676339	-0.005084	0.932356
28.786777	272.043069	4.681344	-0.005340	0.947344
29.738151	281.587153	4.686349	-0.005524	0.962049
31.097635	291.052861	4.691354	-0.005783	0.976521
31.836678	300.608076	4.696358	-0.005927	0.990754
32.453626	310.095448	4.701363	-0.006048	1.004657
33.401637	319.488590	4.706368	-0.006231	1.018318
34.655916	328.785555	4.711373	-0.006470	1.031736
35.132271	338.182989	4.716378	-0.006565	1.044934
36.282626	347.424369	4.721382	-0.006785	1.057913
36.837821	356.714156	4.726387	-0.006895	1.070661
38.463937	365.755478	4.731392	-0.007203	1.083174
39.187931	374.933981	4.736397	-0.007344	1.095518
39.486906	384.139826	4.741402	-0.007406	1.107664
40.005102	393.233321	4.746406	-0.007508	1.119582
41.173212	402.186822	4.751411	-0.007731	1.131339
42.869241	411.015763	4.756416	-0.008053	1.142930
43.798019	419.972236	4.761421	-0.008232	1.154400
43.737254	429.022062	4.766426	-0.008226	1.165661
45.020516	437.800272	4.771430	-0.008471	1.176764
46.383703	446.537284	4.776435	-0.008730	1.187728
47.519757	455.306187	4.781440	-0.008948	1.198584
48.416774	464.066883	4.786445	-0.009120	1.209282
48.632151	472.927852	4.791450	-0.009166	1.219868
48.816866	481.754655	4.796454	-0.009206	1.230317
49.672420	490.387207	4.801459	-0.009371	1.240584
50.185332	499.092701	4.806464	-0.009472	1.250783
51.516747	507.597852	4.811469	-0.009726	1.260828
52.496024	516.175551	4.816474	-0.009914	1.270809
53.354316	524.744452	4.821478	-0.010079	1.280678
53.531358	533.420577	4.826483	-0.010118	1.290462
53.845217	542.047088	4.831488	-0.010182	1.300144
54.067092	550.679724	4.836493	-0.010229	1.309743
55.711187	559.045320	4.841498	-0.010540	1.319242
56.463407	567.515528	4.846502	-0.010686	1.328623
57.141653	575.975378	4.851507	-0.010818	1.337913
57.980517	584.413576	4.856512	-0.010979	1.347145
58.612233	592.875770	4.861517	-0.011102	1.356302
59.590818	601.237895	4.866522	-0.011290	1.365352
60.350808	609.664183	4.871526	-0.011437	1.374372
60.719668	618.124806	4.876531	-0.011511	1.383301
61.563429	626.509731	4.881536	-0.011674	1.392175
62.479860	634.833907	4.886541	-0.011850	1.400943
62.918350	643.267835	4.891546	-0.011937	1.409687
63.648430	651.634061	4.896550	-0.012078	1.418357
64.490227	659.967835	4.901555	-0.012241	1.426960
64.835894	668.395195	4.906560	-0.012310	1.435522
65.200929	676.764151	4.911565	-0.012384	1.443979
65.493269	685.144852	4.916570	-0.012444	1.452386
66.174788	693.453366	4.921574	-0.012576	1.460736
67.104710	701.721795	4.926579	-0.012755	1.469040
67.316309	710.126190	4.931584	-0.012799	1.477314
67.290713	718.502690	4.936589	-0.012800	1.485477
68.320466	726.706836	4.941594	-0.012997	1.493595
69.190834	734.933635	4.946598	-0.013165	1.501666
70.061828	743.159295	4.951603	-0.013332	1.509693
70.598106	751.465391	4.956608	-0.013437	1.517702
70.880065	759.776796	4.961613	-0.013495	1.525633
71.442892	768.074372	4.966618	-0.013605	1.533554
72.514732	776.250517	4.971622	-0.013810	1.541398
72.639516	784.610021	4.976627	-0.013839	1.549229
72.955485	792.916231	4.981632	-0.013903	1.557000
73.157382	801.186307	4.986637	-0.013946	1.564682
74.025880	809.369205	4.991642	-0.014113	1.572345
74.664445	817.607248	4.996646	-0.014238	1.579987
74.888828	825.906890	5.001651	-0.014285	1.587588
75.588861	834.115091	5.006656	-0.014420	1.595138
76.526513	842.257745	5.011661	-0.014600	1.602629
77.663514	850.389121	5.016666	-0.014817	1.610103
78.389678	858.637200	5.021670	-0.014958	1.617587
79.414239	866.777056	5.026675	-0.015154	1.624982
79.955211	875.094843	5.031680	-0.015260	1.632433
80.565570	883.285430	5.036685	-0.015379	1.639747
80.999043	891.530386	5.041690	-0.015465	1.647052
81.644138	899.742385	5.046694	-0.015591	1.654325
82.407203	907.915171	5.051699	-0.015738	1.661548
83.189823	916.096036	5.056704	-0.015889	1.668749
83.819926	924.306056	5.061709	-0.016012	1.675923
84.094423	932.558258	5.066714	-0.016068	1.683054
84.669449	940.738727	5.071718	-0.016180	1.690135
84.986294	948.983698	5.076723	-0.016245	1.697205
85.138824	957.241530	5.081728	-0.016279	1.704236
85.795741	965.372898	5.086733	-0.016406	1.711197
86.274516	973.571436	5.091738	-0.016501	1.718163
86.876259	981.723591	5.096742	-0.016618	1.725079
87.251803	989.930697	5.101747	-0.016693	1.731982
88.031349	998.071151	5.106752	-0.016844	1.738856
88.615868	1006.220920	5.111757	-0.016958	1.745684
89.141898	1014.406534	5.116762	-0.017061	1.752508
89.559161	1022.603045	5.121766	-0.017144	1.759300
89.947217	1030.766361	5.126771	-0.017222	1.766034
90.682832	1038.917112	5.131776	-0.017364	1.772777
91.064532	1047.099865	5.136781	-0.017440	1.779476
91.546099	1055.271836	5.141786	-0.017535	1.786153
91.962989	1063.502029	5.146790	-0.017618	1.792844
92.116020	1071.670739	5.151795	-0.017652	1.799427
92.060396	1079.897261	5.156800	-0.017647	1.806007
92.906221	1087.952418	5.161805	-0.017810	1.812538
93.449507	1096.086296	5.166810	-0.017916	1.819070
94.147861	1104.197943	5.171814	-0.018052	1.825580
94.179266	1112.423054	5.176819	-0.018063	1.832075
95.056947	1120.504694	5.181824	-0.018231	1.838537
95.519055	1128.637355	5.186829	-0.018323	1.844966
95.745734	1136.829470	5.191834	-0.018370	1.851390
96.637250	1144.917964	5.196838	-0.018542	1.857791
96.788082	1153.091841	5.201843	-0.018575	1.864148
97.418814	1161.217795	5.206848	-0.018698	1.870503
98.186940	1169.299396	5.211853	-0.018846	1.876819
99.009749	1177.378998	5.216858	-0.019004	1.883117
99.952210	1185.461414	5.221862	-0.019185	1.889411
100.337749	1193.638344	5.226867	-0.019262	1.895691
100.715386	1201.836769	5.231872	-0.019338	1.901965
101.369532	1209.938630	5.236877	-0.019465	1.908177
101.992235	1218.052816	5.241882	-0.019586	1.914375
102.576839	1226.200698	5.246886	-0.019700	1.920574
103.320554	1234.279015	5.251891	-0.019844	1.926718
103.902002	1242.443483	5.256896	-0.019958	1.932888
104.063302	1250.631991	5.261901	-0.019993	1.939010
104.478054	1258.769154	5.266906	-0.020076	1.945102
104.399614	1267.015623	5.271910	-0.020066	1.951201
104.407956	1275.143931	5.276915	-0.020073	1.957203
105.630630	1283.085164	5.281920	-0.020306	1.963184
105.798952	1291.256618	5.286925	-0.020343	1.969199
106.106299	1299.385798	5.291930	-0.020405	1.975180
106.424771	1307.527091	5.296934	-0.020470	1.981153
106.792537	1315.632344	5.301939	-0.020543	1.987087
107.702220	1323.687703	5.306944	-0.020718	1.993026
108.155957	1331.805595	5.311949	-0.020808	1.998943
108.829820	1339.863315	5.316954	-0.020939	2.004822
109.402899	1347.988328	5.321958	-0.021051	2.010722
109.724979	1356.137240	5.326963	-0.021116	2.016594
110.263205	1364.249685	5.331968	-0.021221	2.022447
110.241750	1372.434991	5.336973	-0.021223	2.028275
110.733587	1380.522784	5.341978	-0.021319	2.034071
111.871609	1388.488051	5.346982	-0.021537	2.039831
112.248866	1396.595008	5.351987	-0.021612	2.045596
112.786319	1404.709324	5.356992	-0.021717	2.051366
113.098837	1412.865575	5.361997	-0.021781	2.057126
113.648064	1420.952582	5.367002	-0.021888	2.062846
114.065422	1429.084534	5.372006	-0.021971	2.068567
114.547792	1437.157999	5.377011	-0.022066	2.074239
115.002166	1445.279444	5.382016	-0.022156	2.079925
115.374314	1453.382477	5.387021	-0.022231	2.085575
115.216862	1461.590761	5.392026	-0.022207	2.091229
115.674334	1469.693163	5.397030	-0.022297	2.096856
116.345240	1477.707005	5.402035	-0.022428	2.102428
117.235841	1485.757705	5.407040	-0.022599	2.108033
117.850741	1493.872405	5.412045	-0.022718	2.113639
118.060443	1502.001154	5.417050	-0.022763	2.119200
118.407991	1510.087324	5.422054	-0.022833	2.124731
118.936161	1518.163200	5.427059	-0.022936	2.130257
120.306202	1526.137757	5.432064	-0.023197	2.135783
120.311771	1534.321057	5.437069	-0.023203	2.141303
120.888419	1542.389818	5.442074	-0.023316	2.146787
121.751054	1550.449491	5.447078	-0.023481	2.152278
121.980002	1558.588256	5.452083	-0.023529	2.157746
122.271213	1566.692573	5.457088	-0.023589	2.163184
122.217574	1574.883336	5.462093	-0.023584	2.168633
122.563849	1582.970418	5.467098	-0.023654	2.174038
122.936746	1591.063718	5.472102	-0.023729	2.179435
123.695396	1599.042192	5.477107	-0.023875	2.184780
124.590773	1607.095984	5.482112	-0.024047	2.190173
125.236487	1615.177780	5.487117	-0.024172	2.195549
125.499427	1623.294217	5.492122	-0.024227	2.200898
125.854943	1631.401958	5.497126	-0.024298	2.206237
126.334263	1639.489817	5.502131	-0.024393	2.211561
126.168495	1647.688053	5.507136	-0.024367	2.216885
126.833858	1655.680015	5.512141	-0.024496	2.222139
127.502744	1663.720791	5.517146	-0.024626	2.227411
128.144696	1671.792166	5.522150	-0.024751	2.232689
127.881072	1679.988201	5.527155	-0.024707	2.237952
128.344130	1688.036695	5.532160	-0.024798	2.243174
128.274947	1696.196223	5.537165	-0.024791	2.248407
128.221717	1704.318573	5.542170	-0.024786	2.253605
128.798415	1712.339515	5.547174	-0.024899	2.258783
129.149069	1720.395664	5.552179	-0.024969	2.263951
129.359660	1728.524656	5.557184	-0.025014	2.269141
129.992542	1736.574954	5.562189	-0.025137	2.274307
130.687537	1744.551475	5.567194	-0.025272	2.279420
131.194416	1752.598751	5.572198	-0.025371	2.284549
131.260675	1760.721624	5.577203	-0.025389	2.289675
131.643273	1768.809015	5.582208	-0.025465	2.294796
132.263238	1776.825901	5.587213	-0.025586	2.299881
132.905912	1784.851851	5.592218	-0.025711	2.304962
133.495832	1792.942516	5.597222	-0.025826	2.310069
133.625247	1801.060527	5.602227	-0.025855	2.315141
133.751642	1809.176762	5.607232	-0.025884	2.320200
134.257346	1817.211400	5.612237	-0.025983	2.325231
134.784342	1825.278289	5.617242	-0.026087	2.330272
135.087549	1833.387342	5.622246	-0.026149	2.335309
135.181246	1841.481700	5.627251	-0.026171	2.340309
135.562211	1849.552701	5.632256	-0.026247	2.345307
136.338539	1857.589077	5.637261	-0.026397	2.350307
136.882938	1865.638976	5.642266	-0.026504	2.355285
137.222164	1873.726257	5.647270	-0.026572	2.360258
138.155637	1881.689477	5.652275	-0.026751	2.365194
138.356408	1889.809580	5.657280	-0.026794	2.370154
138.769941	1897.905959	5.662285	-0.026876	2.375108
139.240888	1905.972083	5.667290	-0.026969	2.380037
139.431501	1914.086631	5.672294	-0.027010	2.384962
139.391141	1922.233691	5.677299	-0.027008	2.389878
140.114187	1930.223473	5.682304	-0.027147	2.394751
140.643383	1938.252950	5.687309	-0.027251	2.399622
141.103074	1946.282913	5.692314	-0.027342	2.404478
141.421259	1954.405001	5.697318	-0.027407	2.409368
141.907455	1962.463557	5.702323	-0.027502	2.414223
141.966102	1970.594207	5.707328	-0.027519	2.419077
142.222188	1978.655579	5.712333	-0.027571	2.423896
142.271525	1986.774123	5.717338	-0.027586	2.428723
143.370646	1994.775844	5.722342	-0.027796	2.433554
143.531957	2002.849014	5.727347	-0.027831	2.438343
144.218493	2010.824610	5.732352	-0.027964	2.443107
144.650503	2018.900035	5.737357	-0.028050	2.447900
145.051047	2026.953505	5.742362	-0.028130	2.452669
145.189328	2035.068450	5.747366	-0.028161	2.457443
145.959458	2043.045328	5.752371	-0.028309	2.462177
146.313239	2051.150841	5.757376	-0.028380	2.466944
146.546140	2059.253089	5.762381	-0.028429	2.471691
146.604132	2067.342795	5.767386	-0.028445	2.476408
147.318627	2075.358193	5.772390	-0.028583	2.481123
147.789185	2083.363333	5.777395	-0.028676	2.485804
148.200010	2091.443739	5.782400	-0.028758	2.490516
148.303756	2099.578692	5.787405	-0.028782	2.495226
148.878012	2107.597415	5.792410	-0.028895	2.499897
148.946035	2115.706835	5.797414	-0.028912	2.504572
149.305740	2123.751732	5.802419	-0.028985	2.509224
150.294596	2131.710892	5.807424	-0.029174	2.513864
150.508932	2139.802846	5.812429	-0.029219	2.518515
151.445819	2147.763484	5.817434	-0.029399	2.523135
151.765186	2155.881166	5.822438	-0.029464	2.527790
151.896894	2163.998980	5.827443	-0.029493	2.532424
151.743875	2172.132661	5.832448	-0.029470	2.537037
152.077872	2180.187105	5.837453	-0.029538	2.541632
152.623156	2188.204967	5.842458	-0.029644	2.546213
152.799802	2196.297823	5.847462	-0.029682	2.550802
153.222292	2204.308878	5.852467	-0.029766	2.555354
154.057628	2212.316161	5.857472	-0.029927	2.559925
154.005104	2220.428144	5.862477	-0.029923	2.564484
154.134221	2228.522508	5.867482	-0.029952	2.569037
154.468407	2236.590482	5.872486	-0.030019	2.573582
154.509740	2244.664293	5.877491	-0.030032	2.578101
155.186187	2252.629304	5.882496	-0.030163	2.582597
155.444878	2260.717243	5.887501	-0.030217	2.587124
156.368273	2268.745381	5.892506	-0.030394	2.591656
156.473459	2276.903155	5.897510	-0.030419	2.596195
157.014402	2284.862341	5.902515	-0.030525	2.600646
157.465057	2292.884107	5.907520	-0.030614	2.605118
157.674321	2300.984451	5.912525	-0.030658	2.609608
157.985956	2309.027995	5.917530	-0.030721	2.614067
158.284058	2317.098512	5.922534	-0.030782	2.618532
158.273004	2325.177002	5.927539	-0.030785	2.622972
159.100159	2333.115371	5.932544	-0.030945	2.627386
159.458269	2341.181904	5.937549	-0.031016	2.631830
159.612994	2349.276735	5.942554	-0.031050	2.636268
160.098018	2357.276774	5.947558	-0.031146	2.640669
160.150390	2365.377912	5.952563	-0.031161	2.645089
160.744201	2373.382277	5.957568	-0.031277	2.649485
161.242849	2381.438228	5.962573	-0.031375	2.653895
161.284891	2389.523031	5.967578	-0.031388	2.658283
161.668857	2397.590072	5.972582	-0.031465	2.662677
162.702725	2405.533527	5.977587	-0.031662	2.667040
163.043012	2413.620933	5.982592	-0.031731	2.671427
163.021462	2421.767944	5.987597	-0.031732	2.675816
163.102913	2429.809423	5.992602	-0.031753	2.680147
163.459825	2437.847759	5.997606	-0.031824	2.684487
163.901264	2445.845306	6.002611	-0.031912	2.688804
163.971254	2453.968925	6.007616	-0.031930	2.693158
164.673306	2461.976256	6.012621	-0.032066	2.697483
164.919162	2470.003649	6.017626	-0.032117	2.701782
164.570961	2478.191065	6.022630	-0.032057	2.706122
164.971590	2486.179199	6.027635	-0.032137	2.710396
165.823097	2494.120998	6.032640	-0.032301	2.714668
166.165013	2502.169697	6.037645	-0.032370	2.718958
166.246667	2510.243181	6.042650	-0.032390	2.723237
167.015065	2518.250981	6.047654	-0.032539	2.727518
166.778210	2526.407299	6.052659	-0.032500	2.731807
167.717155	2534.348801	6.057664	-0.032680	2.736050
168.140234	2542.434997	6.062669	-0.032764	2.740331
169.014073	2550.339847	6.067674	-0.032932	2.744537
169.260794	2558.505509	6.072678	-0.032983	2.748835
169.782708	2566.591064	6.077683	-0.033085	2.753101
169.925258	2574.642521	6.082688	-0.033117	2.757318
170.107467	2582.725634	6.087693	-0.033156	2.761549
170.651908	2590.699802	6.092698	-0.033263	2.765738
171.046837	2598.752097	6.097702	-0.033342	2.769953
171.070502	2606.843893	6.102707	-0.033351	2.774158
171.639580	2614.845147	6.107712	-0.033462	2.778344
171.869430	2622.931898	6.112717	-0.033511	2.782547
172.341676	2630.911317	6.117722	-0.033604	2.786702
172.944185	2638.964476	6.122726	-0.033721	2.790898
173.280437	2647.018265	6.127731	-0.033789	2.795071
173.515610	2655.043919	6.132736	-0.033838	2.799217
173.662823	2663.136852	6.137741	-0.033871	2.803387
173.995529	2671.174663	6.142746	-0.033938	2.807533
174.342338	2679.232663	6.147750	-0.034008	2.811684
175.025537	2687.218539	6.152755	-0.034140	2.815812
175.038479	2695.319905	6.157760	-0.034148	2.819953
175.663670	2703.337233	6.162765	-0.034269	2.824081
175.912679	2711.380685	6.167770	-0.034321	2.828194
176.394486	2719.439230	6.172774	-0.034416	2.832323
176.511477	2727.510003	6.177779	-0.034443	2.836430
177.027995	2735.490580	6.182784	-0.034544	2.840509
177.262486	2743.512821	6.187789	-0.034593	2.844586
177.440149	2751.588425	6.192794	-0.034631	2.848682
177.672967	2759.665738	6.197798	-0.034680	2.852775
177.839623	2767.704741	6.202803	-0.034716	2.856840
178.054500	2775.769645	6.207808	-0.034762	2.860915
178.445844	2783.816778	6.212813	-0.034840	2.864984
178.958961	2791.810738	6.217818	-0.034940	2.869029
179.556055	2799.831663	6.222822	-0.035057	2.873085
179.501902	2807.937355	6.227827	-0.035052	2.877142
179.975412	2815.959856	6.232832	-0.035145	2.881181
180.261151	2823.999424	6.237837	-0.035204	2.885212
180.661678	2831.990490	6.242842	-0.035284	2.889220
181.183106	2840.042648	6.247846	-0.035386	2.893259
181.006707	2848.164557	6.252851	-0.035358	2.897288
181.294632	2856.201004	6.257856	-0.035417	2.901295
181.642225	2864.240794	6.262861	-0.035487	2.905302
182.139563	2872.214604	6.267866	-0.035585	2.909278
182.149427	2880.383421	6.272870	-0.035592	2.913319
183.058565	2888.270622	6.277875	-0.035766	2.917264
183.847019	2896.229274	6.282880	-0.035918	2.921232
183.903900	2904.333557	6.287885	-0.035934	2.925227
184.018843	2912.405691	6.292890	-0.035961	2.929203
184.385082	2920.470013	6.297894	-0.036034	2.933184
184.210816	2928.566239	6.302899	-0.036007	2.937146
184.715763	2936.536689	6.307904	-0.036106	2.941078
185.361752	2944.524939	6.312909	-0.036232	2.945020
185.393055	2952.616603	6.317914	-0.036243	2.948975
185.360270	2960.721047	6.322918	-0.036242	2.952927
185.492691	2968.777246	6.327923	-0.036272	2.956859
185.836627	2976.765315	6.332928	-0.036341	2.960764
186.766842	2984.693850	6.337933	-0.036520	2.964666
187.057861	2992.755602	6.342938	-0.036579	2.968593
187.409917	3000.833820	6.347942	-0.036650	2.972527
187.537740	3008.901389	6.352947	-0.036679	2.976438
187.771177	3016.917813	6.357952	-0.036728	2.980325
188.769282	3024.865552	6.362957	-0.036919	2.984213
188.959877	3032.959134	6.367962	-0.036959	2.988125
189.115272	3041.064618	6.372966	-0.036993	2.992035
189.380332	3049.110550	6.377971	-0.037048	2.995917
189.487284	3057.126751	6.382976	-0.037073	2.999772
189.628779	3065.176342	6.387981	-0.037105	3.003640
189.241907	3073.304529	6.392986	-0.037038	3.007513
189.675917	3081.302634	6.397990	-0.037124	3.011361
190.205724	3089.292515	6.402995	-0.037228	3.015205
190.548971	3097.290420	6.408000	-0.037297	3.019038
191.110672	3105.306999	6.413005	-0.037407	3.022886
191.463389	3113.320093	6.418010	-0.037478	3.026717
191.007658	3121.551795	6.423014	-0.037398	3.030606
191.796884	3129.454680	6.428019	-0.037550	3.034397
192.670335	3137.403159	6.433024	-0.037718	3.038209
192.574419	3145.517294	6.438029	-0.037705	3.042046
192.994191	3153.530117	6.443034	-0.037789	3.045855
193.749116	3161.506238	6.448038	-0.037935	3.049660
193.629458	3169.644292	6.453043	-0.037918	3.053492
194.373671	3177.585787	6.458048	-0.038061	3.057270
194.843494	3185.666297	6.463053	-0.038154	3.061095
194.988371	3193.719096	6.468058	-0.038186	3.064886
195.131320	3201.798790	6.473062	-0.038218	3.068684
195.363185	3209.871384	6.478067	-0.038267	3.072480
195.395472	3217.958672	6.483072	-0.038278	3.076267
196.034224	3225.911293	6.488077	-0.038402	3.080016
196.195037	3233.909707	6.493082	-0.038437	3.083759
196.744068	3241.938362	6.498086	-0.038545	3.087530
197.066675	3249.994954	6.503091	-0.038610	3.091299
197.886892	3257.928093	6.508096	-0.038768	3.095029
198.433870	3265.978435	6.513101	-0.038875	3.098796
198.388658	3274.078312	6.518106	-0.038872	3.102554
198.786444	3282.130157	6.523110	-0.038951	3.106305
198.888099	3290.196353	6.528115	-0.038975	3.110044
199.559449	3298.161941	6.533120	-0.039105	3.113760
199.607320	3306.257891	6.538125	-0.039119	3.117501
200.229461	3314.218323	6.543130	-0.039240	3.121203
200.958135	3322.175770	6.548134	-0.039381	3.124903
200.887331	3330.308203	6.553139	-0.039373	3.128643
200.893082	3338.386935	6.558144	-0.039380	3.132357
201.538088	3346.401759	6.563149	-0.039505	3.136066
