NSUF 21-4345: A first Investigation in Lanthanide-induced Grain Boundary Embrittlement in HT9 Cladding via In-situ Micro-tensile Testing
Fuel cladding chemical interaction (FCCI) between HT9 cladding and UZr based metallic fuel often leads to significant change of the composition and microstructure in the inner...