NEUP CINR-17-12609: Development of Advanced High-Cr Ferritic/Martensitic Steels
Utilize steel microalloying technologies to remove free interstitial atoms from High-Cr Ferritic/Martensitic steels such as HT-9 that result in moderate temperature (300-400°C)...
read more