201.781608	3354.385453	6.568154	-0.039556	3.139739
201.962508	3362.438062	6.573158	-0.039595	3.143436
202.139442	3370.493816	6.578163	-0.039633	3.147129
202.988008	3378.478763	6.583168	-0.039796	3.150817
203.238750	3386.547124	6.588173	-0.039848	3.154511
203.311958	3394.582338	6.593178	-0.039867	3.158177
203.315336	3402.669500	6.598182	-0.039873	3.161860
203.984445	3410.635263	6.603187	-0.040002	3.165513
204.476391	3418.630055	6.608192	-0.040099	3.169167
204.561606	3426.752721	6.613197	-0.040120	3.172856
204.459139	3434.855716	6.618202	-0.040106	3.176524
205.368473	3442.750458	6.623206	-0.040281	3.180139
205.490837	3450.779764	6.628211	-0.040309	3.183775
206.161012	3458.792653	6.633216	-0.040439	3.187424
206.474093	3466.876072	6.638221	-0.040502	3.191084
206.878537	3474.867190	6.643226	-0.040583	3.194703
207.423044	3482.912321	6.648230	-0.040690	3.198348
207.605637	3490.967813	6.653235	-0.040729	3.201977
207.507172	3499.024155	6.658240	-0.040716	3.205591
207.931169	3507.057403	6.663245	-0.040800	3.209213
208.225206	3515.069195	6.668250	-0.040860	3.212815
208.638455	3523.126873	6.673254	-0.040942	3.216440
209.050537	3531.124788	6.678259	-0.041024	3.220033
209.059782	3539.201055	6.683264	-0.041031	3.223639
209.949819	3547.175218	6.688269	-0.041202	3.227234
210.049219	3555.268187	6.693274	-0.041226	3.230844
210.759014	3563.207813	6.698278	-0.041363	3.234408
210.678771	3571.342321	6.703283	-0.041353	3.238020
211.213035	3579.278730	6.708288	-0.041458	3.241567
211.428586	3587.360469	6.713293	-0.041503	3.245161
211.719038	3595.367391	6.718298	-0.041563	3.248720
211.752051	3603.460334	6.723302	-0.041574	3.252304
211.690959	3611.568918	6.728307	-0.041568	3.255886
212.189270	3619.477814	6.733312	-0.041666	3.259399
212.658691	3627.497324	6.738317	-0.041758	3.262956
212.893294	3635.528532	6.743322	-0.041807	3.266504
213.319919	3643.567088	6.748326	-0.041892	3.270060
213.485622	3651.646602	6.753331	-0.041928	3.273619
213.927208	3659.617028	6.758336	-0.042015	3.277137
214.495572	3667.620146	6.763341	-0.042127	3.280672
215.083366	3675.584773	6.768346	-0.042241	3.284186
214.848130	3683.735163	6.773350	-0.042203	3.287744
215.188125	3691.756535	6.778355	-0.042271	3.291265
215.767110	3699.719040	6.783360	-0.042384	3.294767
215.784503	3707.847519	6.788365	-0.042393	3.298314
215.934982	3715.871595	6.793370	-0.042426	3.301818
216.410766	3723.854619	6.798374	-0.042520	3.305313
217.078020	3731.856254	6.803379	-0.042649	3.308819
217.073240	3739.957726	6.808384	-0.042654	3.312339
217.148530	3748.064188	6.813389	-0.042673	3.315860
217.554199	3755.989595	6.818394	-0.042753	3.319312
218.047001	3763.997840	6.823398	-0.042850	3.322800
218.238710	3772.057643	6.828403	-0.042891	3.326294
218.773717	3780.028794	6.833408	-0.042996	3.329760
219.034156	3788.133611	6.838413	-0.043050	3.333269
219.626425	3796.095846	6.843418	-0.043165	3.336726
219.812426	3804.165842	6.848422	-0.043205	3.340210
220.038280	3812.189292	6.853427	-0.043253	3.343671
220.412417	3820.234924	6.858432	-0.043327	3.347145
220.790605	3828.306200	6.863437	-0.043403	3.350625
221.211099	3836.258555	6.868442	-0.043487	3.354053
221.828587	3844.260961	6.873446	-0.043607	3.357506
222.316293	3852.292055	6.878451	-0.043703	3.360963
222.671611	3860.273138	6.883456	-0.043774	3.364389
222.765022	3868.411899	6.888461	-0.043797	3.367870
223.113834	3876.440261	6.893466	-0.043867	3.371310
223.329856	3884.473162	6.898470	-0.043912	3.374743
223.815492	3892.489488	6.903475	-0.044008	3.378175
224.291411	3900.497429	6.908480	-0.044102	3.381600
224.518725	3908.552837	6.913485	-0.044149	3.385032
224.454517	3916.612241	6.918490	-0.044143	3.388452
224.825339	3924.676959	6.923494	-0.044217	3.391886
225.531916	3932.660046	6.928499	-0.044354	3.395295
225.262125	3940.698193	6.933504	-0.044309	3.398688
225.827894	3948.701685	6.938509	-0.044419	3.402093
226.157506	3956.684063	6.943514	-0.044486	3.405477
226.249927	3964.746517	6.948518	-0.044508	3.408884
226.457940	3972.799871	6.953523	-0.044552	3.412286
226.951535	3980.772684	6.958528	-0.044649	3.415662
227.575383	3988.761927	6.963533	-0.044771	3.419046
227.505787	3996.825979	6.968538	-0.044763	3.422434
227.842613	4004.918133	6.973542	-0.044831	3.425844
228.037891	4012.964867	6.978547	-0.044873	3.429226
228.320206	4020.957213	6.983552	-0.044930	3.432586
229.081899	4028.949599	6.988557	-0.045077	3.435959
229.724922	4036.886904	6.993562	-0.045202	3.439301
230.095995	4044.932570	6.998566	-0.045277	3.442676
230.357354	4053.021595	7.003571	-0.045330	3.446062
231.212590	4060.972239	7.008576	-0.045495	3.449407
231.096349	4069.129594	7.013581	-0.045479	3.452802
231.416498	4077.150955	7.018586	-0.045543	3.456152
232.128701	4085.121030	7.023590	-0.045681	3.459490
232.076656	4093.200831	7.028595	-0.045677	3.462845
232.003632	4101.263820	7.033600	-0.045668	3.466188
232.993165	4109.205778	7.038605	-0.045858	3.469514
233.039559	4117.259659	7.043610	-0.045872	3.472852
233.315456	4125.319307	7.048614	-0.045928	3.476196
233.632046	4133.309514	7.053619	-0.045992	3.479510
234.725888	4141.217526	7.058624	-0.046201	3.482812
234.864051	4149.324829	7.063629	-0.046232	3.486162
234.970225	4157.365278	7.068634	-0.046257	3.489480
235.460506	4165.401620	7.073638	-0.046354	3.492805
235.489279	4173.497172	7.078643	-0.046364	3.496137
235.542984	4181.498166	7.083648	-0.046380	3.499427
236.086370	4189.504282	7.088653	-0.046486	3.502732
236.256312	4197.551660	7.093658	-0.046523	3.506039
236.342201	4205.571458	7.098662	-0.046544	3.509329
236.573487	4213.659817	7.103667	-0.046592	3.512648
236.570391	4221.684303	7.108672	-0.046597	3.515930
237.009778	4229.665477	7.113677	-0.046684	3.519206
237.554022	4237.606301	7.118682	-0.046790	3.522466
237.912590	4245.684111	7.123686	-0.046863	3.525773
238.337954	4253.704687	7.128691	-0.046947	3.529055
238.731236	4261.714717	7.133696	-0.047025	3.532328
239.264088	4269.759163	7.138701	-0.047130	3.535617
239.604064	4277.767099	7.143706	-0.047198	3.538882
239.783640	4285.831135	7.148710	-0.047237	3.542162
240.174415	4293.854131	7.153715	-0.047315	3.545429
240.061422	4301.944217	7.158720	-0.047299	3.548704
240.846048	4309.963706	7.163725	-0.047450	3.551975
241.009758	4317.995162	7.168730	-0.047486	3.555229
241.897831	4325.875281	7.173734	-0.047657	3.558441
242.486748	4333.919509	7.178739	-0.047772	3.561706
242.504719	4341.920225	7.183744	-0.047780	3.564934
243.037865	4349.962871	7.188749	-0.047885	3.568192
243.371691	4358.043670	7.193754	-0.047952	3.571456
243.751336	4366.012882	7.198758	-0.048028	3.574673
243.648091	4374.117397	7.203763	-0.048014	3.577927
243.764197	4382.179384	7.208768	-0.048041	3.581167
244.117499	4390.129810	7.213773	-0.048112	3.584368
244.523051	4398.152195	7.218778	-0.048192	3.587595
245.331489	4406.134918	7.223782	-0.048348	3.590816
245.565146	4414.189617	7.228787	-0.048397	3.594045
245.772793	4422.227809	7.233792	-0.048441	3.597264
246.243750	4430.253904	7.238797	-0.048534	3.600483
246.060629	4438.327637	7.243802	-0.048505	3.603699
246.630080	4446.296940	7.248806	-0.048616	3.606893
246.665752	4454.360423	7.253811	-0.048628	3.610105
247.125945	4462.355426	7.258816	-0.048719	3.613300
247.262993	4470.451919	7.263821	-0.048750	3.616523
247.732478	4478.389276	7.268826	-0.048842	3.619689
248.208067	4486.416786	7.273830	-0.048936	3.622889
248.327542	4494.504078	7.278835	-0.048963	3.626099
248.598890	4502.478873	7.283840	-0.049019	3.629266
249.119869	4510.532031	7.288845	-0.049121	3.632468
248.903115	4518.619239	7.293850	-0.049086	3.635660
249.434513	4526.539940	7.298854	-0.049190	3.638804
249.879596	4534.570406	7.303859	-0.049279	3.641987
250.053646	4542.589319	7.308864	-0.049316	3.645154
250.636620	4550.617277	7.313869	-0.049430	3.648334
250.925413	4558.667710	7.318874	-0.049489	3.651512
251.223617	4566.671433	7.323878	-0.049550	3.654668
251.314901	4574.729316	7.328883	-0.049572	3.657838
251.628891	4582.736500	7.333888	-0.049636	3.660991
252.344917	4590.662185	7.338893	-0.049774	3.664120
252.227323	4598.801964	7.343898	-0.049757	3.667308
252.450836	4606.835800	7.348902	-0.049804	3.670460
252.696687	4614.849563	7.353907	-0.049855	3.673603
253.210258	4622.848643	7.358912	-0.049956	3.676744
253.321156	4630.871307	7.363917	-0.049982	3.679881
253.590379	4638.846801	7.368922	-0.050037	3.683001
253.816627	4646.907410	7.373926	-0.050085	3.686151
254.448775	4654.905656	7.378931	-0.050208	3.689284
254.861965	4662.931498	7.383936	-0.050290	3.692419
254.941764	4671.052004	7.388941	-0.050310	3.695580
255.149864	4679.013311	7.393946	-0.050354	3.698680
255.222680	4687.085428	7.398950	-0.050373	3.701816
255.887778	4695.063434	7.403955	-0.050502	3.704929
255.947796	4703.101902	7.408960	-0.050518	3.708046
256.864946	4711.125368	7.413965	-0.050694	3.711178
256.984925	4719.180899	7.418970	-0.050722	3.714298
257.299899	4727.176189	7.423974	-0.050785	3.717398
257.231851	4735.277241	7.428979	-0.050778	3.720526
257.796362	4743.138597	7.433984	-0.050888	3.723575
257.771226	4751.277087	7.438989	-0.050889	3.726713
258.335919	4759.236196	7.443994	-0.050999	3.729794
258.788051	4767.266296	7.448998	-0.051089	3.732897
259.015922	4775.342279	7.454003	-0.051136	3.736010
258.672813	4783.369632	7.459008	-0.051078	3.739087
259.394660	4791.376647	7.464013	-0.051217	3.742180
259.539514	4799.398636	7.469018	-0.051249	3.745262
259.350460	4807.430916	7.474022	-0.051219	3.748338
259.931995	4815.465826	7.479027	-0.051333	3.751430
260.014405	4823.446610	7.484032	-0.051353	3.754487
260.443710	4831.456687	7.489037	-0.051439	3.757562
260.673547	4839.464979	7.494042	-0.051487	3.760628
261.053873	4847.441730	7.499046	-0.051563	3.763683
261.393503	4855.518579	7.504051	-0.051631	3.766773
261.122460	4863.585052	7.509056	-0.051586	3.769841
261.904384	4871.553190	7.514061	-0.051737	3.772895
262.254947	4879.620024	7.519066	-0.051807	3.775974
262.855477	4887.549851	7.524070	-0.051924	3.779004
263.094930	4895.662528	7.529075	-0.051974	3.782092
262.856712	4903.721965	7.534080	-0.051935	3.785146
263.407538	4911.728233	7.539085	-0.052043	3.788197
263.451742	4919.793910	7.544090	-0.052056	3.791255
264.112956	4927.691257	7.549094	-0.052184	3.794261
264.336934	4935.809337	7.554099	-0.052231	3.797339
264.685704	4943.759627	7.559104	-0.052301	3.800353
265.574973	4951.709888	7.564109	-0.052472	3.803377
265.552123	4959.809174	7.569114	-0.052473	3.806434
265.682434	4967.817095	7.574118	-0.052503	3.809458
266.053068	4975.883224	7.579123	-0.052577	3.812507
266.066310	4983.902851	7.584128	-0.052585	3.815527
266.731303	4991.880617	7.589133	-0.052714	3.818544
266.800853	4999.957909	7.594138	-0.052732	3.821583
267.419920	5007.853463	7.599142	-0.052852	3.824563
267.507738	5016.003320	7.604147	-0.052874	3.827625
267.556671	5024.020503	7.609152	-0.052888	3.830633
267.968453	5032.029270	7.614157	-0.052970	3.833644
268.533738	5040.028821	7.619162	-0.053080	3.836652
268.368409	5048.064378	7.624166	-0.053055	3.839656
269.166928	5056.051520	7.629171	-0.053209	3.842660
269.017794	5064.138066	7.634176	-0.053186	3.845678
269.384514	5072.139898	7.639181	-0.053260	3.848673
269.843446	5080.210614	7.644186	-0.053350	3.851693
270.270647	5088.178260	7.649190	-0.053435	3.854672
270.915112	5096.182549	7.654195	-0.053560	3.857667
270.894030	5104.248232	7.659200	-0.053562	3.860669
271.104762	5112.280927	7.664205	-0.053606	3.863660
271.641238	5120.277890	7.669210	-0.053711	3.866643
271.822229	5128.289633	7.674214	-0.053750	3.869621
272.070203	5136.452863	7.679219	-0.053802	3.872655
272.681115	5144.425257	7.684224	-0.053921	3.875623
272.703887	5152.409188	7.689229	-0.053930	3.878581
273.583878	5160.360611	7.694234	-0.054099	3.881542
273.550535	5168.388774	7.699238	-0.054098	3.884510
274.044186	5176.398055	7.704243	-0.054195	3.887480
274.058591	5184.414807	7.709248	-0.054203	3.890441
274.402283	5192.423767	7.714253	-0.054272	3.893403
274.593264	5200.538006	7.719258	-0.054313	3.896399
275.032071	5208.430542	7.724262	-0.054400	3.899315
275.364422	5216.536054	7.729267	-0.054467	3.902306
275.670456	5224.473611	7.734272	-0.054529	3.905232
276.062595	5232.495869	7.739277	-0.054607	3.908188
276.315495	5240.561649	7.744282	-0.054660	3.911156
276.742854	5248.551112	7.749286	-0.054745	3.914096
276.776687	5256.675999	7.754291	-0.054756	3.917077
276.970331	5264.628115	7.759296	-0.054797	3.919994
277.255218	5272.626601	7.764301	-0.054856	3.922929
277.408555	5280.687678	7.769306	-0.054889	3.925881
277.494967	5288.700341	7.774310	-0.054911	3.928812
277.822255	5296.762792	7.779315	-0.054977	3.931764
277.920521	5304.757036	7.784320	-0.055000	3.934685
278.445398	5312.774396	7.789325	-0.055103	3.937619
278.517887	5320.812914	7.794330	-0.055122	3.940551
278.774867	5328.798172	7.799334	-0.055175	3.943464
279.442427	5336.866096	7.804339	-0.055305	3.946413
279.150330	5344.884895	7.809344	-0.055255	3.949324
279.102406	5352.992383	7.814349	-0.055252	3.952270
279.144485	5360.998977	7.819354	-0.055265	3.955178
279.556094	5368.915260	7.824358	-0.055347	3.958059
279.720456	5376.977470	7.829363	-0.055382	3.960985
280.470368	5384.832616	7.834368	-0.055527	3.963845
280.533275	5392.988747	7.839373	-0.055544	3.966800
280.918159	5400.965702	7.844378	-0.055621	3.969693
281.315097	5409.001605	7.849382	-0.055700	3.972605
281.707460	5417.064557	7.854387	-0.055778	3.975525
281.822845	5425.033108	7.859392	-0.055805	3.978404
282.316674	5433.096206	7.864397	-0.055902	3.981322
282.139174	5441.090928	7.869402	-0.055874	3.984201
282.389820	5449.134609	7.874406	-0.055926	3.987102
282.600678	5457.206156	7.879411	-0.055971	3.990012
283.043046	5465.166542	7.884416	-0.056058	3.992883
283.212806	5473.243327	7.889421	-0.056095	3.995789
283.110278	5481.247856	7.894426	-0.056081	3.998662
283.662331	5489.232861	7.899430	-0.056189	4.001537
284.334580	5497.151068	7.904435	-0.056320	4.004388
284.456655	5505.221592	7.909440	-0.056348	4.007283
285.014930	5513.247734	7.914445	-0.056457	4.010167
285.047269	5521.320373	7.919450	-0.056468	4.013056
285.158352	5529.342756	7.924454	-0.056494	4.015927
285.622413	5537.340468	7.929459	-0.056586	4.018792
285.694372	5545.357952	7.934464	-0.056604	4.021656
286.091998	5553.354730	7.939469	-0.056683	4.024517
286.222017	5561.445913	7.944474	-0.056713	4.027404
286.142558	5569.491227	7.949478	-0.056703	4.030269
286.719914	5577.529754	7.954483	-0.056816	4.033141
287.167808	5585.513446	7.959488	-0.056905	4.035989
287.320956	5593.448697	7.964493	-0.056938	4.038813
287.755831	5601.513983	7.969498	-0.057025	4.041685
287.672741	5609.473889	7.974502	-0.057014	4.044510
288.556623	5617.518424	7.979507	-0.057184	4.047378
288.767352	5625.499491	7.984512	-0.057229	4.050211
289.554928	5633.499445	7.989517	-0.057380	4.053058
289.618484	5641.605258	7.994522	-0.057397	4.055928
290.028445	5649.550665	7.999526	-0.057479	4.058746
290.302749	5657.646403	8.004531	-0.057535	4.061612
290.212740	5665.644509	8.009536	-0.057524	4.064436
290.526133	5673.732387	8.014541	-0.057587	4.067296
290.919967	5681.764196	8.019546	-0.057666	4.070136
291.562277	5689.688343	8.024550	-0.057791	4.072939
291.667101	5697.784838	8.029555	-0.057815	4.075793
291.984474	5705.723642	8.034560	-0.057880	4.078592
292.096233	5713.837444	8.039565	-0.057906	4.081448
292.819421	5721.730405	8.044570	-0.058046	4.084234
293.093828	5729.804380	8.049574	-0.058102	4.087074
293.131529	5737.909113	8.054579	-0.058114	4.089920
292.880964	5745.940702	8.059584	-0.058073	4.092734
293.582583	5753.888397	8.064589	-0.058209	4.095530
294.215917	5761.854446	8.069594	-0.058332	4.098330
294.712878	5769.921022	8.074598	-0.058429	4.101161
294.526130	5777.998088	8.079603	-0.058400	4.103984
294.968674	5785.953233	8.084608	-0.058487	4.106771
295.518297	5793.936464	8.089613	-0.058595	4.109568
295.319872	5802.018987	8.094618	-0.058563	4.112387
295.505299	5810.020888	8.099622	-0.058603	4.115181
295.911836	5818.023980	8.104627	-0.058684	4.117977
296.067668	5826.082968	8.109632	-0.058718	4.120786
296.212483	5834.056465	8.114637	-0.058750	4.123564
296.635244	5842.087329	8.119642	-0.058834	4.126364
297.193934	5850.009829	8.124646	-0.058943	4.129126
297.068328	5858.208073	8.129651	-0.058925	4.131973
296.966937	5866.179814	8.134656	-0.058912	4.134739
297.119245	5874.167799	8.139661	-0.058945	4.137513
297.643303	5882.172201	8.144666	-0.059048	4.140295
297.334926	5890.239159	8.149670	-0.058996	4.143086
297.616891	5898.249378	8.154675	-0.059054	4.145864
298.262734	5906.204441	8.159680	-0.059179	4.148625
298.742376	5914.248985	8.164685	-0.059274	4.151413
299.079569	5922.228541	8.169690	-0.059342	4.154174
299.188363	5930.328749	8.174694	-0.059367	4.156973
299.319625	5938.326848	8.179699	-0.059397	4.159735
298.945145	5946.402329	8.184704	-0.059332	4.162515
299.325097	5954.351287	8.189709	-0.059408	4.165259
299.363336	5962.429606	8.194714	-0.059420	4.168042
299.667236	5970.422985	8.199718	-0.059482	4.170796
300.210070	5978.429537	8.204723	-0.059589	4.173557
300.815515	5986.422121	8.209728	-0.059706	4.176311
300.639778	5994.437102	8.214733	-0.059679	4.179062
300.904254	6002.519070	8.219738	-0.059733	4.181840
301.788250	6010.396279	8.224742	-0.059903	4.184552
302.211346	6018.511011	8.229747	-0.059987	4.187339
301.799026	6026.581973	8.234752	-0.059916	4.190099
302.236945	6034.615925	8.239757	-0.060002	4.192854
302.310036	6042.669719	8.244762	-0.060021	4.195610
302.428768	6050.632284	8.249766	-0.060049	4.198334
303.215853	6058.630375	8.254771	-0.060200	4.201076
303.180646	6066.629796	8.259776	-0.060199	4.203807
303.619884	6074.631286	8.264781	-0.060286	4.206542
304.039008	6082.615945	8.269786	-0.060369	4.209269
304.162704	6090.717506	8.274790	-0.060397	4.212031
304.735276	6098.685816	8.279795	-0.060509	4.214751
305.361644	6106.651326	8.284800	-0.060631	4.217469
305.857250	6114.655891	8.289805	-0.060729	4.220197
306.031667	6122.771828	8.294810	-0.060766	4.222957
306.253012	6130.728885	8.299814	-0.060813	4.225662
306.593471	6138.778415	8.304819	-0.060881	4.228397
306.950036	6146.799648	8.309824	-0.060953	4.231122
306.880709	6154.854420	8.314829	-0.060945	4.233852
307.064303	6162.900885	8.319834	-0.060985	4.236579
306.963462	6170.895086	8.324838	-0.060971	4.239284
307.272363	6178.956406	8.329843	-0.061034	4.242015
307.167620	6186.882485	8.334848	-0.061020	4.244694
307.705428	6194.895502	8.339853	-0.061125	4.247407
308.333752	6202.900939	8.344858	-0.061247	4.250116
308.723303	6210.929159	8.349862	-0.061325	4.252829
308.945623	6218.974185	8.354867	-0.061371	4.255544
309.805124	6226.873817	8.359872	-0.061537	4.258215
310.183690	6235.016523	8.364877	-0.061612	4.260961
310.496962	6242.996764	8.369882	-0.061676	4.263650
310.749844	6251.037799	8.374886	-0.061728	4.266358
310.970994	6259.080331	8.379891	-0.061775	4.269063
311.257602	6267.103858	8.384896	-0.061833	4.271761
311.122508	6275.183758	8.389901	-0.061813	4.274472
311.286943	6283.172700	8.394906	-0.061849	4.277154
312.145585	6291.055791	8.399910	-0.062014	4.279805
312.307152	6299.115651	8.404915	-0.062049	4.282507
312.368606	6307.155490	8.409920	-0.062066	4.285200
312.812209	6315.182358	8.414925	-0.062154	4.287890
313.091586	6323.235786	8.419930	-0.062211	4.290586
313.361451	6331.215234	8.424934	-0.062267	4.293255
313.840913	6339.191272	8.429939	-0.062361	4.295924
