316-P_400C_3DPA_(ID-464)

This is the mechanical testing data archive from a neutron irradiation campaign of nuclear structural alloys fabricated by powder metallurgy with hot isostatic pressing (PM-HIP). Data in this archive include uniaxial tensile testing data, fractography of selected tensile bars, and nanoindentation. The irradiation campaign was designed to facilitate a direct comparison of PM-HIP to conventional casting or forging. Five common nuclear structural alloys were included in the campaign: 316L stainless steel, SA508 pressure vessel steel, Grade 91 ferritic steel, and Ni-base alloys 625 and 690. Irradiations were carried out in the Advanced Test Reactor (ATR) at Idaho National Laboratory (INL) to target doses of 1 and 3 displacements per atom (dpa) at target temperatures of 300ºC and 400ºC through the DOE Office of Nuclear Energy, Nuclear Science User Facilities (NSUF) project 15-8242.

Data and Resources

Download all

Datatype Name Last Modified
3999_Position 115_00000.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00001.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00002.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00003.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00004.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00005.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00006.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00007.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00008.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00009.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00010.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00011.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00012.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00013.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00014.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00015.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00016.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00017.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00018.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00019.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00020.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00021.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00022.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00023.txt

February 10, 2026, 15:05 (UTC)
3999_Position 115_00024.txt

February 10, 2026, 15:05 (UTC)
3999_Position 117_00000.txt

February 10, 2026, 15:05 (UTC)
3999_Position 117_00001.txt

February 10, 2026, 15:05 (UTC)
3999_Position 117_00002.txt

February 10, 2026, 15:05 (UTC)
3999_bulk_ReadMe.txt

February 10, 2026, 15:05 (UTC)

Additional Info

Field Value
Author Janelle Wharry, Caleb Clement, Yangyang Zhao, Katelyn Baird, David Frazer, Jatuporn Burns, Yu Lu, Yaqiao Wu, Collin Knight, Donna Guillen, David Gandy
Last Updated March 5, 2026, 16:04 (UTC)
Created February 10, 2026, 15:05 (UTC)
DOI Link https://doi.org/10.48806/3021744
Instrument
Statement of Credit