3885_Position 113_00003.txt
Dataset description:
This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in...
Source: G91-P_400C_3DPA_(ID-636)
Additional Information
| Field | Value |
|---|---|
| Data last updated | February 10, 2026 |
| Metadata last updated | February 10, 2026 |
| Created | February 10, 2026 |
| Format | TXT |
| License | Creative Commons Attribution |
| Datastore active | False |
| Has views | True |
| Id | 38515849-17d2-4606-9e08-4bd6c721e598 |
| Mimetype | text/plain |
| Package id | 1f101ecf-6071-4d0d-a71a-78650235b6e5 |
| Position | 3 |
| Size | 316.9 KiB |
| State | active |
| Tracking summary | {'total': 0, 'recent': 0} |
| Url type | upload |