G91-P_400C_3DPA_(ID-636)

This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in this archive include uniaxial tensile testing data, fractography of selected tensile bars, and nanoindentation. The irradiation campaign was designed to facilitate a direct comparison of PM-HIP to conventional casting or forging. Five common nuclear structural alloys were included in the campaign: 316L stainless steel, SA508 pressure vessel steel, Grade 91 ferritic steel, and Ni-base alloys 625 and 690. Irradiations were carried out in the Advanced Test Reactor (ATR) at Idaho National Laboratory (INL) to target doses of 1 and 3 displacements per atom (dpa) at target temperatures of 300ºC and 400ºC through the DOE Office of Nuclear Energy, Nuclear Science User Facilities (NSUF) project 15-8242.

Data and Resources

Download all

Datatype Name Last Modified
3885_Position 113_00000.txt

February 10, 2026, 15:04 (UTC)
3885_Position 113_00001.txt

February 10, 2026, 15:04 (UTC)
3885_Position 113_00002.txt

February 10, 2026, 15:04 (UTC)
3885_Position 113_00003.txt

February 10, 2026, 15:04 (UTC)
3885_Position 113_00004.txt

February 10, 2026, 15:04 (UTC)
3885_Position 113_00005.txt

February 10, 2026, 15:04 (UTC)
3885_Position 113_00006.txt

February 10, 2026, 15:04 (UTC)
3885_Position 113_00007.txt

February 10, 2026, 15:04 (UTC)
3885_Position 113_00008.txt

February 10, 2026, 15:04 (UTC)
3885_Position 113_00009.txt

February 10, 2026, 15:04 (UTC)
3885_Position 113_00010.txt

February 10, 2026, 15:04 (UTC)
3885_Position 113_00011.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00012.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00013.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00014.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00015.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00016.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00017.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00018.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00019.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00020.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00021.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00022.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00023.txt

February 10, 2026, 15:05 (UTC)
3885_Position 113_00024.txt

February 10, 2026, 15:05 (UTC)
3885_bulk_ReadMe.txt

February 10, 2026, 15:05 (UTC)

Additional Info

Field Value
Author Janelle Wharry, Caleb Clement, Yangyang Zhao, Katelyn Baird, David Frazer, Jatuporn Burns, Yu Lu, Yaqiao Wu, Collin Knight, Donna Guillen, David Gandy
Last Updated March 5, 2026, 16:05 (UTC)
Created February 10, 2026, 15:04 (UTC)
DOI Link https://doi.org/10.48806/3021758
Instrument
Statement of Credit