3999_Position 117_00000.txt
Dataset description:
This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in...
Source: 316-P_400C_3DPA_(ID-464)
Additional Information
| Field | Value |
|---|---|
| Data last updated | February 10, 2026 |
| Metadata last updated | February 10, 2026 |
| Created | February 10, 2026 |
| Format | TXT |
| License | Creative Commons Attribution |
| Datastore active | False |
| Has views | True |
| Id | f1c5ed31-5edb-447f-ba0d-9da1829310a6 |
| Mimetype | text/plain |
| Package id | e45e2677-72d8-45a8-9a3e-900e586be64d |
| Position | 25 |
| Size | 316.3 KiB |
| State | active |
| Url type | upload |