313.797989	6347.254845	8.434944	-0.062358	4.298615
314.232570	6355.291965	8.439949	-0.062444	4.301300
314.841427	6363.222871	8.444954	-0.062563	4.303949
314.832520	6371.335490	8.449958	-0.062567	4.306652
315.253878	6379.340654	8.454963	-0.062650	4.309321
315.307939	6387.389591	8.459968	-0.062666	4.312000
315.766409	6395.285696	8.464973	-0.062756	4.314629
315.491268	6403.422648	8.469978	-0.062710	4.317331
315.967817	6411.295392	8.474982	-0.062804	4.319950
316.352057	6419.366438	8.479987	-0.062881	4.322632
316.681951	6427.343280	8.484992	-0.062947	4.325281
316.846522	6435.420633	8.489997	-0.062983	4.327960
317.122055	6443.456973	8.495002	-0.063040	4.330624
317.105023	6451.473450	8.500006	-0.063042	4.333278
317.215331	6459.485154	8.505011	-0.063068	4.335930
317.908281	6467.432104	8.510016	-0.063202	4.338564
318.321710	6475.464536	8.515021	-0.063284	4.341221
318.511159	6483.499791	8.520026	-0.063324	4.343877
318.943750	6491.491775	8.525030	-0.063410	4.346518
319.242928	6499.598884	8.530035	-0.063471	4.349194
319.586467	6507.606835	8.535040	-0.063540	4.351837
319.887222	6515.645423	8.540045	-0.063602	4.354487
319.905637	6523.684047	8.545050	-0.063610	4.357134
320.451406	6531.585712	8.550054	-0.063717	4.359738
320.631379	6539.671408	8.555059	-0.063756	4.362398
321.149995	6547.591207	8.560064	-0.063857	4.365005
321.569093	6555.620822	8.565069	-0.063941	4.367645
321.702836	6563.695904	8.570074	-0.063971	4.370297
321.994570	6571.706872	8.575079	-0.064030	4.372927
322.710446	6579.683286	8.580083	-0.064169	4.375547
322.878136	6587.707781	8.585088	-0.064205	4.378177
323.131082	6595.767825	8.590093	-0.064258	4.380818
323.198610	6603.756513	8.595098	-0.064275	4.383433
323.446096	6611.819847	8.600103	-0.064327	4.386071
323.710176	6619.819967	8.605107	-0.064381	4.388688
323.958665	6627.896038	8.610112	-0.064433	4.391328
324.492160	6635.861392	8.615117	-0.064537	4.393931
324.658980	6643.954739	8.620122	-0.064573	4.396573
324.874451	6651.838491	8.625127	-0.064619	4.399145
325.490356	6659.896514	8.630131	-0.064739	4.401774
325.632031	6667.853602	8.635136	-0.064770	4.404367
325.616658	6675.994965	8.640141	-0.064773	4.407016
326.076324	6683.975838	8.645146	-0.064863	4.409615
326.361728	6692.013835	8.650151	-0.064922	4.412230
326.193680	6700.085220	8.655155	-0.064896	4.414851
326.528787	6708.099317	8.660160	-0.064963	4.417455
326.909413	6716.087633	8.665165	-0.065039	4.420049
327.308956	6724.105505	8.670170	-0.065119	4.422652
327.041049	6732.159251	8.675175	-0.065074	4.425261
327.199143	6740.208328	8.680179	-0.065109	4.427869
327.262857	6748.268666	8.685184	-0.065126	4.430478
327.624478	6756.230279	8.690189	-0.065199	4.433056
327.981065	6764.252780	8.695194	-0.065270	4.435652
328.570253	6772.167073	8.700199	-0.065385	4.438213
329.101234	6780.207036	8.705203	-0.065489	4.440812
329.092897	6788.201637	8.710208	-0.065493	4.443393
329.199656	6796.231964	8.715213	-0.065518	4.445984
329.720430	6804.313767	8.720218	-0.065620	4.448592
329.868153	6812.339468	8.725223	-0.065653	4.451178
330.505792	6820.273135	8.730227	-0.065777	4.453736
330.810512	6828.369039	8.735232	-0.065839	4.456343
330.717399	6836.363149	8.740237	-0.065827	4.458914
330.960097	6844.417105	8.745242	-0.065877	4.461504
331.631131	6852.308214	8.750247	-0.066007	4.464042
331.732712	6860.455470	8.755251	-0.066031	4.466658
331.428037	6868.497512	8.760256	-0.065980	4.469237
331.627434	6876.535066	8.765261	-0.066022	4.471816
332.136819	6884.420081	8.770266	-0.066122	4.474345
332.318484	6892.501425	8.775271	-0.066161	4.476934
332.823211	6900.452466	8.780275	-0.066260	4.479482
333.095244	6908.515764	8.785280	-0.066316	4.482063
333.546594	6916.439872	8.790285	-0.066405	4.484599
333.694461	6924.581676	8.795290	-0.066438	4.487201
333.868587	6932.526518	8.800295	-0.066476	4.489739
334.371837	6940.599992	8.805299	-0.066575	4.492318
334.377020	6948.594365	8.810304	-0.066581	4.494869
334.711418	6956.608902	8.815309	-0.066648	4.497425
335.124487	6964.609566	8.820314	-0.066731	4.499976
335.029398	6972.621857	8.825319	-0.066718	4.502528
335.368766	6980.646427	8.830323	-0.066786	4.505083
335.592047	6988.738855	8.835328	-0.066833	4.507658
335.855454	6996.684289	8.840333	-0.066888	4.510185
335.934041	7004.776852	8.845338	-0.066907	4.512757
335.958586	7012.680918	8.850343	-0.066917	4.515267
336.372259	7020.688624	8.855347	-0.066999	4.517810
337.064636	7028.664664	8.860352	-0.067133	4.520342
337.244812	7036.692015	8.865357	-0.067172	4.522887
337.135117	7044.805695	8.870362	-0.067157	4.525458
337.354714	7052.767887	8.875367	-0.067203	4.527979
337.873634	7060.773203	8.880371	-0.067305	4.530515
338.132880	7068.807361	8.885376	-0.067358	4.533056
337.829813	7076.869061	8.890381	-0.067307	4.535604
338.143486	7084.854543	8.895386	-0.067371	4.538128
338.302079	7092.865738	8.900391	-0.067406	4.540658
338.309112	7100.877821	8.905395	-0.067412	4.543186
338.486717	7108.898891	8.910400	-0.067450	4.545717
338.669566	7116.859083	8.915405	-0.067490	4.548227
339.051057	7124.966885	8.920410	-0.067566	4.550782
339.412345	7132.933768	8.925415	-0.067638	4.553291
339.693148	7140.931607	8.930419	-0.067696	4.555809
340.151179	7148.930693	8.935424	-0.067786	4.558326
340.319883	7156.942429	8.940429	-0.067823	4.560845
340.463811	7164.966794	8.945434	-0.067855	4.563366
340.665608	7172.977365	8.950439	-0.067898	4.565882
340.948152	7181.031714	8.955443	-0.067956	4.568410
341.200846	7189.073908	8.960448	-0.068008	4.570933
341.295219	7197.117651	8.965453	-0.068031	4.573455
341.826623	7205.126368	8.970458	-0.068135	4.575965
341.899433	7213.095494	8.975463	-0.068154	4.578460
342.130450	7221.125990	8.980467	-0.068202	4.580974
342.459899	7229.087575	8.985472	-0.068268	4.583464
342.332319	7237.123951	8.990477	-0.068250	4.585976
342.596654	7245.193702	8.995482	-0.068304	4.588498
342.791831	7253.179330	9.000487	-0.068346	4.590992
343.196583	7261.183420	9.005491	-0.068426	4.593490
343.509076	7269.206462	9.010496	-0.068490	4.595993
344.129327	7277.130518	9.015501	-0.068610	4.598464
344.172678	7285.237836	9.020506	-0.068624	4.600990
344.679661	7293.128216	9.025511	-0.068723	4.603448
344.738059	7301.270499	9.030515	-0.068739	4.605982
344.687457	7309.297199	9.035520	-0.068735	4.608479
345.405592	7317.271477	9.040525	-0.068874	4.610959
345.181108	7325.351738	9.045530	-0.068838	4.613469
345.633046	7333.302631	9.050535	-0.068927	4.615938
346.269381	7341.279606	9.055539	-0.069051	4.618415
346.136109	7349.362704	9.060544	-0.069031	4.620922
346.486388	7357.331186	9.065549	-0.069101	4.623393
347.120520	7365.428448	9.070554	-0.069225	4.625902
347.315972	7373.403136	9.075559	-0.069266	4.628372
347.600290	7381.444569	9.080563	-0.069325	4.630861
347.883371	7389.412721	9.085568	-0.069382	4.633326
348.026408	7397.445009	9.090573	-0.069414	4.635810
348.524561	7405.395372	9.095578	-0.069512	4.638267
348.633576	7413.454658	9.100583	-0.069538	4.640756
348.560869	7421.487092	9.105587	-0.069529	4.643236
348.952032	7429.548855	9.110592	-0.069607	4.645723
349.133913	7437.515923	9.115597	-0.069647	4.648180
349.604658	7445.550065	9.120602	-0.069739	4.650656
349.557398	7453.572433	9.125607	-0.069736	4.653127
349.911743	7461.576837	9.130611	-0.069807	4.655591
350.070684	7469.638318	9.135616	-0.069842	4.658071
349.969608	7477.647134	9.140621	-0.069828	4.660534
350.402798	7485.625038	9.145626	-0.069914	4.662986
350.225365	7493.615841	9.150631	-0.069886	4.665441
350.792692	7501.660519	9.155635	-0.069997	4.667911
350.893863	7509.730398	9.160640	-0.070021	4.670387
351.166833	7517.713249	9.165645	-0.070077	4.672836
351.496890	7525.748382	9.170650	-0.070144	4.675299
351.831460	7533.683933	9.175655	-0.070211	4.677730
351.701169	7541.746124	9.180659	-0.070192	4.680199
351.379858	7549.773300	9.185664	-0.070138	4.682656
351.539540	7557.683314	9.190669	-0.070173	4.685075
351.939473	7565.784049	9.195674	-0.070252	4.687552
352.117492	7573.716885	9.200679	-0.070291	4.689976
352.469638	7581.818050	9.205683	-0.070361	4.692449
352.836046	7589.774320	9.210688	-0.070435	4.694878
352.504959	7597.862369	9.215693	-0.070378	4.697346
352.806625	7605.857589	9.220698	-0.070440	4.699783
352.774219	7613.910071	9.225703	-0.070439	4.702238
353.492276	7621.817114	9.230707	-0.070578	4.704645
353.805254	7629.888799	9.235712	-0.070641	4.707102
354.242777	7637.863795	9.240717	-0.070728	4.709528
354.071245	7646.002432	9.245722	-0.070701	4.712004
354.501419	7653.891422	9.250727	-0.070787	4.714401
354.504114	7662.012653	9.255731	-0.070792	4.716868
354.840204	7669.963031	9.260736	-0.070860	4.719282
355.059055	7678.018837	9.265741	-0.070906	4.721727
354.944145	7686.020382	9.270746	-0.070890	4.724154
355.359710	7694.041499	9.275751	-0.070972	4.726585
355.416360	7702.031746	9.280755	-0.070988	4.729006
355.595246	7710.083598	9.285760	-0.071027	4.731444
356.130472	7717.981059	9.290765	-0.071132	4.733834
356.266623	7726.191769	9.295770	-0.071162	4.736318
356.508162	7734.127712	9.300775	-0.071212	4.738717
356.535109	7742.191280	9.305779	-0.071223	4.741154
356.729893	7750.162028	9.310784	-0.071264	4.743562
357.464263	7758.146110	9.315789	-0.071406	4.745971
357.489410	7766.275015	9.320794	-0.071416	4.748423
357.544526	7774.239611	9.325799	-0.071431	4.750826
358.505610	7782.143053	9.330803	-0.071616	4.753206
358.736013	7790.229290	9.335808	-0.071664	4.755642
358.984894	7798.230745	9.340813	-0.071715	4.758050
359.163203	7806.312526	9.345818	-0.071754	4.760483
359.486646	7814.238901	9.350823	-0.071819	4.762866
359.516051	7822.311084	9.355827	-0.071830	4.765293
360.337770	7830.316786	9.360832	-0.071988	4.767697
360.617963	7838.309269	9.365837	-0.072045	4.770097
360.561689	7846.429556	9.370842	-0.072040	4.772535
360.612984	7854.378116	9.375847	-0.072055	4.774920
360.839974	7862.413654	9.380851	-0.072102	4.777329
361.467690	7870.398056	9.385856	-0.072224	4.779720
361.444590	7878.434130	9.390861	-0.072225	4.782128
361.575077	7886.466497	9.395866	-0.072255	4.784533
362.064920	7894.441113	9.400871	-0.072351	4.786918
362.076352	7902.483538	9.405875	-0.072359	4.789324
362.430497	7910.552655	9.410880	-0.072430	4.791735
362.844936	7918.423945	9.415885	-0.072512	4.794086
363.210347	7926.567388	9.420890	-0.072585	4.796517
363.134116	7934.491289	9.425895	-0.072576	4.798883
363.147932	7942.586557	9.430899	-0.072584	4.801299
363.690247	7950.494450	9.435904	-0.072690	4.803655
363.830479	7958.586894	9.440909	-0.072722	4.806067
364.006606	7966.633606	9.445914	-0.072760	4.808464
364.208141	7974.629153	9.450919	-0.072802	4.810844
364.451022	7982.608297	9.455923	-0.072853	4.813218
364.895073	7989.990550	9.460928	-0.072940	4.815412
364.725755	7994.622249	9.465933	-0.072912	4.816790

364.953890	7997.181126	9.470938	-0.072956	4.817550
365.306599	7998.354685	9.475943	-0.073022	4.817898
365.302034	7998.901803	9.480947	-0.073022	4.818060
365.250620	7999.840081	9.485952	-0.073013	4.818339
365.528902	7999.815443	9.490957	-0.073065	4.818331
365.520839	7999.857348	9.495962	-0.073063	4.818344
365.325609	7999.841081	9.500967	-0.073027	4.818339
365.761406	7999.865816	9.505971	-0.073108	4.818345
365.813485	7999.910626	9.510976	-0.073118	4.818358
365.147460	7999.957382	9.515981	-0.072994	4.818375
365.439629	7999.969693	9.520986	-0.073048	4.818377
365.870197	7999.923986	9.525991	-0.073128	4.818362
365.711785	7999.964929	9.530995	-0.073099	4.818375
365.726582	7999.950422	9.536000	-0.073101	4.818370
365.765536	7999.890022	9.541005	-0.073109	4.818352
365.977549	7999.951677	9.546010	-0.073148	4.818370
366.318339	7999.890065	9.551015	-0.073212	4.818350
366.483399	7999.840806	9.556019	-0.073242	4.818335
366.319795	7999.913191	9.561024	-0.073212	4.818357
366.355409	7999.931522	9.566029	-0.073218	4.818362
366.537465	7999.899296	9.571034	-0.073252	4.818352
366.206351	7999.941079	9.576039	-0.073191	4.818366
366.370645	7999.968486	9.581043	-0.073221	4.818373
366.095634	8000.006818	9.586048	-0.073170	4.818386
366.196315	7999.982956	9.591053	-0.073189	4.818378
366.510744	8000.012373	9.596058	-0.073247	4.818386
367.094726	7999.893096	9.601063	-0.073356	4.818348
367.141428	7999.902123	9.606067	-0.073365	4.818350
367.303610	7999.911647	9.611072	-0.073395	4.818353
366.822200	7999.959819	9.616077	-0.073305	4.818369
366.975472	7999.970273	9.621082	-0.073334	4.818371
367.237364	7999.920210	9.626087	-0.073382	4.818355
367.636259	7999.859377	9.631091	-0.073457	4.818336
367.776393	7999.836043	9.636096	-0.073483	4.818328
367.554452	7999.854077	9.641101	-0.073441	4.818334
368.112369	7999.883607	9.646106	-0.073545	4.818341
367.927445	7999.916843	9.651111	-0.073511	4.818352
367.616161	7999.944184	9.656115	-0.073453	4.818361
367.920118	7999.941952	9.661120	-0.073510	4.818359
368.205270	7999.833378	9.666125	-0.073563	4.818326
367.829631	7999.916579	9.671130	-0.073493	4.818352
368.004152	7999.918916	9.676135	-0.073525	4.818352
367.673150	7999.965950	9.681139	-0.073464	4.818367
367.797092	7999.972861	9.686144	-0.073487	4.818369
368.078002	7999.886289	9.691149	-0.073539	4.818342
368.236333	7999.888409	9.696154	-0.073568	4.818342
368.159286	7999.878973	9.701159	-0.073554	4.818339
368.031603	7999.920328	9.706163	-0.073530	4.818352
368.192730	7999.917233	9.711168	-0.073560	4.818351
367.874077	7999.946576	9.716173	-0.073501	4.818361
368.168569	7999.946319	9.721178	-0.073556	4.818359
367.967970	7999.944681	9.726183	-0.073518	4.818360
368.497601	7999.837281	9.731187	-0.073617	4.818326
368.136058	7999.957435	9.736192	-0.073550	4.818363
367.822037	7999.958479	9.741197	-0.073491	4.818364
367.935137	7999.956842	9.746202	-0.073512	4.818364
368.291030	7999.943752	9.751207	-0.073578	4.818358
367.619542	7999.994628	9.756211	-0.073453	4.818376
368.296482	7999.948025	9.761216	-0.073579	4.818359
368.302976	7999.910296	9.766221	-0.073581	4.818348
368.263819	7999.973845	9.771226	-0.073573	4.818367
367.931486	7999.967291	9.776231	-0.073511	4.818367
368.489799	7999.935905	9.781235	-0.073615	4.818355
368.717443	7999.917947	9.786240	-0.073658	4.818349
368.492238	7999.872912	9.791245	-0.073616	4.818336
368.684196	7999.945860	9.796250	-0.073651	4.818357
368.493499	7999.951707	9.801255	-0.073616	4.818360
368.575981	7999.925501	9.806259	-0.073631	4.818352
368.898959	7999.900416	9.811264	-0.073691	4.818343
368.940721	7999.853706	9.816269	-0.073699	4.818329
369.036047	7999.892798	9.821274	-0.073717	4.818340
369.141162	7999.866895	9.826279	-0.073736	4.818332
369.317126	7999.846143	9.831283	-0.073769	4.818325
369.465470	7999.872290	9.836288	-0.073797	4.818332
369.146247	7999.877464	9.841293	-0.073737	4.818335
369.479379	7999.915542	9.846298	-0.073799	4.818345
369.433256	7999.903368	9.851303	-0.073791	4.818342
369.187092	7999.888513	9.856307	-0.073745	4.818338
369.604188	7999.852085	9.861312	-0.073822	4.818326
369.351298	7999.835039	9.866317	-0.073775	4.818322
369.937196	7999.781967	9.871322	-0.073884	4.818304
369.454714	7999.807011	9.876327	-0.073795	4.818313
369.448576	7999.815331	9.881331	-0.073793	4.818315
369.803852	7999.858959	9.886336	-0.073860	4.818327
369.690185	7999.780752	9.891341	-0.073838	4.818304
369.635312	7999.828336	9.896346	-0.073828	4.818319
369.571482	7999.845336	9.901351	-0.073816	4.818324
370.003949	7999.773401	9.906355	-0.073897	4.818301
370.251777	7999.827144	9.911360	-0.073943	4.818316
369.587215	7999.860250	9.916365	-0.073819	4.818328
369.607689	7999.915147	9.921370	-0.073823	4.818344
369.825080	7999.877093	9.926375	-0.073863	4.818332
369.487686	7999.916687	9.931379	-0.073801	4.818345
369.741503	7999.935846	9.936384	-0.073848	4.818350
369.573600	7999.851659	9.941389	-0.073817	4.818326
369.518648	7999.824661	9.946394	-0.073806	4.818318
369.412619	7999.869458	9.951399	-0.073787	4.818332
369.436398	7999.870826	9.956403	-0.073791	4.818332
369.335784	7999.895737	9.961408	-0.073772	4.818340
369.476307	7999.866107	9.966413	-0.073798	4.818330
369.242381	7999.917592	9.971418	-0.073755	4.818347
369.262339	7999.925212	9.976423	-0.073759	4.818349
369.568856	7999.865243	9.981427	-0.073816	4.818330
369.683423	7999.938208	9.986432	-0.073837	4.818351
369.835071	7999.828894	9.991437	-0.073865	4.818318
369.809227	7999.861110	9.996442	-0.073860	4.818328
369.981261	7999.885475	10.001447	-0.073892	4.818334
369.700611	7999.880660	10.006451	-0.073840	4.818334
369.303164	7999.959366	10.011456	-0.073766	4.818359
369.751281	7999.862430	10.016461	-0.073849	4.818328
370.102373	7999.851380	10.021466	-0.073915	4.818324
369.839667	7999.891975	10.026471	-0.073866	4.818337
369.665355	7999.894889	10.031475	-0.073833	4.818338
369.745614	7999.934830	10.036480	-0.073848	4.818350
369.225047	7999.927850	10.041485	-0.073751	4.818350
369.094378	8000.021687	10.046490	-0.073727	4.818378
368.996983	8000.002523	10.051495	-0.073709	4.818373
369.166935	7999.955430	10.056499	-0.073741	4.818358
369.490050	7999.973416	10.061504	-0.073801	4.818362
369.170013	7999.949167	10.066509	-0.073741	4.818356
369.239221	8000.002615	10.071514	-0.073754	4.818372
369.168671	7999.985912	10.076519	-0.073741	4.818367
369.399207	8000.010010	10.081523	-0.073784	4.818374
369.521697	8000.020055	10.086528	-0.073807	4.818376
369.642556	7999.927135	10.091533	-0.073829	4.818348
369.503669	7999.973592	10.096538	-0.073803	4.818362
369.655518	7999.964072	10.101543	-0.073831	4.818359
369.712298	7999.975337	10.106547	-0.073842	4.818362
369.840141	7999.998059	10.111552	-0.073866	4.818368
370.165597	7999.923639	10.116557	-0.073926	4.818345
370.598276	7999.873767	10.121562	-0.074007	4.818328
370.394993	7999.815365	10.126567	-0.073969	4.818312
370.308172	7999.821553	10.131571	-0.073953	4.818314
370.341573	7999.880826	10.136576	-0.073959	4.818331
370.359247	7999.912575	10.141581	-0.073962	4.818341
369.885994	7999.935640	10.146586	-0.073874	4.818349
370.144213	7999.924396	10.151591	-0.073922	4.818345
370.441309	7999.853797	10.156595	-0.073978	4.818323
370.524761	7999.849663	10.161600	-0.073993	4.818321
370.191873	7999.949192	10.166605	-0.073931	4.818352
369.972311	8000.006123	10.171610	-0.073890	4.818370
370.175581	7999.938467	10.176615	-0.073928	4.818349
369.970565	7999.926263	10.181619	-0.073890	4.818346
370.365209	7999.927353	10.186624	-0.073963	4.818345
369.939607	7999.936350	10.191629	-0.073884	4.818349
370.085077	7999.960360	10.196634	-0.073911	4.818356
370.058147	7999.921131	10.201639	-0.073906	4.818344
370.250907	7999.899554	10.206643	-0.073942	4.818337
370.277632	7999.972393	10.211648	-0.073947	4.818359
370.088945	7999.913137	10.216653	-0.073912	4.818342
369.998700	7999.969701	10.221658	-0.073895	4.818359
369.738609	7999.996675	10.226663	-0.073847	4.818368
369.509528	8000.033519	10.231667	-0.073804	4.818380
369.452669	7999.974981	10.236672	-0.073793	4.818363
369.863657	7999.939524	10.241677	-0.073870	4.818351
369.894380	7999.963044	10.246682	-0.073876	4.818358
369.675270	7999.958004	10.251687	-0.073835	4.818357
369.882405	7999.991244	10.256691	-0.073873	4.818366
369.851495	8000.041250	10.261696	-0.073868	4.818381
369.895260	7999.998768	10.266701	-0.073876	4.818368
369.437462	8000.067209	10.271706	-0.073790	4.818390
369.993427	7999.995880	10.276711	-0.073894	4.818367
370.238304	7999.971852	10.281715	-0.073939	4.818359
370.740445	7999.963880	10.286720	-0.074033	4.818354
370.700752	7999.903470	10.291725	-0.074026	4.818337
