Sample1

This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in this archive include uniaxial tensile testing data, fractography of selected tensile bars, and nanoindentation. The irradiation campaign was designed to facilitate a direct comparison of PM-HIP to conventional casting or forging. Five common nuclear structural alloys were included in the campaign: 316L stainless steel, SA508 pressure vessel steel, Grade 91 ferritic steel, and Ni-base alloys 625 and 690. Irradiations were carried out in the Advanced Test Reactor (ATR) at Idaho National Laboratory (INL) to target doses of 1 and 3 displacements per atom (dpa) at target temperatures of 300ºC and 400ºC through the DOE Office of Nuclear Energy, Nuclear Science User Facilities (NSUF) project 15-8242.

Data and Resources

Download all

Datatype Name Last Modified
Snap_0_0-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_0.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_1-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_1.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_10-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_10.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_11-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_11.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_12-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_12.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_13-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_13.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_14-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_14.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_2-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_2.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_3-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_3.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_4-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_4.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_5-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_5.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_6-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_6.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_7-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_7.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_8-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_8.bmp

February 10, 2026, 15:01 (UTC)
Snap_0_9-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_0_9.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_0-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_0.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_1-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_1.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_10-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_10.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_11-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_11.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_12-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_12.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_13-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_13.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_14-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_14.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_2-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_2.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_3-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_3.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_4-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_4.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_5-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_5.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_6-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_6.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_7-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_7.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_8-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_8.bmp

February 10, 2026, 15:01 (UTC)
Snap_10_9-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_10_9.bmp

February 10, 2026, 15:01 (UTC)
Snap_11_0-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_11_0.bmp

February 10, 2026, 15:01 (UTC)
Snap_11_1-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_11_1.bmp

February 10, 2026, 15:01 (UTC)
Snap_11_10-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_11_10.bmp

February 10, 2026, 15:01 (UTC)
Snap_11_11-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_11_11.bmp

February 10, 2026, 15:01 (UTC)
Snap_11_12-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_11_12.bmp

February 10, 2026, 15:01 (UTC)
Snap_11_13-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_11_13.bmp

February 10, 2026, 15:01 (UTC)
Snap_11_14-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_11_14.bmp

February 10, 2026, 15:01 (UTC)
Snap_11_2-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_11_2.bmp

February 10, 2026, 15:01 (UTC)
Snap_11_3-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_11_3.bmp

February 10, 2026, 15:01 (UTC)
Snap_11_4-bmp.hdr

February 10, 2026, 15:01 (UTC)
Snap_11_4.bmp

February 10, 2026, 15:02 (UTC)
Snap_11_5-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_11_5.bmp

February 10, 2026, 15:02 (UTC)
Snap_11_6-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_11_6.bmp

February 10, 2026, 15:02 (UTC)
Snap_11_7-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_11_7.bmp

February 10, 2026, 15:02 (UTC)
Snap_11_8-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_11_8.bmp

February 10, 2026, 15:02 (UTC)
Snap_11_9-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_11_9.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_0-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_0.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_1-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_1.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_10-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_10.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_11-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_11.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_12-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_12.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_13-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_13.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_14-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_14.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_2-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_2.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_3-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_3.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_4-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_4.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_5-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_5.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_6-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_6.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_7-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_7.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_8-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_8.bmp

February 10, 2026, 15:02 (UTC)
Snap_12_9-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_12_9.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_0-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_0.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_1-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_1.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_10-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_10.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_11-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_11.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_12-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_12.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_13-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_13.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_14-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_14.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_2-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_2.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_3-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_3.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_4-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_4.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_5-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_5.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_6-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_6.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_7-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_7.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_8-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_8.bmp

February 10, 2026, 15:02 (UTC)
Snap_13_9-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_13_9.bmp

February 10, 2026, 15:02 (UTC)
Snap_14_0-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_14_0.bmp

February 10, 2026, 15:02 (UTC)
Snap_14_1-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_14_1.bmp

February 10, 2026, 15:02 (UTC)
Snap_14_10-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_14_10.bmp

February 10, 2026, 15:02 (UTC)
Snap_14_11-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_14_11.bmp

February 10, 2026, 15:02 (UTC)
Snap_14_12-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_14_12.bmp

February 10, 2026, 15:02 (UTC)
Snap_14_13-bmp.hdr

February 10, 2026, 15:02 (UTC)
Snap_14_13.bmp

February 10, 2026, 15:03 (UTC)
Snap_14_14-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_14_14.bmp

February 10, 2026, 15:03 (UTC)
Snap_14_2-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_14_2.bmp

February 10, 2026, 15:03 (UTC)
Snap_14_3-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_14_3.bmp

February 10, 2026, 15:03 (UTC)
Snap_14_4-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_14_4.bmp

February 10, 2026, 15:03 (UTC)
Snap_14_5-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_14_5.bmp

February 10, 2026, 15:03 (UTC)
Snap_14_6-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_14_6.bmp

February 10, 2026, 15:03 (UTC)
Snap_14_7-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_14_7.bmp

February 10, 2026, 15:03 (UTC)
Snap_14_8-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_14_8.bmp

February 10, 2026, 15:03 (UTC)
Snap_14_9-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_14_9.bmp

February 10, 2026, 15:03 (UTC)
Snap_1_0-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_1_0.bmp

February 10, 2026, 15:03 (UTC)
Snap_1_1-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_1_1.bmp

February 10, 2026, 15:03 (UTC)
Snap_1_10-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_1_10.bmp

February 10, 2026, 15:03 (UTC)
Snap_1_11-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_1_11.bmp

February 10, 2026, 15:03 (UTC)
Snap_1_12-bmp.hdr

February 10, 2026, 15:03 (UTC)
Snap_1_12.bmp

February 10, 2026, 15:03 (UTC)

Additional Info

Field Value
Author Janelle Wharry, Caleb Clement, Yangyang Zhao, Katelyn Baird, David Frazer, Jatuporn Burns, Yu Lu, Yaqiao Wu, Collin Knight, Donna Guillen, David Gandy
Last Updated March 5, 2026, 16:04 (UTC)
Created February 10, 2026, 15:01 (UTC)
DOI Link https://doi.org/10.48806/3021741
Instrument
Statement of Credit