3999_Position 115_00014.txt
Dataset description:
This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in...
Source: 316-P_400C_3DPA_(ID-464)
Additional Information
| Field | Value |
|---|---|
| Data last updated | February 10, 2026 |
| Metadata last updated | February 10, 2026 |
| Created | February 10, 2026 |
| Format | TXT |
| License | Creative Commons Attribution |
| Datastore active | False |
| Has views | True |
| Id | 12ee1349-0092-4b9a-9b28-50e2ae00f6e3 |
| Mimetype | text/plain |
| Package id | e45e2677-72d8-45a8-9a3e-900e586be64d |
| Position | 14 |
| Size | 317.4 KiB |
| State | active |
| Url type | upload |