371.121117	7999.838727	10.296730	-0.074104	4.818316
369.977403	8000.001963	10.301735	-0.073891	4.818369
370.942275	7999.892000	10.306739	-0.074070	4.818332
370.801653	7999.895365	10.311744	-0.074044	4.818334
370.578797	7999.882921	10.316749	-0.074003	4.818331
370.943313	7999.809024	10.321754	-0.074071	4.818308
371.021807	7999.874155	10.326759	-0.074085	4.818327
370.782624	7999.833129	10.331763	-0.074041	4.818315
371.175431	7999.849952	10.336768	-0.074114	4.818319
371.058454	7999.856785	10.341773	-0.074092	4.818321
371.507786	7999.801885	10.346778	-0.074176	4.818303
371.178441	7999.892008	10.351783	-0.074114	4.818331
370.887840	7999.938531	10.356787	-0.074060	4.818346
371.142364	7999.845302	10.361792	-0.074108	4.818318
370.981646	7999.871507	10.366797	-0.074078	4.818326
370.998949	7999.896950	10.371802	-0.074081	4.818334
371.053812	7999.894533	10.376807	-0.074091	4.818333
370.632085	7999.911985	10.381811	-0.074012	4.818339
370.893128	7999.932293	10.386816	-0.074061	4.818344
370.486886	7999.941549	10.391821	-0.073985	4.818349
370.539328	7999.934899	10.396826	-0.073995	4.818347
370.698209	7999.922322	10.401831	-0.074025	4.818342
370.377247	7999.945328	10.406835	-0.073965	4.818350
370.969967	7999.956430	10.411840	-0.074075	4.818351
370.698440	7999.927575	10.416845	-0.074025	4.818344
371.057351	7999.942894	10.421850	-0.074092	4.818347
370.834382	7999.970365	10.426855	-0.074050	4.818356
370.661647	7999.881908	10.431859	-0.074018	4.818330
370.919016	7999.971498	10.436864	-0.074066	4.818356
371.145965	7999.860040	10.441869	-0.074108	4.818322
371.079691	7999.879109	10.446874	-0.074096	4.818328
370.939999	7999.916102	10.451879	-0.074070	4.818339
371.118915	7999.882785	10.456883	-0.074103	4.818329
371.167820	7999.928611	10.461888	-0.074112	4.818342
370.923418	7999.911674	10.466893	-0.074066	4.818338
371.280155	7999.867087	10.471898	-0.074133	4.818324
370.986691	7999.982903	10.476903	-0.074078	4.818359
370.507823	7999.985932	10.481907	-0.073989	4.818362
370.844219	7999.974687	10.486912	-0.074052	4.818357
370.867304	7999.957137	10.491917	-0.074056	4.818352
370.771543	7999.972659	10.496922	-0.074038	4.818357
371.126736	7999.890234	10.501927	-0.074104	4.818331
371.528777	7999.798984	10.506931	-0.074179	4.818302
371.617994	7999.831694	10.511936	-0.074196	4.818312
371.476414	7999.839248	10.516941	-0.074169	4.818315
371.323512	7999.840347	10.521946	-0.074141	4.818315
371.330899	7999.891918	10.526951	-0.074142	4.818331
371.257420	7999.836306	10.531955	-0.074128	4.818315
371.564187	7999.891895	10.536960	-0.074186	4.818330
371.330832	7999.862501	10.541965	-0.074142	4.818322
371.310166	7999.919999	10.546970	-0.074138	4.818339
371.331877	7999.883522	10.551975	-0.074142	4.818328
371.199217	7999.805057	10.556979	-0.074118	4.818305
371.711470	7999.864453	10.561984	-0.074213	4.818321
371.497313	7999.874184	10.566989	-0.074173	4.818325
371.771653	7999.823239	10.571994	-0.074224	4.818309
371.790915	7999.835052	10.576999	-0.074228	4.818312
371.927896	7999.851596	10.582003	-0.074253	4.818316
371.430267	7999.960470	10.587008	-0.074161	4.818351
371.200763	7999.931128	10.592013	-0.074118	4.818343
371.684277	7999.848324	10.597018	-0.074208	4.818316
371.626164	7999.915825	10.602023	-0.074197	4.818337
371.584793	7999.878501	10.607027	-0.074189	4.818326
371.480289	7999.944329	10.612032	-0.074170	4.818346
371.334310	7999.936066	10.617037	-0.074143	4.818344
371.552638	7999.907480	10.622042	-0.074183	4.818334
371.494142	7999.942411	10.627047	-0.074172	4.818345
371.404302	7999.912841	10.632051	-0.074156	4.818337
371.431604	7999.933166	10.637056	-0.074161	4.818343
371.443627	7999.917569	10.642061	-0.074163	4.818338
371.228401	7999.955649	10.647066	-0.074123	4.818350
371.305389	7999.934621	10.652071	-0.074137	4.818344
370.953578	7999.954060	10.657075	-0.074072	4.818351
371.151987	7999.972478	10.662080	-0.074109	4.818355
371.551285	7999.893797	10.667085	-0.074183	4.818330
371.783940	7999.866454	10.672090	-0.074226	4.818321
371.720971	7999.899224	10.677095	-0.074214	4.818331
371.481269	7999.871845	10.682099	-0.074170	4.818324
371.404908	7999.928596	10.687104	-0.074156	4.818341
371.179564	7999.938177	10.692109	-0.074114	4.818345
370.911959	7999.971352	10.697114	-0.074064	4.818356
371.012762	7999.980057	10.702119	-0.074083	4.818358
371.066686	7999.916700	10.707123	-0.074093	4.818339
371.276631	7999.947879	10.712128	-0.074132	4.818348
371.051284	7999.973217	10.717133	-0.074090	4.818356
371.112496	7999.930968	10.722138	-0.074101	4.818343
371.482921	7999.912827	10.727143	-0.074170	4.818336
371.626682	7999.901099	10.732147	-0.074197	4.818332
371.398681	7999.951613	10.737152	-0.074154	4.818348
370.915316	7999.981892	10.742157	-0.074064	4.818359
371.356377	7999.977305	10.747162	-0.074146	4.818356
371.462353	8000.012342	10.752167	-0.074166	4.818366
371.143441	7999.958688	10.757171	-0.074107	4.818351
370.961624	8000.002469	10.762176	-0.074073	4.818365
371.148801	7999.989222	10.767181	-0.074108	4.818360
371.405999	7999.910735	10.772186	-0.074156	4.818336
371.654910	7999.946640	10.777191	-0.074202	4.818346
371.688437	7999.865150	10.782195	-0.074208	4.818321
371.635980	7999.888607	10.787200	-0.074198	4.818329
371.322749	7999.903311	10.792205	-0.074140	4.818334
371.291948	7999.892392	10.797210	-0.074134	4.818331
371.403470	7999.982128	10.802215	-0.074155	4.818357
371.495783	7999.894075	10.807219	-0.074172	4.818331
371.511104	7999.954157	10.812224	-0.074175	4.818349
371.592967	7999.924791	10.817229	-0.074190	4.818339
371.748686	7999.857547	10.822234	-0.074219	4.818319
371.823535	7999.931035	10.827239	-0.074233	4.818340
371.873881	7999.871831	10.832243	-0.074242	4.818323
371.524242	7999.959581	10.837248	-0.074177	4.818350
371.883187	7999.853045	10.842253	-0.074244	4.818317
371.466599	7999.891574	10.847258	-0.074167	4.818330
371.611918	7999.958654	10.852263	-0.074194	4.818349
371.600713	7999.902826	10.857267	-0.074192	4.818333
371.905853	7999.861749	10.862272	-0.074248	4.818320
371.932168	7999.902020	10.867277	-0.074253	4.818331
371.687662	7999.944959	10.872282	-0.074208	4.818345
371.575930	7999.980226	10.877287	-0.074187	4.818356
372.101576	7999.903241	10.882291	-0.074285	4.818331
371.701528	7999.976657	10.887296	-0.074210	4.818354
371.837047	7999.939607	10.892301	-0.074235	4.818343
371.622536	7999.923070	10.897306	-0.074195	4.818339
371.984613	7999.924778	10.902311	-0.074263	4.818338
372.250182	7999.782322	10.907315	-0.074312	4.818295
372.232459	7999.867174	10.912320	-0.074309	4.818320
372.088332	7999.846329	10.917325	-0.074282	4.818314
372.056264	7999.860605	10.922330	-0.074276	4.818319
372.035865	7999.886592	10.927335	-0.074272	4.818326
372.090008	7999.850551	10.932339	-0.074282	4.818315
372.065253	7999.878581	10.937344	-0.074278	4.818324
372.089721	7999.825333	10.942349	-0.074282	4.818308
371.947304	7999.929520	10.947354	-0.074256	4.818339
372.307337	7999.909140	10.952359	-0.074323	4.818332
372.067799	7999.819783	10.957363	-0.074278	4.818306
372.225816	7999.881782	10.962368	-0.074308	4.818324
372.168993	7999.865260	10.967373	-0.074297	4.818320
372.387373	7999.836676	10.972378	-0.074338	4.818310
372.287579	7999.866850	10.977383	-0.074319	4.818320
372.163352	7999.864131	10.982387	-0.074296	4.818319
372.449855	7999.825956	10.987392	-0.074349	4.818307
372.109457	7999.885466	10.992397	-0.074286	4.818326
371.976353	7999.888931	10.997402	-0.074261	4.818327
372.413029	7999.834913	11.002407	-0.074342	4.818310
372.164218	7999.805310	11.007411	-0.074296	4.818302
372.354707	7999.863542	11.012416	-0.074331	4.818318
372.118187	7999.900285	11.017421	-0.074287	4.818330
371.925445	7999.921859	11.022426	-0.074252	4.818337
372.359935	7999.885670	11.027431	-0.074332	4.818325
372.190816	7999.849783	11.032435	-0.074301	4.818315
372.346661	7999.903348	11.037440	-0.074330	4.818330
371.849570	7999.940795	11.042445	-0.074237	4.818343
372.297963	7999.832309	11.047450	-0.074321	4.818309
372.450623	7999.882680	11.052455	-0.074349	4.818324
372.283411	7999.893041	11.057459	-0.074318	4.818327
372.584850	7999.839309	11.062464	-0.074374	4.818310
372.614363	7999.796633	11.067469	-0.074380	4.818297
372.800465	7999.776019	11.072474	-0.074414	4.818290
372.578084	7999.867579	11.077479	-0.074373	4.818319
372.635891	7999.787465	11.082483	-0.074384	4.818295
372.477902	7999.820009	11.087488	-0.074354	4.818305
372.291256	7999.888937	11.092493	-0.074319	4.818326
372.422122	7999.848673	11.097498	-0.074344	4.818314
372.958388	7999.739265	11.102503	-0.074444	4.818279
372.737942	7999.726850	11.107507	-0.074402	4.818276
372.589161	7999.793134	11.112512	-0.074375	4.818296
372.783067	7999.781029	11.117517	-0.074411	4.818292
372.869055	7999.763274	11.122522	-0.074427	4.818286
372.580668	7999.918028	11.127527	-0.074373	4.818334
372.616651	7999.853378	11.132531	-0.074380	4.818314
372.737762	7999.890721	11.137536	-0.074402	4.818325
372.690984	7999.826011	11.142541	-0.074394	4.818306
372.753220	7999.820542	11.147546	-0.074405	4.818304
372.778772	7999.861854	11.152551	-0.074410	4.818316
372.736707	7999.812965	11.157555	-0.074402	4.818302
372.693504	7999.872263	11.162560	-0.074394	4.818320
372.904299	7999.742728	11.167565	-0.074433	4.818280
372.644750	7999.802273	11.172570	-0.074385	4.818299
372.527961	7999.889997	11.177575	-0.074363	4.818325
372.509340	7999.871887	11.182579	-0.074360	4.818320
373.088751	7999.793524	11.187584	-0.074468	4.818295
372.692666	7999.864892	11.192589	-0.074394	4.818317
372.591399	7999.874036	11.197594	-0.074375	4.818320
372.697695	7999.870210	11.202599	-0.074395	4.818319
372.418286	7999.892720	11.207603	-0.074343	4.818327
372.506269	7999.933820	11.212608	-0.074359	4.818339
372.640398	7999.882044	11.217613	-0.074384	4.818323
372.909867	7999.815277	11.222618	-0.074434	4.818302
373.065554	7999.832073	11.227623	-0.074463	4.818306
372.700611	7999.868142	11.232627	-0.074395	4.818318
372.723215	7999.928324	11.237632	-0.074399	4.818336
372.747417	7999.868769	11.242637	-0.074404	4.818318
373.003032	7999.793411	11.247642	-0.074451	4.818295
372.942682	7999.871389	11.252647	-0.074440	4.818318
372.816649	7999.778301	11.257651	-0.074417	4.818291
372.564993	7999.857911	11.262656	-0.074370	4.818316
372.409681	7999.851623	11.267661	-0.074341	4.818315
372.463818	7999.847097	11.272666	-0.074351	4.818313
372.665873	7999.864515	11.277671	-0.074389	4.818317
372.567173	7999.866341	11.282675	-0.074370	4.818318
372.951216	7999.827375	11.287680	-0.074442	4.818305
373.338390	7999.776895	11.292685	-0.074514	4.818289
372.877987	7999.826389	11.297690	-0.074428	4.818305
373.236301	7999.870069	11.302695	-0.074495	4.818317
373.018842	7999.857693	11.307699	-0.074454	4.818314
372.890993	7999.879087	11.312704	-0.074430	4.818321
372.678473	7999.915101	11.317709	-0.074391	4.818332
372.617210	7999.872257	11.322714	-0.074379	4.818320
372.298756	7999.964627	11.327719	-0.074320	4.818349
372.563021	7999.910396	11.332723	-0.074369	4.818331
372.831284	7999.881431	11.337728	-0.074419	4.818322
372.630050	7999.896587	11.342733	-0.074382	4.818327
372.461186	7999.884864	11.347738	-0.074350	4.818324
372.309003	7999.950053	11.352743	-0.074322	4.818344
372.227031	7999.933194	11.357747	-0.074307	4.818339
372.301633	7999.942598	11.362752	-0.074321	4.818342
372.659553	7999.889625	11.367757	-0.074387	4.818325
372.524584	7999.931933	11.372762	-0.074362	4.818338
372.772250	7999.919500	11.377767	-0.074408	4.818333
373.010646	7999.793487	11.382771	-0.074453	4.818295
372.791424	7999.910301	11.387776	-0.074412	4.818330
372.399528	7999.997483	11.392781	-0.074339	4.818358
372.376927	7999.866915	11.397786	-0.074335	4.818319
372.333718	7999.957728	11.402791	-0.074327	4.818346
372.750199	7999.849864	11.407795	-0.074404	4.818313
373.050858	7999.831839	11.412800	-0.074460	4.818306
372.740675	7999.873896	11.417805	-0.074402	4.818320
372.770396	7999.846980	11.422810	-0.074408	4.818312
373.178921	7999.864021	11.427815	-0.074484	4.818315
372.587800	7999.894951	11.432819	-0.074374	4.818327
372.492762	7999.973513	11.437824	-0.074356	4.818350
373.219871	7999.829901	11.442829	-0.074491	4.818305
373.195887	7999.794910	11.447834	-0.074487	4.818295
372.920813	7999.858449	11.452839	-0.074436	4.818315
372.987991	7999.818380	11.457843	-0.074448	4.818302
372.895813	7999.858111	11.462848	-0.074431	4.818315
372.988737	7999.857257	11.467853	-0.074448	4.818314
373.117203	7999.791748	11.472858	-0.074472	4.818294
373.049238	7999.889583	11.477863	-0.074460	4.818323
373.091655	7999.835525	11.482867	-0.074467	4.818307
372.881242	7999.928295	11.487872	-0.074428	4.818335
372.721844	7999.944012	11.492877	-0.074399	4.818341
373.059648	7999.777313	11.497882	-0.074461	4.818290
372.976962	7999.829778	11.502887	-0.074446	4.818306
372.510811	7999.897054	11.507891	-0.074359	4.818328
372.547784	7999.916459	11.512896	-0.074366	4.818333
372.313903	7999.977399	11.517901	-0.074323	4.818352
372.307543	7999.952100	11.522906	-0.074321	4.818345
372.995426	7999.915113	11.527911	-0.074449	4.818331
373.020504	7999.852418	11.532915	-0.074454	4.818312
373.095370	7999.898595	11.537920	-0.074468	4.818326
372.755105	7999.987520	11.542925	-0.074405	4.818354
373.364480	7999.836024	11.547930	-0.074518	4.818306
373.097963	7999.970062	11.552935	-0.074468	4.818347
372.932584	7999.965739	11.557939	-0.074438	4.818346
372.683465	7999.979201	11.562944	-0.074391	4.818351
372.361608	7999.995888	11.567949	-0.074331	4.818358
372.581967	7999.955775	11.572954	-0.074372	4.818345
372.826739	7999.984273	11.577959	-0.074418	4.818352
372.331893	7999.963971	11.582963	-0.074326	4.818348
372.885423	7999.922028	11.587968	-0.074429	4.818334
372.980652	7999.906498	11.592973	-0.074446	4.818329
373.164990	7999.806021	11.597978	-0.074481	4.818298
372.741601	7999.946357	11.602983	-0.074402	4.818341
372.694441	7999.916308	11.607987	-0.074393	4.818333
372.314315	8000.008901	11.612992	-0.074322	4.818362
372.149167	7999.990925	11.617997	-0.074292	4.818357
372.108722	7999.995633	11.623002	-0.074284	4.818359
372.295149	8000.009691	11.628007	-0.074319	4.818362
372.618296	7999.943644	11.633011	-0.074379	4.818341
372.627114	7999.967924	11.638016	-0.074381	4.818348
372.228641	8000.025603	11.643021	-0.074306	4.818367
372.787588	7999.948016	11.648026	-0.074410	4.818342
372.389023	8000.024603	11.653031	-0.074336	4.818366
372.185557	8000.026072	11.658035	-0.074298	4.818367
372.341333	8000.047072	11.663040	-0.074327	4.818373
372.450913	8000.018077	11.668045	-0.074348	4.818364
372.240963	7999.978489	11.673050	-0.074309	4.818353
372.720715	7999.997537	11.678055	-0.074398	4.818357
372.531144	7999.981333	11.683059	-0.074363	4.818353
372.644838	7999.967101	11.688064	-0.074384	4.818348
372.856136	7999.985696	11.693069	-0.074423	4.818353
372.955601	7999.905090	11.698074	-0.074441	4.818328
373.156179	7999.940349	11.703079	-0.074479	4.818338
373.032514	7999.949192	11.708083	-0.074456	4.818341
372.596142	8000.018968	11.713088	-0.074375	4.818364
373.216565	7999.936955	11.718093	-0.074490	4.818337
372.514202	7999.984249	11.723098	-0.074359	4.818354
373.052974	7999.982029	11.728103	-0.074460	4.818351
372.431643	7999.991543	11.733107	-0.074344	4.818356
372.659460	7999.991449	11.738112	-0.074386	4.818355
373.016197	7999.946865	11.743117	-0.074453	4.818340
372.831409	7999.993757	11.748122	-0.074418	4.818355
372.794834	7999.993265	11.753127	-0.074411	4.818355
372.881494	7999.955558	11.758131	-0.074428	4.818344
373.094431	7999.895386	11.763136	-0.074467	4.818325
373.177061	7999.909101	11.768141	-0.074483	4.818329
372.934160	7999.882726	11.773146	-0.074437	4.818322
373.523388	7999.836011	11.778151	-0.074547	4.818305
373.312438	7999.902512	11.783155	-0.074508	4.818326
373.294250	7999.850791	11.788160	-0.074504	4.818311
373.460039	7999.900290	11.793165	-0.074535	4.818325
373.408273	7999.905897	11.798170	-0.074525	4.818327
373.544700	7999.908779	11.803175	-0.074551	4.818327
373.194151	7999.941888	11.808179	-0.074486	4.818338
373.337859	7999.922807	11.813184	-0.074512	4.818332
372.894185	7999.990384	11.818189	-0.074430	4.818354
372.991986	7999.928665	11.823194	-0.074448	4.818335
372.982976	7999.971614	11.828199	-0.074446	4.818348
372.636881	8000.012138	11.833203	-0.074382	4.818361
372.614232	8000.022338	11.838208	-0.074378	4.818364
372.584317	8000.005127	11.843213	-0.074372	4.818359
372.830710	7999.982172	11.848218	-0.074418	4.818352
372.547945	8000.035101	11.853223	-0.074365	4.818369
372.988509	7999.925460	11.858227	-0.074447	4.818334
373.313463	7999.904610	11.863232	-0.074508	4.818327
373.344975	7999.972267	11.868237	-0.074514	4.818347
373.285390	7999.951505	11.873242	-0.074502	4.818341
372.999446	8000.036958	11.878247	-0.074449	4.818367
372.653933	8000.045973	11.883251	-0.074385	4.818371
373.332290	7999.968941	11.888256	-0.074511	4.818346
373.401960	7999.987735	11.893261	-0.074524	4.818351
373.197597	7999.953473	11.898266	-0.074486	4.818342
373.346865	7999.970184	11.903271	-0.074514	4.818346
373.096600	7999.966821	11.908275	-0.074467	4.818346
372.813189	7999.979822	11.913280	-0.074414	4.818351
373.279311	7999.948263	11.918285	-0.074501	4.818340
372.885452	7999.945073	11.923290	-0.074428	4.818340
372.956708	8000.012212	11.928295	-0.074441	4.818360
372.721333	8000.043717	11.933299	-0.074397	4.818370
372.701593	8000.008784	11.938304	-0.074394	4.818360
373.216144	7999.950561	11.943309	-0.074489	4.818341
373.040074	7999.909326	11.948314	-0.074457	4.818329
373.471957	7999.944541	11.953319	-0.074537	4.818338
373.420747	7999.918639	11.958323	-0.074527	4.818330
373.616017	7999.876088	11.963328	-0.074564	4.818317
373.513488	7999.924085	11.968333	-0.074545	4.818332
373.257017	7999.904881	11.973338	-0.074497	4.818327
373.878014	7999.845987	11.978343	-0.074612	4.818307
373.596508	7999.913641	11.983347	-0.074560	4.818328
373.491953	7999.874417	11.988352	-0.074541	4.818317
373.542345	7999.884547	11.993357	-0.074550	4.818320
373.529402	7999.921141	11.998362	-0.074548	4.818331
373.599800	7999.978815	12.003367	-0.074561	4.818348
373.557029	7999.892095	12.008371	-0.074553	4.818322
373.469738	7999.920337	12.013376	-0.074536	4.818331
373.273906	7999.963928	12.018381	-0.074500	4.818344
373.307897	7999.891897	12.023386	-0.074506	4.818323
373.578471	7999.951209	12.028391	-0.074557	4.818339
373.673681	7999.926224	12.033395	-0.074574	4.818332
373.442859	7999.944133	12.038400	-0.074531	4.818338
373.428404	7999.926078	12.043405	-0.074529	4.818333
373.485034	7999.860655	12.048410	-0.074539	4.818313
373.584427	7999.950234	12.053415	-0.074558	4.818339
373.645560	7999.907982	12.058419	-0.074569	4.818326
373.297154	7999.920109	12.063424	-0.074504	4.818331
373.826975	7999.870497	12.068429	-0.074603	4.818315
373.437142	7999.899927	12.073434	-0.074530	4.818325
373.219467	7999.978943	12.078439	-0.074490	4.818349
373.622567	7999.824676	12.083443	-0.074565	4.818302
373.203907	7999.886286	12.088448	-0.074487	4.818322
373.784614	7999.894085	12.093453	-0.074595	4.818322
373.587406	7999.904041	12.098458	-0.074558	4.818325
373.727285	7999.938486	12.103463	-0.074584	4.818335
373.611251	7999.892804	12.108467	-0.074562	4.818322
373.452508	7999.893822	12.113472	-0.074533	4.818323
373.489367	7999.953146	12.118477	-0.074540	4.818340
373.660115	7999.843031	12.123482	-0.074571	4.818307
373.695482	7999.924397	12.128487	-0.074578	4.818331
