SA508-P_300C_1DPA_(ID-104)

This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in this archive include uniaxial tensile testing data, fractography of selected tensile bars, and nanoindentation. The irradiation campaign was designed to facilitate a direct comparison of PM-HIP to conventional casting or forging. Five common nuclear structural alloys were included in the campaign: 316L stainless steel, SA508 pressure vessel steel, Grade 91 ferritic steel, and Ni-base alloys 625 and 690. Irradiations were carried out in the Advanced Test Reactor (ATR) at Idaho National Laboratory (INL) to target doses of 1 and 3 displacements per atom (dpa) at target temperatures of 300ºC and 400ºC through the DOE Office of Nuclear Energy, Nuclear Science User Facilities (NSUF) project 15-8242.

Data and Resources

Download all

Datatype Name Last Modified
3461_bulk_ReadMe.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00000 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00001 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00002 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00003 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00004 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00005 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00006 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00007 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00008 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00009 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00010 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00011 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00012 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00013 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00014 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00015 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00016 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00017 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00018 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00019 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00020 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00021 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00022 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00023 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00024 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00025 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00026 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00027 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00028 LC.txt

February 10, 2026, 15:06 (UTC)
KGT3461_Position 6_00029 LC.txt

February 10, 2026, 15:06 (UTC)

Additional Info

Field Value
Author Janelle Wharry, Caleb Clement, Yangyang Zhao, Katelyn Baird, David Frazer, Jatuporn Burns, Yu Lu, Yaqiao Wu, Collin Knight, Donna Guillen, David Gandy
Last Updated March 5, 2026, 16:05 (UTC)
Created February 10, 2026, 15:06 (UTC)
DOI Link https://doi.org/10.48806/3021763
Instrument
Statement of Credit