3999_Position 115_00019.txt
Dataset description:
This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in...
Source: 316-P_400C_3DPA_(ID-464)
Additional Information
| Field | Value |
|---|---|
| Data last updated | February 10, 2026 |
| Metadata last updated | February 10, 2026 |
| Created | February 10, 2026 |
| Format | TXT |
| License | Creative Commons Attribution |
| Datastore active | False |
| Has views | True |
| Id | 8accb4ae-8e7c-4e25-a3ee-3e73a6b9ee94 |
| Mimetype | text/plain |
| Package id | e45e2677-72d8-45a8-9a3e-900e586be64d |
| Position | 19 |
| Size | 316.9 KiB |
| State | active |
| Tracking summary | {'total': 0, 'recent': 0} |
| Url type | upload |