373.817225	7999.833584	12.133491	-0.074601	4.818304
374.032361	7999.803906	12.138496	-0.074641	4.818294
373.725082	7999.899578	12.143501	-0.074584	4.818324
373.641438	7999.843826	12.148506	-0.074568	4.818307
373.749448	7999.889398	12.153511	-0.074588	4.818320
373.411025	7999.938428	12.158515	-0.074525	4.818336
373.442626	7999.890527	12.163520	-0.074531	4.818322
373.486334	7999.954146	12.168525	-0.074539	4.818341
373.345722	7999.939649	12.173530	-0.074513	4.818337
373.583977	7999.943899	12.178535	-0.074557	4.818337
373.432486	7999.938712	12.183539	-0.074529	4.818336
373.855777	7999.876112	12.188544	-0.074608	4.818316
373.535260	7999.951646	12.193549	-0.074548	4.818340
373.579642	7999.904967	12.198554	-0.074556	4.818326
373.821516	7999.908216	12.203559	-0.074601	4.818326
373.437048	7999.916707	12.208563	-0.074530	4.818330
373.704139	7999.878272	12.213568	-0.074579	4.818317
374.029033	7999.859524	12.218573	-0.074640	4.818310
373.745447	7999.885128	12.223578	-0.074587	4.818319
373.514036	7999.989173	12.228583	-0.074544	4.818351
373.178716	7999.975213	12.233587	-0.074482	4.818348
373.140899	7999.992563	12.238592	-0.074475	4.818354
373.070122	8000.003167	12.243597	-0.074461	4.818357
373.118183	7999.953386	12.248602	-0.074470	4.818342
373.946111	7999.897273	12.253607	-0.074624	4.818322
373.879559	7999.905833	12.258611	-0.074612	4.818325
373.563903	7999.917349	12.263616	-0.074553	4.818329
373.503597	7999.975368	12.268621	-0.074542	4.818347
373.717598	7999.880542	12.273626	-0.074582	4.818318
374.017830	7999.849907	12.278631	-0.074638	4.818308
374.080684	7999.854952	12.283635	-0.074649	4.818309
373.998421	7999.808673	12.288640	-0.074634	4.818295
373.527254	7999.969378	12.293645	-0.074546	4.818345
373.575611	7999.864973	12.298650	-0.074555	4.818314
373.246426	7999.999220	12.303655	-0.074494	4.818355
373.391677	7999.936038	12.308659	-0.074521	4.818336
373.595786	7999.883100	12.313664	-0.074559	4.818319
373.345453	7999.996346	12.318669	-0.074512	4.818354
373.021798	7999.987795	12.323674	-0.074452	4.818353
373.191811	8000.013189	12.328679	-0.074484	4.818359
373.286796	7999.985049	12.333683	-0.074501	4.818351
373.295773	7999.918985	12.338688	-0.074503	4.818331
373.321188	7999.984459	12.343693	-0.074508	4.818350
373.111067	7999.971130	12.348698	-0.074469	4.818347
373.137635	7999.976738	12.353703	-0.074474	4.818349
373.215002	7999.929452	12.358707	-0.074488	4.818334
373.122056	7999.956567	12.363712	-0.074471	4.818343
372.838382	8000.000030	12.368717	-0.074418	4.818357
372.706759	7999.984604	12.373722	-0.074393	4.818353
373.568591	7999.942602	12.378727	-0.074554	4.818337
373.113026	7999.994261	12.383731	-0.074469	4.818354
373.564157	7999.979309	12.388736	-0.074553	4.818348
373.321674	7999.990758	12.393741	-0.074508	4.818352
373.260085	7999.943707	12.398746	-0.074496	4.818339
373.195436	7999.984858	12.403751	-0.074484	4.818351
373.721502	7999.915235	12.408755	-0.074582	4.818328
373.392871	7999.973852	12.413760	-0.074521	4.818347
373.258201	8000.020366	12.418765	-0.074496	4.818361
373.649823	7999.926876	12.423770	-0.074569	4.818332
373.547561	7999.943360	12.428775	-0.074550	4.818337
373.567519	7999.950981	12.433779	-0.074553	4.818339
373.767358	7999.897986	12.438784	-0.074591	4.818323
373.920390	7999.969377	12.443789	-0.074619	4.818344
373.805349	7999.932112	12.448794	-0.074598	4.818333
373.745083	7999.971222	12.453799	-0.074586	4.818345
373.881143	7999.869045	12.458803	-0.074612	4.818314
374.064760	7999.839995	12.463808	-0.074646	4.818305
374.367555	7999.870326	12.468813	-0.074702	4.818312
374.183795	7999.780661	12.473818	-0.074668	4.818286
374.070495	7999.882091	12.478823	-0.074647	4.818317
374.192820	7999.834358	12.483827	-0.074670	4.818302
374.050744	7999.871318	12.488832	-0.074643	4.818314
373.860881	7999.908687	12.493837	-0.074608	4.818326
373.864867	7999.808938	12.498842	-0.074609	4.818296
374.152466	7999.809649	12.503847	-0.074662	4.818295
374.200000	7999.842854	12.508851	-0.074671	4.818305
374.245588	7999.810898	12.513856	-0.074679	4.818295
374.485361	7999.860343	12.518861	-0.074724	4.818309
374.449684	7999.850408	12.523866	-0.074717	4.818306
374.686536	7999.806315	12.528871	-0.074761	4.818292
374.348808	7999.829090	12.533875	-0.074699	4.818300
374.039012	7999.887959	12.538880	-0.074641	4.818319
374.142705	7999.924019	12.543885	-0.074660	4.818329
374.199362	7999.820776	12.548890	-0.074671	4.818298
374.401465	7999.877068	12.553895	-0.074708	4.818314
374.150992	7999.903117	12.558899	-0.074662	4.818323
373.801408	7999.929935	12.563904	-0.074597	4.818332
374.033778	7999.968775	12.568909	-0.074640	4.818343
374.184175	7999.902509	12.573914	-0.074668	4.818323
374.178648	7999.870917	12.578919	-0.074667	4.818313
374.149739	7999.843214	12.583923	-0.074661	4.818305
374.420890	7999.842654	12.588928	-0.074712	4.818304
374.611237	7999.836806	12.593933	-0.074747	4.818301
374.118501	7999.857499	12.598938	-0.074655	4.818310
374.329105	7999.835114	12.603943	-0.074695	4.818302
374.431920	7999.882719	12.608947	-0.074714	4.818316
374.254614	7999.835162	12.613952	-0.074681	4.818302
374.408056	7999.871891	12.618957	-0.074709	4.818313
374.194388	7999.861665	12.623962	-0.074670	4.818310
374.142102	7999.866214	12.628967	-0.074660	4.818312
374.134583	7999.865062	12.633971	-0.074658	4.818312
374.095441	7999.812008	12.638976	-0.074651	4.818296
374.266634	7999.874188	12.643981	-0.074683	4.818314
374.096991	7999.838290	12.648986	-0.074651	4.818304
374.400035	7999.842361	12.653991	-0.074708	4.818304
374.302537	7999.852606	12.658995	-0.074690	4.818307
374.124938	7999.836561	12.664000	-0.074656	4.818303
374.098651	7999.905543	12.669005	-0.074652	4.818324
374.410908	7999.897132	12.674010	-0.074710	4.818320
374.467079	7999.865318	12.679015	-0.074720	4.818310
374.614240	7999.758037	12.684019	-0.074747	4.818278
374.412526	7999.820460	12.689024	-0.074710	4.818297
374.353840	7999.872198	12.694029	-0.074699	4.818313
373.722161	7999.888923	12.699034	-0.074581	4.818320
373.908611	7999.918741	12.704039	-0.074616	4.818329
374.181763	7999.900349	12.709043	-0.074667	4.818322
374.154153	7999.883168	12.714048	-0.074662	4.818317
374.457511	7999.827362	12.719053	-0.074718	4.818299
374.403701	7999.870761	12.724058	-0.074708	4.818312
373.861240	7999.973778	12.729063	-0.074607	4.818345
373.741433	7999.973218	12.734067	-0.074585	4.818345
373.841077	7999.953545	12.739072	-0.074604	4.818339
373.911510	7999.956591	12.744077	-0.074617	4.818340
373.993166	7999.896756	12.749082	-0.074632	4.818322
374.089647	7999.927467	12.754087	-0.074650	4.818330
373.790470	7999.953912	12.759091	-0.074594	4.818339
373.741464	7999.972162	12.764096	-0.074585	4.818345
374.000980	7999.994558	12.769101	-0.074633	4.818351
374.175523	7999.923364	12.774106	-0.074666	4.818329
374.338184	7999.930802	12.779111	-0.074696	4.818330
373.888012	7999.968874	12.784115	-0.074612	4.818344
373.850040	7999.903229	12.789120	-0.074605	4.818324
374.107446	7999.922445	12.794125	-0.074653	4.818329
374.143978	7999.902975	12.799130	-0.074660	4.818323
373.879436	7999.914127	12.804135	-0.074610	4.818327
373.761891	8000.000792	12.809139	-0.074589	4.818354
373.796748	8000.010714	12.814144	-0.074595	4.818356
374.407727	7999.940133	12.819149	-0.074709	4.818333
373.900575	7999.962732	12.824154	-0.074614	4.818342
374.550128	7999.866404	12.829159	-0.074735	4.818310
374.086275	7999.921102	12.834163	-0.074649	4.818329
373.827964	7999.926035	12.839168	-0.074601	4.818331
373.752580	7999.995407	12.844173	-0.074587	4.818352
373.483714	7999.984440	12.849178	-0.074537	4.818350
373.544904	8000.008373	12.854183	-0.074548	4.818357
373.823513	7999.995307	12.859187	-0.074600	4.818352
373.893616	7999.935316	12.864192	-0.074613	4.818334
373.768758	8000.030288	12.869197	-0.074590	4.818362
373.845525	7999.945173	12.874202	-0.074604	4.818337
373.978162	7999.967966	12.879207	-0.074629	4.818343
374.052100	7999.964756	12.884211	-0.074642	4.818342
373.750174	7999.953344	12.889216	-0.074586	4.818339
373.688618	8000.016599	12.894221	-0.074575	4.818359
373.804670	7999.949872	12.899226	-0.074596	4.818338
373.515458	8000.011119	12.904231	-0.074542	4.818358
373.240006	8000.063096	12.909235	-0.074491	4.818374
373.251206	8000.057993	12.914240	-0.074493	4.818373
373.358491	8000.070989	12.919245	-0.074513	4.818376
373.903672	7999.981663	12.924250	-0.074615	4.818347
374.353208	7999.943580	12.929255	-0.074698	4.818334
374.274745	8000.024468	12.934259	-0.074684	4.818359
373.839828	7999.977651	12.939264	-0.074603	4.818346
373.942093	8000.025248	12.944269	-0.074622	4.818360
374.006578	7999.953626	12.949274	-0.074634	4.818339
373.774096	7999.936844	12.954279	-0.074590	4.818334
373.726847	7999.999241	12.959283	-0.074582	4.818353
373.599766	8000.011189	12.964288	-0.074558	4.818357
373.658550	8000.041393	12.969293	-0.074569	4.818366
373.120275	8000.056222	12.974298	-0.074469	4.818373
373.235181	8000.092432	12.979303	-0.074490	4.818383
373.405231	8000.062149	12.984307	-0.074522	4.818373
373.336550	8000.020254	12.989312	-0.074509	4.818361
373.758502	8000.018569	12.994317	-0.074587	4.818359
373.578957	7999.997246	12.999322	-0.074554	4.818353
373.537093	8000.040805	13.004327	-0.074546	4.818366
374.197971	7999.995056	13.009331	-0.074669	4.818350
373.709989	7999.989548	13.014336	-0.074578	4.818350
373.884187	8000.039163	13.019341	-0.074611	4.818364
373.699525	8000.005164	13.024346	-0.074576	4.818355
373.958377	7999.985529	13.029351	-0.074625	4.818348
373.809530	8000.010842	13.034355	-0.074597	4.818356
373.492840	8000.055961	13.039360	-0.074538	4.818371
373.603188	8000.039584	13.044365	-0.074558	4.818366
373.110901	8000.073940	13.049370	-0.074467	4.818378
373.499705	8000.044495	13.054375	-0.074539	4.818368
373.892789	8000.004602	13.059379	-0.074612	4.818354
373.909249	7999.963851	13.064384	-0.074615	4.818342
374.440746	7999.966790	13.069389	-0.074714	4.818341
373.772072	8000.014533	13.074394	-0.074590	4.818358
373.535588	8000.033416	13.079399	-0.074546	4.818364
374.210045	7999.947929	13.084403	-0.074671	4.818336
374.222773	7999.895571	13.089408	-0.074674	4.818320
374.512251	7999.905763	13.094413	-0.074727	4.818322
374.236412	7999.940926	13.099418	-0.074676	4.818334
374.141261	7999.954354	13.104423	-0.074658	4.818338
374.230192	7999.956599	13.109427	-0.074675	4.818339
373.936858	7999.997829	13.114432	-0.074620	4.818352
374.107155	8000.016926	13.119437	-0.074652	4.818357
373.645176	8000.014919	13.124442	-0.074566	4.818358
373.728990	7999.989781	13.129447	-0.074582	4.818350
373.679011	8000.016422	13.134451	-0.074572	4.818359
373.857840	7999.970499	13.139456	-0.074606	4.818344
373.844550	8000.023897	13.144461	-0.074603	4.818360
374.096161	7999.962143	13.149466	-0.074650	4.818341
374.183418	7999.941253	13.154471	-0.074666	4.818334
374.061552	7999.997395	13.159475	-0.074643	4.818351
373.468789	8000.048259	13.164480	-0.074533	4.818369
373.502784	8000.087585	13.169485	-0.074539	4.818380
373.975276	8000.002536	13.174490	-0.074627	4.818353
373.831282	8000.063633	13.179495	-0.074601	4.818372
373.689425	8000.075383	13.184499	-0.074574	4.818376
373.618129	8000.054463	13.189504	-0.074561	4.818370
373.813151	8000.045527	13.194509	-0.074597	4.818367
373.834152	7999.979624	13.199514	-0.074601	4.818347
373.394689	8000.049357	13.204519	-0.074519	4.818369
373.556180	8000.069385	13.209523	-0.074549	4.818375
373.542868	8000.069205	13.214528	-0.074547	4.818375
373.608577	8000.074289	13.219533	-0.074559	4.818376
373.521506	8000.024793	13.224538	-0.074543	4.818362
373.932605	7999.972536	13.229543	-0.074619	4.818344
374.062005	7999.946960	13.234547	-0.074643	4.818336
374.159379	7999.932509	13.239552	-0.074661	4.818332
374.137332	7999.995245	13.244557	-0.074657	4.818350
373.801204	8000.054810	13.249562	-0.074595	4.818369
373.689219	8000.072214	13.254567	-0.074574	4.818375
373.925443	8000.028113	13.259571	-0.074618	4.818361
373.455663	8000.061720	13.264576	-0.074530	4.818373
374.011286	8000.035568	13.269581	-0.074634	4.818363
373.729442	8000.020223	13.274586	-0.074581	4.818359
373.712897	8000.037859	13.279591	-0.074578	4.818365
373.993619	8000.012215	13.284595	-0.074630	4.818356
374.359048	7999.939384	13.289600	-0.074698	4.818333
374.076866	8000.028040	13.294605	-0.074646	4.818360
374.460605	7999.926040	13.299610	-0.074717	4.818329
374.628940	7999.929352	13.304615	-0.074749	4.818329
374.234211	8000.024899	13.309619	-0.074675	4.818359
374.227417	7999.996442	13.314624	-0.074674	4.818350
374.746843	7999.967703	13.319629	-0.074771	4.818340
374.015975	8000.052429	13.324634	-0.074635	4.818368
374.593857	7999.946735	13.329639	-0.074742	4.818334
374.720010	7999.995705	13.334643	-0.074766	4.818348
374.302408	7999.972231	13.339648	-0.074688	4.818343
373.738371	8000.057099	13.344653	-0.074583	4.818370
373.777913	8000.000899	13.349658	-0.074590	4.818354
374.287582	7999.967827	13.354663	-0.074685	4.818342
374.383615	7999.954408	13.359667	-0.074703	4.818337
374.348026	7999.926615	13.364672	-0.074696	4.818329
374.392959	7999.947178	13.369677	-0.074705	4.818335
374.566295	7999.921142	13.374682	-0.074737	4.818327
374.812980	7999.904496	13.379687	-0.074783	4.818321
374.536931	7999.977475	13.384691	-0.074731	4.818344
374.473494	7999.882071	13.389696	-0.074719	4.818315
374.568270	7999.935872	13.394701	-0.074737	4.818331
374.586693	7999.925613	13.399706	-0.074740	4.818328
374.973618	7999.901397	13.404711	-0.074813	4.818319
375.092907	7999.883039	13.409715	-0.074835	4.818313
374.661910	7999.906660	13.414720	-0.074754	4.818322
374.555292	7999.977715	13.419725	-0.074735	4.818344
374.060337	8000.010983	13.424730	-0.074642	4.818355
374.090380	7999.996678	13.429735	-0.074648	4.818351
374.104220	8000.015773	13.434739	-0.074651	4.818357
374.417233	8000.001069	13.439744	-0.074709	4.818351
373.892516	8000.057049	13.444749	-0.074611	4.818370
374.079727	7999.996531	13.449754	-0.074646	4.818351
374.225712	7999.948065	13.454759	-0.074673	4.818336
374.199317	8000.018097	13.459763	-0.074668	4.818357
373.757274	8000.009003	13.464768	-0.074586	4.818356
373.587999	8000.069761	13.469773	-0.074554	4.818375
374.092932	8000.005108	13.474778	-0.074648	4.818354
374.059263	7999.982593	13.479783	-0.074642	4.818347
374.488289	7999.995712	13.484787	-0.074722	4.818349
373.979013	8000.041394	13.489792	-0.074627	4.818365
374.241178	8000.040714	13.494797	-0.074676	4.818364
374.212738	8000.021421	13.499802	-0.074671	4.818358
374.915098	7999.935259	13.504807	-0.074801	4.818329
375.066701	7999.950954	13.509811	-0.074830	4.818334
374.751716	7999.980337	13.514816	-0.074771	4.818344
374.853977	7999.976457	13.519821	-0.074790	4.818342
374.677065	7999.928904	13.524826	-0.074757	4.818329
374.235830	7999.980753	13.529831	-0.074675	4.818346
374.385578	8000.002726	13.534835	-0.074703	4.818352
374.408118	7999.953651	13.539840	-0.074707	4.818337
375.008269	7999.922846	13.544845	-0.074819	4.818325
375.204163	7999.874001	13.549850	-0.074855	4.818310
375.048005	7999.862446	13.554855	-0.074826	4.818307
375.232941	7999.920611	13.559859	-0.074860	4.818324
374.852055	7999.878720	13.564864	-0.074789	4.818313
374.937030	7999.933440	13.569869	-0.074805	4.818329
374.709458	7999.973453	13.574874	-0.074763	4.818342
374.527045	7999.947888	13.579879	-0.074729	4.818335
375.036251	7999.920063	13.584883	-0.074824	4.818325
374.869939	7999.845337	13.589888	-0.074793	4.818303
374.811301	7999.883419	13.594893	-0.074782	4.818315
374.599136	7999.982471	13.599898	-0.074742	4.818345
374.973761	7999.857235	13.604903	-0.074812	4.818306
374.738851	7999.965437	13.609907	-0.074768	4.818339
374.449942	7999.969957	13.614912	-0.074714	4.818342
374.398794	8000.045959	13.619917	-0.074705	4.818364
374.388484	8000.003797	13.624922	-0.074703	4.818352
374.750493	7999.935123	13.629927	-0.074770	4.818330
374.544319	8000.014294	13.634931	-0.074732	4.818354
374.459759	7999.973235	13.639936	-0.074716	4.818343
374.332817	7999.997792	13.644941	-0.074693	4.818350
374.586375	8000.008553	13.649946	-0.074740	4.818353
374.095753	8000.091255	13.654951	-0.074648	4.818379
374.719692	8000.030304	13.659955	-0.074765	4.818359
374.612078	7999.974227	13.664960	-0.074745	4.818342
374.529245	8000.016186	13.669965	-0.074729	4.818355
374.215651	8000.022475	13.674970	-0.074671	4.818358
374.012959	8000.072278	13.679975	-0.074633	4.818374
374.149694	8000.039446	13.684979	-0.074658	4.818364
374.244960	7999.960883	13.689984	-0.074676	4.818340
374.590316	7999.964474	13.694989	-0.074740	4.818339
374.243394	8000.009186	13.699994	-0.074676	4.818354
374.608157	7999.932144	13.704999	-0.074744	4.818330
374.185702	8000.045178	13.710003	-0.074665	4.818365
374.127455	7999.993968	13.715008	-0.074654	4.818350
374.483671	7999.993501	13.720013	-0.074720	4.818349
375.155046	7999.942643	13.725018	-0.074845	4.818331
375.352467	7999.824481	13.730023	-0.074882	4.818295
375.106186	7999.910467	13.735027	-0.074836	4.818321
374.903182	7999.937153	13.740032	-0.074798	4.818330
374.780637	7999.962820	13.745037	-0.074776	4.818338
374.942747	7999.948189	13.750042	-0.074806	4.818333
374.846013	7999.912219	13.755047	-0.074788	4.818323
374.733944	8000.006313	13.760051	-0.074767	4.818351
374.286134	8000.012899	13.765056	-0.074684	4.818355
374.691666	7999.979478	13.770061	-0.074759	4.818344
374.579099	8000.013683	13.775066	-0.074738	4.818354
374.585719	7999.954940	13.780071	-0.074739	4.818337
374.797118	7999.959882	13.785075	-0.074779	4.818337
375.071301	7999.916291	13.790080	-0.074830	4.818323
375.277294	7999.886491	13.795085	-0.074868	4.818314
375.330299	7999.913467	13.800090	-0.074878	4.818321
375.314726	7999.908004	13.805095	-0.074875	4.818320
375.089527	8000.003729	13.810099	-0.074833	4.818349
375.207951	7999.925477	13.815104	-0.074855	4.818325
375.140455	7999.926670	13.820109	-0.074842	4.818326
375.369738	7999.852009	13.825114	-0.074885	4.818303
375.078426	7999.854395	13.830119	-0.074831	4.818305
375.050656	7999.905499	13.835123	-0.074826	4.818320
374.911142	7999.914128	13.840128	-0.074800	4.818323
374.759769	8000.002441	13.845133	-0.074772	4.818350
375.101618	7999.945052	13.850138	-0.074835	4.818332
375.085275	7999.890201	13.855143	-0.074832	4.818315
374.954700	8000.001907	13.860147	-0.074808	4.818349
374.962552	7999.957887	13.865152	-0.074809	4.818336
375.329875	7999.875627	13.870157	-0.074878	4.818310
375.373849	7999.893026	13.875162	-0.074886	4.818315
375.046053	7999.907529	13.880167	-0.074825	4.818321
375.268285	7999.960943	13.885171	-0.074866	4.818336
374.870533	7999.939836	13.890176	-0.074792	4.818331
375.260121	7999.933516	13.895181	-0.074865	4.818328
375.179230	7999.921922	13.900186	-0.074849	4.818325
374.993893	7999.916278	13.905191	-0.074815	4.818324
375.044763	7999.976843	13.910195	-0.074824	4.818341
375.484369	7999.871392	13.915200	-0.074906	4.818308
374.908914	7999.962408	13.920205	-0.074799	4.818338
375.199874	7999.975774	13.925210	-0.074853	4.818340
374.903547	7999.959182	13.930215	-0.074798	4.818337
375.213619	8000.028486	13.935219	-0.074856	4.818356
374.611943	8000.028800	13.940224	-0.074744	4.818359
374.955593	7999.980890	13.945229	-0.074808	4.818343
374.893097	7999.983201	13.950234	-0.074796	4.818344
374.678494	7999.985568	13.955239	-0.074756	4.818345
374.988766	8000.012850	13.960243	-0.074814	4.818352
