625-F_400C_3DPA_(ID-615)

This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in this archive include uniaxial tensile testing data, fractography of selected tensile bars, and nanoindentation. The irradiation campaign was designed to facilitate a direct comparison of PM-HIP to conventional casting or forging. Five common nuclear structural alloys were included in the campaign: 316L stainless steel, SA508 pressure vessel steel, Grade 91 ferritic steel, and Ni-base alloys 625 and 690. Irradiations were carried out in the Advanced Test Reactor (ATR) at Idaho National Laboratory (INL) to target doses of 1 and 3 displacements per atom (dpa) at target temperatures of 300ºC and 400ºC through the DOE Office of Nuclear Energy, Nuclear Science User Facilities (NSUF) project 15-8242.

Data and Resources

Download all

Datatype Name Last Modified
3927_Position 120_00000.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00001.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00002.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00003.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00004.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00005.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00006.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00007.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00008.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00009.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00010.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00011.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00012.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00013.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00014.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00015.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00016.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00017.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00018.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00019.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00020.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00021.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00022.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00023.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_00024.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_ReadMe.txt

February 10, 2026, 15:05 (UTC)
3927_Position 120_image.jpg

February 10, 2026, 15:05 (UTC)
3927_Position 121_00000.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00001.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00002.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00003.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00004.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00005.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00006.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00007.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00008.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00009.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00010.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00011.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00012.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00013.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00014.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00015.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00016.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00017.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00018.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00019.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00020.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00021.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00022.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00023.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_00024.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_ReadMe.txt

February 10, 2026, 15:05 (UTC)
3927_Position 121_image.jpg

February 10, 2026, 15:06 (UTC)

Additional Info

Field Value
Author Janelle Wharry, Caleb Clement, Yangyang Zhao, Katelyn Baird, David Frazer, Jatuporn Burns, Yu Lu, Yaqiao Wu, Collin Knight, Donna Guillen, David Gandy
Last Updated March 5, 2026, 16:04 (UTC)
Created February 10, 2026, 15:05 (UTC)
DOI Link https://doi.org/10.48806/3021746
Instrument
Statement of Credit