374.890651	7999.960052	13.965248	-0.074796	4.818337
375.258775	7999.903017	13.970253	-0.074864	4.818319
375.376764	7999.926664	13.975258	-0.074886	4.818325
375.248058	7999.931236	13.980263	-0.074862	4.818327
375.337326	7999.941891	13.985267	-0.074879	4.818330
375.482829	7999.896570	13.990272	-0.074906	4.818316
375.350976	7999.969387	13.995277	-0.074881	4.818338
375.456040	7999.965546	14.000282	-0.074901	4.818336
375.276561	7999.925311	14.005287	-0.074867	4.818325
375.305314	7999.995035	14.010291	-0.074873	4.818346
375.491592	7999.909290	14.015296	-0.074907	4.818320
375.487034	7999.922885	14.020301	-0.074906	4.818324
375.109432	7999.968235	14.025306	-0.074836	4.818339
375.540537	7999.836404	14.030311	-0.074916	4.818298
375.874456	7999.889220	14.035315	-0.074978	4.818312
375.645775	7999.849374	14.040320	-0.074936	4.818301
376.076273	7999.823644	14.045325	-0.075016	4.818292
376.186369	7999.841933	14.050330	-0.075036	4.818297
375.660500	7999.852720	14.055335	-0.074939	4.818302
375.985480	7999.884405	14.060339	-0.074999	4.818310
376.031138	7999.892372	14.065344	-0.075008	4.818312
375.657187	7999.979794	14.070349	-0.074938	4.818340
375.454798	7999.958160	14.075354	-0.074900	4.818334
374.922802	8000.020344	14.080359	-0.074801	4.818355
375.185790	8000.016525	14.085363	-0.074850	4.818353
375.175649	7999.918684	14.090368	-0.074848	4.818324
375.111455	7999.927275	14.095373	-0.074836	4.818326
375.235098	7999.944695	14.100378	-0.074859	4.818331
374.916846	7999.971933	14.105383	-0.074800	4.818340
374.670676	8000.048466	14.110387	-0.074754	4.818364
374.790046	7999.954468	14.115392	-0.074776	4.818336
374.700286	7999.999485	14.120397	-0.074760	4.818349
374.565632	8000.041798	14.125402	-0.074735	4.818363
374.659251	8000.022044	14.130407	-0.074752	4.818356
374.695290	8000.023578	14.135411	-0.074759	4.818357
374.715199	8000.015440	14.140416	-0.074762	4.818354
374.937992	7999.991119	14.145421	-0.074804	4.818346
374.581080	8000.068264	14.150426	-0.074737	4.818370
374.702567	7999.953284	14.155431	-0.074760	4.818336
374.554102	8000.048990	14.160435	-0.074732	4.818365
375.032093	7999.987128	14.165440	-0.074821	4.818344
374.690420	8000.059225	14.170445	-0.074758	4.818367
375.034753	7999.988212	14.175450	-0.074822	4.818345
374.852016	7999.965793	14.180455	-0.074788	4.818339
375.272286	8000.002960	14.185459	-0.074866	4.818348
374.717782	7999.983948	14.190464	-0.074763	4.818345
374.990239	7999.931929	14.195469	-0.074813	4.818328
375.400897	7999.945854	14.200474	-0.074890	4.818331
375.631017	7999.849142	14.205479	-0.074933	4.818301
375.218066	7999.986467	14.210483	-0.074856	4.818344
375.147230	7999.953997	14.215488	-0.074843	4.818334
374.918356	7999.991891	14.220493	-0.074800	4.818346
375.308459	7999.920443	14.225498	-0.074873	4.818324
375.506405	7999.884232	14.230503	-0.074909	4.818312
375.667884	7999.952589	14.235507	-0.074940	4.818332
375.375684	7999.939204	14.240512	-0.074885	4.818329
375.784771	7999.833342	14.245517	-0.074961	4.818296
375.753004	7999.888594	14.250522	-0.074955	4.818312
375.588333	7999.839103	14.255527	-0.074925	4.818298
375.400360	7999.935329	14.260531	-0.074890	4.818328
375.350535	7999.985086	14.265536	-0.074880	4.818343
375.089034	8000.010985	14.270541	-0.074832	4.818351
375.420764	7999.970270	14.275546	-0.074893	4.818338
375.442379	7999.841338	14.280551	-0.074897	4.818300
375.601811	7999.910718	14.285555	-0.074927	4.818320
375.496885	7999.932419	14.290560	-0.074908	4.818326
375.569236	7999.911328	14.295565	-0.074921	4.818320
375.547359	7999.933095	14.300570	-0.074917	4.818326
375.603936	7999.920198	14.305575	-0.074927	4.818322
375.739438	7999.932525	14.310579	-0.074953	4.818325
376.070150	7999.883391	14.315584	-0.075014	4.818310
376.071230	7999.798307	14.320589	-0.075014	4.818284
375.995624	7999.781530	14.325594	-0.075000	4.818280
375.925988	7999.787947	14.330599	-0.074987	4.818282
376.087545	7999.781714	14.335603	-0.075017	4.818279
375.658036	7999.844225	14.340608	-0.074937	4.818300
375.657498	7999.869431	14.345613	-0.074937	4.818307
375.801669	7999.837750	14.350618	-0.074964	4.818297
375.774411	7999.810067	14.355623	-0.074959	4.818289
375.644219	7999.879755	14.360627	-0.074935	4.818310
375.612904	7999.858322	14.365632	-0.074929	4.818304
375.885060	7999.839918	14.370637	-0.074980	4.818297
375.479699	7999.934272	14.375642	-0.074904	4.818327
375.482259	7999.935356	14.380647	-0.074905	4.818327
375.914983	7999.894948	14.385651	-0.074985	4.818314
375.755306	7999.878091	14.390656	-0.074955	4.818309
375.398852	7999.854387	14.395661	-0.074889	4.818304
375.680124	7999.888635	14.400666	-0.074941	4.818313
375.693950	7999.859404	14.405671	-0.074944	4.818304
375.856164	7999.897304	14.410675	-0.074974	4.818315
375.580734	7999.868385	14.415680	-0.074923	4.818307
375.501800	7999.911447	14.420685	-0.074908	4.818320
375.331778	7999.983751	14.425690	-0.074876	4.818342
375.422737	7999.863106	14.430695	-0.074893	4.818306
375.555464	7999.942633	14.435699	-0.074918	4.818329
375.147151	7999.929787	14.440704	-0.074842	4.818327
375.212542	7999.921210	14.445709	-0.074854	4.818324
375.561692	7999.925904	14.450714	-0.074919	4.818324
375.635442	7999.834443	14.455719	-0.074933	4.818297
375.780914	7999.895231	14.460723	-0.074960	4.818314
375.731006	7999.856738	14.465728	-0.074951	4.818303
375.740892	7999.545900	14.470733	-0.074952	4.818211

375.629337	7996.326853	14.475738	-0.074929	4.817254
375.452853	7990.744963	14.480743	-0.074893	4.815596
375.655381	7984.115168	14.485747	-0.074926	4.813623
375.531719	7976.832330	14.490752	-0.074898	4.811457
375.247311	7969.158608	14.495757	-0.074840	4.809174
375.395792	7961.465762	14.500762	-0.074863	4.806882
375.251889	7953.431428	14.505767	-0.074831	4.804489
375.129494	7945.629675	14.510771	-0.074803	4.802163
375.216547	7937.538090	14.515776	-0.074814	4.799750
375.254635	7929.558758	14.520781	-0.074816	4.797369
375.277743	7921.577982	14.525786	-0.074815	4.794986
375.032638	7913.610667	14.530791	-0.074764	4.792607
375.371054	7905.581857	14.535795	-0.074822	4.790206
375.258336	7897.567662	14.540800	-0.074796	4.787811
374.865004	7889.554507	14.545805	-0.074717	4.785415
375.100434	7881.585547	14.550810	-0.074756	4.783029
375.073745	7873.528119	14.555815	-0.074746	4.780616
375.209610	7865.570197	14.560819	-0.074766	4.778232
374.925945	7857.601597	14.565824	-0.074708	4.775844
375.013235	7849.547068	14.570829	-0.074719	4.773428
374.604768	7841.598972	14.575834	-0.074637	4.771045
374.781074	7833.471292	14.580839	-0.074665	4.768604
374.869869	7825.555781	14.585843	-0.074676	4.766226
374.951767	7817.499759	14.590848	-0.074686	4.763805
374.906925	7809.576456	14.595853	-0.074673	4.761423
374.869836	7801.526472	14.600858	-0.074661	4.759002
374.945335	7793.569711	14.605863	-0.074669	4.756607
375.098289	7785.504593	14.610867	-0.074693	4.754178
374.603811	7777.602019	14.615872	-0.074595	4.751798
374.647834	7769.491419	14.620877	-0.074598	4.749354
374.704799	7761.508247	14.625882	-0.074604	4.746946
374.444279	7753.468810	14.630887	-0.074550	4.744521
373.681708	7745.650157	14.635891	-0.074403	4.742162
373.561875	7737.588107	14.640896	-0.074375	4.739727
373.661536	7729.494586	14.645901	-0.074389	4.737281
373.546979	7721.526623	14.650906	-0.074362	4.734872
373.940103	7713.458765	14.655911	-0.074430	4.732431
373.753913	7705.485116	14.660915	-0.074390	4.730018
373.810813	7697.453198	14.665920	-0.074395	4.727585
373.462616	7689.501297	14.670925	-0.074325	4.725177
373.426682	7681.585239	14.675930	-0.074314	4.722777
373.252618	7673.530445	14.680935	-0.074276	4.720335
373.046880	7665.603156	14.685939	-0.074232	4.717929
372.810746	7657.602738	14.690944	-0.074183	4.715501
372.884879	7649.519710	14.695949	-0.074192	4.713045
373.258273	7641.475161	14.700954	-0.074256	4.710600
373.437563	7633.408107	14.705959	-0.074284	4.708147
373.156401	7625.465271	14.710963	-0.074227	4.705730
372.632007	7617.524590	14.715968	-0.074124	4.703314
373.300896	7609.463817	14.720973	-0.074243	4.700858
373.293206	7601.517121	14.725978	-0.074236	4.698437
372.997813	7593.516168	14.730983	-0.074176	4.695998
372.990442	7585.501031	14.735987	-0.074169	4.693553
373.047598	7577.500516	14.740992	-0.074175	4.691111
372.551420	7569.492265	14.745997	-0.074077	4.688666
373.013203	7561.456353	14.751002	-0.074158	4.686211
373.087716	7553.452059	14.756007	-0.074167	4.683764
373.039435	7545.545522	14.761011	-0.074153	4.681346
373.066973	7537.466799	14.766016	-0.074152	4.678874
372.887407	7529.546884	14.771021	-0.074114	4.676450
372.683919	7521.523100	14.776026	-0.074071	4.673992
372.617008	7513.452928	14.781031	-0.074053	4.671519
372.574547	7505.448173	14.786035	-0.074040	4.669064
372.665797	7497.460030	14.791040	-0.074052	4.666614
372.802413	7489.384592	14.796045	-0.074072	4.664135
372.633268	7481.533666	14.801050	-0.074035	4.661724
372.541579	7473.431976	14.806055	-0.074013	4.659234
372.012853	7465.568958	14.811059	-0.073909	4.656817
372.263304	7457.387803	14.816064	-0.073950	4.654300
372.509144	7449.468568	14.821069	-0.073991	4.651863
372.477492	7441.377059	14.826074	-0.073980	4.649371
372.210205	7433.429776	14.831079	-0.073925	4.646922
372.308539	7425.371192	14.836083	-0.073938	4.644438
372.600098	7417.451351	14.841088	-0.073987	4.641996
372.460817	7409.406485	14.846093	-0.073956	4.639513
372.346189	7401.533768	14.851098	-0.073929	4.637082
372.234429	7393.410621	14.856103	-0.073903	4.634573
372.386631	7385.485424	14.861107	-0.073926	4.632123
371.751479	7377.437487	14.866112	-0.073803	4.629634
371.642033	7369.468820	14.871117	-0.073777	4.627168
371.966936	7361.378556	14.876122	-0.073832	4.624664
371.785035	7353.429715	14.881127	-0.073793	4.622202
371.795899	7345.429332	14.886131	-0.073790	4.619722
371.773962	7337.436354	14.891136	-0.073781	4.617243
371.552210	7329.436174	14.896141	-0.073734	4.614761
372.014067	7321.379019	14.901146	-0.073815	4.612260
371.619769	7313.334829	14.906151	-0.073736	4.609762
371.420454	7305.451182	14.911155	-0.073694	4.607311
371.461466	7297.437444	14.916160	-0.073697	4.604820
371.390280	7289.443509	14.921165	-0.073678	4.602333
371.509197	7281.417079	14.926170	-0.073695	4.599835
371.501206	7273.399508	14.931175	-0.073688	4.597338
371.517312	7265.383195	14.936179	-0.073686	4.594840
371.316259	7257.397259	14.941184	-0.073643	4.592350
371.225425	7249.388204	14.946189	-0.073621	4.589851
371.231046	7241.366077	14.951194	-0.073617	4.587347
370.973977	7233.358681	14.956199	-0.073564	4.584846
370.651714	7225.474979	14.961203	-0.073499	4.582382
370.238832	7217.388497	14.966208	-0.073417	4.579853
370.364677	7209.411328	14.971213	-0.073435	4.577358
370.585042	7201.353144	14.976218	-0.073471	4.574837
370.164475	7193.403908	14.981223	-0.073387	4.572347
370.466586	7185.291251	14.986227	-0.073438	4.569805
370.692520	7177.325861	14.991232	-0.073475	4.567309
370.469440	7169.308049	14.996237	-0.073428	4.564793
370.846712	7161.398025	15.001242	-0.073493	4.562312
370.901472	7153.303608	15.006247	-0.073498	4.559770
370.609118	7145.429797	15.011251	-0.073439	4.557295
370.321024	7137.327032	15.016256	-0.073380	4.554748
370.508296	7129.337410	15.021261	-0.073409	4.552235
370.698725	7121.306489	15.026266	-0.073439	4.549708
370.683210	7113.297480	15.031271	-0.073431	4.547186
370.832890	7105.269774	15.036275	-0.073454	4.544657
370.636754	7097.420689	15.041280	-0.073412	4.542182
370.073907	7089.358460	15.046285	-0.073302	4.539638
370.011407	7081.405355	15.051290	-0.073285	4.537128
370.183613	7073.206471	15.056295	-0.073312	4.534539
370.126962	7065.341303	15.061299	-0.073296	4.532054
369.904189	7057.303335	15.066304	-0.073250	4.529513
370.039345	7049.315877	15.071309	-0.073270	4.526987
370.128362	7041.254386	15.076314	-0.073281	4.524436
369.774455	7033.331947	15.081319	-0.073210	4.521926
369.368935	7025.350547	15.086323	-0.073129	4.519396
369.287812	7017.396016	15.091328	-0.073109	4.516874
369.487490	7009.259977	15.096333	-0.073141	4.514294
369.627168	7001.327818	15.101338	-0.073162	4.511777
369.760977	6993.231047	15.106343	-0.073181	4.509206
369.701520	6985.276565	15.111347	-0.073165	4.506679
369.346620	6977.233716	15.116352	-0.073094	4.504121
369.559169	6969.252814	15.121357	-0.073128	4.501583
369.780513	6961.229163	15.126362	-0.073164	4.499030
369.774475	6953.237202	15.131367	-0.073158	4.496485
369.750776	6945.208849	15.136371	-0.073148	4.493927
369.456608	6937.306873	15.141376	-0.073088	4.491406
369.326746	6929.265530	15.146381	-0.073059	4.488840
369.117182	6921.256259	15.151386	-0.073014	4.486283
369.358430	6913.174488	15.156391	-0.073054	4.483703
368.786621	6905.314994	15.161395	-0.072942	4.481189
368.465904	6897.288906	15.166400	-0.072877	4.478622
368.393874	6889.296397	15.171405	-0.072859	4.476065
368.454277	6881.258904	15.176410	-0.072865	4.473492
368.703885	6873.199032	15.181415	-0.072906	4.470912
368.599388	6865.201295	15.186419	-0.072881	4.468348
368.348681	6857.255057	15.191424	-0.072829	4.465799
368.339099	6849.212698	15.196429	-0.072822	4.463219
368.139091	6841.287653	15.201434	-0.072780	4.460674
368.142458	6833.205817	15.206439	-0.072775	4.458078
368.293596	6825.195423	15.211443	-0.072798	4.455504
368.565103	6817.211066	15.216448	-0.072843	4.452938
367.895566	6809.211775	15.221453	-0.072714	4.450361
367.831130	6801.272894	15.226458	-0.072696	4.447804
367.833020	6793.186420	15.231463	-0.072691	4.445199
367.863520	6785.249479	15.236467	-0.072692	4.442641
368.192041	6777.128410	15.241472	-0.072748	4.440024
368.026654	6769.214502	15.246477	-0.072712	4.437469
368.306961	6761.163476	15.251482	-0.072759	4.434871
367.995911	6753.189780	15.256487	-0.072696	4.432293
368.366946	6745.107902	15.261491	-0.072759	4.429682
368.557840	6737.161110	15.266496	-0.072790	4.427113
368.375894	6729.127937	15.271501	-0.072751	4.424512
368.712722	6721.193587	15.276506	-0.072808	4.421944
368.876801	6713.101111	15.281511	-0.072833	4.419323
368.676993	6705.208586	15.286515	-0.072791	4.416763
368.521270	6697.145787	15.291520	-0.072757	4.414147
368.002480	6689.265641	15.296525	-0.072655	4.411586
367.964546	6681.232433	15.301530	-0.072643	4.408976
368.036702	6673.190420	15.306535	-0.072651	4.406363
368.081044	6665.146004	15.311539	-0.072654	4.403747
367.942865	6657.227830	15.316544	-0.072623	4.401170
367.466523	6649.233644	15.321549	-0.072529	4.398565
367.484188	6641.243386	15.326554	-0.072527	4.395962
367.708337	6633.211667	15.331559	-0.072564	4.393345
367.166899	6625.267814	15.336563	-0.072458	4.390751
367.233110	6617.240172	15.341568	-0.072465	4.388132
367.521854	6609.151625	15.346573	-0.072513	4.385492
367.574522	6601.220729	15.351578	-0.072518	4.382901
367.183454	6593.249260	15.356583	-0.072440	4.380293
367.462872	6585.235332	15.361587	-0.072487	4.377673
367.371525	6577.252970	15.366592	-0.072464	4.375059
367.146406	6569.271591	15.371597	-0.072417	4.372444
366.934139	6561.271002	15.376602	-0.072373	4.369820
367.075171	6553.228648	15.381607	-0.072394	4.367184
367.199759	6545.146753	15.386611	-0.072411	4.364533
367.114952	6537.264464	15.391616	-0.072391	4.361945
366.769213	6529.246377	15.396621	-0.072321	4.359308
366.914634	6521.320084	15.401626	-0.072343	4.356704
366.786099	6513.221529	15.406631	-0.072314	4.354039
366.747297	6505.241643	15.411635	-0.072301	4.351413
366.950800	6497.188052	15.416640	-0.072334	4.348762
366.646344	6489.216425	15.421645	-0.072272	4.346133
366.725275	6481.259725	15.426650	-0.072281	4.343510
367.186108	6473.195692	15.431655	-0.072362	4.340854
366.996477	6465.247361	15.436659	-0.072321	4.338228
366.726276	6457.279398	15.441664	-0.072266	4.335594
366.885347	6449.203102	15.446669	-0.072290	4.332926
366.914961	6441.227359	15.451674	-0.072291	4.330289
366.409334	6433.291292	15.456679	-0.072191	4.327658
366.232744	6425.239962	15.461683	-0.072153	4.324991
366.889077	6417.248282	15.466688	-0.072270	4.322348
366.558157	6409.203180	15.471693	-0.072203	4.319679
366.337366	6401.287418	15.476698	-0.072157	4.317051
366.447140	6393.156588	15.481703	-0.072172	4.314353
366.712564	6385.210982	15.486707	-0.072216	4.311716
366.374763	6377.237859	15.491712	-0.072148	4.309063
366.225269	6369.236723	15.496717	-0.072115	4.306401
366.448912	6361.192346	15.501722	-0.072151	4.303726
366.484724	6353.189728	15.506727	-0.072153	4.301062
366.527305	6345.176893	15.511731	-0.072156	4.298392
366.392584	6337.221533	15.516736	-0.072125	4.295739
365.934383	6329.223766	15.521741	-0.072035	4.293067
366.256540	6321.184666	15.526746	-0.072089	4.290386
366.022589	6313.204037	15.531751	-0.072041	4.287719
366.125528	6305.169676	15.536755	-0.072055	4.285034
366.281647	6297.248025	15.541760	-0.072079	4.282387
366.045570	6289.178991	15.546765	-0.072029	4.279684
365.990502	6281.280620	15.551770	-0.072014	4.277039
366.125785	6273.121872	15.556775	-0.072034	4.274306
365.997971	6265.206680	15.561779	-0.072005	4.271651
365.850784	6257.182598	15.566784	-0.071972	4.268958
366.049540	6249.160127	15.571789	-0.072004	4.266267
365.608082	6241.206856	15.576794	-0.071916	4.263591
365.834070	6233.128661	15.581799	-0.071953	4.260878
366.114398	6225.146715	15.586803	-0.072000	4.258196
365.424012	6217.250516	15.591808	-0.071867	4.255532
365.074801	6209.214021	15.596813	-0.071796	4.252822
365.438203	6201.179833	15.601818	-0.071859	4.250118
365.528204	6193.144105	15.606823	-0.071870	4.247410
365.773930	6185.092994	15.611827	-0.071911	4.244696
365.212851	6177.281577	15.616832	-0.071801	4.242053
365.348492	6169.155320	15.621837	-0.071821	4.239309
365.500815	6161.165778	15.626842	-0.071844	4.236610
365.485368	6153.137627	15.631847	-0.071836	4.233894
364.767624	6145.258481	15.636851	-0.071697	4.231219
364.845605	6137.206428	15.641856	-0.071707	4.228493
364.372484	6129.182649	15.646861	-0.071613	4.225768
364.593596	6121.202702	15.651866	-0.071649	4.223064
364.580575	6113.177404	15.656871	-0.071642	4.220340
364.562669	6105.162973	15.661875	-0.071633	4.217619
364.678023	6097.159480	15.666880	-0.071649	4.214900
364.410933	6089.170927	15.671885	-0.071594	4.212181
364.674852	6081.101297	15.676890	-0.071638	4.209438
364.552893	6073.189912	15.681895	-0.071610	4.206743
364.301822	6065.167964	15.686899	-0.071558	4.204008
364.414752	6057.213257	15.691904	-0.071574	4.201297
363.782578	6049.182730	15.696909	-0.071451	4.198550
364.026809	6041.229385	15.701914	-0.071491	4.195838
364.198517	6033.105401	15.706919	-0.071518	4.193065
363.899178	6025.101556	15.711923	-0.071457	4.190326
364.182305	6017.113026	15.716928	-0.071505	4.187597
363.685233	6009.128484	15.721933	-0.071407	4.184859
364.260354	6001.120963	15.726938	-0.071509	4.182123
364.132094	5993.108602	15.731943	-0.071480	4.179376
364.478533	5985.122997	15.736947	-0.071539	4.176641
364.034816	5977.186062	15.741952	-0.071451	4.173913
363.878418	5969.151520	15.746957	-0.071417	4.171152
363.890005	5961.169008	15.751962	-0.071414	4.168409
363.843132	5953.174806	15.756967	-0.071400	4.165660
363.793320	5945.166966	15.761971	-0.071385	4.162904
363.934598	5937.159284	15.766976	-0.071406	4.160149
363.343508	5929.247181	15.771981	-0.071291	4.157416
363.860454	5921.116732	15.776986	-0.071382	4.154619
363.848667	5913.120652	15.781991	-0.071375	4.151861
363.935774	5905.110838	15.786995	-0.071385	4.149097
363.712860	5897.173077	15.792000	-0.071339	4.146352
363.521714	5889.141059	15.797005	-0.071298	4.143573
363.870433	5881.132850	15.802010	-0.071358	4.140807
363.422683	5873.210693	15.807015	-0.071269	4.138059
363.220821	5865.216093	15.812019	-0.071226	4.135288
363.223782	5857.250577	15.817024	-0.071222	4.132527
362.975264	5849.157942	15.822029	-0.071170	4.129717
363.152126	5841.208157	15.827034	-0.071198	4.126960
363.209857	5833.111013	15.832039	-0.071203	4.124149
363.362761	5825.202425	15.837043	-0.071227	4.121402
363.310466	5817.177920	15.842048	-0.071212	4.118611
363.086738	5809.188103	15.847053	-0.071165	4.115827
363.417850	5801.210362	15.852058	-0.071221	4.113054
362.984768	5793.206673	15.857063	-0.071135	4.110259
362.759674	5785.202933	15.862067	-0.071088	4.107464
362.896900	5777.148057	15.867072	-0.071108	4.104656
362.724713	5769.200590	15.872077	-0.071071	4.101878
362.976196	5761.166269	15.877082	-0.071113	4.099074
362.964756	5753.131171	15.882087	-0.071105	4.096264
362.813332	5745.172477	15.887091	-0.071072	4.093477
362.844926	5737.192089	15.892096	-0.071073	4.090683
362.659666	5729.147784	15.897101	-0.071033	4.087862
362.806405	5721.144199	15.902106	-0.071055	4.085058
362.931197	5713.183447	15.907111	-0.071073	4.082266
363.019812	5705.162066	15.912115	-0.071084	4.079451
362.929251	5697.209744	15.917120	-0.071062	4.076656
362.705488	5689.170061	15.922125	-0.071015	4.073826
362.647550	5681.215905	15.927130	-0.070999	4.071026
362.217550	5673.199908	15.932135	-0.070914	4.068197
361.658188	5665.220058	15.937139	-0.070805	4.065377
362.156626	5657.160313	15.942144	-0.070892	4.062543
361.997667	5649.154067	15.947149	-0.070857	4.059716
362.235754	5641.167050	15.952154	-0.070896	4.056900
361.828786	5633.217348	15.957159	-0.070816	4.054084
361.530507	5625.232362	15.962163	-0.070755	4.051257
361.786575	5617.175599	15.967168	-0.070797	4.048410
361.402797	5609.202235	15.972173	-0.070721	4.045581
361.949227	5601.203615	15.977178	-0.070817	4.042755
361.815100	5593.205703	15.982183	-0.070787	4.039917
361.761091	5585.229213	15.987187	-0.070772	4.037086
361.888683	5577.194753	15.992192	-0.070790	4.034236
361.949115	5569.118913	15.997197	-0.070796	4.031367
361.905297	5561.120269	16.002202	-0.070783	4.028522
361.858669	5553.130938	16.007207	-0.070769	4.025679
361.846522	5545.155333	16.012211	-0.070761	4.022839
361.763610	5537.210540	16.017216	-0.070741	4.020007
361.882193	5529.167507	16.022221	-0.070757	4.017141
361.864493	5521.176758	16.027226	-0.070749	4.014289
361.362209	5513.258963	16.032231	-0.070650	4.011453
361.048804	5505.254262	16.037235	-0.070587	4.008587
361.443999	5497.201027	16.042240	-0.070655	4.005714
361.390758	5489.229610	16.047245	-0.070640	4.002861
361.493776	5481.239911	16.052250	-0.070654	4.000001
360.980802	5473.314936	16.057255	-0.070553	3.997153
361.190315	5465.175808	16.062259	-0.070587	3.994237
360.847408	5457.276989	16.067264	-0.070518	3.991396
360.884552	5449.200455	16.072269	-0.070519	3.988496
360.547801	5441.301642	16.077274	-0.070452	3.985652
360.769197	5433.255583	16.082279	-0.070488	3.982762
360.535368	5425.225424	16.087283	-0.070439	3.979867
360.917668	5417.218586	16.092288	-0.070505	3.976990
360.321175	5409.263085	16.097293	-0.070388	3.974112
360.217295	5401.298722	16.102298	-0.070364	3.971237
360.424429	5393.210590	16.107303	-0.070397	3.968321
360.434768	5385.195164	16.112307	-0.070394	3.965426
360.041990	5377.323206	16.117312	-0.070316	3.962573
359.891015	5369.258590	16.122317	-0.070282	3.959653
360.250200	5361.269052	16.127322	-0.070344	3.956767
360.779930	5353.124084	16.132327	-0.070437	3.953825
360.132978	5345.243677	16.137331	-0.070312	3.950956
360.496246	5337.187788	16.142336	-0.070374	3.948040
360.672491	5329.182534	16.147341	-0.070402	3.945137
360.268275	5321.277397	16.152346	-0.070321	3.942256
360.046847	5313.252053	16.157351	-0.070275	3.939334
360.437468	5305.240474	16.162355	-0.070342	3.936426
360.171834	5297.255105	16.167360	-0.070287	3.933513
360.088368	5289.221725	16.172365	-0.070267	3.930583
359.976622	5281.281428	16.177370	-0.070241	3.927685
360.101666	5273.211457	16.182375	-0.070259	3.924742
359.828737	5265.304365	16.187379	-0.070203	3.921849
359.550519	5257.313868	16.192384	-0.070146	3.918922
359.824782	5249.260820	16.197389	-0.070191	3.915982
359.962415	5241.246583	16.202394	-0.070212	3.913050
359.515149	5233.290947	16.207399	-0.070123	3.910127
359.568699	5225.265147	16.212403	-0.070128	3.907185
359.509202	5217.262537	16.217408	-0.070112	3.904248
359.705215	5209.252986	16.222413	-0.070143	3.901311
359.710222	5201.264023	16.227418	-0.070139	3.898375
359.596383	5193.315573	16.232423	-0.070112	3.895450
359.258809	5185.322651	16.237427	-0.070044	3.892501
359.124574	5177.333234	16.242432	-0.070014	3.889556
359.014323	5169.332524	16.247437	-0.069988	3.886605
359.310890	5161.299354	16.252442	-0.070038	3.883648
359.347338	5153.309455	16.257447	-0.070040	3.880699
358.964665	5145.402198	16.262451	-0.069963	3.877770
359.620332	5137.264064	16.267456	-0.070080	3.874775
359.117985	5129.207057	16.272461	-0.069981	3.871783
358.645165	5121.254289	16.277466	-0.069888	3.868829
359.226888	5113.232213	16.282471	-0.069991	3.865868
358.857087	5105.262420	16.287475	-0.069917	3.862905
358.570212	5097.327825	16.292480	-0.069859	3.859954
358.604335	5089.313884	16.297485	-0.069860	3.856978
358.331448	5081.349734	16.302490	-0.069804	3.854011
358.405514	5073.338341	16.307495	-0.069812	3.851033
358.839439	5065.230217	16.312499	-0.069888	3.848023
358.908397	5057.285905	16.317504	-0.069895	3.845065
358.386663	5049.363564	16.322509	-0.069793	3.842100
358.536949	5041.334830	16.327514	-0.069816	3.839107
358.737386	5033.371206	16.332519	-0.069848	3.836137
359.007188	5025.267648	16.337523	-0.069893	3.833115
358.742142	5017.391238	16.342528	-0.069838	3.830163
358.750960	5009.293927	16.347533	-0.069835	3.827132
358.239969	5001.363771	16.352538	-0.069734	3.824150
358.195895	4993.385651	16.357543	-0.069721	3.821158
358.171496	4985.385185	16.362547	-0.069711	3.818155
358.152688	4977.403993	16.367552	-0.069702	3.815158
357.948166	4969.376287	16.372557	-0.069659	3.812136
358.246781	4961.304014	16.377562	-0.069709	3.809107
358.342211	4953.326586	16.382567	-0.069722	3.806107
357.944310	4945.361272	16.387571	-0.069643	3.803097
357.985859	4937.411333	16.392576	-0.069645	3.800101
357.988416	4929.396414	16.397581	-0.069641	3.797077
358.087416	4921.364631	16.402586	-0.069654	3.794046
358.049842	4913.363299	16.407591	-0.069641	3.791022
358.291746	4905.273610	16.412595	-0.069681	3.787968
358.034085	4897.353106	16.417600	-0.069628	3.784964
358.022195	4889.394130	16.422605	-0.069621	3.781948
358.552595	4881.327153	16.427610	-0.069714	3.778903
358.295067	4873.398629	16.432615	-0.069661	3.775888
358.364649	4865.358308	16.437619	-0.069669	3.772837
357.784329	4857.467865	16.442624	-0.069556	3.769825
357.709703	4849.438952	16.447629	-0.069536	3.766769
357.833081	4841.410658	16.452634	-0.069554	3.763716
357.878433	4833.466677	16.457639	-0.069557	3.760691
357.974317	4825.419458	16.462643	-0.069570	3.757625
358.129847	4817.419138	16.467648	-0.069594	3.754576
357.605574	4809.496454	16.472653	-0.069491	3.751538
357.477864	4801.491332	16.477658	-0.069462	3.748475
357.764830	4793.439249	16.482663	-0.069510	3.745402
357.887950	4785.424593	16.487667	-0.069528	3.742337
358.060398	4777.426300	16.492672	-0.069555	3.739277
357.794148	4769.452345	16.497677	-0.069500	3.736212
357.908857	4761.445647	16.502682	-0.069516	3.733143
357.728976	4753.473641	16.507687	-0.069477	3.730076
357.653627	4745.471401	16.512691	-0.069458	3.726998
357.785028	4737.463869	16.517696	-0.069477	3.723921
357.494678	4729.519022	16.522701	-0.069418	3.720854
357.242944	4721.544298	16.527706	-0.069366	3.717775
357.019064	4713.530763	16.532711	-0.069319	3.714678
356.742611	4705.522654	16.537715	-0.069262	3.711580
356.550056	4697.519006	16.542720	-0.069221	3.708483
356.941387	4689.416966	16.547725	-0.069289	3.705360
356.965965	4681.495337	16.552730	-0.069288	3.702296
356.692652	4673.488268	16.557735	-0.069232	3.699187
356.791242	4665.491186	16.562739	-0.069245	3.696090
357.184979	4657.472790	16.567744	-0.069313	3.692990
356.911315	4649.461159	16.572749	-0.069257	3.689872
356.902364	4641.470567	16.577754	-0.069250	3.686766
356.713155	4633.498999	16.582759	-0.069210	3.683661
356.638255	4625.563310	16.587763	-0.069191	3.680570
356.717420	4617.584522	16.592768	-0.069200	3.677463
356.624801	4609.531412	16.597773	-0.069178	3.674321
356.455765	4601.589659	16.602778	-0.069141	3.671217
356.045710	4593.616228	16.607783	-0.069059	3.668091
355.552989	4585.630765	16.612787	-0.068962	3.664956
355.992582	4577.632245	16.617792	-0.069039	3.661838
355.880453	4569.569614	16.622797	-0.069013	3.658678
355.762270	4561.582106	16.627802	-0.068986	3.655544
355.046958	4553.726873	16.632807	-0.068847	3.652443
355.274230	4545.558861	16.637811	-0.068884	3.649242
355.428637	4537.632557	16.642816	-0.068908	3.646132
355.433970	4529.602879	16.647821	-0.068904	3.642974
355.305138	4521.649128	16.652826	-0.068874	3.639840
355.272539	4513.670903	16.657831	-0.068863	3.636695
355.181768	4505.621436	16.662835	-0.068841	3.633519
354.699602	4497.704265	16.667840	-0.068746	3.630381
354.598549	4489.650737	16.672845	-0.068722	3.627196
355.127188	4481.540171	16.677850	-0.068815	3.624005
355.069757	4473.628555	16.682855	-0.068799	3.620872
355.306279	4465.579675	16.687859	-0.068838	3.617691
354.735537	4457.722170	16.692864	-0.068727	3.614560
355.255658	4449.605357	16.697869	-0.068818	3.611355
354.806846	4441.672128	16.702874	-0.068729	3.608192
355.156423	4433.598296	16.707879	-0.068789	3.604993
355.362691	4425.592953	16.712883	-0.068822	3.601815
354.883671	4417.749887	16.717888	-0.068728	3.598678
354.551449	4409.784835	16.722893	-0.068661	3.595494
354.601948	4401.725227	16.727898	-0.068665	3.592281
354.999558	4393.610409	16.732903	-0.068734	3.589053
354.906706	4385.676528	16.737907	-0.068711	3.585880
354.997802	4377.694690	16.742912	-0.068723	3.582691
355.122820	4369.624624	16.747917	-0.068741	3.579464
355.264453	4361.687502	16.752922	-0.068762	3.576288
355.290593	4353.678863	16.757927	-0.068762	3.573078
354.590294	4345.770844	16.762931	-0.068626	3.569883
354.552699	4337.783047	16.767936	-0.068614	3.566673
354.420116	4329.763068	16.772941	-0.068584	3.563444
354.285730	4321.824223	16.777946	-0.068554	3.560245
353.994743	4313.881995	16.782951	-0.068495	3.557037
353.696425	4305.840818	16.787955	-0.068434	3.553785
353.395026	4297.826710	16.792960	-0.068373	3.550542
353.828267	4289.696689	16.797965	-0.068448	3.547271
353.797126	4281.713766	16.802970	-0.068437	3.544043
353.921129	4273.784051	16.807975	-0.068455	3.540838
353.828701	4265.758719	16.812979	-0.068432	3.537584
354.291074	4257.718754	16.817984	-0.068513	3.534339
354.183646	4249.772378	16.822989	-0.068488	3.531111
354.023627	4241.776706	16.827994	-0.068453	3.527859
353.497185	4233.852308	16.832999	-0.068350	3.524621
352.969259	4225.947824	16.838003	-0.068246	3.521388
353.635898	4217.818758	16.843008	-0.068365	3.518098
353.770626	4209.796100	16.848013	-0.068385	3.514832
353.314284	4201.896119	16.853018	-0.068295	3.511594
353.498424	4193.872959	16.858023	-0.068324	3.508323
352.979932	4185.885209	16.863027	-0.068222	3.505041
353.318203	4177.875492	16.868032	-0.068280	3.501774
353.169168	4169.892721	16.873037	-0.068247	3.498500
353.293837	4161.869844	16.878042	-0.068265	3.495215
353.159035	4153.900244	16.883047	-0.068235	3.491940
353.243880	4145.840855	16.888051	-0.068245	3.488633
352.956448	4137.922893	16.893056	-0.068186	3.485368
352.575150	4129.989695	16.898061	-0.068110	3.482091
352.584229	4121.959985	16.903066	-0.068107	3.478784
352.289582	4114.022976	16.908071	-0.068047	3.475501
351.953681	4106.000912	16.913075	-0.067979	3.472180
351.916603	4098.000223	16.918080	-0.067967	3.468873
351.989000	4089.949229	16.923085	-0.067975	3.465547
352.394026	4081.908989	16.928090	-0.068045	3.462233
352.445973	4073.899832	16.933095	-0.068050	3.458917
352.560360	4065.872906	16.938099	-0.068066	3.455592
352.384148	4057.975241	16.943104	-0.068028	3.452308
351.989202	4050.026559	16.948109	-0.067949	3.448992
352.678972	4041.897973	16.953114	-0.068072	3.445635
352.872147	4033.943223	16.958119	-0.068103	3.442331
352.460448	4025.990714	16.963123	-0.068021	3.439003
352.729283	4018.013534	16.968128	-0.068066	3.435685
352.867214	4009.996532	16.973133	-0.068086	3.432343
352.754948	4001.995455	16.978138	-0.068060	3.428996
352.282346	3994.130104	16.983143	-0.067967	3.425689
351.703270	3986.191316	16.988147	-0.067854	3.422345
351.713666	3978.159676	16.993152	-0.067851	3.418979
351.553480	3970.114605	16.998157	-0.067816	3.415598
351.657405	3962.090215	17.003162	-0.067830	3.412232
352.240643	3953.994556	17.008167	-0.067933	3.408850
351.747102	3946.101029	17.013171	-0.067836	3.405511
351.752809	3938.114531	17.018176	-0.067832	3.402147
352.053291	3930.070123	17.023181	-0.067882	3.398766
351.838130	3922.147837	17.028186	-0.067837	3.395415
351.761828	3914.141085	17.033191	-0.067818	3.392030
351.651612	3906.078124	17.038195	-0.067792	3.388616
351.641560	3898.117941	17.043200	-0.067785	3.385247
351.934782	3890.089494	17.048205	-0.067834	3.381855
351.641529	3882.180656	17.053210	-0.067774	3.378490
351.866278	3874.157119	17.058215	-0.067811	3.375092
351.833439	3866.135261	17.063219	-0.067800	3.371681
351.776254	3858.145660	17.068224	-0.067784	3.368280
351.455527	3850.204700	17.073229	-0.067719	3.364887
351.599131	3842.228448	17.078234	-0.067740	3.361492
351.379863	3834.297053	17.083239	-0.067694	3.358099
351.337154	3826.250918	17.088243	-0.067681	3.354661
351.364331	3818.290109	17.093248	-0.067681	3.351258
351.446787	3810.224615	17.098253	-0.067691	3.347808
351.630531	3802.194871	17.103258	-0.067720	3.344375
350.977962	3794.370212	17.108263	-0.067594	3.340994
350.305573	3786.414552	17.113267	-0.067463	3.337553
350.355215	3778.367705	17.118272	-0.067467	3.334096
349.909338	3770.426970	17.123277	-0.067379	3.330662
350.047403	3762.364292	17.128282	-0.067399	3.327195
350.256073	3754.323907	17.133287	-0.067433	3.323736
350.459252	3746.317592	17.138291	-0.067466	3.320289
350.505081	3738.342298	17.143296	-0.067469	3.316845
350.290618	3730.355406	17.148301	-0.067424	3.313382
349.742373	3722.425094	17.153306	-0.067316	3.309928
349.655514	3714.447946	17.158311	-0.067295	3.306467
350.198466	3706.297724	17.163315	-0.067391	3.302952
350.254147	3698.329470	17.168320	-0.067396	3.299494
350.282914	3690.356208	17.173325	-0.067396	3.296028
350.193038	3682.402853	17.178330	-0.067374	3.292563
350.236929	3674.374796	17.183335	-0.067377	3.289067
350.296017	3666.368890	17.188339	-0.067383	3.285578
349.741448	3658.546395	17.193344	-0.067275	3.282140
349.209192	3650.568973	17.198349	-0.067170	3.278632
349.688321	3642.472231	17.203354	-0.067254	3.275108
349.392780	3634.550949	17.208359	-0.067194	3.271627
349.985025	3626.426602	17.213363	-0.067299	3.268088
349.642665	3618.506171	17.218368	-0.067230	3.264597
349.411879	3610.571945	17.223373	-0.067182	3.261101
349.603687	3602.521176	17.228378	-0.067212	3.257568
349.309901	3594.577494	17.233383	-0.067152	3.254057
349.461880	3586.536452	17.238387	-0.067175	3.250518
349.387887	3578.581117	17.243392	-0.067156	3.247004
349.441294	3570.558915	17.248397	-0.067161	3.243462
349.495280	3562.573617	17.253402	-0.067166	3.239932
349.445656	3554.639181	17.258407	-0.067152	3.236417
349.188073	3546.659122	17.263411	-0.067098	3.232869
349.211164	3538.638187	17.268416	-0.067097	3.229310
349.417444	3530.591856	17.273421	-0.067131	3.225744
349.778894	3522.546596	17.278426	-0.067193	3.222181
349.784142	3514.608452	17.283431	-0.067188	3.218647
349.323710	3506.656955	17.288435	-0.067098	3.215084
349.684316	3498.643001	17.293440	-0.067159	3.211523
349.387043	3490.677735	17.298445	-0.067099	3.207952
349.224151	3482.664633	17.303450	-0.067063	3.204361
349.433067	3474.733553	17.308455	-0.067097	3.200819
349.316119	3466.722822	17.313459	-0.067070	3.197224
348.872427	3458.838942	17.318464	-0.066982	3.193667
348.810197	3450.786155	17.323469	-0.066965	3.190047
348.874089	3442.799694	17.328474	-0.066972	3.186458
348.652808	3434.814565	17.333479	-0.066926	3.182853
347.956677	3426.883437	17.338483	-0.066791	3.179247
348.738914	3418.803625	17.343488	-0.066931	3.175635
348.883074	3410.795672	17.348493	-0.066953	3.172024
348.364556	3402.823034	17.353498	-0.066851	3.168395
348.215625	3394.885542	17.358503	-0.066818	3.164794
348.694715	3386.830033	17.363507	-0.066902	3.161163
348.548020	3378.882309	17.368512	-0.066870	3.157549
348.611594	3370.852278	17.373517	-0.066876	3.153904
348.325238	3362.926467	17.378522	-0.066818	3.150285
347.877479	3355.014255	17.383527	-0.066729	3.146661
347.780383	3346.982821	17.388531	-0.066706	3.142995
347.800297	3338.956688	17.393536	-0.066704	3.139332
348.070380	3330.937512	17.398541	-0.066749	3.135679
348.220441	3322.905437	17.403546	-0.066772	3.132011
348.483610	3314.878193	17.408551	-0.066816	3.128346
348.566457	3306.872862	17.413555	-0.066826	3.124678
348.493812	3298.974051	17.418560	-0.066807	3.121048
348.395728	3291.015084	17.423565	-0.066784	3.117384
347.764092	3283.107795	17.428570	-0.066661	3.113716
347.961880	3275.077607	17.433575	-0.066693	3.110024
348.046211	3267.037904	17.438579	-0.066703	3.106319
347.952514	3259.090655	17.443584	-0.066680	3.102644
347.856512	3251.098456	17.448589	-0.066657	3.098944
347.780814	3243.136026	17.453594	-0.066638	3.095253
347.373866	3235.225664	17.458599	-0.066557	3.091567
347.306685	3227.172582	17.463603	-0.066539	3.087826
348.117045	3219.066989	17.468608	-0.066685	3.084098
347.528834	3211.215498	17.473613	-0.066570	3.080418
347.623658	3203.216425	17.478618	-0.066583	3.076696
347.772606	3195.180602	17.483623	-0.066605	3.072956
347.292680	3187.207326	17.488627	-0.066511	3.069210
347.363073	3179.212525	17.493632	-0.066518	3.065475
346.984516	3171.281911	17.498637	-0.066443	3.061745
347.041975	3163.254682	17.503642	-0.066448	3.057986
346.989800	3155.263319	17.508647	-0.066433	3.054233
346.778410	3147.318969	17.513651	-0.066389	3.050491
346.979704	3139.304952	17.518656	-0.066421	3.046731
346.664037	3131.355411	17.523661	-0.066357	3.042971
346.831968	3123.330162	17.528666	-0.066383	3.039195
346.999602	3115.382238	17.533671	-0.066409	3.035451
346.572522	3107.422706	17.538675	-0.066324	3.031667
346.606579	3099.420174	17.543680	-0.066325	3.027881
346.889799	3091.352639	17.548685	-0.066373	3.024072
346.791440	3083.405139	17.553690	-0.066349	3.020296
346.563908	3075.491811	17.558695	-0.066302	3.016525
346.397355	3067.484304	17.563699	-0.066266	3.012707
346.390888	3059.502782	17.568704	-0.066259	3.008905
346.422860	3051.482120	17.573709	-0.066260	3.005082
346.282881	3043.546829	17.578714	-0.066229	3.001285
346.185598	3035.598821	17.583719	-0.066205	2.997480
346.033279	3027.581471	17.588723	-0.066172	2.993634
345.873104	3019.607892	17.593728	-0.066137	2.989804
345.959402	3011.582393	17.598733	-0.066148	2.985956
345.279472	3003.708062	17.603738	-0.066016	2.982137
345.827627	2995.613257	17.608743	-0.066113	2.978270
345.475897	2987.660164	17.613747	-0.066042	2.974420
346.032526	2979.584375	17.618752	-0.066140	2.970552
346.157499	2971.586900	17.623757	-0.066158	2.966696
345.512790	2963.739431	17.628762	-0.066033	2.962866
345.536835	2955.767880	17.633767	-0.066032	2.959006
345.479960	2947.764713	17.638771	-0.066017	2.955122
345.250830	2939.806319	17.643776	-0.065969	2.951245
345.351928	2931.781337	17.648781	-0.065982	2.947348
345.282460	2923.783033	17.653786	-0.065964	2.943450
345.070136	2915.851351	17.658791	-0.065919	2.939571
345.267307	2907.795134	17.663795	-0.065951	2.935649
345.241617	2899.834111	17.668800	-0.065941	2.931756
344.773784	2891.931168	17.673805	-0.065849	2.927862
344.902416	2883.883973	17.678810	-0.065867	2.923924
345.075458	2875.925269	17.683815	-0.065894	2.920027
344.889990	2867.947654	17.688819	-0.065855	2.916097
345.544946	2859.848247	17.693824	-0.065971	2.912146
345.476800	2851.853859	17.698829	-0.065953	2.908203
344.922293	2843.961228	17.703834	-0.065845	2.904278
344.857315	2836.027436	17.708839	-0.065828	2.900354
345.394188	2827.929918	17.713843	-0.065922	2.896376
345.032128	2820.031464	17.718848	-0.065850	2.892443
344.779870	2812.056802	17.723853	-0.065798	2.888472
344.689286	2804.058742	17.728858	-0.065775	2.884493
344.824877	2796.119033	17.733863	-0.065796	2.880550
344.925279	2788.098286	17.738867	-0.065809	2.876560
344.940245	2780.100769	17.743872	-0.065807	2.872570
344.643018	2772.182162	17.748877	-0.065746	2.868597
344.620435	2764.179319	17.753882	-0.065737	2.864592
344.491442	2756.234015	17.758887	-0.065707	2.860604
344.224532	2748.261452	17.763891	-0.065652	2.856589
344.747174	2740.195361	17.768896	-0.065745	2.852566
344.811493	2732.214385	17.773901	-0.065751	2.848554
344.866087	2724.204862	17.778906	-0.065756	2.844522
345.012795	2716.292575	17.783911	-0.065778	2.840538
344.637315	2708.366009	17.788915	-0.065703	2.836511
344.377428	2700.422823	17.793920	-0.065650	2.832477
344.142236	2692.445154	17.798925	-0.065601	2.828421
343.859183	2684.458756	17.803930	-0.065543	2.824352
344.015567	2676.454137	17.808935	-0.065567	2.820293
343.715353	2668.513170	17.813939	-0.065506	2.816234
343.402482	2660.558350	17.818944	-0.065442	2.812162
343.498322	2652.508488	17.823949	-0.065455	2.808059
343.341818	2644.549119	17.828954	-0.065420	2.803981
343.333635	2636.601202	17.833959	-0.065414	2.799912
343.129114	2628.625676	17.838963	-0.065370	2.795811
343.209592	2620.608604	17.843968	-0.065380	2.791700
343.077989	2612.645718	17.848973	-0.065350	2.787598
343.263947	2604.611950	17.853978	-0.065380	2.783473
343.219177	2596.660643	17.858983	-0.065366	2.779370
342.961306	2588.717776	17.863987	-0.065313	2.775252
343.195297	2580.703553	17.868992	-0.065351	2.771122
343.476541	2572.661841	17.873997	-0.065398	2.766973
343.497766	2564.680207	17.879002	-0.065397	2.762834
343.440267	2556.787696	17.884007	-0.065381	2.758730
342.836791	2548.896163	17.889011	-0.065264	2.754587
343.173977	2540.784768	17.894016	-0.065321	2.750381
343.579182	2532.775525	17.899021	-0.065392	2.746227
343.085875	2524.867945	17.904026	-0.065294	2.742063
342.579644	2516.999822	17.909031	-0.065195	2.737912
342.593754	2508.954959	17.914035	-0.065192	2.733695
342.903176	2500.909115	17.919040	-0.065245	2.729490
342.766904	2493.000137	17.924045	-0.065214	2.725322
342.722508	2485.009375	17.929050	-0.065201	2.721111
343.015154	2477.018244	17.934055	-0.065250	2.716914
343.119178	2469.010655	17.939059	-0.065264	2.712690
343.309338	2461.011563	17.944064	-0.065294	2.708469
343.262436	2453.048195	17.949069	-0.065280	2.704246
342.772461	2445.183861	17.954074	-0.065184	2.700040
342.559904	2437.258508	17.959079	-0.065139	2.695812
342.381901	2429.266520	17.964083	-0.065101	2.691545
342.607468	2421.218896	17.969088	-0.065138	2.687268
341.899218	2413.381856	17.974093	-0.065001	2.683035
342.144415	2405.324591	17.979098	-0.065041	2.678740
342.289542	2397.332503	17.984103	-0.065063	2.674467
342.431519	2389.312224	17.989107	-0.065084	2.670171
342.395897	2381.336991	17.994112	-0.065072	2.665881
342.651118	2373.334831	17.999117	-0.065115	2.661589
342.056817	2365.449368	18.004122	-0.064999	2.657297
341.797381	2357.542078	18.009127	-0.064945	2.653008
341.042534	2349.649776	18.014131	-0.064800	2.648687
341.537853	2341.515823	18.019136	-0.064886	2.644311
341.608282	2333.585543	18.024141	-0.064894	2.640011
342.051428	2325.514936	18.029146	-0.064972	2.635652
341.991762	2317.582858	18.034151	-0.064955	2.631328
341.549669	2309.661104	18.039155	-0.064868	2.626976
341.679390	2301.662091	18.044160	-0.064887	2.622613
341.713354	2293.700791	18.049165	-0.064888	2.618258
341.707943	2285.724355	18.054170	-0.064882	2.613884
341.677315	2277.751929	18.059175	-0.064871	2.609503
341.338138	2269.835267	18.064179	-0.064802	2.605124
341.487928	2261.843274	18.069184	-0.064825	2.600730
341.465410	2253.911505	18.074189	-0.064816	2.596350
340.919401	2245.911533	18.079194	-0.064709	2.591888
341.009738	2237.869620	18.084199	-0.064720	2.587440
340.778666	2229.912432	18.089203	-0.064672	2.583009
340.846775	2221.963736	18.094208	-0.064680	2.578596
340.612011	2214.035882	18.099213	-0.064631	2.574165
340.604836	2206.024423	18.104218	-0.064624	2.569696
341.195102	2197.964093	18.109223	-0.064729	2.565235
341.289586	2190.002540	18.114227	-0.064741	2.560785
341.318891	2182.077535	18.119232	-0.064741	2.556344
341.319976	2174.109065	18.124237	-0.064736	2.551869
340.746795	2166.237137	18.129242	-0.064625	2.547399
340.692158	2158.275616	18.134247	-0.064609	2.542908
340.787430	2150.275815	18.139251	-0.064622	2.538398
340.641521	2142.335757	18.144256	-0.064589	2.533896
340.481233	2134.379813	18.149261	-0.064554	2.529377
340.326341	2126.401495	18.154266	-0.064520	2.524837
339.969497	2118.532236	18.159271	-0.064449	2.520335
340.245933	2110.471958	18.164275	-0.064495	2.515764
340.331192	2102.481223	18.169280	-0.064506	2.511210
340.550444	2094.463829	18.174285	-0.064541	2.506642
339.918953	2086.604808	18.179290	-0.064418	2.502093
339.653990	2078.689723	18.184295	-0.064364	2.497531
339.893920	2070.632932	18.189299	-0.064403	2.492917
340.200649	2062.615225	18.194304	-0.064455	2.488322
340.509536	2054.602388	18.199309	-0.064507	2.483722
340.154591	2046.729567	18.204314	-0.064436	2.479144
340.313749	2038.778068	18.209319	-0.064461	2.474551
340.129289	2030.819361	18.214323	-0.064421	2.469919
339.709567	2022.920806	18.219328	-0.064338	2.465295
340.285668	2014.865662	18.224333	-0.064440	2.460647
340.068659	2006.939978	18.229338	-0.064394	2.456005
339.945590	1999.001278	18.234343	-0.064366	2.451355
339.737474	1991.057267	18.239347	-0.064322	2.446685
339.958093	1983.053495	18.244352	-0.064358	2.442005
340.145853	1975.096589	18.249357	-0.064388	2.437341
339.841162	1967.147058	18.254362	-0.064326	2.432634
340.319766	1959.088161	18.259367	-0.064410	2.427914
340.114107	1951.145680	18.264371	-0.064366	2.423201
339.892680	1943.254827	18.269376	-0.064320	2.418507
339.488622	1935.371752	18.274381	-0.064239	2.413795
339.857625	1927.301668	18.279386	-0.064303	2.409023
339.905670	1919.321931	18.284391	-0.064307	2.404270
339.825511	1911.414280	18.289395	-0.064287	2.399541
339.963067	1903.451869	18.294400	-0.064307	2.394787
339.574211	1895.574621	18.299405	-0.064229	2.390032
339.247561	1887.604217	18.304410	-0.064163	2.385217
339.257138	1879.671879	18.309415	-0.064160	2.380442
339.504401	1871.645552	18.314419	-0.064201	2.375620
338.965024	1863.771603	18.319424	-0.064095	2.370816
338.729678	1855.830326	18.324429	-0.064046	2.365986
339.005292	1847.787844	18.329434	-0.064092	2.361127
339.321995	1839.817422	18.334439	-0.064146	2.356306
339.254106	1831.869577	18.339443	-0.064128	2.351456
339.117471	1823.921987	18.344448	-0.064098	2.346591
338.850456	1816.001855	18.349453	-0.064043	2.341722
338.294501	1808.133741	18.354458	-0.063934	2.336850
338.249278	1800.177050	18.359463	-0.063920	2.331956
338.554357	1792.106833	18.364467	-0.063972	2.327011
338.042320	1784.228487	18.369472	-0.063871	2.322106
338.291832	1776.225759	18.374477	-0.063913	2.317177
337.996891	1768.305421	18.379482	-0.063853	2.312243
338.332636	1760.283714	18.384487	-0.063910	2.307289
338.512313	1752.293247	18.389491	-0.063938	2.302331
338.636710	1744.347987	18.394496	-0.063956	2.297386
338.451408	1736.450083	18.399501	-0.063916	2.292432
338.413886	1728.471500	18.404506	-0.063904	2.287430
337.884591	1720.651075	18.409511	-0.063800	2.282474
337.520520	1712.743521	18.414515	-0.063728	2.277466
337.624376	1704.716349	18.419520	-0.063742	2.272413
338.062525	1696.651280	18.424525	-0.063818	2.267354
337.763278	1688.748289	18.429530	-0.063757	2.262321
337.588286	1680.854082	18.434535	-0.063719	2.257294
337.313099	1672.925903	18.439539	-0.063663	2.252225
337.341616	1664.949032	18.444544	-0.063663	2.247140
337.283463	1657.004038	18.449549	-0.063647	2.242056
337.602855	1648.976390	18.454554	-0.063701	2.236942
337.814679	1641.022775	18.459559	-0.063735	2.231854
337.360026	1633.141692	18.464563	-0.063646	2.226741
337.213675	1625.200757	18.469568	-0.063613	2.221605
337.198818	1617.265743	18.474573	-0.063605	2.216474
337.203970	1609.302966	18.479578	-0.063601	2.211314
336.981225	1601.391727	18.484583	-0.063554	2.206154
337.222339	1593.393173	18.489587	-0.063594	2.200969
337.370755	1585.434557	18.494592	-0.063616	2.195788
337.169834	1577.545429	18.499597	-0.063574	2.190609
336.481243	1569.675763	18.504602	-0.063441	2.185384
336.814061	1561.674410	18.509607	-0.063497	2.180156
337.235605	1553.637923	18.514611	-0.063571	2.174900
337.288335	1545.681962	18.519616	-0.063575	2.169651
337.120172	1537.797523	18.524621	-0.063539	2.164414
336.783762	1529.928413	18.529626	-0.063471	2.159160
336.412350	1522.052307	18.534631	-0.063397	2.153884
336.601306	1514.060566	18.539635	-0.063427	2.148572
336.082918	1506.185266	18.544640	-0.063325	2.143257
336.149945	1498.238812	18.549645	-0.063332	2.137937
335.974774	1490.268574	18.554650	-0.063294	2.132564
336.662741	1482.191116	18.559655	-0.063417	2.127190
336.469430	1474.313367	18.564659	-0.063376	2.121851
335.813490	1466.508735	18.569664	-0.063249	2.116502
335.705764	1458.557776	18.574669	-0.063224	2.111095
335.893791	1450.516964	18.579674	-0.063253	2.105641
335.946298	1442.594662	18.584679	-0.063258	2.100241
336.110670	1434.628077	18.589683	-0.063283	2.094808
335.511686	1426.800770	18.594688	-0.063167	2.089380
335.368009	1418.881769	18.599693	-0.063135	2.083920
335.723166	1410.845139	18.604698	-0.063196	2.078415
335.406710	1402.993853	18.609703	-0.063132	2.072956
335.498656	1395.016139	18.614707	-0.063143	2.067436
335.827088	1387.017989	18.619712	-0.063199	2.061911
335.386635	1379.204057	18.624717	-0.063112	2.056421
335.384764	1371.234347	18.629722	-0.063107	2.050852
335.405885	1363.312244	18.634727	-0.063105	2.045304
335.276535	1355.401609	18.639731	-0.063076	2.039734
335.345795	1347.460982	18.644736	-0.063084	2.034147
335.626831	1339.486060	18.649741	-0.063131	2.028543
335.371765	1331.587646	18.654746	-0.063078	2.022922
335.678840	1323.621010	18.659751	-0.063130	2.017296
335.197979	1315.787590	18.664755	-0.063036	2.011665
335.073969	1307.863191	18.669760	-0.063007	2.005992
335.145490	1299.942848	18.674765	-0.063016	2.000326
335.343895	1291.968450	18.679770	-0.063047	1.994619
335.329106	1284.066670	18.684775	-0.063039	1.988925
335.310605	1276.132393	18.689779	-0.063031	1.983191
334.797272	1268.309909	18.694784	-0.062930	1.977467
335.131779	1260.319990	18.699789	-0.062987	1.971697
334.949574	1252.420589	18.704794	-0.062948	1.965920
334.373466	1244.614335	18.709799	-0.062836	1.960151
333.976009	1236.754262	18.714803	-0.062757	1.954345
333.752305	1228.840181	18.719808	-0.062710	1.948500
334.211661	1220.786390	18.724813	-0.062790	1.942611
334.171797	1212.855332	18.729818	-0.062777	1.936740
334.330143	1204.911443	18.734823	-0.062802	1.930863
333.905259	1197.050710	18.739827	-0.062717	1.924964
333.789287	1189.150271	18.744832	-0.062691	1.919053
334.084058	1181.188211	18.749837	-0.062740	1.913123
334.071192	1173.253496	18.754842	-0.062733	1.907161
333.843104	1165.401737	18.759847	-0.062685	1.901218
334.306306	1157.401809	18.764851	-0.062766	1.895224
334.137262	1149.522114	18.769856	-0.062730	1.889229
333.766588	1141.697293	18.774861	-0.062655	1.883233
334.133906	1133.704225	18.779866	-0.062719	1.877176
333.789835	1125.875989	18.784871	-0.062649	1.871141
333.588734	1117.985830	18.789875	-0.062607	1.865057
333.035119	1110.167749	18.794880	-0.062499	1.858966
333.596149	1102.144672	18.799885	-0.062598	1.852830
333.511535	1094.229451	18.804890	-0.062577	1.846679
333.561548	1086.323910	18.809895	-0.062581	1.840532
333.047031	1078.532727	18.814899	-0.062480	1.834385
333.550963	1070.527939	18.819904	-0.062569	1.828173
333.414583	1062.672009	18.824909	-0.062538	1.821980
333.196271	1054.804195	18.829914	-0.062492	1.815746
333.189860	1046.904153	18.834919	-0.062486	1.809491
333.574677	1038.926370	18.839923	-0.062553	1.803200
333.546335	1031.057005	18.844928	-0.062542	1.796923
333.688270	1023.130982	18.849933	-0.062563	1.790600
333.752017	1015.208657	18.854938	-0.062570	1.784248
333.162814	1007.460899	18.859943	-0.062455	1.777932
332.969518	999.579176	18.864947	-0.062414	1.771534
332.431548	991.759566	18.869952	-0.062309	1.765120
332.361425	983.888755	18.874957	-0.062291	1.758701
332.276378	975.984992	18.879962	-0.062270	1.752229
332.172194	968.092385	18.884967	-0.062245	1.745739
332.347254	960.171134	18.889971	-0.062273	1.739238
332.217889	952.302262	18.894976	-0.062243	1.732716
331.925200	944.471710	18.899981	-0.062184	1.726180
332.108342	936.539191	18.904986	-0.062213	1.719597
332.356386	928.634212	18.909991	-0.062254	1.713020
332.307483	920.748478	18.914995	-0.062239	1.706395
332.046668	912.913014	18.920000	-0.062186	1.699757
332.092665	905.054612	18.925005	-0.062189	1.693116
331.808735	897.199089	18.930010	-0.062131	1.686406
332.278802	889.243852	18.935015	-0.062213	1.679686
332.479336	881.357289	18.940019	-0.062246	1.672962
331.885268	873.599793	18.945024	-0.062130	1.666213
332.150103	865.687799	18.950029	-0.062174	1.659421
332.294232	857.793858	18.955034	-0.062196	1.652600
332.031443	849.991189	18.960039	-0.062142	1.645774
331.846687	842.176892	18.965043	-0.062102	1.638920
331.802859	834.308055	18.970048	-0.062089	1.632009
331.145187	826.548987	18.975053	-0.061961	1.625078
331.197836	818.653878	18.980058	-0.061966	1.618098
331.696505	810.693017	18.985063	-0.062054	1.611093
331.718147	802.839051	18.990067	-0.062053	1.604085
331.620387	795.012308	18.995072	-0.062029	1.597053
331.512064	787.202054	19.000077	-0.062004	1.590004
331.158789	779.405928	19.005082	-0.061933	1.582900
330.714911	771.649983	19.010087	-0.061845	1.575787
330.805204	763.762860	19.015091	-0.061857	1.568600
331.319280	755.816393	19.020096	-0.061948	1.561389
331.087445	748.047217	19.025101	-0.061899	1.554197
330.872998	740.220330	19.030106	-0.061854	1.546921
330.886786	732.387303	19.035111	-0.061852	1.539638
330.717114	724.589752	19.040115	-0.061815	1.532327
331.058824	716.667589	19.045120	-0.061873	1.524941
330.631497	708.965864	19.050125	-0.061789	1.517610
330.649781	701.098243	19.055130	-0.061787	1.510154
330.665254	693.277991	19.060135	-0.061785	1.502706
330.805746	685.450074	19.065139	-0.061806	1.495233
330.283326	677.716415	19.070144	-0.061704	1.487709
330.443730	669.880285	19.075149	-0.061728	1.480155
329.848332	662.181084	19.080154	-0.061612	1.472576
330.391222	654.205759	19.085159	-0.061708	1.464870
330.262098	646.440092	19.090163	-0.061679	1.457220
330.187787	638.642998	19.095168	-0.061660	1.449509
330.456988	630.800907	19.100173	-0.061705	1.441767
330.571132	622.993342	19.105178	-0.061721	1.433993
330.306978	615.258616	19.110183	-0.061667	1.426187
330.245408	607.488953	19.115187	-0.061651	1.418336
330.048939	599.735382	19.120192	-0.061609	1.410435
329.774580	592.019551	19.125197	-0.061553	1.402515
329.660348	584.250712	19.130202	-0.061527	1.394523
329.192987	576.542336	19.135207	-0.061434	1.386486
329.249095	568.744014	19.140211	-0.061440	1.378399
329.287531	560.949926	19.145216	-0.061442	1.370266
329.488973	553.148200	19.150221	-0.061474	1.362105
329.189683	545.452169	19.155226	-0.061414	1.353919
329.104516	537.695282	19.160231	-0.061393	1.345655
329.125061	529.945184	19.165235	-0.061391	1.337367
329.243807	522.162600	19.170240	-0.061408	1.329010
328.984995	514.481084	19.175245	-0.061355	1.320641
329.219774	506.660798	19.180250	-0.061394	1.312158
328.662229	498.977403	19.185255	-0.061285	1.303623
329.046286	491.179745	19.190259	-0.061351	1.295081
328.719425	483.501555	19.195264	-0.061286	1.286482
328.872864	475.769436	19.200269	-0.061309	1.277855
328.729734	468.075999	19.205274	-0.061277	1.269157
328.639691	460.387086	19.210279	-0.061256	1.260414
328.860164	452.642203	19.215283	-0.061292	1.251606
328.332690	445.050091	19.220288	-0.061188	1.242766
328.744742	437.300410	19.225293	-0.061260	1.233864
328.831606	429.577103	19.230298	-0.061271	1.224864
328.451621	421.987015	19.235303	-0.061195	1.215861
328.487514	414.305578	19.240307	-0.061197	1.206767
328.110949	406.711744	19.245312	-0.061122	1.197624
328.359468	399.007555	19.250317	-0.061163	1.188405
328.047393	391.408983	19.255322	-0.061100	1.179127
328.276972	383.727013	19.260327	-0.061138	1.169787
328.184210	376.104069	19.265331	-0.061116	1.160376
327.884885	368.515555	19.270336	-0.061055	1.150887
327.922038	360.870858	19.275341	-0.061057	1.141321
327.721583	353.282835	19.280346	-0.061015	1.131694
327.399443	345.730592	19.285351	-0.060950	1.122004
327.471062	338.118867	19.290355	-0.060958	1.112239
327.659347	330.483317	19.295360	-0.060988	1.102383
327.691558	322.910869	19.300365	-0.060989	1.092486
327.204720	315.422917	19.305370	-0.060894	1.082492
327.273296	307.857384	19.310375	-0.060901	1.072429
327.429643	300.267256	19.315379	-0.060926	1.062258
327.584998	292.691317	19.320384	-0.060950	1.052008
327.782684	285.146865	19.325389	-0.060981	1.041710
327.201263	277.750749	19.330394	-0.060868	1.031328
327.193011	270.241669	19.335399	-0.060862	1.020821
326.873173	262.817766	19.340403	-0.060798	1.010249
326.809738	255.341284	19.345408	-0.060781	0.999554
327.089272	247.810456	19.350413	-0.060828	0.988751
327.010947	240.351592	19.355418	-0.060808	0.977842
327.408225	232.841039	19.360423	-0.060878	0.966857
327.006099	225.513875	19.365427	-0.060798	0.955812
326.522150	218.188424	19.370432	-0.060703	0.944618
326.567041	210.787937	19.375437	-0.060707	0.933316
326.394990	203.438161	19.380442	-0.060670	0.921896
326.348482	196.088174	19.385447	-0.060656	0.910367
326.370713	188.739666	19.390451	-0.060656	0.898711
326.500741	181.386396	19.395456	-0.060675	0.886926
326.347354	174.138400	19.400461	-0.060642	0.875072
325.881790	166.934528	19.405466	-0.060550	0.863038
325.894874	159.684460	19.410471	-0.060548	0.850897
325.513322	152.519656	19.415475	-0.060472	0.838607
325.064650	145.362235	19.420480	-0.060384	0.826127
324.998986	138.178531	19.425485	-0.060367	0.813528
324.425043	131.100916	19.430490	-0.060256	0.800759
323.481355	124.122854	19.435495	-0.060075	0.787846
323.104965	117.055064	19.440499	-0.060001	0.774736
321.906061	110.164521	19.445504	-0.059773	0.761460
321.165335	103.222992	19.450509	-0.059630	0.748005
320.536173	96.278041	19.455514	-0.059509	0.734336
320.029361	89.354271	19.460519	-0.059410	0.720492
319.518282	82.474850	19.465523	-0.059310	0.706466
318.279329	75.933760	19.470528	-0.059075	0.692587